Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “dendrites”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

A single-ion-conducting polymer and high-entropy Li-garnet composite electrolyte with simultaneous enhancement in ion transport and mechanical properties

Enabling the lithium metal anode has been the holy grail for improving the energy density for the next generation advanced batteries. Developing electrolytes that will suppress Li dendrite growth and provide sufficient ionic conductivity remains a major challenge in this field. In this study, we develop a polymer–ceramic composite electrolyte for lithium metal batteries. The polymer matrix is a vinyl ethylene carbonate (VEC) based single-ion-conducting polymer electrolyte. The ceramic filler is a Li 7 La 3 Zr 0.5 Nb 0.5 Ta 0.5 Hf 0.5 O 12 high-entropy Li-garnet (HE Li-garnet) ceramic, which is less prone to surface Li 2 CO 3 formation compared to Al-doped Li garnets. The addition of HE Li-garnet leads to a 7-fold increase in the ionic conductivity (8.6 × 10 −5 S cm −1 at 30 °C) compared to the pure polymer, while maintaining a high Li + transference of 0.73. Proton nuclear magnetic resonance and thermogravimetric analysis results suggest that the addition of HE Li-garnet results in a lower degree of polymerization of VEC, leaving more unpolymerized VEC monomers in the matrix, serving as the governing mechanism for conductivity enhancement. The favorable interactions between HE Li-garnet particles and the polymer matrix lead to a stable and well-mixed composite with 2-fold enhancement of storage modulus at 40 °C. The simultaneous ion transport and mechanical property enhancement significantly improves the composite electrolyte's dendrite resistance and cycle life in Li symmetric cells. This work highlights the positive role HE Li-garnet can play in improving polymer electrolytes to enable lithium metal anodes.

Ock, Ji-young [Oak Ridge National Laboratory (ORNL↗

Interface-induced fast Li+ transport in mixed ionic–electronic conductors

Interfacial instability between lithium metal and solid-state electrolytes limits the performance of all-solid-state lithium metal batteries (ASSLBs), leading to parasitic reactions, non-uniform Li+ flux, and dendrite growth. Here, we develop a composite interlayer composed of the anti-perovskite Li2OHCl0.75Br0.25 (AP) and carbon nanotubes (CNTs) to enhance both interfacial stability and ionic transport. The AP–CNT interlayer exhibits enhanced Li+ conductivity arising from interfacial electron transfer from AP to CNTs, which generates a built-in electric field that facilitates Li+ migration. Lithium symmetric cells incorporating this interlayer achieve a high critical current density of 2.4 mA cm−2 at 55 °C. This design integrates chemical robustness with coupled ion–electron transport, offering a generalizable strategy for safe, dendrite-free, and high-performance ASSLBs.

He, Chenche↗

Interactions that define the arrangement of sugar-binding sites in BDCA-2 and dectin-2 dimers

The sugar-binding receptors dectin-2 and blood dendritic cell antigen 2 (BDCA-2) bind oligosaccharide ligands through extracellular carbohydrate-recognition domains (CRDs) and initiate intracellular signaling through Fc receptor γ adapters (FcRγ). Dectin-2 stimulates macrophages in response to pathogen binding while BDCA-2 modulates cytokine production in plasmacytoid dendritic cells. The oligomeric states of these receptors and the orientations of their CRDs have been investigated by analysis of a naturally occurring disulfide-bonded variant of BDCA-2 and by replacement of transmembrane domains with N-terminal dimerization domains to create extracellular domain dimers of both dectin-2 and BDCA-2. Analysis of these constructs, as well as previously described crystal structures of the CRDs from these proteins and a novel structure of an extended version of the extracellular domain of dectin-2, showed that there is only limited interaction of the CRDs in the dimers, but interactions can be stabilized by the presence of the neck region. The resulting orientation of sugar-binding sites in the dimers would favor crosslinking of multiple dimers by oligosaccharide ligands, causing clustering of FcRγ to initiate signaling.

carbohydrate-binding protein↗

Modeling Electrodeposition in 3D Porous Architectures for Solid-State Li-Metal Batteries

Li-metal storage in three-dimensional (3D) electrodes is considered a potential dendrite-mitigation strategy. The large surface area and high porosity of these electrodes result in reduced local Li-plating current densities. The porous topology provides a scaffold for Li-deposition and stripping, maintaining both mechanical integrity and Li accessibility. The goal of this study is to understand how characteristics, such as geometry and material properties, affect the current distribution and deposition pattern. To this end, we developed a computational method to track material growth driven by electrodeposition within a complex geometry. This method ensures that the finite-element discretization remains conforming to the moving boundary while preserving an adequate mesh quality, and thus maintains solution accuracy. Using this new computational tool, we analyze the conditions under which porous anode architectures effectively expand the surface area of the charge-transfer interface, and self-regulate current density and dendrite growth.

