Thermal conductivity of zirconia thermal barrier coatings

Thermal barrier coatings (TBC's) applied to the hot gas components of turbine engines lead to enhanced fuel efficiency and component reliability. Understanding the mechanisms which control the thermal transport behavior of the TBC's is of primary importance. Physical vapor deposition (PVD) and plasma spraying (PS) are the two most commonly used coating techniques. These techniques produce coatings with unique microstructures which control their performance and stability. The PS coatings were applied with either standard powder or hollow sphere particles. The hollow sphere particles yielded a lower density and lower thermal conductivity coating. The thermal conductivity of both fully and partially stabilized zirconia, before and after thermal aging, will be compared. The thermal conductivity of the coatings permanently increases upon exposed to high temperatures. These increases are attributed to microstructural changes within the coatings. Sintering of the as-fabricated plasma sprayed lamellar structure is observed by scanning electron microscopy of coatings isothermally heat treated at temperatures greater than 1100 C. During this sintering process the planar porosity between lamella is converted to a series of small spherical pores. The change in pore morphology is the primary reason for the observed increase in thermal conductivity. This increase in thermal conductivity can be modeled using a relationship which depends on both the temperature and time of exposure. Although the PVD coatings are less susceptible to thermal aging effects, preliminary results suggest that they have a higher thermal conductivity than PS coatings, both before and after thermal aging. The increases in thermal conductivity due to thermal aging for partially stabilized plasma sprayed zirconia have been found to be less than for fully stabilized plasma sprayed zirconia coatings. The high temperature thermal diffusivity data indicate that if these coatings reach a temperature above 1100 C during operation, they will begin to lose their effectiveness as a thermal barrier.

Dinwiddie, R. B.↗

Spectral Emittance of Uncoated and Ceramic-Coated Inconel and Type 321 Stainless Steel

The normal spectral emittance of Inconel and type 321 stainless steel with different surface treatments was measured at temperatures of 900, 1,200, 1,500, and 1,800 F over a wavelength range of 1.5 to 15 microns. The measurements involved comparison of the radiant energy emitted by the heated specimen with that emitted by a comparison standard at the same temperature by means of a recording double-beam infrared spectrophotometer. The silicon carbide comparison standard had previously been calibrated against a laboratory black-body furnace. Surface treatments included electropolishing, sandblasting, electro-polishing followed by oxidation in air for 1/2 hour at 1,800 F, sandblasting followed by oxidation in air for 1/2 hour at 1,800 F, application of National Bureau of Standards coating A-418, and application of NBS ceramic coating N-143. The normal spectral emittance of both alloys in the electropolished condition was low and decreased very slightly with increasing wavelength while in the sandblasted condition it was somewhat higher and did not vary appreciably with wavelength. The oxidation treatment greatly increased the normal spectral emittance of both the electropolished and sandblasted type 321 stainless steel specimens and of the electropolished Inconel specimens and introduced some spectral selectivity into the curves. The oxidation increased the normal spectral emittance of the sandblasted Inconel specimens only moderately. Of the specimens to which a coating about 0.002 inch thick was applied, those coated with A-418 had higher emittance at all wavelengths than did those coated with N-143, and the coated specimens of Inconel had higher spectral emittance at all wavelengths than did the corresponding specimens of type 321 stainless steel. Both coatings were found to be partially transparent to the emitted energy at this thickness but essentially opaque at a thickness of 0.005 inch. Coated specimens with 0.005 inch or more of coating did not show the effect of the underlying metal on spectral emittance, and there was no significant difference at wavelengths greater than about five microns in the normal spectral emittance of specimens having the two coatings. At shorter wavelengths the normal spectral emittance of specimens coated with A-418 was greater than that of specimens coated with N-143.

