Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “glass formulation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

DETERMINATION OF HLW GLASS MELT RATE USING X-RAY COMPUTED TOMOGRAPHY

The purpose of the high-level waste (HLW) glass melt rate study is two-fold: (1) to gain a better understanding of the impact of feed chemistry on melt rate through bench-scale testing, and (2) to develop a predictive tool for melt rate in support of the on-going frit development efforts for the Defense Waste Processing Facility (DWPF). In particular, the focus is on predicting relative melt rates, not the absolute melt rates, of various HLW glass formulations solely based on feed chemistry, i.e., the chemistry of both waste and glass-forming frit for DWPF. Critical to the successful melt rate modeling is the accurate determination of the melting rates of various HLW glass formulations. The baseline procedure being used at the Savannah River National Laboratory (SRNL) is to; (1) heat a 4 inch-diameter stainless steel beaker containing a mixture of dried sludge and frit in a furnace for a preset period of time, (2) section the cooled beaker along its diameter, and (3) measure the average glass height across the sectioned face using a ruler. As illustrated in Figure 1-1, the glass height is measured for each of the 16 horizontal segments up to the red lines where relatively large-sized bubbles begin to appear. The linear melt rate (LMR) is determined as the average of all 16 glass height readings divided by the time during which the sample was kept in the furnace. This 'visual' method has proved useful in identifying melting accelerants such as alkalis and sulfate and further ranking the relative melt rates of candidate frits for a given sludge batch. However, one of the inherent technical difficulties of this method is to determine the glass height in the presence of numerous gas bubbles of varying sizes, which is prevalent especially for the higher-waste-loading glasses. That is, how the red lines are drawn in Figure 1-1 can be subjective and, therefore, may influence the resulting melt rates significantly. For example, if the red lines are drawn too low, a significant amount of glassy material interspersed among the gas bubbles will be excluded, thus underestimating the melt rate. Likewise, if they are drawn too high, many large voids will be counted as glass, thus overestimating the melt rate. As will be shown later in this report, there is also no guarantee that a given distribution of glass and gas bubbles along a particular sectioned plane will always be representative of the entire sample volume. Poor reproducibility seen in some LMR data may be related to these difficulties of the visual method. In addition, further improvement of the existing melt rate model requires that the overall impact of feed chemistry on melt rate be reflected on measured data at a greater quantitative resolution on a more consistent basis than the visual method can provide. An alternate method being pursued is X-ray computed tomography (CT). It involves X-ray scanning of glass samples, performing CT on the 2-D X-ray images to build 3-D volumetric data, and adaptive segmentation analysis of CT results to not only identify but quantify the distinct regions within each sample based on material density and morphologies. The main advantage of this new method is that it can determine the relative local density of the material remaining in the beaker after the heat treatment regardless of its morphological conditions by selectively excluding all the voids greater than a given volumetric pixel (voxel) size, thus eliminating much of the subjectivity involved in the visual method. As a result, the melt rate data obtained from CT scan will give quantitative descriptions not only on the fully-melted glass, but partially-melted and unmelted feed materials. Therefore, the CT data are presumed to be more reflective of the actual melt rate trends in continuously-fed melters than the visual data. In order to test the applicability of X-ray CT scan to the HLW glass melt rate study, several new series of HLW simulant/frit mixtures were melted in the Melt Rate Furnace (MRF) and the contents of each cooled but un-sectioned beaker were CT scanned and analyzed. For comparison purposes, a cross-sectional X-ray image of each sample was used to estimate the melt rate using the visual method. In order to see the impact of feed chemistry on melt rate more clearly, a total of ten frit-only glasses (i.e., no waste) were also made, CT scanned and analyzed. In addition, two historical glass series which were previously sectioned were re-joined and CT scanned; the results were then compared to the visual data obtained earlier. All the work performed on these historical samples will be documented separately in another report. This report describes the methodologies used to interpret and apply the results of X-ray CT scans to the HLW melt rate study and further highlights some of the key results on the compositional dependence of melt rate and the cross-comparison of the visual and CT results.

