Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “cathode additives”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

The Influence of Cr-Additives on the Polarization Resistance of Praseodymium-Doped Ceria Cathodes for Solid Oxide Fuel Cells

While Cr poisoning of the oxygen reduction reaction (ORR) at SOFC cathodes is widely agreed to involve deactivation of oxygen exchange sites, the degradation mechanism remains ambiguous. Here, we selected an alternative cathode material Pr 0.1 Ce 0.9 O 2− δ , free of Sr segregation, to systematically investigate the effect of Cr-induced degradation in ORR. We expand on our previous studies in which the acidity/basicity of binary additives was found to be a strong indicator of the rate of oxygen surface exchange, by electrochemically investigating the ORR activity of the PCO cathode by impedance spectroscopy. Serial infiltration with acidic Cr-based oxides was found to degrade ORR activity as reflected in a 20-fold increase in area specific resistance (ASR) without corresponding changes in activation energy, with the opposite trend obtained with Ca-based oxides. Detected changes in total capacitance, attributed to changes in surface capacitance, also suggest depressed/enhanced PCO surface redox behavior with Cr/Ca-based infiltrants. Taken together, these results point to a more universal source of ORR poisoning/activation, based on acidity/basicity, rather than physical blocking of active sites. With this improved understanding, one can expect progress to be made in the coming years in optimizing means for protecting catalytic surfaces from degradation and/or improving their performance.

25 ENERGY STORAGE↗

Cathode pre-lithiation/sodiation for next-generation batteries

Electrochemical energy storage is playing a pivotal role in the global pursuit of a clean and sustainable energy future. Lithium-ion batteries (LIBs) are the state-of-the-art technology, but future energy requirements demand higher energy densities and a more diverse battery landscape to meet a wide variety of applications. Unfortunately, many next-generation LIB chemistries and beyond-LIB technologies suffer from large first-cycle irreversible capacity caused by active ion loss. The field of pre-lithiation/sodiation has recently emerged as researchers attempt to mitigate active ion loss and boost the energy density of next-generation LIBs and sodium-ion batteries. Herein, we highlight recent advances in cathode pre-lithiation/sodiation using sacrificial additives and pre-lithiation/sodiation of cathode active materials.

25 ENERGY STORAGE↗

Stabilizing alkaline fuel cells with a niobium-doped brookite titanium dioxide catalyst support

Anion-exchange membrane fuel cells represent a promising and scalable approach for hydrogen energy utilization. However, their development is hindered by the weak bonding between metal catalysts and carbon supports, along with challenges in fabricating electronically/ionically conductive electrodes. Here, we report a composite cathode of Nb-doped brookite TiO 2 nanorods that have robust stability when combined with Pt nanoscale catalysts in an alkaline fuel cell. The composite cathode, fabricated without the addition of an ionomer, delivers a power density of 419 mW cm −2 at a current density of 650 mA cm −2 and a voltage retention of 81% at 100 mA cm −2 after 25 h, substantially outperforming a cathode fabricated from commercial Pt/C. Further investigations of the chemical structure, anion exchange capacity, and mass transfer resistance reveal that a solvent residue derived from N-methylpyrrolidone plays an important role in charge transfer and mass transport in the alkaline fuel cell.

alkaline fuel cell↗

Impact of polymer additives on crack mitigation of rod-coated fuel cell cathode catalyst layers

Cracks in catalyst layers (CLs) are a potential source of long-term failure in a fuel cell membrane electrode assembly (MEA). While modifications to the CL ink formulation can affect the degree of cracking, these changes may lead to lower initial performance than their cracked analogues due to the established link between formulation and performance. In this work, we explored the use of polymeric additives to mitigate CL cracks. Small quantities of poly (acrylic acid), poly (ethylene oxide), poly (methyl methacrylate), or poly (vinyl alcohol) - 5 wt% relative to ionomer mass - were added to the ink prior to its final mixing. Poly (vinyl alcohol) resulted in crack-free CLs, whereas the other polymers resulted in CLs with similar crack percentages as the control CL. Through a combination of transmission electron microscopy, X-ray computed tomography, and infrared spectroscopy, we ascribed the crack-mitigating mechanism of poly (vinyl alcohol) to its ability to hydrogen-bond with Nafion, the ion conducting polymer binder in the catalyst ink. Initial performance of this non-cracked electrode exhibited nearly identical electrochemical behavior to its cracked counterpart, demonstrating that PVA additives successfully reduce cracks while maintaining cell initial performance.

