Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SOLDERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Investigation of electrochemical migration on Sn-0.7Cu-0.3Ag-0.03P-0.005Ni solder alloy in HNO{sub 3} solution

Current issue in lead-free solder in term of its reliability is still under investigation. This high impact research attempts to investigate the electrochemical migration (ECM) on Sn-0.7Cu-0.3Ag-0.03P-0.005Ni solder alloy by Water Drop Test (WDT) in different concentration of HNO{sub 3} solution. The concentration of HNO{sub 3} solution used in this research was 0.05, 0.10, 0.50 and 1M. Optical Microscope (OM), Field Emission Scanning Electron Microscope (FESEM) and Energy Dispersive X-Ray Analysis (EDX) were carried out in order to analysis the ECM behavior based on the growth of dendrite formation after WDT. In general, the results demonstrated that dendrite growth is faster in higher concentration compared with low concentration of HNO{sub 3}. The concentration of HNO{sub 3} solution used has a strong correlation with Mean-Time-To-Failure (MTTF). As the concentration of HNO{sub 3} increases, the MTTF value decreases. Based on the MTTF results the solder alloy in 1M HNO{sub 3} solution is most susceptible to ECM. SnO{sub 2} forms as a corrosion by-product in the samples proved by EDX analysis. The solder alloy poses a high reliability risk in microelectronic devices during operation in 1M HNO{sub 3} solution.

36 MATERIALS SCIENCE↗

Gold-Tin Solder Wetting Behavior for Package Lid Seals

This study examined the cause of nonwetted regions of the gold (Au) finish on iron-nickel (Fe–Ni) alloy lids that seal ceramic packages using the 80Au-20Sn solder (wt %, abbreviated Au–Sn) and their impact on the final lid-to-ceramic frame solder joint. The Auger electron spectroscopy (AES) surface and depth profile techniques identified surface and through-thickness contaminants in the Au metallization layer. In one case, the AES analysis identified background levels of carbon (C) contamination on the surface; however, the depth profile detected Fe and Ni contaminants that originated from the plating process. The Fe and Ni could impede the completion of wetting and spreading to the edge of the Au metallization. The Au layer of lids not exposed to a Au–Sn solder reflow step had significant surface and through-thickness C contamination. Inorganic contaminants were absent. Subsequent simulated reflow processes removed the C contamination from the Au layer without driving Ni diffusion from the underlying solderable layer. Finally, an Au metallization having negligible C contamination developed elevated C levels after exposure to a simulated reflow process due to C contamination diffusing into it from the underlying Ni layer. However, the second reflow step removed that contamination from the Au layer, thereby allowing the metallization to support the formation of lid-to-ceramic frame Au–Sn joints without risk to their mechanical strength or hermeticity.

36 MATERIALS SCIENCE↗

Maintaining Low Voiding Solder Die Attach for Power Die While Minimizing Die Tilt

This paper addresses work to minimize voiding and die tilt in solder attachment of a large power die, measuring 9.0 mm X 6.5 mm X 0.1 mm (0.354” x 0.256” x 0.004”), to a heat spreader. As demands for larger high power die continue, minimizing voiding and die tilt is of interest for improved die functionality, yield, manufacturability, and reliability. High-power die generate considerable heat, which is important to dissipate effectively through control of voiding under high thermal load areas of the die while maintaining a consistent bondline (minimizing die tilt). Voiding was measured using acoustic imaging and die tilt was measured using two different optical measurement systems. 80Au-20Sn solder reflow was achieved using a batch vacuum solder system with optimized fixturing. Minimizing die tilt proved to be the more difficult of the two product requirements to meet. Process development variables included tooling, weight and solder preform thickness.

Hamm, Randy↗

Reliability of Sn-3.5Ag Solder Joints in High Temperature Packaging Applications

There is a significant need for next generation, high performance power electronic packages and systems with wide band gap devices to operate at high temperatures in automotive and electricity transmission applications. Sn-3.5Ag solder is a candidate for use in such packages with potential operating temperatures up to 200oC. However, there is a need to understand thermal cycling reliability of Sn-3.5Ag solders subject to such operating conditions. The results of a study on the damage evolution occurring in large area Sn-3.5Ag solders joints between silicon dies and DBC substrates subject to thermal cycling between 200oC and 5oC is presented in this paper. Damage accumulation was followed using high resolution X-ray radiography techniques while nonlinear finite element models were developed based on the mechanical property data available in literature to understand the relationship between the stress state within the solder joint and the damage evolution occurring under thermal cycling conditions. It was observed that regions of damage observed in the experiments do not correspond to the finite element predictions of the location of regions of maximum plastic work.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

A constitutive model for Sn-Pb solder.

