Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “TENSILE PROPERTIES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Tensile properties of the modified 13Cr martensitic stainless steels

This paper reports the influence of Mo and Ni on the tensile properties of the modified 13Cr martensitic stainless steels in tempered condition. Four steels with different content of Mo and Ni were prepared by induction melting followed by hot forging, quenching and tempering. The experimental results showed that the addition of about 1% and 3% Mo has a beneficial effect to increase both the tensile strength and the elongation of the steels. On the contrary, the addition of about 3% Ni into the martensitic stainless steel results in decreasing of both the tensile strength and the elongation. Among the alloys investigated the 13Cr3Mo type steel exhibited largest tensile strength of 1348 MPa and largest elongation of 12%. The observation on the tensile fractured surfaces by using scanning electron microscope supported these findings.

36 MATERIALS SCIENCE↗

Enhanced high-temperature tensile property by gradient twin structure of duplex high-Nb-containing TiAl alloy

A pre-deformation process was employed for a TiAl alloy via high-temperature torsion, in which the stability of the constituent phases was tailored, resulting in enhanced hardening capability and ductility via a gradient microstructure. A sample with a pre-torsion of 360° exhibited a yield strength of 475 MPa and an ultimate tensile strength of 592 MPa, with a tensile ductility of 47% at 850 °C. The tensile properties were significantly enhanced compared with the as-forged sample, which exhibited values of 395 MPa, 494 MPa, and 4.6%, respectively. The physical mechanisms for the significant enhancement of the mechanical property of the TiAl alloys were studied in-depth via of transmission electron microscopy, electron-backscattered diffraction, and high-energy X-ray diffraction techniques. The high strength is mainly attributed to the twin structure formed during torsion, while high fracture elongation correlates to the recrystallization of the γ phase at twin-twin sections and the load partitioning regulated by a hierarchical microstructure. When the tensile micro-strains along the loading direction and transverse direction in the γ phase of the pre-deformed TiAl alloy, a higher mechanical performance was obtained. Moreover, the fracture mode of the pre-torsional tensile sample is a combination of pores and cleavage facets which resulted from the microstructure after torsion. Finally, the gradient twin structure approach in this study provides a strategy for developing TiAl alloys with exceptionally high-temperature tensile property, and the results of the micromechanical behavior-microstructure-property relationship may improve the understanding of the plastic deformation of TiAl alloys.

36 MATERIALS SCIENCE↗

Creep and Tensile Properties of Direct Metal Laser Sintered (DMLS) Inconel 738LC Coupons and Comparison to Cast Properties

Due to the nature of sCO2 power cycles, a number of turbine parts must have good mechanical properties at elevated temperatures. For recompression cycles, the turbine inlet temperature is between 600°C - 750°C, which puts nearly all high-temperature turbine parts into a creep regime. The high-strength parts in these applications are often composed of materials having high nickel or chrome contents, and are often termed superalloys. At these temperatures, the blades must survive mechanical loads due to centrifugal stress and blade loading. While centrifugal stress is primarily a function of tip velocity and its associated centrifugal acceleration, blade loading is a function of power density. Since sCO2 turbomachinery is approaching the power density of rocket engines, blade loading tends to be quite large. Another result of this high power density is that blade passages for 1-10 MW turbines tend to be quite small, making conventional fabrication methods challenging and costly; this leads engineers to pioneer new techniques to address these challenges. The authors of the current work are addressing this challenge by applying additive manufacturing techniques in the production of a 10 MW radial inflow impeller. While a comprehensive database exists for the mechanical properties of forged and cast superalloys, data is sparse for superalloys fashioned by direct metal laser sintering (DMLS) or other additive manufacturing methods. For the remainder of this work, the term printed will refer to components manufactured using one of these processes for brevity. The current work stems from the desire to manufacture a radial inflow turbine impeller using additive manufactured (AM) Inconel 738. While Siemens has adopted the use of DMLS printed Inconel 738 for use in select aviation engine parts, creep and tensile properties have not been published to the extent needed to validate a given design. The current work will show creep and tensile properties of AM Inconel 738 in the horizontal and vertical build directions and their respective comparison to cast Inconel 738 properties.

