Microstructure and mechanical properties of bulk and plasma-sprayed y2O3-partially stabilized zirconia

Bulk 8.0 weight percent yttria partially stabilied zirconia (PSZ) was studied by light microscopy, transmission electron microscopy, X-ray analysis, microhardness testing, and fracture toughness testing. The as received PSZ contained spheroidal and grain boundary precipitates up to 4 micrometers in size. Spheroids up to 1.26 micrometers were metastable tetragonal; large spheroids were monoclinic. Grinding the PSZ into powder did not cause a significant amount of tetragonal to transform to monoclinic. This indicates that transformation toughness is not a significant mechanism in PSZ. Aging the PSZ at 1500 C caused the fine tetragonal precipitates to grow from 0.06 to 0.12 micrometers, in 250 minutes. A peak hardness of 1400 kg/sq mm was attained after 50 minutes. Solution annealing and quenching the as received PSZ eliminated the large precipitates, but fine tetragonal precipitates reformed on quenching. Aging at 1500 C caused the fine 0.02 micrometers tetragonal precipitates to grow into plates about 0.10 by 0.50 micrometers. A peak hardness of 1517 kg/sq mm was obtained after 250 minutes. On further aging, monoclinic percipitates formed along grain boundaries. The fracture toughness of the aged and unaged solution annealed and quenched PSZ was found to be between 2 and 3 MN /square root of m cubed. This range of fracture toughness is consistent with PSZ's that do not undergo transformation toughening.

Valentine, P. G.↗

Flexible machine-learning interatomic potential for simulating structural disordering behavior of Li 7 La 3 Zr 2 O 12 solid electrolytes

Batteries based on solid-state electrolytes, including Li 7 La 3 Zr 2 O 12 (LLZO), promise improved safety and increased energy density; however, atomic disorder at grain boundaries and phase boundaries can severely deteriorate their performance. Machine-learning (ML) interatomic potentials offer a uniquely compelling solution for simulating chemical processes, rare events, and phase transitions associated with these complex interfaces by mixing high scalability with quantum-level accuracy, provided that they can be trained to properly address atomic disorder. To this end, we report the construction and validation of an ML potential that is specifically designed to simulate crystalline, disordered, and amorphous LLZO systems across a wide range of conditions. The ML model is based on a neural network algorithm and is trained using ab initio data. Performance tests prove that the developed ML potential can predict accurate structural and vibrational characteristics, elastic properties, and Li diffusivity of LLZO comparable to ab initio simulations. As a demonstration of its applicability to larger systems, we show that the potential can correctly capture grain boundary effects on diffusivity, as well as the thermal transition behavior of LLZO. Here these examples show that the ML potential enables simulations of transitions between well-defined and disordered structures with quantum-level accuracy at speeds thousands of times faster than ab initio methods.

25 ENERGY STORAGE↗

Investigation of Microstructures and Tensile Properties of 316L Stainless Steel Fabricated via Laser Powder Bed Fusion

In this study, a thorough investigation of the microstructures and tensile properties of 316L stainless steel fabricated via laser powder bed fusion (L-PBF) was done. 316L stainless steel specimens with two different thicknesses of 1.5 mm and 4.0 mm fabricated under similar conditions were utilized. Microstructural characterization was performed using optical microscopy (OM) and scanning electron microscopy (SEM) equipped with electron backscatter diffraction (EBSD). Melt pools and cellular structures were observed using OM, whereas EBSD was utilized to obtain the grain size, grain boundary characteristics, and crystallographic texture. The 1.5 mm thick sample demonstrated a yield strength (YS) of 538.42 MPa, ultimate tensile strength (UTS) of 606.47 MPa, and elongation to failure of 69.88%, whereas the 4.0 mm thick sample had a YS of 551.21 MPa, UTS of 619.58 MPa, and elongation to failure of 73.66%. These results demonstrated a slight decrease in mechanical properties with decreasing thickness, with a 2.4% reduction in YS, 2.1% reduction in UTS, and 5.8% reduction in elongation to failure. In addition to other microstructural features, the cellular structures were observed to be the major contributors to the high mechanical properties. Using the inverse pole figure (IPF) maps, both thicknesses depicted a crystallographic texture of {001} <101> in their as-built state. However, when subjected to tensile loads, texture transitions to {111} <001> and {111} <011> were observed for the 1.5 mm and 4.0 mm samples, respectively. Additionally, EBSD analysis revealed the pre-existence of high-density dislocation networks and a high fraction of low-angle grain boundaries. Interestingly, twinning was observed, suggesting that the plastic deformation occurred through dislocation gliding and deformation twinning.