36 MATERIALS SCIENCE↗

Evaluation of Impurity Extremes in a Plutonium-loaded Borosilicate Glass

A vitrification technology utilizing a lanthanide borosilicate (LaBS) glass appears to be a viable option for the disposition of excess weapons-usable plutonium that is not suitable for processing into mixed oxide (MOX) fuel. A significant effort to develop a glass formulation and vitrification process to immobilize plutonium was completed in the mid-1990's. The LaBS glass formulation was found to be capable of immobilizing in excess of 10 wt % Pu and to be tolerant of a range of impurities. To confirm the results of previous testing with surrogate Pu feeds containing impurities, four glass compositions were selected for fabrication with actual plutonium oxide and impurities. The four compositions represented extremes in impurity type and concentration. The homogeneity and durability of these four compositions were measured. The homogeneity of the glasses was evaluated using x-ray diffraction (XRD) and scanning electron microscopy coupled with energy dispersive spectroscopy (SEM/EDS). The XRD results indicated that the glasses were amorphous with no evidence of crystalline species in the glass. The SEM/EDS analyses did show the presence of some undissolved PuO{sub 2} material. The EDS spectra indicated that some of the PuO{sub 2} crystals also contained hafnium oxide. The SEM/EDS analyses showed that there were no heterogeneities in the glass due to the feed impurities. The durability of the glasses was measured using the Product Consistency Test (PCT). The PCT results indicated that the durability of Pu impurity glasses was comparable with Pu glasses without impurities and significantly more durable than the Environmental Assessment (EA) glass used as the benchmark for repository disposition of high-level waste (HLW) glasses. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

EVALUATION OF IMPURITY EXTREMES IN A PLUTONIUM-LOADED BOROSILICATE GLASS

A vitrification technology utilizing a lanthanide borosilicate (LaBS) glass appears to be a viable option for the disposition of excess weapons-useable plutonium that is not suitable for processing into mixed oxide (MOX) fuel. A significant effort to develop a glass formulation and vitrification process to immobilize plutonium was completed in the mid-1990s. The LaBS glass formulation was found to be capable of immobilizing in excess of 10 wt % Pu and to be tolerant of a range of impurities. To confirm the results of previous testing with surrogate Pu feeds containing impurities, four glass compositions were selected for fabrication with actual plutonium oxide and impurities. The four compositions represented extremes in impurity type and concentration. The homogeneity and durability of these four compositions were measured. The homogeneity of the glasses was evaluated using x-ray diffraction (XRD) and scanning electron microscopy coupled with energy dispersive spectroscopy (SEM/EDS). The XRD results indicated that the glasses were amorphous with no evidence of crystalline species in the glass. The SEM/EDS analyses did show the presence of some undissolved PuO{sub 2} material. The EDS spectra indicated that some of the PuO{sub 2} crystals also contained hafnium oxide. The SEM/EDS analyses showed that there were no heterogeneities in the glass due to the feed impurities. The durability of the glasses was measured using the Product Consistency Test (PCT). The PCT results indicated that the durability of Pu impurity glasses was comparable with Pu glasses without impurities and significantly more durable than the Environmental Assessment (EA) glass used as the benchmark for repository disposition of high-level waste (HLW) glasses.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Direct Feed Options for Hanford High Level Waste Vitrification - 17318

