Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “fuel cell cathode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Development of Low Cost, Robust and Durable Cathode Materials to Support Solid Oxide Fuel Cell Commercialization (Final Technical Report)

The project is aimed at addressing critical issues related to chromia-poisoning in the cathode of solid oxide fuel cells. A technical hurdle to the commercialization of solid oxide fuel cells is that chromia sources from the metallic interconnect and the balance of plant (BoP) components will cause chromia-poisoning to the cathode performance. This presents a significant challenge since it is very difficult to eliminate chromia sources in the cathode environment. One aspect of the current project is to evaluate whether SFM (Sr 2 Fe 1.5 Mo 0.5 O 6-δ ) that we have recently developed as redox-stable mixed conducting oxide possesses tolerance to chromia-poisoning. The second focus of this project is to evaluate coating on the cathode materials to mitigate chromia poisoning effect. Both thermodynamic evaluation and experimental approaches have been applied to enhance the knowledge base and fundamental understanding of chromia-tolerance of cathode for solid oxide fuel cells. low cost, robust and durable cathode material to support SOFC commercialization.

30 DIRECT ENERGY CONVERSION↗

Fundamentals of SrCoO 3-δ Based Oxygen Deficient Perovskites as Cathodes for Solid Oxide Fuel Cells

The local structure and oxygen stoichiometry in oxide systems have a profound impact on oxygen electrocatalysis encountered in metal-air batteries and solid oxide fuel cells (SOFCs). However, this knowledge is often obtained under conditions different from the real working conditions of the material, resulting in misinterpretation and misunderstanding. This PhD dissertation aims to obtain the structure and oxygen-stoichiometry information of a class of perovskite oxides under their real working conditions in solid oxide fuel cells. Several perovskite oxides were selected for the study: Sr 0.9 Y 0.1 CoO 3-δ (SYC10), Sr 0.9 Y 0.3 CoO 3-δ (SYC30), SrCo 0.9 Nb 0.1 O 3-δ (SCN10) and SrCo 0.9 Ta0.1O 3-δ (SCT10). The local crystal structure and oxygen stoichiometry of these materials were systematically characterized with in-situ neutron diffraction (ND). The oxygen stoichiometry was also measured by thermogravimetric analysis (TGA) and iodometric titration methods. To establish the correlation among structure, oxygen stoichiometry and oxygen reduction reaction (ORR) activity, high temperature electrochemical impedance spectroscopy, oxygen permeation and single cell testing were also performed. In chapter 2, SYC10 is described to have a more symmetrical structure and $V_o^{··}$ distribution, and higher $V_o^{··}$ concentration than SYC30. Molecular orbital energy analysis based on the local structure of the ORR-active Co1-polyhedra indicates SYC30 has a higher Fermi level relative to O-2p energy level in the active Co1-polyhedra, and thus a higher motional enthalpy for $V_o^{··}$ migration. However, the ORR activity of Y-doped SrCoO 3-δ (SCO) are found uncompetitive with other popular catalysts. In chapter 3 and 4, systematic structural studies are presented for Nb and Ta-doped SCO, namely SCN10 and SCT10, respectively. The methodology of unrevealing the structure-activity relationships in chapter 2 is also found applicable to SYC10, SCN10 and SCT10 as presented in chapter 5. The electrochemical tests indicate that SCT10 is the best catalyst due to its excellent thermal and electrochemical stability. In chapter 6, SCT10 is evaluated in a real solid oxide fuel cell in the form of nanoscaled SCT10 layer coating on the commercial (La 0.6 Sr 0.4 ) 0.95 Co 0.2 Fe 0.8 O 3-δ (LSCF). The bilayer structured cathode shows excellent properties of coarsening-resistant, Sr-segregation-free and high ORR-activity.

Yang, Tianrang↗

Computationally Guided Design of Multiple Impurities Tolerant Cathode for Solid Oxide Fuel Cell Applications