316L stainless steel↗

Evolution of Metastable Phases During Mg Metal Corrosion: An In Situ Cryogenic X-ray Photoelectron Spectroscopy Study

Magnesium and its alloys are potential structural materials candidates for a wide variety of applications due to their high strength-to-weight ratio. However, ductility and poor corrosion resistance under ambient environmental conditions are the bottleneck for industrial deployment. Designing passivation layers and/or corrosion resistant alloys requires fundamental understanding of the corrosion process. The traditional ex-situ spectroscopic measurements of polycrystalline metal surface with ubiquitous surface impurities and grain boundaries only provided an indistinct view of the corrosion process. To clearly distinguish the mechanism and sequence of corrosion process, we employed in-situ cryo-based x-ray photoelectron spectroscopy (XPS) measurements on Mg single crystal surface exposed to aqueous salt solution. Clean Mg (0001) surfaces were exposed to pure D2O and NaCl aqueous solution (5 wt% NaCl+95 wt% D2O). The interfacial reactions were studied using multimodal analysis including XPS, x-ray diffraction (XRD) and scanning electron microscopy (SEM). In contrast to previous studies, our experiments demonstrated the formation of magnesium chloride hydroxide hydrate during aqueous salt corrosion processes. Evidence of metastable ClO* radicals were also found during the initial aqueous salt solution exposure.

Shutthanandan, Vaithiyalingam↗

Understanding the microstructural stability in a y’-strengthened Ni-Fe-Cr-Al-Ti alloy

Ni-Fe-Cr-Al-Ti alloys, with Ni levels near 50 wt.%, have the potential to develop a microstructure consisting of a face-centered cubic ? matrix with the homogeneous precipitation of fine ordered ?’ precipitates similar to traditional Ni-based superalloys with significantly greater Ni content. Scanning electron microscopy (SEM), transmission electron microscopy (TEM), atom probe tomography (APT), and CALPHAD -based thermodynamic modeling were employed to understand the phase stabilities and microstructural evolution in an age-hardenable Ni-27Fe-18Cr-1Co-1.6Al-3.75Ti-1.2Mo-0.03C (wt%) alloy. The primary heat-treatment of solution annealing at 1121°C for 4h and age-hardening treatment at 760 °C for 16h resulted in a microstructure consisting of fine ?’ precipitates in an austenitic matrix along with grain boundary carbides, consistent with thermodynamic calculations. Long-term aging at 900 °C for 250h resulted in the coarsening of ?’ along with a change in the morphology of the precipitates from spherical to a more cuboidal shape. In addition, ? phase formation was observed concomitant with the partial dissolution of the ?’ phase. The ability of computational thermodynamic models to predict microstructural characteristics is discussed.

Gwalani, Bharat↗

Bulk Diffusion of Cl through O Vacancies in α-Cr 2 O 3 : A Density Functional Theory Study

Many metals form passive oxides which are broken or weakened by anionic-induced degradation leading to material failure and anionic diffusion is an important step of this degradation process. The diffusion of anionic species through oxides involves a combination of diffusion along grain boundaries, cracks, and channels, as well as bulk diffusion via point defects which is the focus of this study. Using density functional theory, we study bulk diffusion of Cl through O vacancies in α -Cr 2 O 3 as a model system for passive metal oxides. Little is known about Cl diffusion and bonding characteristics, so we benchmark our work through comparison to numerous studies on O diffusion in α -Cr 2 O 3 to analyze similarities and differences between the O and Cl diffusion in the passivation and degradation process of α -Cr 2 O 3 respectively. Unlike O diffusion, the lowest diffusion barrier for Cl is cross-plane diffusion between two (0001) planes through a vacant cation site but the much shorter in-plane diffusion path within the same coordination polyhedron has 35% higher barrier. This work provides the basis for considering the contributions of Cl bulk-diffusion in the overall diffusion kinetics of Cl through α -Cr 2 O 3 .