In the high level waste (HLW) direct feed (DF) option that is under consideration for early operations of the Hanford Tank Waste Treatment and Immobilization Plant (WTP), the pretreatment facility would be bypassed in order to support an earlier start-up of the HLW vitrification facility. For HLW, this would mean that the ultrafiltration and caustic leaching operations that would otherwise have been performed in the pretreatment facility would either not be performed or would be replaced by an interim pretreatment function (in-tank washing and settling, for example). These changes could result in higher aluminum contents, higher chromium contents, a higher fraction of supernate in the HLW feed, and lower solids contents. This would likely affect glass formulations and waste loadings and have impacts on the downstream vitrification operations. In the present work, new high waste loading glass formulations have been developed and characterized for the DF HLW option. A series of scaled melter tests was then conducted to assess the impacts of increased supernate content resulting from less effective washing on wastes from candidate source tanks for the direct feed option. The melter tests were conducted at solids contents extending below the current WTP baseline, which are likely for the direct feed option. The effects on glass production rate, melter operations, and off-gas carryover were determined, as was the ability of increased bubbling to compensate for the increased evaporative load. A series of waste compositions were investigated that span the range of in-tank washing efficiencies between the baseline WTP full-wash case and the no-wash case. The tests included wastes from tank AY-102 as well as high plutonium wastes from tank A-104. The results from this work provide the initial basis for assessments of the relative merits of progressively more intensive pretreatment in HLW direct feed options versus the practical benefits of minimal pretreatment. Together, these results illustrate that the optimum washing strategy will depend on the specific tank waste composition and will need to be evaluated on a tank-by-tank basis. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Optimization of LAW Glass Former Additives

The primary objective of this work was to collect data to support processing Hanford LAW streams at higher rates through changes in mineralogy, forms, and grain sizes of the GFCs. This was achieved through assessment of LAW feeds with different GFCs by feed rheology testing, testing with a vertical gradient furnace (VGF) system to assess melt rates, and processing selected modified LAW feeds through a DM100 melter to measure glass production rates and processing behavior. A high waste loading glass formulation developed in earlier work [8] for an LAW composition specified by WTP was used for rheology, VGF, and melter testing. The glass composition, ORPLA20, is based on LAW tank AN-105; the glass has a waste loading of 31.4 wt% and a Na2O content of 24.0 wt%. Another high waste loading glass formulation developed in earlier work for an LAW composition specified by WTP was also used for VGF testing to investigate the effects of changes in GFCs on melt rate for a second waste and glass composition. That glass composition is ORPLD6, which is based on LAW tank AN-102; the glass has a waste loading of 25.9 wt% and a Na2O content of 22.0 wt%.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Improved Alumina Loading in High-Level Waste Glasses

Recent tank retrieval and blending strategies at both the Savannah River Site (SRS) and Hanford have identified increased amounts of high-Al2O3 waste streams that are scheduled to be processed through their respective high-level waste (HLW) vitrification facilities. It is well known that the addition of small amounts of Al2O3 to borosilicate glasses generally enhances the durability of the waste glasses. However, at higher Al2O3 concentrations nepheline (NaAlSiO4) formation can result in a severe deterioration of the chemical durability of the slowly cooled glass near the center of the canister. Additionally, higher concentrations of Al2O3 generally increase the liquidus temperature of the melt and decrease the processing rate and thus result in a decreased waste loading in glass. Because of these effects, the maximum concentrations of Al2O3 in glasses have been restricted to the range of 17 wt% or lower. Pacific Northwest National Laboratory (PNNL), Savannah River National Laboratory (SRNL), and Khlopin Radium Institute (KRI) are jointly performing laboratory and scaled melter tests, through US Department of Energy, EM-21 Office of Waste Processing program, to develop glass formulations with increased Al2O3 concentrations. These glasses are formulated for specific DOE waste compositions at Hanford and SRS. The objectives are to avoid nepheline formation while maintaining or meeting waste loading and/or waste throughput expectations as well as satisfying critical process and product performance related constraints. This paper reports the results of recent tests of simulated Hanford HLW glasses containing up to 26 wt% Al2O3 in glass.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Liquidus temperature in the spinel primary phase field: A comparison between optical and crystal fraction methods

Liquidus temperature (TL) was measured for simulated high-level waste borosilicate glasses covering a Hanford composition region, using an optical method and a crystal-fraction extrapolation method with X-ray diffraction data from isothermal heat treatments. The 38 glasses encompassed a one-component-at-a-time variation of a 16-component matrix. The TL values ranged from 1006°C to 1603°C. First-order polynomial models were fitted to data to obtain coefficients in terms of the effect of 1 mass% component addition on the TL: TL-increasing oxides Cr2O3 (264°C), “Others” (minor components, 163°C), oxides of noble metals (137°C), NiO (91°C), Al2O3 and Fe2O3 (~19–21°C); TL-decreasing oxides K2O (-26°C), Na2O (-41°C), and Li2O (-68°C); oxides of little effect MnO, P2O5, ZrO2, F, Bi2O3, SiO2, B2O3, and CaO (9 to -12°C). Also presented are temperatures (T1%) at which glasses contain 1 vol% of spinel as these values are considered relevant to the Hanford Tank Waste Treatment and Immobilization Plant. The measured and estimated values are compared and contrasted and the effect of TL and T1% on glass formulation is discussed.