wilkes, Jason↗

Influence of Sodium on the Tensile Properties of Optimized Grade 92 Steel

This report provides an update on the evaluation of sodium compatibility of advanced alloy, optimized Grade 92, and the reference materials. The report is a deliverable (Level 3) in FY15 (M3AT-15AN1602072), under the Work Package AR-15AN160207, “Sodium Compatibility” performed by Argonne National Laboratory (ANL), as part of Advanced Reactor Technologies program. This work package supports the advanced structural materials development by providing corrosion, microstructure, and tensile property data from the standpoint of sodium compatibility of advanced structural alloys. During this fiscal year, sodium exposure experiments were performed at 600°C in forced convection sodium loops at Argonne National Laboratory. The oxygen content of sodium was controlled by the cold-trapping method to achieve ≈1 wppm oxygen level. Specimens were removed from the sodium loop after a pre-determined exposure time for post-sodium-exposure-examination, including weight and thickness measurements, cross-sectional examinations, microhardness measurements, microstructural characterization, and tensile tests at the sodium exposure temperature. Data of sodium-exposed specimens were compared with thermal aging data obtained at 650°C to separate the effects of sodium exposures and thermal aging. This report adds to the results on corrosion performance, microstructure and tensile properties of ferritic-martensitic exposed to sodium at 600°C. Specimens of G92-0, Opt. G92-4, Opt. G92-4T, and G91-H30176 for times up to 8,200 h, and Opt. G92-8T for 1,653 h were exposed to sodium at 600°C.

36 MATERIALS SCIENCE↗

Tensile Properties of a Cast Al-Si-Mg Alloy with Reduced Si Content and Cr Addition at High Temperature

Tensile properties of an Al-Si-Mg casting alloy with reduced Si content and Cr addition were investigated at room and high temperatures. It was found that the studied alloy exhibits a remarkable performance up to 200 °C, with comparable or slightly higher strength than typical values for Al-Si-Mg-Cu alloys, commonly used for high-temperature applications, and good elongation. This is due to the choice of proper heat treatment and to the formation of dispersoids containing Cr during heat treatment, which are stable at the considered temperatures, as demonstrated by scanning and transmission electron microscopy (STEM) analysis. Interestingly, exposure to 300 °C during tensile tests enhanced an additional formation of dispersoids. It is believed that heating the material in T6 condition led to such observed dispersoids formation since precursors were already present in the Al matrix. This is not sufficient to avoid material softening at 300 °C, but it represents an interesting point in order to develop alternative heat treatment routes for dispersion-strengthened Al alloys.

36 MATERIALS SCIENCE↗

Influence of mechanical alloying and extrusion conditions on the microstructure and tensile properties of Low-Cr ODS FeCrAl alloys

Low-chromium (<10%Cr) high strength oxide dispersion strengthened (ODS) FeCrAl alloys are considered promising candidates for accident tolerant fuel cladding in light water fission reactors. These alloys are designed to combine the beneficial high temperature mechanical properties of ODS materials with the exceptionally high temperature oxidation resistance of FeCrAl in comparison to conventional Zr-containing cladding materials, while also providing good mechanical and aqueous corrosion behavior under normal light water reactor operating conditions. The initial (1st generation) ODS FeCrAl alloys combined gas atomized FeCrAl powders with yttria and other oxides for alloying element additions using the mechanical alloying approach. These alloys exhibited low ductility but excellent high temperature tensile strength while maintaining good oxidation resistance at temperatures up to 1400 °C. In an attempt to improve alloy ductility for accident tolerant fuel cladding applications, new low-Cr ODS FeCrAl alloys with decreased oxygen content were developed with the Zr alloying solute already gas atomized into the powder prior to mechanical alloying. The resultant Fe-10Cr-6.1Al-0.3Zr+0.3Y 2 O 3 (106ZY) powders were ball milled for 10, 20, and 40hr followed by consolidation via hot extrusion at temperatures ranging from 900 to 1050 °C. Increasing the mechanical alloying time decreased the resultant grain size and improved high temperature tensile properties. Decreasing the extrusion temperature refined the grain size and subsequently strengthened the ODS FeCrAl 106ZY alloys while lowering the ductility. Scanning transmission electron microscopy (STEM) and energy dispersive spectroscopy (EDS) demonstrated the Zr solute addition effectively sequestered impurity C and N within the matrix. The root mean square (RMS) hardening superposition model for yield strength shows good agreement with experimental results. Errors between predicted and experimental values are discussed within the scope of processing parameters. As a result, these 2nd generation 106ZY alloys show a distinct increase in alloy ductility without sacrificing the high temperature tensile properties characteristic of legacy or 1st generation ODS FeCrAl alloys.

