At least 91 records · Page 5

Resolving electrochemically triggered topological defect dynamics and structural degradation in layered oxides

Understanding topological defects-controlled structural degradation of layered oxides—a key cathode material for high-performance lithium-ion batteries—plays a critical role in developing next-generation cathode materials. Here, by constructing a nanobattery in an electron microscope enabling atomic-scale monitoring of electrochemcial reactions, we captured the electrochemically driven atomistic dynamics and evolution of dislocations—a most important topological defect in material. We deciphered how dislocations nucleate, move, and annihilate within layered cathodes at the atomic scale. Specifically, we found two types of dislocation configurations, i.e., single dislocations and dislocation dipoles. Both pure dislocation glide/climb and mixed motions were captured, and the dislocation glide and climb velocities were first experimentally measured. Moreover, dislocation activity-mediated structural degradation such as crack nucleation, phase transformation, and lattice reorientation was unraveled. Our work provides deep insights into the atomistic dynamics of electrochemically driven dislocation activities in layered oxides.

Wang, Chunyang (ORCID:0000000184613952)↗

In-Situ Strain Analysis of Potential Habitat Composites Exposed to a Simulated Long-Term Lunar Radiation Exposure

NASA is studying the effects of long-term space radiation on potential multifunctional composite materials for habitats to better determine their characteristics in the harsh space environment. Two composite materials were selected for the study and were placed in a test stand that simulated the stresses of a pressure vessel wall on the material. The samples in the test stand were exposed to radiation at either a fast dose rate or a slow dose rate, and their strain and temperature was recorded during the exposure. It was found that during a fast dose rate exposure the materials saw a decreased strain with time, or a shrinking of the materials. Given previous radiation studies of polymers, this is believed to be a result of crosslinking occurring in the matrix material. However, with a slow dose rate, the materials saw an increase in strain with time, or a stretching of the materials. This result is consistent with scission or degradation of the matrix occurring, possibly due to oxidative degradation.

Rojdev, Kristina↗

Influence of Transition Metal Ion Contaminants on the Performance of Amine-Based Solid Sorbents in Direct Air Capture

Amine-functionalized solid sorbents are a class of sorbent materials proposed for direct air capture (DAC) of CO 2 , yet their long-term performance is susceptible to degradation under realistic operating conditions. Many amines are not thermodynamically stable in air, and amine sorbents oxidize while in use during DAC temperature swing adsorption processes. In this study, we investigate the role of transition metal ion contaminants, specifically Cu 2+ , Fe 2+ , and Ni 2+ , on the oxidative degradation of poly(ethylenimine) (PEI)-impregnated SBA-15 sorbents. By introducing metal ions via different modes mimicking both synthesis-related impurities and impurities derived from environmental exposure, we systematically evaluate sorbent stability after exposure to dry air at an elevated temperature. Thermogravimetric CO 2 uptake measurements reveal that even trace levels of Cu and Fe (as low as ∼4 ppm) can lead to measurable sorbent deactivation after oxidative aging, despite negligible loss in the performance of the control samples. In situ infrared, UV–vis, and X-ray photoelectron spectroscopies indicate that these metals catalyze radical-driven oxidation pathways, altering the chemical structure of the sorbent and accelerating degradation. Our findings underscore the need to account for trace metal contamination during DAC sorbent synthesis and deployment and highlight the importance of environmental contamination pathways.

CO2 capture↗

Environmental effects on the tensile strength of chemically vapor deposited silicon carbide fibers

The room temperature and elevated temperature tensile strengths of commercially available chemically vapor-deposited (CVD) silicon carbide fibers were measured after 15 min heat treatment to 1600 C in various environments. These environments included oxygen, air, argon and nitrogen at one atmosphere and vacuum at 10/9 atmosphere. Two types of fibers were examined which differed in the SiC content of their carbon-rich coatings. Threshold temperature for fiber strength degradation was observed to be dependent on the as-received fiber-flaw structure, on the environment and on the coating. Fractographic analyses and flexural strength measurements indicate that tensile strength losses were caused by surface degradation. Oxidation of the surface coating is suggested as one possible degradation mechanism. The SiC fibers containing the higher percentage of SiC near the surface of the carbon-rich coating show better strength retention and higher elevated temperature strength.