30 DIRECT ENERGY CONVERSION↗

Functional Testing of the Space Station Plasma Contactor

A plasma contactor system has been baselined for the International Space Station Alpha (ISSA) to control the electrical potentials of surfaces to eliminate/mitigate damaging interactions with the space environment. The system represents a dual-use technology which is a direct outgrowth of the NASA electric propulsion program and, in particular, the technology development effort on ion thruster systems. The plasma contactor subsystems include a hollow cathode assembly, a power electronics unit, and an expellant management unit. Under a pre-flight development program these subsystems are being developed to the level of maturity appropriate for transfer to U.S. industry for final development. Development efforts for the hollow cathode assembly include design selection and refinement, validating its required lifetime, and quantifying the cathode performance and interface specifications. To date, cathode components have demonstrated over 10,000 hours lifetime, and a hollow cathode assembly has demonstrated over 3,000 ignitions. Additionally, preliminary integration testing of a hollow cathode assembly with a breadboard power electronics unit has been completed. This paper discusses test results and the development status of the plasma contactor subsystems for ISSA, and in particular, the hollow cathode assembly.

Patterson, Michael J.↗

Unraveling the nature of sulfide ions in hydrometallurgical recycling of NCM622 cathode material

The use of lithium-ion batteries (LIBs) has increased dramatically since its initial inception in the late 20th century. Such a surge in the LIB market and industry has resulted in a huge demand for mineral resources. Besides, the large scale of production will lead to massive amounts of waste batteries in the end. As such, recycling is seen as an end-of-pipe process to resolve sustainability and environmental concerns. The hydrometallurgical recycling is considered to be the most prominent method to recover cathode materials from spent LIBs owing to its high leaching efficiency and low energy costs. A series of procedures including pretreatment of the spent LIBs, acid leaching of the black mass, chemical co-precipitation of the hydroxide precursor, and sintering of the cathode active material need to be operated precisely. In this aspect, the impurities introduced during the process could pose a serious threat to the reaction stability as well as recycling consistency. Here, the impact of sulfide ions on recovered LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NCM622) cathode material with the method of hydrometallurgy is first investigated in detail. This study shows that hydrometallurgical process is not obviously influenced by sulfide impurity. No signs of secondary phase or impurity inclusion are spotted in synthesized cathodes. Under 5 at % sulfide concentration conditions, the obtained NCM622 cathode exhibits a capacity of 159.4 mAh/g after 100 cycles at 1/3C, which is at the same level as virgin benchmark. The difference in rate performance between cathodes with and without additional sulfide is less than 2 % or even smaller. In short, the results indicate a neutral status of sulfide ions in hydrometallurgical recycling.

25 ENERGY STORAGE↗

Synergetic Dual‐Additive Electrolyte Enables Highly Stable Performance in Sodium Metal Batteries

Sodium (Na)-metal batteries (SMBs) are considered one of the most promising candidates for the large-scale energy storage market owing to their high theoretical capacity (1,166 mAh g -1 ) and the abundance of Na raw material. However, the limited stability of electrolytes still hindered the application of SMBs. Herein, sulfolane (Sul) and vinylene carbonate (VC) are identified as effective dual additives that can largely stabilize propylene carbonate (PC)-based electrolytes, prevent dendrite growth, and extend the cycle life of SMBs. The cycling stability of the Na/NaNi 0.68 Mn 0.22 Co 0.1 O 2 (NaNMC) cell with this dual-additive electrolyte is remarkably enhanced, with a capacity retention of 94% and a Coulombic efficiency (CE) of 99.9% over 600 cycles at a 5 C (750 mA g -1 ) rate. The superior cycling performance of the cells can be attributed to the homogenous, dense, and thin hybrid solid electrolyte interphase consisting of F- and S-containing species on the surface of both the Na metal anode and the NaNMC cathode by adding dual additives. Such unique interphases can effectively facilitate Na-ion transport kinetics and avoid electrolyte depletion during repeated cycling at a very high rate of 5 C. This electrolyte design is believed to result in further improvements in the performance of SMBs.