Solid oxide fuel cells (SOFCs) have been recognized as promising candidates in the demand of reducing the dependence on fossil fuels, which is one of the solutions to the threat of global warming. It was reported that the direct chemical-to-electrical energy conversion in SOFCs comes with negligible emission of greenhouse gases and up to 60% working efficiency. SOFC has unique advantages over traditional power generation technologies and other types of fuel cells due to the use of relatively inexpensive materials, low sensitivity to poisoning impurities in fuels, relatively high conversion efficiency, and fuel flexibility (like carbon-based fuels). However, during the SOFC operation, the cathode is exposed to intrinsic and extrinsic airborne contaminants at high temperatures (600–900°C), leading to their reaction with electrode materials, irreversible chemical and structural changes, and electrochemical performance degradation. of which CO2, SO2, Cr6+ and H2O are known to be concerns. Thus, developing a comprehensive understanding of the multiple impurities poisoning of SOFC cathodes in the presence of single or multiple impurities is necessary to address the long-term degradation of the SOFC cathode systems at operating conditions. An integrated computational and experimental approach has been utilized in the current work aiming at the comprehensive investigation of the cathode materials under single or multiple impurities poisoning effects, understanding the multiple impurities poisoning mechanism(s), and improving the long-term durability of the SOFC cathodes to develop better performing impurity-tolerant cathode materials. We first examined the agreement between the simulation approach and the experimental observations at various atmospheric and temperature conditions to confirm the reliability of CALPHAD for poisoning simulations in these cathodes. Then, using this approach, we investigated the accelerated testing protocol, which has become the standard method for conducting impurity poisoning experiments involving these cathode materials. We found our simulation approach is able to predict in which systems, i.e., cathode material and treatment environment, the accelerated testing protocols reflect actual operating conditions. Finally, in-depth simulations were done for these three candidate cathodes under different experimental conditions and suggested directions toward alternative cathode materials that have superior impurity tolerance.

36 MATERIALS SCIENCE↗

The anode supported internal cathode tubular solid oxide fuel cell: Novel production of a cell geometry for combined heat and power applications

An effective strategy for generating combined heat and power (CHP) systems is to use the combustion of hydrocarbons to provide fuel reforming and heat production for solid oxide fuel cell (SOFC) operation. Though tubular SOFCs (tSOFCs) are well suited to the thermal cycling associated with combustion systems, they have a geometric limitation which requires significant alteration to the combustion chamber. These alterations can be eliminated by producing an anode supported internal cathode-tSOFC (IC-tSOFC) which can be directly integrated into the chamber with minimal alterations. Novel methods used to produce IC-tSOFCs are discussed in this work. Scanning electron microscopy (SEM) and performance characterization are used to analyze fabricated cells. Finally, with a peak power density of 369 mW∙cm –2 , and an open circuit voltage (OCV) of 0.98 V, it is confirmed that novel production methods for IC-tSOFCs have been successful.

08 HYDROGEN↗

Fuel cell system

A fuel cell system comprising: a fuel cell, a fuel gas supplier configured to supply fuel gas to an anode of the fuel cell, an oxidant gas supplier configured to supply oxidant gas to a cathode of the fuel cell, a humidity adjuster configured to adjust a relative humidity of the fuel gas and a relative humidity of the oxidant gas, and a controller, wherein the controller detects the relative humidity of the fuel gas at an anode inlet of the fuel cell, and the controller detects the relative humidity of the oxidant gas at a cathode outlet of the fuel cell, and wherein, based on detection results, the controller controls the humidity adjuster so that the relative humidity of the fuel gas at the anode inlet is higher than the relative humidity of the oxidant gas at the cathode outlet.

Ando, Masaki↗

Hydrogen generation using a fuel cell system with an REP

A fuel cell system includes a fuel cell having an anode and a cathode configured to output cathode exhaust. The fuel cell is configured to generate waste heat. The fuel cell system further includes a reformer configured to partially reform a feed gas using the waste heat and output a hydrogen-containing stream. The fuel cell system further includes a reformer-electrolyzer-purifier (“REP”) having an REP anode configured to receive a first portion of the hydrogen-containing stream and an REP cathode.

Jahnke, Fred C.↗

Do Melamine and Melamine-Formaldehyde Surface Modifiers Improve Fuel Cell Activity and Durability?

Precious group metal-based catalysts based on Pt- and Pt-alloys are currently used as catalysts for the kinetically sluggish Oxygen Reduction Reaction (ORR) on the cathode of fuel cells. The activity of Pt or Pt-alloy catalysts towards ORR is severely compromised by the adsorption of spectator-species such as sulfonate anions from perfluorosulfonic acid (PFSA) ionomer or Pt-O(H) ad via water activation. Considering recent evidence pointing to the improvement in ORR activity via the use of melamine organic molecule or melamine-formaldehyde copolymeric additives as surface blocking agents for the prevention of sulfonate or Pt-OH ad adsorption, we evaluated these additives in fuel cells. The catalysts were modified with either of these additives and characterized using ex situ and in situ methods to verify successful adsorption and eventual performance in fuel cells. These surface modifying agents were found to suppress Pt-OH ad formation as well as suppress ORR activity. There was no evidence to point out that these additives improved ORR activity and H 2 /air polarization performance in a fuel cell MEA on supported, polycrystalline Pt catalyst.