Bhatt, R. T.↗

Detection of diffusion limited oxidation in thermally aged ethylene propylene rubber cable insulation material

The lifetime prediction of electrical cable insulation in nuclear power plants (NPPs) is primarily based on accelerated aging. Polymeric insulation exposed to accelerated aging at high temperatures may demonstrate diffusion limited oxidation (DLO) where oxygen within the material is consumed faster than can be supplied by diffusion from the surrounding air. This situation leads to equilibrium oxidation at the exposed surfaces and limited oxidation away from the surfaces. Therefore, DLO results in a heterogeneously aged material which can lead to underestimation of lifetime for in-service cable insulation. In this study, the presence of inhomogeneous aging caused by DLO was evaluated on cross-sectioned cable insulation specimens made of ethylene propylene rubber (EPR). The studies were performed on thermally aged specimens (165 °C, 1 day and 165 °C, 16 days) using local measurement techniques including nanoindentation, micro-Fourier transform infrared spectroscopy (FTIR), and scanning electron microscopy (SEM) - energy dispersive spectroscopy (EDS). All the results indicate some degree of heterogenous aging, with 165 °C, 16 days, aging demonstrating highest degree of oxidative degradation on the inside edges presumably caused due to copper catalyzed oxidation.

Pallaka, Madhusudhan Reddy↗

Thermal barrier coating life prediction model development

The objective of this program is to develop an integrated life prediction model accounting for all potential life-limiting Thermal Barrier Coating (TBC) degradation and failure modes including spallation resulting from cyclic thermal stress, oxidative degradation, hot corrosion, erosion, and foreign object damage (FOD). The mechanisms and relative importance of the various degradation and failure modes will be determined, and the methodology to predict predominant mode failure life in turbine airfoil application will be developed and verified. An empirically based correlative model relating coating life to parametrically expressed driving forces such as temperature and stress will be employed. The two-layer TBC system being investigated, designated PWA264, currently is in commercial aircraft revenue service. It consists of an inner low pressure chamber plasma-sprayed NiCoCrAlY metallic bond coat underlayer (4 to 6 mils) and an outer air plasma-sprayed 7 w/o Y2O3-ZrO2 (8 to 12 mils) ceramic top layer.

Demasi, J.↗

Thermal barrier coating life prediction model development

The objective is to develop an integrated life prediction model accounting for all potential life-limiting thermal barrier coating (TBC) degradation and failure modes, including spallation resulting from cyclic thermal stress, oxidation degradation, hot corrosion, erosion and foreign object damage.

Demasi, J. T.↗

Conversion and Extraction of Insoluble Organic Materials in Meteorites

We endeavor to develop and implement methods in our laboratory to convert and extract insoluble organic materials (IOM) from low car-bon bearing meteorites (such as ordinary chondrites) and Precambrian terrestrial rocks for the purpose of determining IOM structure and prebiotic chemistries preserved in these types of samples. The general scheme of converting and extracting IOM in samples is summarized in Figure 1. First, powdered samples are solvent extracted in a micro-Soxhlet apparatus multiple times using solvents ranging from non-polar to polar (hexane - non-polar, dichloromethane - non-polar to polar, methanol - polar protic, and acetonitrile - polar aprotic). Second, solid residue from solvent extractions is processed using strong acids, hydrochloric and hydrofluoric, to dissolve minerals and isolate IOM. Third, the isolated IOM is subjected to both thermal (pyrolysis) and chemical (oxidation) degradation to release compounds from the macromolecular material. Finally, products from oxidation and pyrolysis are analyzed by gas chromatography - mass spectrometry (GCMS). We are working toward an integrated method and analysis scheme that will allow us to determine prebiotic chemistries in ordinary chondrites and Precambrian terrestrial rocks. Powerful techniques that we are including are stepwise, flash, and gradual pyrolysis and ruthenium tetroxide oxidation. More details of the integrated scheme will be presented.