3D electrode architectures↗

TorchDendrite

SAND2025-11595O The TorchDendrite library implements hardware-informed dendrites using PyTorch and SNNTorch as backends. It allows the integration of dendrite-inspired neurons into machine learning networks built with both SNNTorch and PyTorch. TorchDendrite will be available on Github. Sandia National Laboratories is a multimission laboratory managed and operated by National Technology & Engineering Solutions of Sandia, LLC, a wholly owned subsidiary of Honeywell International Inc., for the U.S. Department of Energy’s National Nuclear Security Administration under contract DE-NA0003525.

Chance, Frances↗

Evaluation of Physical Microphysical Property Retrieval Algorithms During the 2020 IMPACTS Field Campaign

The NASA Investigation of Microphysics and Precipitation for Atlantic Coast Threatening Snowstorms (IMPACTS) field campaign provides high-quality, high-altitude aircraft lidar (532 nm), radar (W-band) and in-cloud microphysical aircraft data taken during wintertime storm events impacting the United States. This study evaluates two mass-dimensional relationships (Brown and Francis (1995, BF95); Heymsfield (2014, H14) and two lidar-radar microphysical retrieval algorithms (Cloudsat and CALIPSO Ice Cloud Property Product (2C-ICE); VarPy (a variational method derived from the satellite lidar-radar data community)) to estimate aircraft-retrieved volume extinction coefficient (σ), ice water content (IWC), and effective radius (r e ) during the 2020 IMPACTS deployment. BF95 and H14 have a close 1:1 correlation (R 2 = 0.98) with in-situ observations of σ. However, only BF95 displays a linear, consistent, and almost temperature-independent low bias for IWC and r e , which likely arises from the environmental conditions used to determine each. Unlike the field-campaign-derived BF95 and H14 relationships, VarPy and 2C-ICE directly ingest the aircraft-based lidar and radar data to simulate σ, IWC, and r e . For all three microphysical parameters, VarPy and 2C-ICE retrieval errors became notably more pronounced around the dendritic growth zone (-15°C to -10°C) and near freezing (≥-5°C), which suggests that both algorithms experience difficulty addressing riming and aggregation processes and with larger particles (dendrites and plates) due in part to their simplified ice particle assumptions. However, the mean-melt diameter ice-particle assumption did yield more accurate IWC estimates, which led to slightly better overall results for VarPy.

54 ENVIRONMENTAL SCIENCES↗

Effects of Size on Characteristics of Electroslag Remelted (ESR) HAYNES®282® alloy ingots

The effects of varying ingot diameters on the characteristics of round ESR ingots of 282 alloy are evaluated through a combined experimental and modeling study. Ingots of four different diameters --100 mm, 150 mm, 200 mm and 500 mm, were sectioned and analyzed using metallography to assess spatial variations in dendritic structure (primary / secondary dendrite arm spacings – PDAS/SDAS) across these ingots. Melt parameters of the processes were input into the simulation code, MeltFlow-ESR™ to theoretically predict PDAS/SDAS in the ingots. The values for PDAS/SDAS predicted by the simulations are compared with those measured by experiments and quantitative differences in these values are discussed in the context of the capability and limitations of the model and measurement methods. Both the predicted and measured values show that the PDAS/SDAS values increase with increasing ingot size. In addition, the relation with other ingot characteristics, such as local solidification time as well as the likelihood for freckle formation are discussed. The implication of these results for down-stream ingot processing and for ingot soundness are discussed.