25 ENERGY STORAGE↗

Enhancing the Electrode Gravimetric Capacity of Li 1.2 Mn 0.4 Ti 0.4 O 2 Cathode Using Interfacial Carbon Deposition and Carbon Nanotube-Mediated Electrical Percolation

Mn-based cation disordered rocksalt oxides (Mn-DRX) are emerging as promising cathode materials for next-generation Li-ion batteries due to their high specific capacities and cobalt and nickel free characteristic. However, to reach the theoretical capacity, solid-state method synthesized Mn-DRX materials require activation via post-synthetic ball milling, typically incorporating more than 20 wt.% conductive carbon that adversely reduces the electrode level gravimetric capacity. To solve this issue, we firstly deposit amorphous carbon on the surface of the Li 1.2 Mn 0.4 Ti 0.4 O 2 (LMTO) particles to increase the electrical conductivity by a five order of magnitude. Although the cathode material gravimetric first charge capacity reaches 180 mAh/g, its highly irreversible behavior leads to a 70 mAh/g first discharge capacity. Subsequently, to ensure a good electrical percolation network, the LMTO material is ball milled with multi-wall carbon nanotube (CNT) to obtain a 78.7 wt.% LMTO active material loading in the cathode electrode (LMTO-CNT). As a result, a 210 mAh/g cathode electrode gravimetric first charge and 165 mAh/g first discharge capacity are obtained, compared to the respective capacity values of 222 mAh/g and 155 mAh/g for the LMTO ball milled with 20 wt.% SuperP C65 electrode (LMTO-SP). After 50 cycles, the LMTO-CNT delivers a 121 mAh/g electrode gravimetric discharge capacity, largely outperforming the 44 mAh/g value of the LMTO-SP. In conclusion, our study demonstrates that while ball milling is necessary to achieve the theoretical capacity of LMTO, a careful selection of the additive, such as CNT, effectively reduces the required carbon quantity to achieve a higher electrode gravimetric discharge capacity.

25 ENERGY STORAGE↗

Influence of Electrolyte Additives on Interfacial Stability of Manganese-Rich Lithium-Ion Battery Cathodes

Affordable, long-lasting energy storage has become critical to support increased electricity demand in recent years. Cobalt-free, lithium- and manganese-rich lithium nickel manganese oxide (LMR-NM) cathodes stand to reduce cost and supply-chain concerns associated with traditional cobalt-containing cathodes for lithium-ion batteries by leveraging more earth-abundant materials; however, they have shown issues with long-term cycling stability. Here, we investigate lithium difluoro(oxalate)borate (LiDFOB), tris(trimethylsilyl) phosphite (TMSPi), and vinylene carbonate (VC) electrolyte additives for their ability to improve cycling performance of LMR-NM (0.3 Li 2 MnO 3 + 0.7 LiMn 0.5 Ni 0.5 0 2 ) cells. Cryogenic scanning transmission electron microscopy (cryo-STEM) with electron energy loss spectroscopy enables the construction of a structure–function relationship between cathode electrolyte interphase (CEI) characteristics and the electrochemical performance of cells aged with these additives. We find the combination of 2 wt % TMSPi + 1 wt % LiDFOB performs better than any single additive, achieving a 28% improvement in specific capacity over the baseline electrolyte after long-term cycling. We attribute this to LiDFOB mitigating Mn ion dissolution, with cryo-STEM showing Mn stabilized up to the CEI surface, coupled with improved CEI structure and chemistry enabled by TMSPi, evidenced by a moderately thick (∼7–15 nm) CEI that appears to protect against further electrolyte reactions with the particle. These results, achieved through site-specific nanoscale characterization, directly reveal mechanisms through which electrolyte engineering can improve the performance of earth-abundant cathodes, enabling informed development of more affordable and reliable batteries to meet future energy storage needs.

25 ENERGY STORAGE↗

Minimizing Cr-Evaporation from Balance of Plant Components by Utilizing Cost-Effective Alumina-Forming Austenitic Steels

