Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “mechanical adhesion”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Semi-2-interpenetrating polymer networks of high temperature systems

A semi-interpenetrating (semi-IPN) polymer system of the semi-2-IPN type is described in which a polymer of acetylene-terminated imidesulfone (ATPISO2) is cross linked in the presence of polyimidesulfone (PISO2). Six different formulations obtained by mixing of either ATPISO2-1n or ATPISO2-3n with PISO2 in three different proportions were characterized in terms of glass transition temperature, thermooxidative stability, inherent viscosity, and dynamic mechanical properties. Adhesive (lap shear) strength was tested at elevated temperatures on aged samples of adhesive scrim cloth prepared from each resin. Woven graphite (Celion 1000)/polyimide composites were tested for flexural strength, flexural modulus, and shear strength. The network polymers have properties intermediate between those of the component polymers alone, have greatly improved processability over either polyimide, and are able to form good adhesive bonds and composites, making the semi-2-IPN systems superior materials for aerospace structures.

Hanky, A. O.↗

Criterion for mixed mode fracture in composite bonded joints

A study was undertaken to characterize the debond growth mechanism of adhesively bonded composite joints under mode I, mixed mode I-II, and mode II static loadings. The bonded system consisted of graphite-epoxy composite adherends bonded with a toughened epoxy adhesive. The mode I, mode II and mixed mode I-II fracture energies of the tested adhesives were found to be equal to each other. The criterion for mixed mode fracture in composite bonded joints was found.

Mall, S.↗

Criterion for mixed mode fracture in composite bonded joints

A study was undertaken to characterize the debond growth mechanism of adhesively bonded composite joints under mode I, mixed mode I-II, and mode II static loadings. The bonded system consisted of graphite/epoxy (T300/5208) composite adherends bonded with a toughened epoxy (EC 3445) adhesive. The mode I, mode II and mixed-mode I-II fracture energies of the tested adhesive were found to be equal to each other. Furthermore, the criterion for mixed mode fracture in composite bonded joints was determined.

Mall, S.↗

Cryotank Skin/Stringer Bondline Analysis

The need for light weight structure for advanced launch systems have presented great challenges and led to the usage of composites materials in a variety of structural assemblies where joining of two or more components is imperative. Although joints can be mechanically bolted, adhesive bonding has always been a very desirable method for joining the composite components, particularly for the cryotank systems, to achieve maximum structural efficiency. This paper presents the analytical approach resulted from the conceptual development of the DC-Y composite cryotank, conducted under the NASA/Boeing NRA 8-12 Partnership, to support the continued progress of SSTO (Single-Stage-To-Orbit) concepts. One of the critical areas of design was identified as the bonded interface between the skin (tank wall) and stringer. The approach to analyze this critical area will be illustrated through the steps which were used to evaluate the structural integrity of the bondline. Detailed finite element models were developed and numerous coupon test data were also gathered as part of the approach. Future plan is to incorporate this approach as a building block in analyzing bondline for the cryotank systems of RLVs (Reusable Launch Vehicles).

Nguyen, Bao↗

JWST ISIM Distortion Analysis Challenge

Very tight distortion requirements are imposed on the JWST's ISM structure due to the sensitivity of the telescope's mirror segment and science instrument positioning. The ISIM structure is a three dimensional truss with asymmetric gusseting and metal fittings. One of the primary challenges for ISIM's analysis team is predicting the thermal distortion of the structure both from the bulk cooldown from ambient to cryo, and the smaller temperature changes within the cryogenic operating environment. As a first cut to estimate thermal distortions, a finite element model of bar elements was created. Elements representing joint areas and metal fittings use effective properties that match the behavior of the stack-up of the composite tube, gusset and adhesive under mechanical and thermal loads. These properties were derived by matching tip deflections of a solid model simplified T-joint. Because of the structure s asymmetric gusseting, this effective property model is a first attempt at predicting rotations that cannot be captured with a smeared CTE approach. In addition to the finite element analysis, several first order calculations have been performed to gauge the feasibility of the material design. Because of the stringent thermal distortion requirements at cryogenic temperatures, a composite tube material with near zero or negative CTE is required. A preliminary hand analysis of the contribution of the various components along the distortion path between FGS and the other instruments, neglecting second order effects were examined. A plot of bounding tube longitudinal and transverse CTEs for thermal stability requirements was generated to help determine the feasibility of meeting these requirements. This analysis is a work in progress en route to a large degree of freedom hi-fidelity FEA model for distortion analysis. Methods of model reduction, such as superelements, are currently being investigated.