Richmond, Joseph C.↗

Effects of Conformal Coat on Tin Whisker Growth

A whisker from a tin plated part was blamed for the loss of a commercial spacecraft in 1998. Although pure tin finishes are prohibited by NASA, tin plated parts, such as hybrids, relays and commercial off the shelf (COTS) parts, are something discovered to have been installed in NASA spacecraft. Invariably, the assumption is that a conformal coat will prevent the growth of, or short circuits caused by, tin whiskers. This study measures the effect a Uralane coating has on the initiation and growth of tin whiskers, on the ability of this coating to prevent a tin whisker from emerging from the coating, and on the ability to prevent shorting. A sample of fourteen brass substrates (1 inch by 4 inches by 1/16 inch) were plated by two separate processes: half of the specimens were 'bright' tin plated directly over the brass substrate and half received a copper flash over the brass substrate prior to 'bright' tin plating. Each specimen was coated on one half of the substrate with three bi-directional sprays of Uralane 5750 to a nominal thickness of 25 to 75 micrometers (1 to 3 mils). Several specimens of both types, Cu and non-Cu flashed, were placed in an oven maintained at 50 C as others' work suggests that this is the optimal temperature for whisker formation. The remaining specimens were maintained at room ambient conditions. The surfaces of each specimen have been regularly inspected using both optical (15 to 400x power) and Scanning Electronic Microscopy (SEM). Many types of growths, including needle-like whiskers, first appeared approximately three months after plating on the non-conformally coated sides of all specimens. At four months, 4 to 5 times more growth sites were observed on the coated side; however, the density of growth sites on the non-conformally coated side has since increased rapidly, and now, at one year, is about the same for both sides. The density of growth sites is estimated at 90/sq mm with 30 percent of the sites growing whiskers (needle-like forms) with the potential to cause short circuit bridging. The average growth rate of the needle-like whiskers on the non-conformally coated areas is about 130 micrometers per year with some outliers reaching 800 micrometers after one year. It is more difficult to make growth measurements under the conformal coat. As yet no whiskers have been observed to penetrate through the coating surface, however, a number of tin nodules appear on the verge of breaking through the thinner regions of the coating surface. These domes are developing sharper and sharper tips, as if a growing whisker is about to push its way through a tough skin. Our observations are that the specimens with copper flash show a much lower density of nucleation sites and significantly slower whisker growth compared to the specimens that have only bright tin plating over brass. The specimens kept at room temperature have a higher whisker density than those stored at 50 C. This is an unexpected result and does not agree with the published findings of others. All of the whiskers originate from small surface defects (thin, tiny scratches) that appear over the entire surface of each specimen.

Kadesch, Jong S.↗

Sintering and Fracture Behavior of Plasma-sprayed Thermal Barrier Coatings

Thermal barrier coatings will be more aggressively designed to protect gas turbine engine hot-section components in order to meet future engine higher fuel efficiency and lower emission goals. There is a need to characterize the fundamental sintering and fracture behavior of the current ZrO2-(7 to 8)wt%Y2O3 coating, in order to fully take advantage of the coating capability. In addition, a thorough evaluation of the coating behavior and temperature limits will be useful for more accurately assessing the benefit gained from future advanced coating systems. In this study, the sintering behavior of plasma-sprayed ZrO2-8wt%Y2O3 coatings was systematically investigated as a function of temperature and time using a dilatometer in the temperature range of 1200-1500 C. The coating sintering kinetics obtained by dilatometry were compared with the coating thermal conductivity increase kinetics, determined by a steady-state laser heat-flux testing approach, under high temperature and thermal gradient sintering conditions. The mode I, mode II, and mixed mode I-mode II fracture behavior of as-processed and sintering-annealed coatings was determined in asymmetric flexure loading at ambient and elevated temperatures in order to evaluate the coating sintering effects on the fracture envelope of K(sub I) versus K(sub II). The coating thermal conductivity cyclic response associated with the interface delamination of the coating systems under simulated engine heat-flux conditions will be discussed in conjunction with the sintering and fracture testing results.

Zhu, Dongming↗

Effect of an Opaque Reflecting Layer on the Thermal Behavior of a Thermal Barrier Coating

A parametric study using a two-flux approximation of the radiative transfer equation was performed to examine the effects of an opaque reflective layer on the thermal behavior of a typical semitransparent thermal barrier coating on an opaque substrate. Some ceramic materials are semitransparent in the wavelength ranges where thermal radiation is important. Even with an opaque layer on each side of the semitransparent thermal barrier coating, scattering and absorption can have an effect on the heat transfer. In this work, a thermal barrier coating that is semitransparent up to a wavelength of 5 micrometers is considered. Above 5 micrometers wavelength, the thermal barrier coating is opaque. The absorption and scattering coefficient of the thermal barrier was varied. The thermal behavior of the thermal barrier coating with an opaque reflective layer is compared to a thermal barrier coating without the reflective layer. For a thicker thermal barrier coating with lower convective loading, which would be typical of a combustor liner, a reflective layer can significantly decrease the temperature in the thermal barrier coating and substrate if the scattering is weak or moderate and for strong scattering if the absorption is large. The layer without the reflective coating can be about as effective as the layer with the reflective coating if the absorption is small and the scattering strong. For low absorption, some temperatures in the thermal barrier coating system can be slightly higher with the reflective layer. For a thin thermal barrier coating with high convective loading, which would be typical of a blade or vane that sees the hot sections of the combustor, the reflective layer is not as effective. The reflective layer reduces the surface temperature of the reflective layer for all conditions considered. For weak and moderate scattering, the temperature of the TBC-substrate interface is reduced but for strong scattering, the temperature of the substrate is increased slightly.