A solid oxide fuel cell (SOFC) is a clean and efficient energy conversion device. The development of intermediate-temperature SOFCs has made it preferable to use metallic interconnects (MICs) to greatly reduce the cost and significantly increase the efficiency compared to ceramic interconnect materials. However, gaseous chromium species will evaporate from the chromium-containing layer formed on the surface of commonly used MICs and balance of plant (BoP) components. Volatile chromium species have been shown to form solid deposits which poison the cathodes of SOFCs, causing drastic cell performance degradation and thereby limiting commercialization. In order to alleviate the Cr poisoning and achieve long-term high performance of SOFC stacks, various Al2O3-forming austenitic (AFA) stainless steels applied at different temperatures are evaluated in this project. Based on our Phase I results (500 h operation), it is shown that on the AFAs, an alumina-based protective layer forms under high temperature that is invulnerable to water vapor effects and suppresses the diffusion of chromium and manganese which can prevent the generation of spinels on the alloy surface. Therefore, 310S, OC4 and OC5 at 800 °C and 625, OC11 and OC11LZ at 900 °C are selected to be tested in the Phase II long-term operation. From the results, we find that besides the lower Cr evaporation rates and better oxidation resistance of AFAs than benchmark alloys after short-term (500 h) operation, AFAs also possess the sturdy and compact alumina layer after a long-term operation (5000 h). A protective oxide layer is of great importance for the long-term high-temperature operation of structural materials. The high-temperature oxidation behavior of AFAs and commercial 310S and 625 alloys in Air + 10% H 2 O at 800 °C and 900 °C is systematically investigated. Severe breakaway oxidation and minor spallation are observed for the 310S and 625 after the long-term operation, while the AFAs show high oxidation resistance. It is found that the formation of a continuous alumina layer could greatly prevent the volatilization of chromium vapors. In addition, the corresponding evolving models are discussed. Chromium evaporation from BoP components in high-temperature environment could severely deteriorate the electrochemical performance of SOFC. Several methods were applied to evaluate the Cr evaporation rates of BoP after 500 h exposure at 800 °C to 900 °C in air with 10% H 2 O. An optimal method was designed to exclude the effect of silicon (Si) deposits from quartz tube and sodium (Na) deposits from the sodium carbonate on the oxidation process and the chemical interaction between Cr gaseous species and alumina tube which could provide further quantitative correlation of the evaporated Cr species quantities and degradation rates of SOFC. Based on the great performance of AFAs after long-term operation, AFAs are assembled with Anode-supported cells (ASC) to investigate the the Cr deposition of anode-supported cell under a constant current density of 0.5 A cm -2 at 800 °C with AFA alloys compared with commercial alloys. In addition, the anodic and cathodic processes are deconvoluted by distribution of relaxation times (DRT) method which are comprehensively discussed. It is found out that the voltage exhibited a slight decrease of 5.09 % and 1.54 % in the presence of OC11 and OC11LZA alloy, respectively. However, a considerable decrease of 22.14 % and 12.06 % was determined in the presence of 310S and 625 alloy, respectively. AFAs possessing the low-cost, low Cr evaporation rates and the high oxidation resistance will make it of great potential to replace the existing BoP components.

36 MATERIALS SCIENCE↗

Minimizing Cr-Evaporation from Balance Of Plant Components By Utilizing Cost-Effective Alumina-Forming Austenitic Steels

A solid oxide fuel cell (SOFC) is a clean and efficient energy conversion device. The development of intermediate-temperature SOFCs has made it preferable to use metallic interconnects (MICs) to greatly reduce the cost and significantly increase the efficiency compared to ceramic interconnect materials. However, gaseous chromium species will evaporate from the chromium-containing layer formed on the surface of commonly used MICs and balance of plant (BoP) components. Volatile chromium species have been shown to form solid deposits which poison the cathodes of SOFCs, causing drastic cell performance degradation and thereby limiting commercialization. In order to alleviate the Cr poisoning and achieve long-term high performance of SOFC stacks, various Al 2 O 3 -forming austenitic (AFA) stainless steels applied at different temperatures are evaluated in this project. Based on our Phase I results (500 h operation), it is shown that on the AFAs, an alumina-based protective layer forms under high temperature that is invulnerable to water vapor effects and suppresses the diffusion of chromium and manganese which can prevent the generation of spinels on the alloy surface. Therefore, 310S, OC4 and OC5 at 800 °C and 625, OC11 and OC11LZ at 900 °C are selected to be tested in the Phase II long-term operation. From the results, we find that besides the lower Cr evaporation rates and better oxidation resistance of AFAs than benchmark alloys after short-term (500 h) operation, AFAs also possess the sturdy and compact alumina layer after a long-term operation (5000 h). A protective oxide layer is of great importance for the long-term high-temperature operation of structural materials. The high-temperature oxidation behavior of AFAs and commercial 310S and 625 alloys in Air + 10% H 2 O at 800 °C and 900 °C is systematically investigated. Severe breakaway oxidation and minor spallation are observed for the 310S and 625 after the long-term operation, while the AFAs show high oxidation resistance. It is found that the formation of a continuous alumina layer could greatly prevent the volatilization of chromium vapors. In addition, the corresponding evolving models are discussed. Chromium evaporation from BoP components in high-temperature environment could severely deteriorate the electrochemical performance of SOFC. Several methods were applied to evaluate the Cr evaporation rates of BoP after 500 h exposure at 800 °C to 900 °C in air with 10% H 2 O. An optimal method was designed to exclude the effect of silicon (Si) deposits from quartz tube and sodium (Na) deposits from the sodium carbonate on the oxidation process and the chemical interaction between Cr gaseous species and alumina tube which could provide further quantitative correlation of the evaporated Cr species quantities and degradation rates of SOFC. Based on the great performance of AFAs after long-term operation, AFAs are assembled with Anode-supported cells (ASC) to investigate the the Cr deposition of anode-supported cell under a constant current density of 0.5 A cm -2 at 800 °C with AFA alloys compared with commercial alloys. In addition, the anodic and cathodic processes are deconvoluted by distribution of relaxation times (DRT) method which are comprehensively discussed. It is found out that the voltage exhibited a slight decrease of 5.09 % and 1.54 % in the presence of OC11 and OC11LZA alloy, respectively. However, a considerable decrease of 22.14 % and 12.06 % was determined in the presence of 310S and 625 alloy, respectively. AFAs possessing the low-cost, low Cr evaporation rates and the high oxidation resistance will make it of great potential to replace the existing BoP components.