Cifie, Emmanuel↗

Mitigation of Silver Ion Loss from Solution by Polymer Coating of Metal Surfaces, Part II

“Spacecraft potable water systems require a biocidal agent that effectively provides both immediate and residual disinfection over long periods of time. Ionic silver (Ag+) is a leading candidate for this application, but suffers from rapid concentration loss due to interactions with the metal storage containers and tubing. In order to maintain biocidal efficacy in systems with long periods of dormancy and to reduce the required rate of Ag+ injection, it is necessary to develop alternative materials and coatings for certified metal alloys that significantly reduce the Ag+loss.”1In this work, we continue our investigation of vapor-deposited parylene (AF4, and now C) polymers as conformal barrier coatings under long-term (ca. 1-year) immersion in ca. 400 ppb Ag+. The performanceof internal coatings in tubing/two-ferrule fitting systems is characterized. We report successful “aging” and high concentration Ag+pretreatment of parylene coatings for quantitative reduction of Ag+loss rates. In addition, we observe long-term blister-free adhesion of mechanically anchored parylene-AF4 on nano-structured Ti-6Al-4V alloy and chemically bonded parylene-C on 316L stainless steel. Finally, we report preliminary experiments with mechanical and chemical anchoring of laboratory-deposited parylene-C on 316L.

Silver↗

Development of Radioluminescent Tritium Polymeric Material for High Visibility Applications

The Development of Radioluminescent Tritium Polymeric Material for High Visibility Applications effort investigates the nature and properties of materials consisting of tritium lights combined with various silicone adhesives. Physical, mechanical, and optical properties will be observed/measured, including their durability in the low earth orbit environment. Tritium or hydrogen-three is a radioactive isotope of hydrogen that emits beta particles as it undergoes a process called beta decay. A beta particle is a high-energy, high-speed electron (or positron) emitted from radioactive decay of an atomic nucleus. Because it is a gas, tritium must be bound to a material or encapsulated in a sealed glass container. The gaseous tritium can then be combined with a phosphor source which when struck with beta particles, fluoresces and emits light. Such a light source is referred to as a gaseous tritium light source (GTLS). A self-powered, radioluminescent tritium material capable of surviving multiple space environments has the potential to fulfill visibility requirements levied on space flight hardware and facilitate additional long term internal and external lighting needs such as for imaging, docking, tracking, and xEMU suits for lunar exploration on the moon.

Lauren Fisher↗

A fundamental approach to adhesion: Synthesis, surface analysis, thermodynamics and mechanics

The effects of composites as adherends was studied. Several other variables were studied by fractography: aluminum powder adhesive filler, fiber glass cloth scrim or adhesive carrier, new adhesives PPQ-413 and LARC-13, and strength-test temperature. When the new results were juxtaposed with previous work, it appeared that complex interactions between adhesive, adherend, bonding, and testing conditions govern the observed strength and fracture-surface features. The design parameters likely to have a significant effect upon strength-test results are listed.

Dwight, D. W.↗

Fatigue behavior of adhesively bonded joints

The fatigue damage mechanism of composite to composite adhesively bonded joints was characterized. The mechanics of the possible modes of fatigue damage propagation in these joints when subjected to constant amplitude cyclic mechanical loading were investigated. The possible failure modes in composite bonded joints may be cyclic debonding (i.e., progressive separation of the adhesive), interlaminar damage (delamination), adherend fatigue or a combination of these. Two composite systems - graphite/epoxy adhesively bonded to graphite/epoxy and Kevlar 49/epoxy adhesively bonded to Kevlar 49/epoxy were investigated. Both composite systems consisted of quasi-isotropic lay-ups, i.e., 0 deg/-45 deg/+45 deg/90 degs. The two adhesives, employed in the study were (1) EC 3445 with cure temperature of 250 F for secondary bonding and (2) FM 300 with cure temperature of 350 F for co-cure bonding.

Mall, S.↗

Friction, wear, transfer and wear surface morphology of ultra-high-molecular-weight polyethylene

Tribological studies at 25 C in a 50-percent-relative-humidity air atmosphere were conducted using hemispherically tipped 440 C HT (high temperature) stainless steel pins sliding against ultra-high-molecular-weight polyethylene (UHMWPE) disks. The results indicate that sliding speed, sliding distance, contact stress and specimen geometry can markedly affect friction, UHMWPE wear, UHMWPE transfer and the type of wear mechanisms that occur. Adhesion appears to be the predominant wear mechanism; but after long sliding distances at slow speeds, heavy ridges of transfer result which can induce fatigue-like wear on the UHMWPE disk wear track. In one instance, abrasive wear to the metallic pin was observed. This was caused by a hard particle embedded in the UHMWPE disk wear track.