Krishnamurthy, Ramanathan↗

A Self-Healing, Flowable, Yet Solid Electrolyte Suppresses Li-Metal Morphological Instabilities

In this article, lithium metal (Li 0 ) solid-state batteries encounter implementation challenges due to dendrite formation, side reactions, and movement of the electrode–electrolyte interface in cycling. Notably, voids and cracks formed during battery fabrication/operation are hot spots for failure. Here, a self-healing, flowable yet solid electrolyte composed of mobile ceramic crystals embedded in a reconfigurable polymer network is reported. This electrolyte can auto-repair voids and cracks through a two-step self-healing process that occurs at a fast rate of 5.6 µm h -1 . A dynamical phase diagram is generated, showing the material can switch between liquid and solid forms in response to external strain rates. The flowability of the electrolyte allows it to accommodate the electrode volume change during Li 0 stripping. Simultaneously, the electrolyte maintains a solid form with high tensile strength (0.28 MPa), facilitating the regulation of mossy Li 0 deposition. The chemistries and kinetics are studied by operando synchrotron X-ray and in situ transmission electron microscopy (TEM). Solid-state NMR reveals a dual-phase ion conduction pathway and rapid Li + diffusion through the stable polymer-ceramic interphase. This designed electrolyte exhibits extended cycling life in Li 0 –Li 0 cells, reaching 12 000 h at 0.2 mA cm -2 and 5000 h at 0.5 mA cm -2 . Furthermore, owing to its high critical current density of 9 mA cm -2 , the Li 0 –LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) full cell demonstrates stable cycling at 5 mA cm -2 for 1100 cycles, retaining 88% of its capacity, even under near-zero stack pressure conditions.

25 ENERGY STORAGE↗

Achieving Electrode Smoothing by Controlling the Nucleation Phase of Metal Deposition Through Polymer‐Substrate Binding

Polymer additives [like polyethylene oxide (PEO)] are widely used for smooth electrode deposition in aqueous zinc and many other battery systems. However, the precise mechanism by which they regulate morphology and suppress dendrite formation remains unclear. In this study, the knowledge gap is addressed by using in situ electrochemical atomic force microscopy to directly observe the interfacial evolution during Zn electrodeposition and polymer adsorption on Cu substrates in the presence of varying concentrations of ZnSO 4 and PEO. Contrary to previous literature assumptions, which emphasize the binding to the growing Zn crystal surfaces or Zn 2+ ions, the results demonstrate that PEO smooths Zn films by promoting nucleation of (002)-oriented Zn platelets through interactions with the Cu substrate. Density functional theory simulations support this finding by showing that PEO adsorption on Cu modifies the interfacial energy of Zn/Cu/electrolyte interfaces, favoring the stabilization of Zn (002) on the Cu substrate, as well as confines Zn electrodeposition to a narrow near-surface region. In conclusion, these findings elucidate a novel design principle for electrode smoothing, emphasizing the importance of substrate selection paired with polymer additives that exhibit an attractive interaction with the substrate but minimal interaction with growing crystals, offering a mechanistic perspective for improved battery performance.

Electrodeposition↗

Interface Design for High‐Performance All‐Solid‐State Lithium Batteries

All‐solid‐state batteries suffer from high interface resistance and lithium dendrite growth leading to low Li plating/stripping Coulombic efficiency (CE) of <90% and low critical current density at high capacity. Here, in this work, both challenges are simultaneously addressed and the Li plating/stripping CE is significantly increased to 99.6% at 0.2 mA cm −2 /0.2 mAh cm −2 , and critical current density (CCD) of > 3.0 mA cm −2 /3.0 mAh cm −2 by inserting a mixed ionic‐electronic conductive (MIEC) and lithiophobic LiF‐C‐Li 3 N‐Bi nanocomposite interlayer between Li 6 PS 5 Cl electrolyte and Li anode. The highly lithiophobic LiF‐C‐Li 3 N‐Bi interlayer with high ionic conductivity (10 −5 S cm −1 ) and low electronic conductivity (3.4×10 −7 S cm −1 ) enables Li to plate on the current collector (CC) surface rather than on Li 6 PS 5 Cl surface avoiding Li 6 PS 5 Cl electrolyte reduction. During initial Li plating on CC, Li penetrates into porous LiF‐C‐Li 3 N‐Bi interlayer and lithiates Bi nanoparticles into Li 3 Bi. The lithiophilic Li 3 Bi and Li 3 N nanoparticles in LiF‐C‐Li 3 N‐Li 3 Bi sub‐interlayer will move to CC along with plated Li, forming LiF‐C/Li 3 N‐Li 3 Bi lithiophobic/lithiophilic sublayer during the following Li stripping. This interlayer enables Co 0.1 Fe 0.9 S 2 /Li 6 PS 5 Cl/Li cell with an areal capacity of 1.4 mAh cm −2 to achieve a cycle life of >850 cycles at 150 mA g −1 . The lithiophobic/lithiophilic interlayer enables solid‐state metal batteries to simultaneously achieve high energy and long cycle life.