01 COAL, LIGNITE, AND PEAT↗

Direct reuse of graphite and lithium nickel manganese cobalt oxide (NMC) recovered from ultrafast-laser ablation debris in Li-ion battery electrodes

Here we demonstrate that debris collected from the ultrafast-laser ablation of graphite anodes can be directly reused in a lithium-ion battery with little to no negative effects on electrochemical performance. Further, we show that while post-ablation NMC (LiNi 0.33 Mn 0.33 Co 0.33 O) cathode debris will require additional processing before being incorporated into an electrode, its critical materials (nickel, manganese, and cobalt) are not lost during ablation and can be recovered for recycling. Pre- and post-ablation materials are characterized with a suite of diagnostics, including SEM, TEM, X-ray CT, EDS, and XRD, to study changes in material morphology, composition and crystal structure. Graphite exhibited little to no morphological or compositional changes and a slight annealing of its crystal structure. NMC underwent profound morphological and crystallographic changes, but retained its elemental composition. Finally, post-ablation materials were re-manufactured into electrodes and cycled vs lithium metal. Graphite showed equal or better capacity and Coulombic efficiency compared to pre-ablation electrodes, while the post-ablation NMC exhibited severely reduced electrochemical performance. Furthermore, we discuss the outlook for application of this work to advanced manufacturing lines that produce next-generation, laser-patterned electrodes.

25 ENERGY STORAGE↗

Anion-exchange membranes with internal microchannels for water control in CO 2 electrolysis

Electrochemical reduction of carbon dioxide (CO 2 R) poses substantial promise to convert abundant feedstocks (water and CO 2 ) to value-added chemicals and fuels using solely renewable energy. However, recent membrane-electrode assembly (MEA) devices that have been demonstrated to achieve high rates of CO 2 R are limited by water management within the cell, due to both consumption of water by the CO 2 R reaction and electro-osmotic fluxes that transport water from the cathode to the anode. Additionally, crossover of potassium (K + ) ions poses concern at high current densities where saturation and precipitation of the salt ions can degrade cell performance. Herein, a device architecture incorporating an anion-exchange membrane (AEM) with internal water channels to mitigate MEA dehydration is proposed and demonstrated. A macroscale, two-dimensional continuum model is used to assess water fluxes and local water content within the modified MEA, as well as to determine the optimal channel geometry and composition. The modified AEMs are then fabricated and tested experimentally, demonstrating that the internal channels can both reduce K + cation crossover as well as improve AEM conductivity and therefore overall cell performance. This work demonstrates the promise of these materials, and operando water-management strategies in general, in handling some of the major hurdles in the development of MEA devices for CO 2 R.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Anion sublattice design enables superionic conductivity in crystalline oxyhalides