08 HYDROGEN↗

Carbon Support Microstructure Impact on High Current Density Transport Resistances in PEMFC Cathode

Cell voltages at high current densities (HCD) of an operating proton-exchange membrane fuel cell (PEMFC) cathode suffer from losses due to the local-O 2 and bulk-H + transport resistances in the catalyst layer. Particularly, the microstructure of high surface area carbon (HSC) support upon which both the platinum catalyst and ionomer are dispersed play a pivotal role in controlling the reactant transport to the active site in the catalyst layer. In this study, we perform a systematic analysis of the underlying microstructure of platinum-cobalt catalyst dispersed on various HSC supports in terms of their surface area and pore-size distribution. The carbon microstructure was found to strongly influence the PtCo nanoparticle dispersion, catalyst layer ionomer distribution and transport losses governing the performance at HCD. Catalyst layer electrochemical diagnostics carried out to quantify local-O 2 transport resistance and bulk-H + transport resistance in the cathode were found to be directly correlated to the micropore (<2 nm) and macropore (>8 nm) surface areas of the carbon support, respectively. Finally, a 1D-performance model has been developed to assimilate our understanding of the catalyst layer microstructure and transport resistances at HCD.

25 ENERGY STORAGE↗

Performance investigation of alkaline direct methanol fuel cell with commercial PGM-free cathodic materials

Because little progress has been made in investigating the performance of alkaline direct methanol fuel cells (ADMFCs) with commercial materials (including platinum group metal (PGM)-free catalysts, anion exchange ionomers (AEIs), and anion exchange membranes (AEMs)), the objective of this work is to evaluate the performance of ADMFCs with all commercial materials, in order to establish a reference against which the performance of newly developed materials can be compared. Fe-N-C catalysts, Fumasep (FAA-3-50) based AEMs, and FAA3 based AEIs are here employed, and the parameters such as of operating temperature and methanol concentration are investigated and optimized. Electrochemical measurements show a performance increase with the temperature from 40 to 60 °C, and with the methanol concentration (from 1 to 5 M); followed by insignificant decrease with the further increase to 10 M. The best performance is achieved with 5 M methanol at 60 °C, and the remarkable powder density of 48.2 mW cm -2 was demonstrated under these conditions. This work provides insight into the large-scale application of ADMFC with commercial PGM-free materials.

25 ENERGY STORAGE↗

A Liquid–Vapor Two-Phase Model of Direct Methanol Fuel Cells With Platinum Group Metal-Free Cathode Catalyst

Abstract This study has developed a two-dimensional, two-phase transport model to investigate the transport characteristics in direct methanol fuel cells (DMFCs) using platinum group metal (PGM)-free cathode catalysts. The model considered anisotropic properties of the gas diffusion layer (GDL) caused by current collector’s mechanical compression, the interfacial mass transfer of water and methanol between liquid and vapor, and unique properties of the cathode PGM-free catalyst layer. Results showed that the liquid methanol solution from the anode could provide sufficient water to hydrate the proton exchange membrane (PEM), and the relative humidity of the cathode air did not impact the membrane hydration. Fully hydrating the cathode air may deteriorate the fuel cell performance, especially when the operating temperature is close to 100 °C because the exponential increase of the saturated water pressure with temperature decreased the partial pressure of oxygen. The optimized operating temperature increased with the increase of air pressure and was about 80 °C at 1.5 atm cathode pressure. To achieve the US Department of Energy’s performance target of 300 mW/cm2 peak power density, catalytic activities of both the anode and cathode catalysts need to be improved by one order of magnitude compared with the state-of-the-art commercial catalysts.