crystal fraction↗

Towards increased waste loading in high level waste glasses: Developing a better understanding of crystallization behavior

A number of waste components in US defense high level radioactive wastes (HLW) have proven challenging for current Joule heated ceramic melter (JCHM) operations and have limited the ability to increase waste loadings beyond already realized levels. Many of these ''troublesome'' waste species cause crystallization in the glass melt that can negatively impact product quality or have a deleterious effect on melter processing. Thus, recent efforts at US Department of Energy laboratories have focused on understanding crystallization behavior within HLW glass melts and investigating approaches to mitigate the impacts of crystallization so that increases in waste loading can be realized. Advanced glass formulations have been developed to highlight the unique benefits of next-generation melter technologies such as the Cold Crucible Induction Melter (CCIM). Crystal-tolerant HLW glasses have been investigated to allow sparingly soluble components such as chromium to crystallize in the melter but pass out of the melter before accumulating. The Hanford site AZ-101 tank waste composition represents a waste group that is waste loading limited primarily due to high concentrations of Fe 2 O 3 (with higher Al 2 O 3 ). Systematic glass formulation development utilizing slightly higher process temperatures and higher tolerance to spinel crystals demonstrated that an increase in waste loading of more than 20% could be achieved for this waste composition, and by extension higher loadings for wastes in the same group.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Advanced Waste Form and Melter Development for Treatment of Troublesome High-level Wastes

A number of waste components in US defense high level radioactive wastes (HLW) have proven challenging for current Joule heated ceramic melter (JHCM) operations and have limited the ability to increase waste loadings beyond already realized levels. Many of these “troublesome" waste species cause crystallization in the glass melt that can negatively impact product quality or have a deleterious effect on melter processing. Recent efforts at US Department of Energy laboratories have focused on understanding crystallization behavior within HLW glass melts and investigating approaches to mitigate the impacts of crystallization so that increases in waste loading can be realized. Advanced glass formulations have been developed to highlight the unique benefits of next-generation melter technologies such as the Cold Crucible Induction Melter (CCIM). Crystal-tolerant HLW glasses have been investigated to allow sparingly soluble components such as chromium to crystallize in the melter but pass out of the melter before accumulating. The Hanford site AZ-101 tank waste composition represents a waste group that is waste loading limited primarily due to high concentrations of Fe 2 O 3 (with higher Al 2 O 3 ). Systematic glass formulation development utilizing slightly higher process temperatures and higher tolerance to spinel crystals demonstrated that an increase in waste loading of more than 20% could be achieved for this waste composition, and by extension higher loadings for wastes in the same group.

Marra, James↗

Physical and Flow Properties of Glass-Forming Chemicals (V 2 O 5 , SnO, SnO 2 , Cr 2 O 3 , FeCr 2 O 4 , and ZrSiO 4 ) and Mixtures

For an efficient nuclear waste vitrification process at the Waste Treatment and Immobilization Plant (WTP) on the Hanford Site, proper selection and consistent supply of glass-forming chemicals (GFCs) are crucial. Thorough characterization of the GFCs is required to reduce risks in operation of the vitrification facility. Low-activity waste (LAW) will be blended with GFCs to form slurry feeds and then fed to melters and vitrified. To enhance properties of waste glasses, new chemicals are being introduced to the current GFC mixture. In this study, three new GFCs were evaluated for enhanced LAW glass formulations: chromium oxide (Cr 2 O 3 ), vanadium oxide (V 2 O 5 ), and stannic oxide (SnO 2 ). These three oxide components are included in enhanced waste glass formulations, and GFCs with the appropriate physical and flow properties are needed. As a starting point, single metal oxide GFCs, Cr 2 O 3 , V 2 O 5 , and SnO 2 , were sourced and tested. Then, alternative sources of Sn and Cr (SnO and FeCr 2 O 4 ) were tested along with an alternative zircon source (ZrSiO 4 ). This report documents the work performed to collect physical and flow property data on these new GFCs and melter feed slurries generated using these GFCs and simulated low-activity wastes.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of Form of Chromium on Spinel Formation