Spuckler, Charles M.↗

Low Earth Orbit Environmental Durability of Recently Developed Thermal Control Coatings

The Materials International Space Station Experiment provided a means to expose materials and devices to the low Earth orbit environment on the exterior of the International Space Station. By returning the specimens to Earth after flight, the specimens could be evaluated by comparison with pre-flight measurements. One area of continuing interest is thermal control paints and coatings that are applied to exterior surfaces of spacecraft. Though traditional radiator coatings have been available for decades, recent work has focused on new coatings that offer custom deposition or custom optical properties. The custom deposition of interest is plasma spraying and one type of coating recently developed as part of a Small Business Innovative Research effort was designed to be plasma sprayed onto radiator surfaces. The custom optical properties of interest are opposite to those of a typical radiator coating, having a combination of high solar absorptance and low infrared emittance for solar absorber applications, and achieved in practice via a cermet coating. Selected specimens of the plasma sprayed coatings and the solar absorber coating were flown on Materials International Space Station Experiment 7, and were recently returned to Earth for post-flight analyses. For the plasma sprayed coatings in the ram direction, one specimen increased in solar absorptance and one specimen decreased in solar absorptance, while the plasma sprayed coatings in the wake direction changed very little in solar absorptance. For the cermet coating deployed in both the ram and wake directions, the solar absorptance increased. Interestingly, all coatings showed little change in infrared emittance.

Optical Properties↗

Intumescent Coatings as Fire Retardants

The development of fire-retardant coatings to protect surfaces which may be exposed to fire or extreme heat is a subject of intense interest to many industries. A fire-retardant paint has been developed which represents a new chemical approach for preparing intumescent coatings, and potentially, is very important to fire-prevention authorities. The requirements for a superior coating include ease of application, suitability to a wide variety of surfaces and finishes, and stability over an extended period of time within a broad range of ambient temperature and humidity conditions. These innovative coatings, when activated by the heat of a fire, react to form a thick, low-density, polymeric coating or char layer. Water vapor and sulphur dioxide are released during the intumescent reaction. Two fire-protection mechanisms thus become available: (1) the char layer retards the flow of heat, due to the extremely low thermal conductivity; and (2) water vapor and sulfur dioxide are released, providing fire quenching properties. Still another mechanism functions in cases where the char, by virtue of its high oxidation resistance and low thermal conductivity, reaches a sufficiently high temperature to re-radiate much of the incident heat load. The coatings consist of dispersions of selective salts of a nitro-amino-arornatic compound. Specifically, para-nitroaniline bisulfate and the ammonium salt of para-nitroaniline-ortho sulphuric acid (2-amino-5-nitrobenzenesulphuric acid) are used. Suitable vehicles are cellulose nitrate of lacquer grade, a nitrite-phenolic modified rubber, or epoxy-polysulfide copolymer. Three separate formulations have been developed. A solvent is usually employed, such as methylethyl ketone, butyl acetate, or toluene, which renders the coatings suitably thin and which evaporates after the coatings are applied. Generally, the intumescent material is treated as insoluble in the vehicle, and is ground and dispersed in the vehicle and solvent like an ordinary coating pigment. The char found on intumescence is better in terms of yield and physical properties than chars obtained from many previously known intumescent materials. Prior to intumescence, the coating has a density of 85 pounds per cubic foot. After intumescence, the density is approximately 0.3 pounds per cubic loot. The linear expansion of the coatings ranges from 70 to 200 times the applied coating thickness.