Electrochemistry↗

Highly durable platinum group metal-free catalyst fiber cathode MEAs for proton exchange membrane fuel cells

For this work, Fe-based platinum group metal (PGM)-free catalysts were incorporated into electrospun fiber mat or powder cathode membrane-electrode-assemblies (MEAs) with a Nafion 211 membrane and a Pt/C powder anode. Fabrication and characterization tests were performed on MEAs with: (1) a conventional powder cathode with a neat Nafion binder, (2) a fiber mat cathode with a Nafion/polyethylene oxide (PEO) binder, where PEO was extracted before MEA testing, (3) a powder cathode with a blended binder of Nafion and polyvinylidene fluoride (PVDF), and (4) a series of fiber mat cathodes with different Nafion/PVDF binder weight ratios. Cathode degradation occurred, with a loss in power output, in MEAs with a neat Nafion powder cathode or with a Nafion fiber cathode. In contrast, little or no power loss was observed for powder or fiber cathodes when the binder was a blend of Nafion and PVDF. The presence of hydrophobic PVDF drove water and electrogenerated peroxide out of the cathode, away from catalyst particles, which improved cathode durability, but PVDF also decreased the binder conductivity and slowed oxygen reduction kinetics, resulting in lower power densities. A 75:25 w:w Nafion:PVDF fiber cathode MEA was the best compromise for maximizing power and minimizing catalyst degradation. For such a cathode, with a PGM-free cathode catalyst loading of 3.0 mg cm –2 , a power density of 88 mW cm –2 at 0.5 V, 80 °C, and 200 kPa abs pressure was maintained for 80 h of continuous operation.

25 ENERGY STORAGE↗

Degradation & Performance Studies of ALD-Stabilized Nano-Composite SOFC Cathodes

This work showed, definitively, for the first time, that zirconia Atomic Layer Deposited (ALD) overcoats improve the stability of Solid Oxide Fuel Cell (SOFC) cathodes by chemically gettering interfacial Sr that has segregated out of lanthanum strontium cobalt iron oxide (LSCF). The optimum ALD ZrO 2 overcoat thickness was found to be ≥5 nm and <10 nm. Gadolinium doped ceria (GDC) pre-infiltration was also shown, for the first time, to improve SOFC cathode stability through the chemical getting of Sr at the LSCF-backbone and LSCF-gas interfaces. Due to the fact that it can be performed easily in air on large-area electrodes, GDC pre-infiltration is likely more commercially viable than ALD ZrO 2 overcoating as an interfacial Sr gettering technique. Combining ZrO 2 overcoating with GDC pre-infiltration was not successful because the GDC nano-particles gettered the ZrO 2 overcoat instead of the interfacial Sr.

30 DIRECT ENERGY CONVERSION↗

Elucidating the Role of Ionomer in the Performance of Platinum Group Metal-free Catalyst Layer via in situ Electrochemical Diagnostics

The ionomer content in platinum group metal (PGM)-free polymer electrolyte fuel cell (PEFC) cathode catalyst layer (CCL) plays an important role in the electrode gas transport properties, proton conductivity, and hence, membrane electrode assembly (MEA) performance. In this work, the ionomer content in the CCL is varied, influencing electrode microstructure by altering porosity, tortuosity, as well as ionomer distribution and coverage of the catalyst particles. A novel technique consisting of a H 2 pump, combined with a Pt black sensor layer, is used to measure the bulk mass transport resistance of a series of PGM-free CCL prepared with different ionomer contents. The values for bulk electrode mass transport resistance are contrasted with electrode proton transport resistance in the cathode catalyst layer, establishing a clearly defined trade-off between two key performance limiting phenomena and identifying a need for novel PGM-free electrode fabrication strategies.

25 ENERGY STORAGE↗

Catalyst layer formulations for slot-die coating of PEM fuel cell electrodes

The series of electrodes were fabricated by the scalable and manufacturable slot-die coating method for proton exchange membrane fuel cell (PEMFC) application. The inks with different amounts of solids were studied by rheological methods in order to establish a coating window with minimum manufacturing defects. The obtained electrodes were characterized by SEM, AFM, and optical microscopy, which showed that they were uniform and homogeneous with minimum defects. The electrochemical evaluation of the manufactured gas diffusion electrodes (GDE) showed that the main characteristics of the electrodes, like electrochemical surface area, proton resistivity, and double layer capacitance, were found to be close for all samples confirming the reproducibility of the slot-die process. Additionally, we studied the effects of membrane thickness on the performance of the GDE membrane electrode assemblies and determined that a decrease in membrane thickness favored the performance. Furthermore, the obtained results clearly demonstrated the applicability and feasibility of the approach for the Manufacturing of catalyst layers for the fuel cell application with potential for future mass production.