A number of Hanford high level waste (HLW) streams contain sufficiently high concentrations of chromium for it to become the waste loading limiting component in the waste. Chromium has relatively low solubility in borosilicate glasses and leads to the formation of various crystal phases including spinels. The extent of crystal formation must be managed during melter processing to prevent operational issues and potential premature melter failure that can result from excessive accumulation of crystals in the melter. In previous work for the Department of Energy (DOE) Office of River Protection (ORP), high-waste loading glass formulations were developed for representative HLW streams that are high in chromium. Results from those studies suggested that there may be differences in the crystallization behavior between glasses prepared in crucible melts and those prepared in DuraMelter 100 (DM100) joule heated melter runs. Understanding the cause of those differences has the potential to lead to the development of methods to further increase waste loadings for high chromium HLW streams through control of the formation of chromium-bearing crystals. As noted previously, the potential causes include differences in the form of components in the batch, including the form of chromium, as well as redox effects. This report describes the results from work to elucidate the origins of the observed differences and to identify melter feed composition modifications to control the formation of chromium-bearing crystal phases. The work focused on determining the effects of the form of chromium and the concentrations of oxidants in feed batches on spinel crystallization. Also evaluated was the use of potential melter feed additives to influence the redox state of chromium in the melt and its effect on spinel crystallization. As described in the Test Plan for this work, the objectives were accomplished through a combination of crucible-scale tests, small-scale tests with additives to influence redox state, and melter tests. This work builds on previous work performed at the Vitreous State Laboratory (VSL) of The Catholic University of America (CUA) for ORP to increase the waste loadings and processing rates of HLW glass formulations.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Enhanced LAW Glass Correlation - Phase 1

About 50 million gallons of high-level mixed waste is currently stored in underground tanks at the United States Department of Energy’s (DOE’s) Hanford site in the State of Washington. The Hanford Tank Waste Treatment and Immobilization Plant (WTP) will provide DOE’s Office of River Protection (ORP) with a means of treating this waste by vitrification for subsequent disposal. The tank waste will be separated into low- and high-activity waste fractions, which will then be vitrified respectively into Immobilized Low Activity Waste (ILAW) and Immobilized High Level Waste (IHLW) products. The ILAW product will be disposed in an engineered facility on the Hanford site while the IHLW product is designed for acceptance into a national deep geological disposal facility for high-level nuclear waste. The ILAW and IHLW products must meet a variety of requirements with respect to protection of the environment before they can be accepted for disposal. Acceptable glass formulations for vitrification of Hanford low activity waste (LAW) must meet a variety of product quality, processability, and waste loading requirements. To this end, The Vitreous State Laboratory (VSL) at The Catholic University of America (CUA) developed and tested a number of glass formulations during Part A, Part B1 and Part B2 of the WTP development program. The testing resulted in the selection of target glass compositions for the processing of eight of the Phase I LAW tanks. The selected glass compositions were tested at the crucible scale to confirm their compliance with ILAW performance requirements. Duramelter 100 (DM100) and LAW Pilot Melter tests were then conducted to demonstrate the viability of these glass compositions for LAW vitrification at high processing rates.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Low Activity Waste Glass Optimization with Property Models from Machine Learning, Part 2: Experimental Validation and Active Learning

The United States Department of Energy is responsible for managing legacy nuclear waste stored in underground tanks at the Hanford Site. To treat the waste, it is planned as the current baseline to separately vitrify low-activity waste (LAW) and high-level waste fractions. Previously, machine learning (ML) based glass property models (e.g., chemical durability, viscosity, electrical conductivity and SO3 solubility) were developed with prediction uncertainties. A waste glass optimization approach was then established to enable the capability of using these ML models in LAW glass formulation. In this study, the previous ML models were first experimentally validated, and the results were incorporated back into the database to update the ML models. The updated models and formulations showed increased waste loading while reducing the failure rate, demonstrating improved predictive accuracy, reduced uncertainties, and the effectiveness of active learning in guiding high-dimensional, nonlinear LAW glass design. This represents the first experimental validation of ML based LAW glass formulation, with practical benefits such as higher waste loading, shorter mission duration, and lower operational risk.