Parker, J. A.↗

Residual Stresses in a NiCrY-Coated Powder Metallurgy Disk Superalloy

Protective ductile coatings will be necessary to mitigate oxidation and corrosion attack on superalloy disks exposed to increasing operating temperatures in some turbine engine environments. However, such coatings must be resistant to harmful surface cracking during service. The objective of this study was to investigate how residual stresses evolve in such coatings. Cylindrical gage fatigue specimens of powder metallurgy-processed disk superalloy LSHR were coated with a NiCrY coating, shot peened, and then subjected to fatigue in air at room and high temperatures. The effects of shot peening and fatigue cycling on average residual stresses and other aspects of the coating were assessed. Shot peening did induce beneficial compressive residual stresses in the coating and substrate. However, these stresses became more tensile in the coating with subsequent heating and contributed to cracking of the coating in long intervals of cycling at 760 C. Substantial compressive residual stresses remained in the substrate adjacent to the coating, sufficient to suppress fatigue cracking. The coating continued to protect the substrate from hot corrosion pitting, even after fatigue cracks initiated in the coating.

superalloy↗

LCF Life of As-Deposited and Annealed NiCr-Y Coatings for Oxidation and Hot Corrosion Protection of Disk Alloys

Increasing temperatures in aero gas turbines is resulting in oxidation and hot corrosion attack of turbine disks. Since disks are sensitive to low cycle fatigue (LCF), any environmental attack, and especially hot corrosion pitting, can seriously degrade the life of the disk. Application of metallic coatings is one means of protecting disk alloys from this environmental attack. However, the presence of a metallic coating can degrade the LCF life of a disk alloy. Therefore, coatings must be designed which are not only resistant to oxidation and corrosion attack, but do not significantly degrade the LCF life of the alloy.Three different NiCr-Y coating compositions (29, 35.5, 44 wt.% Cr, all with 0.1 wt.% Y) were applied at two thicknesses by Plasma Enhanced Magnetron Sputtering (PEMS) to two similar Ni-based disk alloys. One Ni-35.5Cr-0.1Y coating also received a thin ZrO2 overcoat. The coated samples were also given a short thermal anneal in a low PO2 environment to encourage bonding of the coating and substrate as well as initiating formation of a chromia scale. Without further environmental exposure, the LCF life of coated and uncoated samples was evaluated at 760°C in air. The LCF lifetime of all coated samples was less than that of uncoated samples. The LCF life scaled with the Cr content and the high-Cr, thin coating showed the highest LCF life. Pre and post-test characterization of the various coatings, including identification of crack initiation sites, will be presented and the effect of the coating on the LCF life discussed.

low cycle fatigue↗

Fatigue Behavior of Coated Titanium Alloys

Advanced multi-component TiAlCrTaSiN-based multilayered coatings were developed and processed onto Ti-6Al-4V (Ti-6-4) and GammaMet PX (GMPX or TiAl) alloys by a magnetron-enhanced physical vapor deposition technique. The coatings have recently been in development with the goal of improving advanced titanium alloy, turbine engine component durability and oxidation-erosion resistance. In this work, the performance of the multi-component coating system (including the outer layer nitride based coating and inner TiAlCrSi oxidation barrier bond coat) was studied, and the coating's influence on the fatigue behavior of the titanium-based alloys were compared. Although the multi-component coating was initially optimized to improve the coating's high temperature oxidation and erosion resistance, the lower ductility nitride-based coating needs further work on microstructure or composition to improve its mechanical stress resistance and strain tolerance for use in cyclically loaded, turbine blade operating conditions. This is particularly true for GMPX and other γ-TiAl alloys because these intermetallic titanium alloys have limited ductility and are very sensitive to defects such as coating cracks. However, the inner layer TiAlCrSi-coating had better adhesion and ductility, and may be a suitable choice to improve the oxidation resistance of titanium alloys.

Oxidation Barrier Coatings↗

Black Molecular Adsorber Coatings for Spaceflight Applications

The molecular adsorber coating is a new technology that was developed to mitigate the risk of on-orbit molecular contamination on spaceflight missions. The application of this coating would be ideal near highly sensitive, interior surfaces and instruments that are negatively impacted by outgassed molecules from materials, such as plastics, adhesives, lubricants, epoxies, and other similar compounds. This current, sprayable paint technology is comprised of inorganic white materials made from highly porous zeolite. In addition to good adhesion performance, thermal stability, and adsorptive capability, the molecular adsorber coating offers favorable thermal control characteristics. However, low reflectivity properties, which are typically offered by black thermal control coatings, are desired for some spaceflight applications. For example, black coatings are used on interior surfaces, in particular, on instrument baffles for optical stray light control. Similarly, they are also used within light paths between optical systems, such as telescopes, to absorb light. Recent efforts have been made to transform the white molecular adsorber coating into a black coating with similar adsorptive properties. This result is achieved by optimizing the current formulation with black pigments, while still maintaining its adsorption capability for outgassing control. Different binder to pigment ratios, coating thicknesses, and spray application techniques were explored to develop a black version of the molecular adsorber coating. During the development process, coating performance and adsorption characteristics were studied. The preliminary work performed on black molecular adsorber coatings thus far is very promising. Continued development and testing is necessary for its use on future contamination sensitive spaceflight missions.