25 ENERGY STORAGE↗

New Engineering Concepts to High Energy Density Li-S Batteries

Li-S batteries (LSBs) with energy densities > 500 Wh/kg @ C/5 and >1000 cycles, cycle life operating over wide temperatures has been identified to be critical for meeting the global energy demands. Progress is however, very much limited due to several major hurdles related to the following: (a) poor Li' reaction kinetics (conductivity/diffusivity) enabling full reversible S conversion to Li2S, (b) inferior electron (e) conductivity, specific capacity and cycle life due to electrolyte soluble species of polysulfides (PSs) formed with the reaction of Li ions with sulfur migrating to anode, (c) unstable solid electrolyte interphase (SEI) formation and finally, (d) dendrites that are formed on the Li metal anode severely limiting the cycle life due to polarization at the solid/liquid interfaces causing safety, inferior capacity, energy density, rate, and cycle life issues. Creation of a fully functional economical ≤$80/kWh, high energy density LSBs is vital for enabling its widespread commercial deployment and use in current and next generation electric vehicles.

25 ENERGY STORAGE↗

Long‐Life Lithium‐Metal Batteries with an Ultra‐High‐Nickel Cathode and Electrolytes with Bi‐Anion Activity

Abstract Anion chemistry in electrolytes can greatly dictate the nature and quality of passivation layers on both cathode and anode surfaces. This will be more significant when it comes to highly reactive Li‐metal anode and aggressive high‐nickel cathodes. Herein, a competitive bi‐anion activity is found in electrolytes with the co‐existence of two anions, which leads to a controlled Li‐salt decomposition kinetics and entirely favorable interphasial chemistry on both Li‐metal anode and ultrahigh‐nickel cathode. The proposed bi‐anion localized high‐concentration electrolytes are demonstrated to exhibit superior electrochemical compatibility toward Li metal and long‐term cycling stabilities under both 4.4 and 4.6 V in Li‐metal batteries with ultrahigh‐nickel cathode. This study sheds fresh light on dendrite‐free Li‐metal anodes and provides guidance to achieve high‐energy‐density batteries.

Chemistry↗

Chemo‐Mechanics Interplay Dictates Interface Instability and Asymmetry in Plating and Stripping of Sodium Metal Electrodes

Abstract The development of practical sodium (Na) metal batteries is hindered by key challenges including dendrite growth, dead metal formation, and unstable solid electrolyte interphase (SEI) growth. A fundamental understanding of the chemo‐mechanical interactions at the Na/SEI interface is critical for designing stable Na metal electrodes. In this work, the coupled electrochemical‐mechanical processes governing the morphological evolution and stability of Na metal during plating and stripping are investigated. The heterogeneous nature of transport and morphological interactions at the Na/SEI interface is revealed to result in nonuniform mechanical overpotentials and reaction fronts, eventually leading to Na filaments or pits. The spatio‐temporal evolution of stress heterogeneities during Na plating and stripping is shown to be asymmetric, manifesting in varying morphological nonuniformities and instability modes. The crucial role of external pressure in modulating the electrochemical‐transport interactions, the mechanical response of Na, and the localized reaction currents and stresses at the Na/SEI interface is demonstrated. At different external pressure conditions, the correlation between transport heterogeneities in the SEI and the onset and propagation of interface instability has been delineated. This work highlights the need for synergistic tailoring of external pressure and SEI heterogeneity toward achieving stable electrodeposition and dissolution in Na metal electrodes.