Lu, Xiaonan (ORCID:0000000179708148)↗

Support for DF LAW Flowsheet Development Report [Final Report]

The primary objectives of this work were to develop a glass formulation for the direct feed LAW from Tank AP-105, collect data on primary off-gas system effluents to support the evaluation of potential direct feed LAW flowsheets, and determine the effect of the dilute direct feed LAW stream on processing rates and partitioning of waste components to the exhaust system. Development of a suitable glass formulation for the LAW Tank AP-105 composition made use of information from the ORP Enhanced LAW Glass Correlation that is currently under development. Subsequently, melter feeds at low solids contents indicative of direct feed LAW waste streams were processed on the DM100 to determine glass production rates and bubbling rates required to process the high water content feed. Liquid effluent solutions generated from prototypical primary off-gas system components (SBS and WESP) were collected while processing the LAW Tank AP-105 composition at nominal conditions through the DM10. These solutions were analyzed to determine their steady state compositions and the effects of feed composition and feed water content at nominal processing conditions.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Vitrification Tests with Potential Technetium Capture Streams

About 50 million gallons of high-level waste is currently stored in underground tanks at The United States Department of Energy’s (DOE’s) Hanford site in the State of Washington. The Hanford Tank Waste Treatment and Immobilization Plant (WTP) will provide DOE’s Office of River Protection (ORP) with a means of treating this waste by vitrification for subsequent disposal. The tank waste will be separated into low- and high-activity waste fractions, which will then be vitrified respectively into Immobilized Low Activity Waste (ILAW) and Immobilized High Level Waste (IHLW) products. The ILAW product will be disposed in an engineered facility on the Hanford site while the IHLW product is designed for acceptance at a national deep geological disposal facility for high-level nuclear waste. The ILAW and IHLW products must meet a variety of requirements with respect to protection of the environment before they can be accepted for disposal. The Low Activity Waste (LAW) and High-Level Waste (HLW) at Hanford will be vitrified in Joule Heated Ceramic Melters (JHCMs) to produce stable products for disposal. Technetium is an important radioactive component in the Hanford tank waste and is typically one of the principal contributors to risk in performance assessments for the ILAW disposal facility. Technetium is also one of the more volatile radionuclides and the retention of technetium in the glass under the high temperature conditions prevailing during vitrification can vary over a relatively wide range depending on the feed composition, feed chemistry, and melter operating parameters. In support of the WTP Project, the Vitreous State Laboratory (VSL) at The Catholic University of America (CUA) and EnergySolutions have developed and tested glass formulations for WTP waste envelopes to provide data to meet the WTP contract requirements and to support system design activities. That work is based upon small-scale batch melts (“crucible melts”) using waste simulants. Glass compositions suitable for processing the tank waste streams for the WTP have been identified and tested for processing and product quality requirements at various scales, ranging from crucible melts of a few grams, up to the LAW Pilot Melter at processing rates in excess of 6600 kg/day (2000 kg/m 2 /day). Recent testing performed at VSL for Washington River Protection Solutions, LLC (WRPS) has investigated the baseline “single-pass” retention of technetium over the range of WTP LAW feed compositions and glass formulations as well as the development of potential modifications to the baseline that could increase the single-pass retention. For the WTP melter systems, the liquid waste streams from the primary off-gas system components are recycled back to the pretreatment facility and, ultimately, to subsequent melter feed batches. Such a recycle loop can greatly increase the overall retention of volatile constituents in the glass product over the single-pass value. Accordingly, more recent testing at VSL has been conducted on a melter system that incorporates a recycle flow sheet. The results from that work have provided important performance data for the unit operations in the primary off-gas system with respect to technetium capture and recycle, which is crucial in assessing the amount of technetium that ultimately reports to non-glass waste forms.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The Impact Of The MCU Life Extension Solvent On Sludge Batch 8 Projected Operating Windows