Oware Sarfo, Kofi↗

Development of Mechanistic Fission Gas Release and Swelling Models for UN Fuels in BISON

This report describes the work in NEAMS (Nuclear Energy Advanced Modeling and Simulation) to develop a mechanistic fission gas model for uranium nitride fuels in BISON. The existing Sifgrs (Simple integrated fission gas release and swelling) model tracks the average properties of two bubble populations in the bulk and at the grain boundaries. It was recognized that dislocations play a crucial role in the fission gas swelling of UN, and an irradiation-induced dislocation density model was needed, as well as a model describing how fission gas interacts with dislocations creating a third population of bubbles along dislocations. A mechanistic model that tracks dislocation bubbles was implemented in Sifgrs. This model was used to simulate fission gas swelling and release in UN. Lower-length-scale calculations and experimental observations from carbide fuel were leveraged to help populate the model with essential parameters. As a placeholder, an empirical function was formulated for the evolution of the dislocation network. Because of the difference in evolution of this network at different temperatures, the dislocation bubbles are able to capture behavior that the bulk intragranular bubbles cannot. It was found that the bulk bubbles dominate microscopic swelling at low temperatures, and the dislocation bubbles dominate at higher temperatures. Based on this model, the transition between the two bubble types is the main factor behind the breakaway swelling phenomenon in UN. In order to test the model, a couple of assessments were run. For the lower temperature JOYO pins, the model produces reasonable fission gas release and swelling values. For the higher temperature SP1 pin, the model dramatically underestimates the fission gas release. This issue is attributed to the gas being trapped inside dislocation bubbles, unable to escape to grain boundaries to cause fission gas release, and could be remedied by a mechanistic dislocation model that allows the dislocation density to decrease at very high temperatures. A preliminary mechanistic dislocation model was developed supported by first-principle calculations. These calculations provided valuable insight into how interstitial defects cluster in UN in the {110} orientation, and may eventually form dislocation loops, leading to the conclusion that dislocation loops may nucleate from these clusters. An estimate of the dislocation line energy in UN was obtained and will be improved in future work. The free-energy cluster dynamics code Centipede was used to track interstitial and vacancy absorption at dislocation loops and calculate their growth. In addition, improvements to Centipede were made including new convergence criteria for transient simulations and sink driving force updates.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Transmission electron microscopy characterization of the fuel-cladding chemical interactions in HT9 cladded U-10Zr fuel

Fuel cladding chemical interaction (FCCI) is a key phenomenon needs to be better understood to establish the design basis for U-10Zr metallic fuel performance. Characterizing the microstructure and chemical composition of FCCI at micron and sub-micron scale is critically important toward a more mechanistic understanding of FCCI phenomenon and its potential effects on cladding integrity and metallic fuel performance. This paper, by using transmission electron microscopy, investigated the FCCI region in HT9 cladded U-10Zr fuel irradiated to 5.7% FIMA burnup at a peak inner cladding temperature of 615 °C in Fast Flux Test Facility (FFTF). Four distinct layers are identified in the FCCI region. The migration of Fe into the fuel side leads to the formation of several U-Zr-Fe ternary phases, including ?-Fe0.5Zr0.32U0.18, e-Fe0.3Zr0.4U0.3, and ?-Fe0.06Zr0.23U0.71, mingled with UFe2, U6Fe, and U phase at various Fe penetration depth up to ~ 150 µm. On the cladding side, grain coarsening and significant lanthanides infiltration along grain boundaries are observed. Laves phase, (Fe,Cr)2(Mo,W), which typically does not exist in fresh HT9, is identified in a wide radial range in the cladding. The typical HT9 martensitic lath structure and pre-existing M23C6 precipitates disappear, partially or completely, depending on the radial distance from the fuel-cladding interface. Those microstructural and compositional changes could cause mechanical degradation in the HT9 cladding. The present characterization results will improve the understanding of FCCI phenomenon and facilitate the development of microstructure-informed FCCI modeling for metallic fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Oxidation and Associated Pore Structure Modification During Experimental Alteration of Granite