Locke, Darren R.↗

A comparison of fiber effects on polymer matrix composite oxidation

A number of thermo-oxidative stability studies addressing the effects of fiber reinforcement on composite thermal stability and influence of geometry on the results of aging studies were performed at NASA-Lewis. The information presented herein, a compilation of some results from these studies, shows the influence of the reinforcement fibers on the oxidative degradation of various PMR-15 composites. Reinforcement of graphite and ceramics were studied and three composite oxidation mechanisms were observed. One was a dominant attack of the reinforcement fiber, the second was the aggressive oxidation of the matrix material, and the third was interfacial degradation.

Bowles, Kenneth J.↗

Flammability screening tests of resins

Selected flammability characteristics of glass cloth laminates of thermosetting resins are evaluated. A protocol for the evaluation of the flammability hazards presented by glass cloth laminates of thermosetting resins and the usefulness of that protocol with two laminates are presented. The glass laminates of an epoxy resin, M-751 are evaluated for: (1) determination of smoke generation from the laminates; (2) analysis of products of oxidative degradation of the laminates; (3) determination of minimum oxygen necessary to maintain flaming oxidation; (4) evaluation of toxicological hazards.

Arhart, R. W.↗

Graphite Sheet Coating for Improved Thermal Oxidative Stability of Carbon Fiber Reinforced/PMR-15 Composites

Expanded graphite was compressed into graphite sheets and used as a coating for carbon fiber reinforced PMR-15 composites. BET analysis of the graphite indicated an increase in graphite pore size on compression, however the material was proven to be an effective barrier to oxygen when prepegged with PMR-15 resin. Oxygen permeability of the PMR-15/graphite was an order of magnitude lower than the compressed graphite sheet. By providing a barrier to oxygen permeation, the rate of oxidative degradation of PMR-15 was decreased. As a result, the composite thermo-oxidative stability increased by up to 25%. The addition of a graphite sheet as a top ply on the composites yielded little change in the material's flexural strength or interlaminar shear strength.

Campbell, Sandi↗

Oxidation of Copper Alloy Candidates for Rocket Engine Applications

The gateway to affordable and reliable space transportation in the near future remains long-lived rocket-based propulsion systems; and because of their high conductivities, copper alloys remain the best materials for lining rocket engines and dissipating their enormous thermal loads. However, Cu and its alloys are prone to oxidative degradation -- especially via the ratcheting phenomenon of blanching, which occurs in situations where the local ambient can oscillate between oxidation and reduction, as it does in a H2/02- fuelled rocket engine. Accordingly, resistance to blanching degradation is one of the key requirements for the next generation of reusable launch vehicle (RLV) liner materials. Candidate copper alloys have been studied with a view to comparing their oxidation behavior, and hence resistance to blanching, in ambients corresponding to conditions expected in rocket engine service. These candidate materials include GRCop-84 and GRCop-42 (Cu - Cr-8 - Nb-4 and Cu - Cr-4 - Nb-2 respectively); NARloy-Z (Cu-3%Ag-0.5%Y), and GlidCop (Cu-O.l5%Al2O3 ODS alloy); they represent different approaches to improving the mechanical properties of Cu without incurring a large drop in thermal conductivity. Pure Cu (OFHC-Cu) was included in the study to provide a baseline for comparison. The samples were exposed for 10 hours in the TGA to oxygen partial pressures ranging from 322 ppm to 1.0 atmosphere and at temperatures of up to 700 C, and examined by SEM-EDS and other techniques of metallography. This paper will summarize the results obtained.

Ogbuji, Linus U. Thomas↗

Auger electron spectroscopy study of oxidation of a PdCr alloy used for high-temperature sensors

A Pd-13 wt. percent Cr solid solution is a promising high-temperature strain gage alloy. In bulk form it has a number of properties that are desirable in a resistance strain gage material, such as a linear electrical resistance versus temperature curve to 1000 C and stable electrical resistance in air at 1000 C. However, unprotected fine wire gages fabricated from this alloy perform well only to 600 C. At higher temperatures severe oxidation degrades their electrical performance. In this work Auger electron spectroscopy was used to study the oxidation chemistry of the alloy wires and ribbons. Results indicate that the oxidation is caused by a complex mechanism that is not yet fully understood. As expected, during oxidation, a layer of chromium oxide is formed. This layer, however, forms beneath a layer of metallic palladium. The results of this study have increased the understanding of the oxidation mechanism of Pd-13 wt. percent Cr.