08 HYDROGEN↗

Cost-effective Manufacturing and Morphological Stabilization of Nanostructured Cathodes for Commercial Solid Oxide Fuel Cells (SOFCs) [Slides]

The overall goals of the program were to develop methods for preparing and stabilizing SOFC electrodes by infiltration that can be manufactured on a practical scale, then transfer those methods to cells in stacks. Cathodes prepared by infiltration of nanoparticles into a porous scaffold of the electrolyte have demonstrated outstanding electrochemical performance and mechanical strength but are difficult to manufacture due to the large number of infiltration steps required to produce a conductive composite and show poor stability due to sintering of the nanoparticles. At Penn, the main goal was to develop a fabrication method that uses only a small number of infiltration steps. Infiltration with molten salts and electrodeposition were pursued but deemed impractical. A method in which an electronically conductive scaffold consisted of a composite of a mixed conductor, LSF (La 0.9 Sr 0.1 FeO 3 ), with yttria-stabilized zirconia (YSZ) was found to be promising. While some cation mixing between LSF and YSZ was observed during calcination, there was no evidence for new phases in XRD and incorporation of Zr into the perovskite could be minimized by reducing the Sr content of the LSF. To stabilize nanoparticles infiltrated into the LSF-YSZ composite scaffold, the USC team examined the effects of Atomic Layer Deposition with ZrO 2 and infiltrated nanoparticles. Significantly enhanced stability was observed with the infiltrated nanoparticles. The FuelCell Energy team prepared 4”x4” cells in which an LSF-YSZ composite scaffold was cofired with the YSZ electrolyte and infiltrated with LSCF nanoparticles. Apparently because the LSF-YSZ scaffold layer was very thin in this case, the cation mixing that occurred during calcination resulted in a poor scaffold-electrolyte interface which caused reduced performance.

30 DIRECT ENERGY CONVERSION↗

Improving Durability of Fuel Cells with Platinum-rich Alloy Cathode Catalysts

Pt 3 Co-alloy based nanoparticle catalysts are very active for oxygen reduction reaction (ORR) thereby enabling high performance of proton exchange membrane fuel cells (PEMFC) for automotive propulsion. However, these catalyst materials degrade due to a combination of electrochemical surface area (ECSA) loss and dissolution of cobalt-alloying element from the nanoparticles. Dissolution of cobalt has a two-fold impact on the durability of fuel cells—i) a loss in the low-current density kinetic region due to a decrease in specific activity and ii) a loss in the high-current density transport region due to Co 2+ contamination of the ionomer phase. Cobalt dissolution-contamination needs to be mitigated as it limits fuel cell performance and lifetime for heavy-duty automotive applications. In this article, we study the use of PtCo-alloy catalysts with Pt-rich compositions using catalyst-specific accelerated stress test measurement in membrane electrode assemblies to decrease the amount of dissolved Co and mitigate its subsequent contamination effects. We demonstrate Pt 5 Co and Pt 7 Co compositions to enable significant improvements in durability (∼50 mV and ∼100 mV with respect to Pt 3 Co after 30,000 voltage cycles) with a minor but acceptable compromise in the initial specific activity of the catalyst.

08 HYDROGEN↗

High-performance ionomerless cathode anion-exchange membrane fuel cells with ultra-low-loading Ag–Pd alloy electrocatalysts

Rapid translation of catalysts from fundamental studies to high-performance devices could facilitate the process of developing and commercializing anion-exchange membrane fuel cells (AEMFCs). Traditionally, translation from material screening in three-electrode rotating disk electrode (RDE) cells to AEMFCs is complicated by differences in microenvironments, e.g. solid ionomer/membrane vs liquid electrolyte. Herein, we introduce a platform for translation to devices that utilizes ionomerless ultra-low-loading Ag-Pd alloy electrocatalyst cathodes synthesized by co-physical vapor deposition (PVD). Our ionomerless cathodes allow for systematic H 2 -O 2 AEMFC experiments while demonstrating comparable activity trends to those in three-electrode cells. Furthermore, here we show that our Ag 10 Pd 90 -based AEMFC reaches a peak power density of ~1 W cm$_{geo}^{-2}$ and ~10 W mg$_{PGM Cathode}^{-1}$ satisfying the U.S. Department of Energy’s platinum-group-metal (PGM) loading and cost targets. Our approach shows promise in facilitating the rapid translation between three-electrode studies and AEMFCs, offering a simple and effective design for decreasing PGM loadings.

25 ENERGY STORAGE↗