Weathering plays a crucial role in a number of environmental processes, and the microstructure and evolution of multi-scale pore space is a critically important factor in the weathering of geological formations. In igneous rocks the infiltration of meteoric water into initially relatively dry material can cause the rock to begin to disaggregate, increasing porosity and surface area, and allowing further disaggregation and weathering to occur. These processes, in turn, allow biota to colonize the rock, further enhancing the weathering rate. In some igneous rocks this may be driven by oxidation of primary minerals. One such mineral, biotite, has been repeatedly mentioned as a cause of cracking during oxidation. However, the scale-dependence of the processes by which this occurs are poorly understood. We cannot, therefore, accurately extrapolate laboratory reaction rates to the field in predictive numerical models. In order to better understand the effects of oxidation and test the hypothesis that fracture and disaggregation are initiated by swelling of oxidizing biotites, we reacted granite cores in a selenic acid-rich aqueous solution at 200°C for up to 438 days. Elevated temperatures and selenic acid were used to provide relatively fast reaction rates and highly oxidizing conditions in sealed reaction vessels. These experiments were analyzed using a combination of imaging, X-ray diffraction, Mössbauer spectroscopy, and small- and ultra-small angle neutron scattering to interrogate porosity and microfracture formation. The experimental results show little observable biotite swelling, but significant transport and growth of iron oxides and/or clays along grain boundaries throughout the sample. Significant increases in porosity were also observed at the sample rim, likely associated with feldspar alteration. Fractures and transport were observed throughout the core, suggesting that stresses due to crystallization pressures caused by the growing iron phases may be the initiating factors in granite weathering, possibly followed by biotite swelling after sufficient permeability is achieved.

Anovitz, Lawrence M.↗

Epsilon Metal: A Waste Form for Noble Metals from Used Nuclear Fuel

Epsilon metal (e-metal) is the metallic phase that forms as inclusions at the grain boundaries in the UO2 fuel during reactor operation. This metal is composed of Pd, Mo, Rh, Ru, and Tc. These metallic inclusions are insoluble in strong acid and remnants of these metallic inclusions have been found in the UO2 matrix that remains from the natural reactors in Gabon that were active 1.8 billion years ago, therefore e-metal should be an excellent waste form for the immobilization of the long-lived isotopes 107Pd (6.5 ? 106 a) and 99Tc (2.13 ? 105 a), with 99Tc being the isotope of interest for repository performance. Therefore, the chemical durability of this potential waste form is assessed in this study. Typically, corrosion rates for metallic materials are measured electrochemically because they are quick, inexpensive, and can reveal the mechanism by which a metal corrodes, at least initially. However, in a repository the waste form would be subjected to slowly flowing water without an applied electrical potential over long time periods. Therefore, the corrosion rates of e-metal specimens were measured with both electrochemical tests and the single-pass flow-through test (SPFT). Potentiodynamic and potentiostatic polarization results suggest that a thin passive film exists on the alloy surface, which seems to be responsible for its high corrosion resistance. Additionally, X-Ray photoelectron spectroscopic results suggest that Pd oxides are significantly enriched in the passive film Results from the SPFT show that the dissolution rates were weakly dependent on pH. Only Mo and Re were found in solution and were used for the calculation of the dissolution rates. In general, the electrochemically determined corrosion rates agree reasonably well with the initial dissolution rate measured with the SPFT test, but they are about one or two orders of magnitude higher than the steady state rates. The causes for this discrepancy are discussed.

epsilon-metal, nuclear waste form, corrosion, sing↗

Cluster Dynamics Simulations of Intra-Granular Fission Gas Bubble Size and Pressure Evolution in UO 2