Boyd, Darwin L.↗

Radiation damage in high-voltage silicon solar cells

Three types of open circuit high voltage solar cells were tested to determine their performance after exposure to 1 MeV electron irradiations. The cells with a relatively deep n-type emitter were more susceptible to radiation damage than other high open circuit high voltage cells. The use of diffused or ion implanted junctions leads to open circuit high voltage cell designs that are less susceptible to radiation damage. These latter two types of cells show degradations that are typical of the 0.1 ohm-cm material from which they are fabricated. Furthermore, exposure to ionizing radiation causes oxide degradation and decreased cell performance in cells that depend on a charged oxide to achieve significant cell properties. Hence, the combination of a charged oxide and a relatively deep n-type emitter is not recommended for incorporation into a cell designed for use in the particulate radiation environment of space.

Weinberg, I.↗

Mitigation Methods for Piperazine Oxidation in Post-Combustion Carbon Capture

Piperazine is a promising second-generation solvent for amine scrubbing in post-combustion CO2 capture. However, the oxidative degradation of PZ can cause environmental problems and economic loss. This work presents the effects of two mitigation methods: carbon treating and N2 sparging, on the PZ oxidation in long-term operations. The species and their respective quantities adsorbed by the activated carbon were tested in a bench-scale device. The carbon was then tested in the High Temperature Oxidation Reactor (HTOR), where the solvent oxidizes at a reasonably fast rate. Pilot plant campaigns were also performed at the UT Austin SRP and the National Carbon Capture Center (NCCC) and the effects were verified. When dissolved Fe is removed by carbon treating or other methods, available soluble Fe in the system dissolves and replaces the dissolved Fe. Therefore, all available Fe and ligands need to be removed for the mitigation to be effective. The sources of soluble Fe include fly ash and the corrosion of stainless steel, and the ligands are degradation products. 8 All PZ degraded solvents have two absorbance peaks at 320 nm and 538 nm. The 320 nm peak is caused by dissolved metals, especially Fe, complexed by degradation products. The 320 nm peak is related to the amine degradation level and can be used as a simple and efficient method to estimate the amine degradation rate. The pilot plant data suggest that NO2 can oxidize PZ significantly, possibly through radical reactions. 0.01 mmol/kg-hr absorption of NO2 increased the PZ oxidation rate from 1.2 mmol/kg-hr to 2.5 mmol/kg-hr.

Yuying, Wu↗

Contact Sensor Attachment to Titanium Metal Composites

A Pd-13wt%Cr solid solution is a promising high-temperature strain gage alloy. In bulk form it has a number of properties that are desirable in a resistance strain gage material, such as a linear electrical-resistance-versus-temperature curve to 1000 C and stable electrical resistance in air at 1000 C. However, unprotected fine wire gages fabricated from this alloy perform well only to 600 C. At higher temperatures severe oxidation degrades their electrical performance. In this work Auger electron spectroscopy has been used to study the oxidation chemistry of the alloy wires and ribbons. Results indicate that the oxidation is caused by a complex mechanism that is not yet fully understood. As expected, during oxidation, a layer of chromium oxide is formed. This layer, however, forms beneath a layer of metallic palladium. The results of this study have increased the understanding of the oxidation mechanism of Pd-13wt%Cr.

Vargas-Aburto, Carlos↗

Irradiation Effect on Noble Metal Particles in Water Using in situ Liquid Cell STEM Observation

During geologic disposal of spent nuclear fuel (SNF) in an engineered nuclear waste repository, once all other barriers have degraded, oxidizing may occur at the solid-water interface owing to a self-generated radiolytic field. The repository design includes large quantities of iron (Fe), that is anticipated to corrode under an anoxic environment, and generate hydrogen (H 2 ) gas. This H 2 gas is thought to be able to suppress the dissolution of SNF through a catalytic reaction with noble metal particles (NMP) that are pre-existing in the SNF. This interaction leads to the decomposition of the major oxidant, hydrogen peroxide (H 2 O 2 ). In conclusion, these processes are described in the Fuel Matrix Degradation (FMD) model that is being used to predict SNF degradation rates. The NMP, therefore, plays an important role within the FMD model.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