adsorption↗

Black Molecular Adsorber Coatings for Spaceflight Applications

The molecular adsorber coating is a new technology that was developed to mitigate the risk of on-orbit molecular contamination on spaceflight missions. The application of this coating would be ideal near highly sensitive, interior surfaces and instruments that are negatively impacted by outgassed molecules from materials, such as plastics, adhesives, lubricants, epoxies, and other similar compounds. This current, sprayable paint technology is comprised of inorganic white materials made from highly porous zeolite. In addition to good adhesion performance, thermal stability, and adsorptive capability, the molecular adsorber coating offers favorable thermal control characteristics. However, low reflectivity properties, which are typically offered by black thermal control coatings, are desired for some spaceflight applications. For example, black coatings are used on interior surfaces, in particular, on instrument baffles for optical stray light control. Similarly, they are also used within light paths between optical systems, such as telescopes, to absorb light. Recent efforts have been made to transform the white molecular adsorber coating into a black coating with similar adsorptive properties. This result is achieved by optimizing the current formulation with black pigments, while still maintaining its adsorption capability for outgassing control. Different binder to pigment ratios, coating thicknesses, and spray application techniques were explored to develop a black version of the molecular adsorber coating. During the development process, coating performance and adsorption characteristics were studied. The preliminary work performed on black molecular adsorber coatings thus far is very promising. Continued development and testing is necessary for its use on future contamination sensitive spaceflight missions.

adsorption↗

NASA's Advanced Environmental Barrier Coatings Development for SiC/SiC Ceramic Matrix Composites: Understanding Calcium Magnesium Alumino-Silicate (CMAS) Degradations and Resistance

Environmental barrier coatings (EBCs) and SiCSiC ceramic matrix composites (CMCs) systems will play a crucial role in next generation turbine engines for hot-section component applications because of their ability to significantly increase engine operating temperatures with improved efficiency, reduce engine weight and cooling requirements. The development of prime-reliant environmental barrier coatings is essential to the viability and reliability of the envisioned CMC engine component applications, ensuring integrated EBC-CMC system durability and designs are achievable for successful applications of the game-changing component technologies and lifing methodologies.This paper will emphasize recent NASA environmental barrier coating developments for SiCSiC turbine airfoil components, utilizing advanced coating compositions, state-of-the-art processing methods, and combined mechanical and environment testing and durability evaluations. The coating-CMC degradations in the engine fatigue-creep and operating environments are particularly complex; one of the important coating development aspects is to better understand engine environmental interactions and coating life debits, and we have particularly addressed the effect of Calcium-Magnesium-Alumino-Silicate (CMAS) from road sand or volcano-ash deposits on the durability of the environmental barrier coating systems, and how the temperature capability, stability and cyclic life of the candidate rare earth oxide and silicate coating systems will be impacted in the presence of the CMAS at high temperatures and under simulated heat flux conditions. Advanced environmental barrier coating systems, including HfO2-Si with rare earth dopant based bond coat systems, will be discussed for the performance improvements to achieve better temperature capability and CMAS resistance for future engine operating conditions.

Environmental barrier coatings↗

Fatigue Life of a NiCr-Coated Powder Metallurgy Disk Superalloy After Varied Processing and Exposures

A protective ductile NiCr coating has shown promise to mitigate oxidation and corrosion attack on superalloy disk alloys. The effects of this coating on fatigue life and failure modes of the disk superalloy are an important concern. The objective of this study was to investigate the fatigue life and failure modes of disk superalloy specimens protected by this coating, using varied pre-coating and post-coating processes. Cylindrical gage fatigue specimens of a powder metallurgy-processed disk superalloy were grit blast or wet blast before being coated with a ductile NiCrY coating, then shot peened at low or medium levels after coating. All were then heat treated, some exposed, and finally all were subjected to fatigue at high temperature. The effects of varied pre-coating treatment, post-coating shot peening, and oxidation plus hot corrosion exposures on fatigue life with the coating were compared.