Fission gases such as xenon (Xe) play a critical role in determining the behavior and response of nuclear fuel. Given that Xe has little solubility in UO 2 , it accumulates and forms bubbles, which significantly impact fuel performance. Intra- and inter-granular bubble nucleation and growth can lead to fuel swelling, and once bubbles interconnect at grain boundaries, fission gas can be released into the plenum. At low temperatures, limited uranium vacancy mobility can restrict swelling, therefore causing the bubbles to become highly pressurized. Consequently, this can induce micro-cracking, promote fission gas release (increasing the likelihood of cladding failure), and even lead to fuel pulverization under accident conditions such as a loss of coolant accident. As bubble evolution is strongly influenced by local temperature and fission rate, markedly different behavior occurs across the radial profile of the fuel pellet. Capturing the mechanisms that underpin bubble evolution is therefore important to predict these behaviors in the fuel. Previous models describing important mechanisms informed by lower length scale simulations have been developed under the NEAMS program. These can describe the evolution of a single bubble type (i.e., single value for radius and pressure) at each position in the pellet, for instance using the Centipede cluster dynamic code. However, in reality, a full distribution in bubble sizes and pressures exists within the microstructure at a given position in the pellet. To address this the cluster dynamics code Xolotl, which can predict Xe and vacancy phase space (i.e., bubble distributions) for intra-granular bubbles, has been used before. Prior work benchmarked the Xolotl code against the Centipede cluster dynamics code to ensure compatibility and to verify that mobile defect properties are adequately transferred between the two codes, along with some physics improvements. In this work, we go further by introducing a physics-based set of improvements that will allow us to accurately predict bubble size distributions and internal bubble pressures under representative UO 2 irradiation conditions. The improvements include (i) coupling bubble-defect reaction energies to a virial equation of state (EOS), (ii) including a bubble surface tension contribution, (iii) incorporating radiation-induced re-solution of Xe and vacancies, (iv) enabling pressure-driven dislocation loop punching through an effective emission of interstitial clusters informed by interstitial loop energetics, (v) accounting for radiation induced athermal diffusion of Xe, and (vi) implementing a Booth-type grain boundary sink representation for all mobile defects and defect clusters. After these modifications, we observe good agreement of Xolotl fission gas bubble size and concentration predictions with legacy experimental measurements. Additionally, it allows the distribution of Xe bubble pressures and radius to also be predicted and compared to data produced through the Advanced Fuels Campaign (AFC) program. Here, we have done this by running simulations under conditions similar to the AFC post-irradiation examination (PIE) samples irradiated at North Anna 2 light water reactor (LWR). Our results shows excellent agreement with these experimental measurements.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Solid Electrolyte Bimodal Grain Structures for Improved Cycling Performance

Here, the application of solid-state electrolytes in Li batteries is hampered by the occurrence of Li-dendrite-caused short circuits. To avoid cell failure, the electrolytes can only be stressed with rather low current densities, severely restricting their performance. As grain size and pore distributions significantly affect dendrite growth in ceramic electrolytes such as Li 7 La 3 Zr 2 O 12 and its variants; here, a “detour and buffer” strategy to bring the superiority of both coarse and fine grains into play, is proposed. To validate the mechanism, a coarse/fine bimodal grain microstructure is obtained by seeding unpulverized large particles in the green body. The rearrangement of coarse grains and fine pores is fine-tuned by changing the ratio of pulverized and unpulverized powders. The optimized bimodal microstructure, obtained when the two powders are equally mixed, allows, without extra interface decoration, cycling for over 2000 h as the current density is increased from 1.0 mA·cm -2 , and gradually, up to 2.0 mA·cm -2 . The “detour and buffer” effects are confirmed from postmortem analysis. The complex grain boundaries formed by fine grains discourage the direct infiltration of Li. Simultaneously, the coarse grains further increase the tortuosity of the Li path. This study sheds light on the microstructure optimization for the polycrystalline solid-state electrolytes.

25 ENERGY STORAGE↗

Response of 11 B enriched ZrB 2 ultra-high temperature ceramic to neutron irradiation at elevated temperatures

ZrB 2 , an ultra-high temperature ceramic (UHTC) is being considered for use in fusion reactor first-wall structures, yet its response to irradiation remains poorly understood. This study employed scanning/transmission electron microscopy (S/TEM), synchrotron X-ray diffraction (XRD), finite element calculations, and thermal property measurements to thoroughly investigate the neutron-irradiation effects on 11 B-enriched ZrB 2 . Neutron irradiations were conducted at 220 °C and 620 °C, with a neutron fluence of 2.2 × 10 25 neutron/m 2 (energy > 0.1 MeV), resulting in 3.9 dpa and 4200 appm He. The study revealed the unusual prevalence of prism loops and a > c anisotropic lattice swelling, likely linked to the low c/a ratio of ZrB 2 , leading to grain boundary microcracking. Reducing the grain sizes was effective in reducing intergranular cracking and macroscopic swelling. The observation of cavities in ZrB 2 irradiated at 620 °C, as opposed to 220 °C, prompts questions about the temperature at which vacancies in ZrB 2 become mobile, and the role of neutron absorption by 10 B in elevating irradiation temperatures. Isotopic enrichment in 11 B proves to be a viable strategy for mitigating helium production in transition-metal diborides, which is a critical consideration for nuclear applications. Irradiation-induced defects reduce the thermal diffusivity and conductivity of ZrB 2 by a factor of 4–9, which has important implications for its role as a plasma-facing material in fusion reactors that drive high heat fluxes through first-wall materials. Here, this comprehensive study lays the foundation for understanding ZrB 2 behavior under neutron irradiation and highlights important phenomena to consider for various material applications.