36 MATERIALS SCIENCE↗

Hot rolling of ZK60 magnesium sheet with isotropic tensile properties from tubing made by Shear Assisted Processing and Extrusion (ShAPE)

In order to evaluate the viability of ShAPE processed Mg alloys as a feedstock for fabricating lightweight sheet material, tubes consisting of ShAPE-extruded Mg alloy ZK60 were flattened into plates and hot rolled at 450 °C to reductions of 37%, 68%, and 93%. The mechanical properties and microstructure of the rolled material were characterized through tensile testing and electron backscattered diffraction (EBSD). ZK60 specimens rolled to 68% reduction had tensile properties similar to published properties of rolled ZK60 sheets fabricated using conventional processes, and exhibited negligible tensile anisotropy referenced to the rolling direction. Additional rolling from 68% to 93% reduced the ultimate tensile stress in the rolling direction from 341.74±5.96 MPa to 260.76±22.4MPa. The yield stress and elongation to failure of the material also decreased from 292.16±1.11 MPa to 256.93±18.4 MPa and 6.95±1.94% to 3.38±0.51%, respectively, but negligible little anisotropy was observed with respect to loading direction. EBSD mapping indicated that the as-extruded ZK60 had texture rotated away from the basal direction which developed into a strong basal texture over numerous hot rolling steps. This evolution in texture has been observed after rolling for hot-rolled ZK60 fabricated through conventional extrusion processes. The initial grain structure was found to have experienced noticeable twinning from flattening the tube into plate. After hot rolling, the grain structure became more equiaxed, but the average grain diameter did not change appreciably from 5.15 ± 3.39 µm in the ShAPE extruded material, to 5.27 ± 12.44 µm in the 93% hot rolled sheet. This response to hot rolling is similar to the response of ZK60 fabricated using other methods such as Equal Channel Angular Processing (ECAP). Therefore, this work demonstrates ShAPE has the potential as an alternative method to producing feedstock for Mg alloy sheets. Modifications to the experimental procedure which could lead to improvements in observed properties are briefly discussed.

36 MATERIALS SCIENCE↗

Effect of Local Post Weld Heat Treatment on Tensile Properties in Friction Stir Welded 2219-O Al Alloy

To improve the formability of the aluminum alloy welds and overcome the size limitation of the bulk post weld heat treatment (BPWHT) on large size friction stir welded joints, a local post weld heat treatment method (LPWHT) was proposed. In this method, the resistance heating as the moving heat source is adopted to only heat the weld seam. The temperature field of LPWHT and its influence on the mechanical properties and formability of FSW 2219-O Al alloy joints was investigated. The evaluation of the tensile properties of FSW samples was also examined by mapping the global and local strain distribution using the digital image correlation methodology. The results indicated that the formability was improved greatly after LPWHT, while the hardness distribution of the FSW joint was homogenized. The maximum elongation can reach 1.4 times that of as-welded joints with increase the strength and the strain of the nugget zone increased from 3 to 8% when annealing at 300 °C. The heterogeneity on the tensile deformation of the as-welded joints was improved by the nugget zone showing large local strain value and the reason was given according to the dimple fracture characteristics at different annealing temperatures. The tensile strength and elongation of LPWHT can reach 93.3 and 96.1% of the BPWHT, respectively. Thus, the LPWHT can be advantageous compared to the BPWHT for large size welds.

36 MATERIALS SCIENCE↗

The Influence of Heat Treatments on the Microstructure and Tensile Properties of Additively Manufactured Inconel 939

This study investigated the effect of heat treatment variations on the microstructure and tensile properties of laser powder bed fused Inconel 939 manufactured via laser powder bed fusion. Three different heat treatment schedules, all of which comprise stress relief, hot isostatic pressing, solution annealing, and aging, were followed, and resulting changes in microstructure were analyzed using scanning electron microscopy. Tensile tests were conducted on specimens subjected to different heat treatments to evaluate the mechanical properties at room temperature. Microstructural results showed that solution treatment at 1190 °C for 4 h led to better removal of dendritic microstructure, while second-step aging at 850 °C resulted in monomodal distribution of precipitates. However, the second-step aging temperatures from 750 to 800 °C resulted in bi-modal distribution. The optimal heat treatment schedule, which yielded a superior combination of strength and ductility, involved solution treatment at 1190 °C for 4 h and two-step aging at 1000 °C for 6 h and 800 °C for 4 h.