Fusaro, R. L.↗

Friction, wear, transfer, and wear surface morphology of ultrahigh-molecular-weight polyethylene

Tribological studies at 25 C in a 50-percent-relative-humidity air atmosphere were conducted using hemispherically tipped 440 C HT (high temperature) stainless steel pins sliding against ultra-high-molecular-weight polyethylene (UHMWPE) disks. The results indicate that sliding speed, sliding distance, contact stress and specimen geometry can markedly affect friction, UHMWPE wear, UHMWPE transfer and the type of wear mechanisms that occur. Adhesion appears to be the predominant wear mechanism; but after long sliding distances at slow speeds, heavy ridges of transfer result which can induce fatigue-like wear on the UHMWPE disk wear track. In one instance, abrasive wear to the metallic pin was observed. This was caused by a hard particle embedded in the UHMWPE disk wear track.

Fusaro, R. L.↗

Systems and Methods for Post-Treatment of Dry Adhesive Microstructures

Provided are systems and methods for the post-treatment of dry adhesive microstructures. The microstructures may be post-treated to comprise mushroom-like flaps at their tips to interface with the contact surface. In some aspects, a change in material composition of the microstructures in a dry adhesive may affect mechanical properties to enhance or diminish overall adhesive performance. For example, conductive additives can be added to the material to improve adhesive performance. In other aspects, microstructures comprising conductive material may allow for pre-load engagement sensing systems to be integrated into the microstructures.

Dadkhah Tehrani, Mohammad↗

A fundamental approach to adhesion: Synthesis, surface analysis, thermodynamics and mechanics

Adherend surfaces and fractography were studied using electron spectroscopy for chemical analysis and scanning electron microscopy/energy dispersive analysis of X-rays. In addition, Auger Electron Spectroscopy with depth profiling capability was used. It is shown that contamination of adhesion systems plays an important role not only in determining initial bond strengths but also in the durability of adhesive bonds. It is concluded that the analytical techniques used to characterize and monitor such contamination.

Chen, W.↗

An investigation into the role of adhesion in the erosion of ductile metals

Existing theories of erosion of ductile metals based on cutting and deformation mechanisms predict no material removal at normal incidence which is contradictory to experience. Thus, other mechanisms may be involved. The possible role of adhesive material transfer during erosion is investigated by both single particle impingement experiments and erosion by streams of particles. Examination of the rebounding particles as well as the eroded surface yields evidence of a significant adhesive mechanism for the ductile metals investigated.

Brainard, W. A.↗

An investigation into the role of adhesion in the erosion of ductile metals

Existing theories of erosion of ductile metals based on cutting and deformation mechanisms predict no material removal at normal incidence which is contradictory to experience. Thus, other mechanisms may be involved. The possible role of adhesive material transfer during erosion is investigated by both single-particle impingement experiments and erosion by streams of particles. Examination of the rebounding particles as well as the eroded surfaces yields evidence of a significant adhesive mechanism for the ductile metals investigated.

Brainard, W. A.↗

A fundamental approach to adhesion: Synthesis, surface analysis, thermodynamics and mechanics

Various surface preparations for titanium 6-4 alloy were studied. An anodizing method was investigated, and compared with the results of other chemical treatments, namely, phosphate/fluoride, Pasa-Jell and Turco. The relative durability of the different surface treatments was assessed by monitoring changes in surface chemistry and morphology occasioned by aging at 505 K (450 F). Basic electron spectroscopic data were collected for polyimide and polyphenylquinoxaline adhesives and synthetic precursors. Fractographic studies were completed for several combinations of adherend, adhesive, and testing conditions.

Chen, W.↗

Ultrasonic Evaluation of Thermal Degradation in Adhesive Bonds

The critical role played by adhesive bonds in lap joints is well known. A good knowledge of the mechanical properties of adhesive bonds in lap joints is a prerequisite to the design and reliable prediction of the performance of these bonded structures. Furthermore, the lap joint may be subject to high-temperature environments in service. Early detection of the degree of thermal degradation in adhesive bonds is required under these circumstances. A variety of ultrasonic nondestructive evaluation (NDE) techniques can be used to determine the thickness and the elastic moduli of adhesively bonded joints. In this paper we apply a previously developed technique based on the leaky Lamb wave (LLW) experiment to investigate the possibility of characterizing the thermal degradation of adhesive bonds in lap joints. The degradation of the adhesive bonds is determined through comparison between experimental data and theoretical calculations.

degradation lap joints mechanical properties bonde↗