As a part of the Actinide Removal Process (ARP)/Modular Caustic Side Solvent Extraction Unit (MCU) Life Extension Project, a next generation solvent (NGS) and a new strip acid will be deployed. The strip acid will be changed from dilute nitric acid to dilute boric acid (0.01 M). Because of these changes, experimental testing or evaluations with the next generation solvent are required to determine the impact of these changes (if any) to Chemical Process Cell (CPC) activities, glass formulation strategies, and melter operations at the Defense Waste Processing Facility (DWPF). The introduction of the dilute (0.01 M) boric acid stream into the DWPF flowsheet has a potential impact on glass formulation and frit development efforts since B 2 O 3 is a major oxide in frits developed for DWPF. Prior knowledge of this stream can be accounted for during frit development efforts but that was not the case for Sludge Batch 8 (SB8). Frit 803 has already been recommended and procured for SB8 processing; altering the frit to account for the incoming boron from the strip effluent (SE) is not an option for SB8. Therefore, the operational robustness of Frit 803 to the introduction of SE including its compositional tolerances (i.e., up to 0.0125M boric acid) is of interest and was the focus of this study. The primary question to be addressed in the current study was: What is the impact (if any) on the projected operating windows for the Frit 803 - SB8 flowsheet to additions of B 2 O 3 from the SE in the Sludge Receipt and Adjustment Tank (SRAT)? More specifically, will Frit 803 be robust to the potential compositional changes occurring in the SRAT due to sludge variation, varying additions of ARP and/or the introduction of SE by providing access to waste loadings (WLs) of interest to DWPF? The Measurement Acceptability Region (MAR) results indicate there is very little, if any, impact on the projected operating windows for the Frit 803 - SB8 system regardless of the presence or absence of ARP and SE (up to 2 wt% B 2 O 3 contained in the SRAT and up to 2000 gallons of ARP). It should be noted that 0.95 wt% B 2 O 3 is the nominal projected concentration in the SRAT based on a 0.0125M boric acid flowsheet with 70,000 liters of SE being added to the SRAT.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The Impact Of The MCU Life Extension Solvent On Sludge Batch 8 Projected Operating Windows

As a part of the Actinide Removal Process (ARP)/Modular Caustic Side Solvent Extraction Unit (MCU) Life Extension Project, a next generation solvent (NGS) and a new strip acid will be deployed. The strip acid will be changed from dilute nitric acid to dilute boric acid (0.01 M). Because of these changes, experimental testing or evaluations with the next generation solvent are required to determine the impact of these changes (if any) to Chemical Process Cell (CPC) activities, glass formulation strategies, and melter operations at the Defense Waste Processing Facility (DWPF). The introduction of the dilute (0.01M) boric acid stream into the DWPF flowsheet has a potential impact on glass formulation and frit development efforts since B2O3 is a major oxide in frits developed for DWPF.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Development Of High Waste-Loading HLW Glasses For High Bismuth Phosphate Wastes

This report presents results from tests with new glass formulations that have been developed for several high Bi-P HLW compositions that are expected to be processed at the WTP that have not been tested previously. WTP HLW feed compositions were reviewed to select waste batches that are high in Bi-P and that are reasonably distinct from the Bi-limited waste that has been tested previously. Three such high Bi-P HLW compositions were selected for this work. The focus of the present work was to determine whether the same type of issues as seen in previous work with high-Bi HLW will be seen in HLW with different concentrations of Bi, P and Cr and also whether similar glass formulation development approaches would be successful in mitigating these issues. New glass compositions were developed for each of the three representative Bi-P HLW wastes and characterized with respect to key processing and product quality properties and, in particular, those relating to crystallization and foaming tendency.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