Laser powder bed fusion (L-PBF)↗

Tensile Properties of Alloy 617 Bar Stock

Alloy 617 is approved for non-nuclear construction in the ASME Boiler and Pressure Vessel Code Section I and Section VIII, Division 1 but is not currently qualified for nuclear use in ASME Code Section III. A draft Code Case was developed in the 1980’s to qualify the alloy for nuclear service but efforts were stopped before the approval process was completed. Renewed interest in high temperature nuclear reactors has resulted in a new effort to qualify Alloy 617 for use in nuclear pressure vessels. Tensile properties of the alloy are needed for several aspects of Code qualification. Minimum yield strength and average tensile strength at temperature are used to set time independent allowable stress, Sm, for structural materials in B&PV Code, Section III, Subsection NH. It must also be demonstrated that there is no minimum ductility between room temperatures and 427°C (the upper temperature limit for Subsection NB) to minimize the number of fatigue tests required for developing the fatigue design curve. The bar properties reported here represent data for an additional heat and product form. A forged and rolled plate, designated as a reference material for the program, has been studied extensively and tensile properties are presented for comparison. Both of the product forms that have been characterized in the current program, plate and bar, were produced using current mill practice that includes additional refining using electro-slag re-melting. This additional processing step was not used for some of the materials in the historical database and it is of interest to demonstrate that the properties of contemporary material are comparable to the historical values.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High Temperature Tensile Properties of Unidirectional Hi-Nicalon/Celsian Composites In Air

High temperature tensile properties of unidirectional BN/SiC-coated Hi-Nicalon SiC fiber reinforced celsian matrix composites have been measured from room temperature to 1200 C (2190 F) in air. Young's modulus, the first matrix cracking stress, and the ultimate strength decreased from room temperature to 1200 C (2190 F). The applicability of various micromechanical models, in predicting room temperature values of various mechanical properties for this CMC, has also been investigated. The simple rule of mixtures produced an accurate estimate of the primary composite modulus. The first matrix cracking stress estimated from ACK theory was in good agreement with the experimental value. The modified fiber bundle failure theory of Evans gave a good estimate of the ultimate strength.

Gyekenyesi, John Z.↗

Heat Treatment Effects on the Tensile Properties and Microstructures of a SiC/RBSN Composite in Nitrogen

The room-temperature tensile properties and constituent microstructures of a unidirectionally reinforced SiC/reaction bonded silicon nitride (RBSN) composite have been investigated after heat treatments at 1400, 1600, or 1800 C in nitrogen for up to 100 hr. The composite consisted of approximately 24 vol% of aligned 140 micron diameter, continuous length, chemically vapor deposited SiC fibers in an approximately 40% porous silicon nitride matrix. The composites heat treated at 1400 C for up to 100 hr showed elastic modulus, first matrix cracking strength, and ultimate tensile strength values similar to those of the as-fabricated composites, but those heat treated for 1 hr beyond this temperature displayed losses in all three properties. Recrystallization of the SiC fibers, reaction between the carbon-rich interface coating on the fibers and the RBSN matrix, and dissociation of the RBSN matrix are the reasons for the loss of mechanical properties.

Bhatt, R. T.↗

Tensile properties of a novel W-NiTi heavy alloy with transforming matrix

A new class of W-NiTi heavy alloy was prepared by infiltration and vacuum hot pressing. The W-NiTi heavy alloy containing 90 wt% tungsten of particle size 2-8 gm exhibited excellent tensile properties of the tensile strength (1120 MPa) and elongation (7.8%). In situ synchrotron diffraction experiments provided clear evidence on the reorientation of B19'-NiTi martensite at the initial stage of the deformation and the martensitic transformation from B2-NiTi to B19'-NiTi martensite. Finally, the strain hardening of the heavy alloy resulted from the deformation of the martensite phase and the strain hardening of tungsten particles.

36 MATERIALS SCIENCE↗