36 MATERIALS SCIENCE↗

Anisotropic physics-regularized interpretable machine learning of microstructure evolution

Anisotropic Physics-Regularized Interpretable Machine Learning Microstructure Evolution (APRIMME) is a general-purpose machine learning solution for grain growth simulations. In prior work, PRIMME employed a deep neural network to predict site-specific migration as a function of its neighboring sites to model normal, isotropic, grain growth behavior. This work aims to extend this method by incorporating grain boundary misorientation-based grain growth behavior. APRIMME is trained on anisotropic simulations created using the Monte Carlo-Potts (MCP) model. Furthermore, the results of this work are compared statistically using grain radius, number of sides per grain, mean neighborhood misorientations, and the standard deviation of triple junction dihedral angles, and are found to match in most cases. The exceptions are small and seem to be related to two causes: (1) the deterministic model of APRIMME is learning from the stochastic simulations of MCP, which seems to accentuate triple junction behaviors; and, (2) a bias against very small grains is made evident in a quicker decrease in grains than expected at the beginning of an APRIMME simulation. APRIMME is also evaluated for its general ability to capture anisotropic grain growth behavior by first investigating different test case initial conditions, including a circle grain, three grain, and hexagonal grain microstructures.

36 MATERIALS SCIENCE↗

Updimensioning strategy derived from synthetic equiaxed grain structures for approximating 3D grain size distributions from 2D visualizations with 1D parameters

We generated synthetic equiaxed grain structures using computer graphics software to explore the relationship between various grain size determination methods and true three-dimensional (3D) grain diameters. Mirroring grain measurement techniques, the synthetic 3D grain structures are imaged as 2D micrographs which are measured to yield 1D grain size parameters. Synthetic grain structures provide data at a mass scale and permit exploration of both polished and fractured surface micrographs, revealing one-to-one correspondence between exposed 2D grain cross-sections and individual 3D grains. Analysis of this correspondence yielded a procedure to approximate 3D equiaxed grain size and volume distributions based on the mode of the 2D fractograph grain size distribution. The 3D approximation procedure is shown to be less susceptible to different imaging conditions that affect small, undiscernible grains compared to the standard planimetric and linear intercept methods, which by design also tend to underestimate the 3D grain diameter. The procedure requires larger sample sizes to lower variance and a deeper analysis which could become more practical with machine learning (ML) models for grain boundary segmentation, which synthetic grain structures can help train. This work lays the foundation for analyzing other grain distributions such as columnar and composite grains in similar depth.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Microstructural Investigation of Precipitation Treated A709 Test Samples

This report presents the microstructural characterization using scanning transmission electron microscopy (STEM) of two creep-tested ESR1150-PT specimens, one short-term and one long-term. The results show that during creep testing, the microstructure of the A709 ESR1150-PT material continues to evolve as expected due to the synergistic effect of strain, temperature and time. Key features include dislocation forest and cell structures, precipitates on grain boundaries, precipitates randomly within grains, and precipitates associated with dislocations. In addition, the STEM study of one ESR1100-SA specimen that has been tested to rupture at a relatively low temperature (550°C) for a relatively long term (16226 h) is also presented. The results show that there is a high density of very fine nano precipitates form on dislocations.