coating↗

Coatings for directional eutectics

Coating compositions were evaluated for oxidation protection of directionally solidified composite alloy NiTaC-13. These coatings included three NiCrAlY compositions (30-5-1, 25-10-1 and 20-15-1), two FeCrAlY compositions (30-5-1 and 25-10-1), a CoCrAlY composition (25-10-1), and one duplex coating, Ni-35Cr + Al. Duplicate pin samples of each composition were evaluated using two cyclic furnace oxidation tests of 100 hours at 871 C and 500 hours at 1093 C. The two best coatings were Ni-20Cr-15Al-lY and Ni-35Cr + Al. The two preferred coatings were deposited on pins and were evaluated in detail in .05 Mach cyclic burner rig oxidation to 1093 C. The NiCrAlY coating was protective after 830 hours of cycling, while the duplex coating withstood 630 hours. Test bars were coated and cycled for up to 500 hours. Tensile tests indicated no effect of coatings on strength. In 871 C air stress rupture, a degradation was observed for coated relative to bare material. The cycled NiCrAlY coating offered excellent protection with properties superior to the bare cycled NiTaC-13 in 1093 C air stress rupture.

Jackson, M. R.↗

NASA thermal barrier coatings - Summary and update

The work conducted at the NASA Lewis Research Center to evolve and evaluate a thermal-barrier coating system will be discussed. A durable, two-layer, plasma-sprayed coating consisting of a ceramic layer over a metallic layer was developed that has the potential of insulating hot engine parts and thereby reducing metal temperatures and coolant flow requirements and/or permitting use of less costly and complex cooling configurations and materials. The paper summarizes the results of analytical and experimental investigations of the coatings on flat metal specimens, turbine vanes and blades, and combustor liners. Discussed are results of investigations to determine coating adherence and durability, coating thermal, strength and fatigue properties, and chemical reactions of the coating with oxides and sulfates. Also presented are the effect of the coating on aerodynamic performance of a turbine vane, measured vane and combustor liner temperatures with and without the coating, and predicted turbine metal temperatures and coolant flow reductions potentially possible with the coating. Included also are summaries of some current research related to the coating and potential applications for the coating.

Stepka, F. S.↗

Development of improved high temperature coatings for IN-792 + HF

The development for t-55 l712 engine of high temperature for integral turbine nozzles with improved thermal fatigue resistance without sacrificing oxidation/corrosion protection is discussed. The program evaluated to coating systems which comprised one baseline plasma spray coating (12% Al-NiCoCrALY), three aluminide coatings including the baseline aluminide (701), two CoNiCrAly (6% Al) + aluminide systems and four NiCoCrY + aluminide coating were evaluated. The two-step coating processes were investigated since it offered the advantage of tailoring the composition as well as properly coating surfaces of an integral or segmented nozzle. Cyclic burner rig thermal fatigue and oxidation/corrosion tests were used to evaluate the candidate coating systems. The plasma sprayed 12% Al-NiCoCrAlY was rated the best coating in thermal fatigue resistance and outperformed all coatings by a factor between 1.4 to 2.5 in cycles to crack initiation. However, this coatings is not applicable to integral or segmented nozzles due to the line of sight limitation of the plasma spray process. The 6% Al-CoNiCrAlY + Mod. 701 aluminide (32 w/o Al) was rated the best coating in oxidation/corrosion resistance and was rated the second best in thermal fatigue resistance.

Profant, D. D.↗

Rocket thrust chamber thermal barrier coatings

Subscale rocket thrust chamber tests were conducted to evaluate the effectiveness and durability of thin yttria stabilized zirconium oxide coatings applied to the thrust chamber hot-gas side wall. The fabrication consisted of arc plasma spraying the ceramic coating and bond coat onto a mandrell and then electrodepositing the copper thrust chamber wall around the coating. Chambers were fabricated with coatings .008, and .005 and .003 inches thick. The chambers were thermally cycled at a chamber pressure of 600 psia using oxygen-hydrogen as propellants and liquid hydrogen as the coolant. The thicker coatings tended to delaminate, early in the cyclic testing, down to a uniform sublayer which remained well adhered during the remaining cycles. Two chambers with .003 inch coatings were subjected to 1500 thermal cycles with no coating loss in the throat region, which represents a tenfold increase in life over identical chambers having no coatings. An analysis is presented which shows that the heat lost to the coolant due to the coating, in a rocket thrust chamber design having a coating only in the throat region, can be recovered by adding only one inch to the combustion chamber length.

Quentmeyer, R. J.↗