Singla, Aditya [School of Mechanical Engineering P↗

Cation-Diffusive Carbon Interlayers Stabilize Na Metal and Double the Current in Na-S Redox-Flow Batteries for Grid-Scale Energy Storage

The sodium-sulfur nonaqueous redox-flow batteries (Na-S NARFBs) using earth-abundant elements are highly attractive due to the low material cost and improved energy density for grid-scale energy storage. However, the low current performance, poor Na0/Na+ redox kinetics, and Na dendrite growth pose severe challenges. We introduce cation-diffusive layers (CDLs): thin and Na+ affinitive interlayers at the Na anode that direct Na+ transport and stabilize Na deposition. Benchmarking three archetypal materials—carbon paper (CP), glass microfiber paper (GF), and foam—across Na-Na and Na-Cu, and Na-S cells identifies CP as the optimum. CP reduces symmetric cell overpotential by more than 70%, achieves 98% Na plating-stripping efficiency, and doubles the Na-S cell current density from 0.5 to 1.0 mA cm−2 without sacrificing capacity or efficiency. Ex situ electrochemical and SEM/XPS analysis, combined with molecular dynamics (MD) studies, reveal that electron-rich carbon fibers disperse supporting salt aggregates, enrich near-surface Na+ density, and create ion transport pathways for fast Na0/Na+ exchange while mitigating membrane degradation. Because of the ion-centric mechanism, CDLs can be generalized to other metal-anode designs. Further, this work establishes CDL design rules—cationic affinity and appropriate micro/nanostructure—as a simple, scalable route to high-current, durable metal-anode flow batteries.

Wu, Wenda [ORNL] (ORCID:000900033307687X)↗

Perspective on Lewis Acid‐Base Interactions in Emerging Batteries

Lewis acid-base interactions are common in chemical processes presented in diverse applications, such as synthesis, catalysis, batteries, semiconductors, and solar cells. The Lewis acid-base interactions allow precise tuning of material properties from the molecular level to more aggregated and organized structures. This review will focus on the origin, development, and prospects of applying Lewis acid-base interactions for the materials design and mechanism understanding in the advancement of battery materials and chemistries. The covered topics relate to aqueous batteries, lithium-ion batteries, solid-state batteries, alkali metal-sulfur batteries, and alkali metal-oxygen batteries. In this review, the Lewis acid-base theories will be first introduced. Thereafter the application strategies for Lewis acid-base interactions in solid-state and liquid-based batteries will be introduced from the aspects of liquid electrolyte, solid polymer electrolyte, metal anodes, and high-capacity cathodes. The underlying mechanism is highlighted in regard to ion transport, electrochemical stability, mechanical property, reaction kinetics, dendrite growth, corrosion, and so on. Last but not least, perspectives on the future directions related to Lewis acid-base interactions for next-generation batteries are like to be shared.

Lewis acid-base interactions↗

All‐Solid‐State Lithium–Sulfur Batteries of High Cycling Stability and Rate Capability Enabled by a Self‐Lithiated Sn‐C Interlayer

Abstract All‐solid‐state lithium–sulfur batteries (ASSLSBs) have attracted intense interest due to their high theoretical energy density and intrinsic safety. However, constructing durable lithium (Li) metal anodes with high cycling efficiency in ASSLSBs remains challenging due to poor interface stability. Here, a compositionally stable, self‐lithiated tin (Sn)‐carbon (C) composite interlayer (LSCI) between Li anode and solid‐state electrolyte (SSE), capable of homogenizing Li‐ion transport across the interlayer, mitigating decomposition of SSE, and enhancing electrochemical/structural stability of interface, is developed for ASSLSBs. The LSCI‐mediated Li metal anode enables stable Li plating/stripping over 7000 h without Li dendrite penetration. The ASSLSBs equipped with LSCI thus exhibit excellent cycling stability of over 300 cycles (capacity retention of ≈80%) under low applied pressure (<8 MPa) and demonstrate improved rate capability even at 3C. The enhanced electrochemical performance and corresponding insights of the designed LSCI broaden the spectrum of advanced interlayers for interface manipulation, advancing the practical application of ASSLSBs.

Ye, Lei↗

Heterogeneous Solid Electrolyte Interphase Interactions Dictate Interface Instability in Sodium Metal Electrodes

Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.

25 ENERGY STORAGE↗