36 MATERIALS SCIENCE↗

Elucidating the mechanical and thermal response of nanotwinned Ni alloys

Transformative advances in nanoscale materials synthesis, characterization and modeling are enabling the synthesis of materials with unprecedent properties and greater understanding of the nanoscale mechanisms that underpin these properties. Nanotwinned Cu alloys have received considerable attention due to their impressive balance of strength and ductility, but they have limited microstructural stability. Recent instantiation of nanotwins in sputter deposited Ni-Mo-W, and several commercial Ni-based superalloys, point to the potential development of a new class of high temperature materials with a very beneficial suite of mechanical and physical properties. The experimental study described in this report was undertaken to elucidate the nanoscale origins of the thermal and mechanical behavior of nanotwinned Ni alloys. Micropillar compression experiments have shown nanotwinned Ni 85 Mo 15-x W x alloys to possess unusually high strengths above 3.5GPa and enhanced microstructural stability. The strength of these nanotwinned alloys is determined by the abrupt formation of shear bands. This study focused on identifying the nanoscale trigger, or triggers, for shear banding in nanotwinned materials using in situ experiments and atomic-scale postmortem analysis. Contrasting and comparing the mechanical response and postmortem nanostructures of “Mo-rich” and “W-rich” nanotwinned specimens elucidated the importance of the lateral motion of easy glide defects that results in erasure of twins and local coarsening of the nanotwinned microstructure. This twin coarsening was then associated with very localized plasticity, strain softening, and shear band formation. The difference between alloys was further studied by considering the role of various material factors: stacking fault energy, coherent twin boundary spacing and flatness, grain size, and the interactions of solute atoms with twin and grain boundaries. The effect of alloy composition and sputtering power and temperature were also investigated and used to control twin spacing and geometry. Combined with atomic-scale simulations, these experiments insights should allow us to identify strategies for achieving concomitant ultrahigh strength and ductility in nanotwinned Ni alloys. In parallel but synergistic studies, our work was buoyed by collaborative state-of-the-art nanoscale orientation and strain mapping at the DOE National Center for Electron Microscopy (NCEM). For example, novel 4D-STEM techniques were used to acquire nanoscale strain maps. The extremely fine twin spacing limited our measurements of atomic-scale thermal expansion within twins, but recent results from NCEM suggest that it will soon be possible to conduct such measurements and to unravel the origins of the novel thermal expansion characteristics of nanotwinned Ni alloys.

36 MATERIALS SCIENCE↗

Mitigate Stress Corrosion Cracking (SCC) in High-strength Al Castings (CRADA 508)

Development of high strength, corrosion resistant, aluminum alloys is important to a number of industries, including automotive, aerospace, power, etc. Understanding how processing methods such as casting, chemistry, additives and recycle content affect an alloy’s microstructure and performance in real world environments is crucial to their implementation. One major concern is how the repeated exposure to saline solutions can be detrimental to the structural integrity of aluminum alloy components. This study was undertaken as a collaboration between Eck Industries and PNNL to investigate the stress corrosion cracking (SCC) and corrosion behavior of aluminum alloys. This work examines the SCC response of three different materials set. First is cast A206 Al alloy produced by three different casting techniques (i.e., permanent mold, and sand casting with and without chill) and with or without nano forming additives as potential grain refiners. The second materials set comprises Al alloy tubes extruded by PNNL’s ShAPE process and produced using raw material with three different ratios of twitch and pre-consumer Al 6061 scrap. Finally, the third materials set comprises two Al-Si-Mg-Fe alloys with controlled Si% and Fe% to mimic recycle grade Al alloys. The corrosion behavior of these materials was characterized using SCC testing and scanning electrochemical cell microscopy (SECCM) technique; mechanical behavior was characterized using tensile testing, and microstructure was characterized using optical and electron microscopy techniques. Of the A206 Al alloys, the samples with nano forming additives performed poorly compared to those without. The best SCC performance (i.e. least degradation in mechanical properties) was demonstrated by A206 alloy sand cast with chill while the permanent mold sample showed the worst SCC performance. The SECCM was performed on A206 alloy sand cast with chill to understand the effect of microstructure and determine the location-dependent corrosion properties on grain boundaries (GB) and inside grains (IG) on the sample. The corrosion potential and current measured on GB and IG at various points on the sample established that the GB locations are more cathodic and corrosive than the IG locations. Further work needs to be conducted to investigate the mechanisms behind the observed dependence of SCC on casting technique and nano forming additives. Among the ShAPE extruded tubes, SECCM data suggests the decreasing order of tendency to corrode as follows: 100% twitch > 75% twitch > 50% twitch. Finally, both variants of the Al-Si-Mg-Fe alloys showed a large volume fraction of Fe- and Si-containing intermetallics and additional work is needed to discern differences in their respective corrosion responses. In summary, correlating local electrochemical behavior (e.g. via SECCM) with micro/nanostructure, in conjunction with bulk mechanical behavior, can help identify the right fabrication method and alloy chemistry to minimize SCC issues in Al alloys.

36 MATERIALS SCIENCE↗