Solid-state batteries are attractive energy storage systems as a result of their inherent safety, but their development hinges on advanced solid-state electrolytes (SSEs). Most SSEs remain largely confined to single-anion systems (e.g., sulfides, oxides, halides, and polymers). Through mixed-anion design strategy, we develop crystalline Li 3 Ta 3 O 4 Cl 10 (LTOC) and its derivatives with excellent ionic conductivities (up to 13.7 millisiemens per centimeter at 25°C) and electrochemical stability. The LTOC structure features mixed-anion spiral chains, consisting of corner-shared oxygen and terminal chlorine atoms, which induces continuous “tetrahedron-tetrahedron” Li-ion migration pathways with low energy barriers. Additionally, LTOC demonstrates holistic cathode compatibility, enabling solid-state batteries operation at 4.9 volts versus Li/Li + and low temperature, down to −50°C. In conclusion, these findings describe a promising class of superionic conductors for high-performance solid-state batteries.

Zhao, Feipeng [Western University, London, ON (Can↗

An exploratory study of the microstructure of mullite fibers

Mullite fibers of three compositions, ranging from SiO2-rich to Al2O3-rich, were investigated by a number of transmission electron microscopy (TEM) techniques. The fibers were examined in the as-received condition and after subjecting them to thermal exposures as high as 142 C. The investigative techniques used included direct TEM of microtomed sections of mounted fibers and TEM of replicas of polished, chemically etched, and cathodically etched fibers. In addition, X-ray diffraction line broadening analyses was used for determining average crystallite size. A preliminary description of the microstructure of mullite fibers is given.

Santoro, G. J.↗

Neutralizer Hollow Cathode Simulations and Validation with Experiments

The fidelity of electric propulsion physics-based models depends largely on the validity of their predictions over a range of operating conditions and geometries. In general, increased complexity of the physics requires more extensive comparisons with laboratory data to identify the region(s) that lie outside the validity of the model assumptions and to quantify the uncertainties within its range of application. This paper presents numerical simulations of neutralizer hollow cathodes at various operating conditions and orifice sizes. The simulations were performed using a two-dimensional axisymmetric model that solves numerically a relatively extensive system of conservation laws for the partially-ionized gas in these devices. The results for the plasma are compared directly with Langmuir probe measurements. The computed keeper voltages are also compared with the observed values. Wherever model inputs and/or specific physics of the cathode discharge are uncertain, additional sensitivity calculations have been performed to quantify the uncertainties.

partially ionized gases↗

Analysis of an all-solid state nanobattery using molecular dynamics simulations under an external electric field

Present Li-ion battery (LIB) technology requires strong improvements in performance, energy capacity, charging-time, and cost to expand their application to e-mobility and grid storage. Li-metal is one of the most promising materials to replace commercial anodes such as graphite because of its 10 times higher specific capacity. However, Li-metal has high reactivity with commercial liquid electrolytes; thus, new solid materials are proposed to replace liquid electrolytes when Li-metal anodes are used. We present a theoretical analysis of the charging process in a full nanobattery, containing a LiCoO 2 cathode, a Li 7 P2S 8 I solid-state electrolyte (SSE), a Li-metal anode as well as Al and Cu collectors for the cathode and anode, respectively. In addition, we added a Li 3 P/Li 2 S film as a solid electrolyte interphase (SEI) layer between the Li-anode and SSE. Thus, we focus this study on the SEI and SSE. We simulated the charging of the nanobattery with an external voltage by applying an electric field. We estimated temperature profiles within the nanobattery and analyzed Li-ion transport through the SSE and SEI. Here, we observed a slight temperature rise at the SEI due to reactions forming $PS_{3}^{–}$ and $P_{2}S_{7}^{4}$$^{–}$ fragments at the interfaces; however, this temperature profile changes due to the charging current under the presence of the external electric field ε = 0.75 V Å –1 . Without the external field, the calculated open-circuit voltage (OCV) was 3.86 V for the battery, which is within the range of values of commercial cobalt-based LIBs. This voltage implies a spontaneous fall of available Li-ions from the anode to the cathode (during discharge). The charge of this nanobattery requires overcoming the OCV plus an additional voltage that determines the charging current. Thus, we applied an external potential able to neutralize the OCV, plus an additional 1.6 V to induce the transport of Li + from the cathode up to the anode. Several interesting details about Li + transport paths through the SSE and SEI are discussed.

25 ENERGY STORAGE↗