Unraveling the Pyrolytic Behavior and Kinetics of Single Polymers and Plastic-Rich Municipal Solid Waste Using Thermal Analysis
Pyrolysis is a highly promising thermochemical recycling technology for converting heterogenous plastic waste into sustainable fuels in a single step. Therefore, understanding the pyrolysis mechanism is essential for enabling rational reactor design and enhancing efficient recycling techniques. In this study, the thermal degradation behaviors and corresponding kinetics of pure polymers (PE, PP, and PET) and plastic-rich MSW were examined using simultaneous thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC). Experiments were carried out in the temperature range of 30-800°C with variable heating rates from 5°C/min to 20°C/min in an ultra-high purity Argon atmosphere. Our results indicated that the plastic pyrolysis was an endothermic process, with varying decomposition temperature ranges depending on their structure and composition. Various iso-conversional model-free methods (Friedman, Flynn-Wall-Ozawa, Starink, and Kissinger-Akahira-Sunose) were utilized to determine the apparent activation energy of the plastic degradation, which increased in the following order: PET (214 kJ/mol), PP (218 kJ/mol), PE (245 kJ/mol), and MSW (249 kJ/mol). Finally, Criado’s master plots were employed to identify the best-fitting reaction model and the pre-exponential factor was subsequently determined.