A unified creep plasticity damage (UCPD) model for Sn-Pb solder is developed in this paper. Stephens and Frear (1999) studied the creep behavior of near-eutectic 60Sn-40Pb solder subjected to low strain rates and found that the inelastic (creep and plastic) strain rate could be accurately described using a hyperbolic Sine function of the applied effective stress. A recently developed high-rate servo-hydraulic method was employed to characterize the temperature and strain-rate dependent stress-strain behavior of eutectic Sn-Pb solder over a wide range of strain rates (10{sup -4} to 10{sup 2} per second). The steady state inelastic strain rate data from these latest experiments were also accurately captured by the hyperbolic Sine equation developed by Stephens and Frear. Thus, this equation was used as the basis for the UCPD model for Sn-Pb solder developed in this paper. Stephens, J.J., and Frear, D.R., Metallurgical and Materials Transactions A, Volume 30A, pp. 1301-1313, May 1999.

36 MATERIALS SCIENCE↗

Induction soldering of photovoltaic system components

A method comprises positioning a pair of photovoltaic wafers in a side-by-side arrangement. An interconnect is placed on the pair of wafers such that the interconnect overlaps both wafers of the pair, solder material being provided between the interconnect and the respective wafers. A solder head is then located adjacent the interconnect, and the coil is energized to effect inductive heating of the solder material. The solder head comprises an induction coil shaped to define an eye, and a magnetic field concentrator located at least partially in the eye of the coil. The magnetic field concentrator defines a passage extending axially through the eye of the coil, and may be of a material with a high magnetic permeability.

14 SOLAR ENERGY↗

Liquid-phase diffusion bonding: Temperature effects and solute redistribution in high temperature lead-free composite solders

Liquid-phase diffusion bonding (LPDB) is being studied as the primary phenomena occurring in the development of a high temperature lead-free composite solder paste composed of gas-atomized Cu-10Ni, wt.% (Cu-11Ni, at.%) powder blended with Sn-0.7Cu-0.05Ni-0.01Ge (Sn-1.3Cu-0.1Ni-0.02Ge, at.%) Nihon-Superior SN100C solder powder. Powder compacts were used as a model system. LPDB promotes enhanced interdiffusion of the low-melting alloy matrix with the solid Cu-10Ni reinforcement powder above the matrix liquidus temperature. The initial study involved the effective intermetallic compound (IMC) compositions and microstructures that occur at varying reflow temperatures and times between 250-300°C and 30-60s, respectively. Certain reflow temperatures encourage adequate interdiffusion to form a continuous highly-conductive network throughout the composite solder joints. The diffusion of nickel, in particular, has a disperse pattern that foreshadows the possibility of a highly-conductive low-melting solder that can be successfully utilized at high temperatures.

42 ENGINEERING↗

Three-dimensional (3D) visualization of reflow porosity and modeling of deformation in Pb-free solder joints

The volume, size, and dispersion of porosity in solder joints are known to affect mechanical performance and reliability. Most of the techniques used to characterize the three-dimensional (3D) nature of these defects are destructive. With the enhancements in high resolution computed tomography (CT), the detection limits of intrinsic microstructures have been significantly improved. Furthermore, the 3D microstructure of the material can be used in finite element models to understand their effect on microscopic deformation. In this paper we describe a technique utilizing high resolution (< 1 {mu}m) X-ray tomography for the three-dimensional (3D) visualization of pores in Sn-3.9Ag-0.7Cu/Cu joints. The characteristics of reflow porosity, including volume fraction and distribution, were investigated for two reflow profiles. The size and distribution of porosity size were visualized in 3D for four different solder joints. In addition, the 3D virtual microstructure was incorporated into a finite element model to quantify the effect of voids on the lap shear behavior of a solder joint. The presence, size, and location of voids significantly increased the severity of strain localization at the solder/copper interface.

36 MATERIALS SCIENCE↗

Cooling thermal parameters and microstructure features of directionally solidified ternary Sn–Bi–(Cu,Ag) solder alloys

Low temperature soldering technology encompasses Sn–Bi based alloys as reference materials for joints since such alloys may be molten at temperatures less than 180 °C. Despite the relatively high strength of these alloys, segregation problems and low ductility are recognized as potential disadvantages. Thus, for low-temperature applications, Bi–Sn eutectic or near-eutectic compositions with or without additions of alloying elements are considered interesting possibilities. In this context, additions of third elements such as Cu and Ag may be an alternative in order to reach sounder solder joints. The length scale of the phases and their proportions are known to be the most important factors affecting the final wear, mechanical and corrosions properties of ternary Sn–Bi–(Cu,Ag) alloys. In spite of this promising outlook, studies emphasizing interrelations of microstructure features and solidification thermal parameters regarding these multicomponent alloys are rare in the literature. In the present investigation Sn–Bi–(Cu,Ag) alloys were directionally solidified (DS) under transient heat flow conditions. A complete characterization is performed including experimental cooling thermal parameters, segregation (XRF), optical and scanning electron microscopies, X-ray diffraction (XRD) and length scale of the microstructural phases. Experimental growth laws relating dendritic spacings to solidification thermal parameters have been proposed with emphasis on the effects of Ag and Cu. The theoretical predictions of the Rappaz-Boettinger model are shown to be slightly above the experimental scatter of secondary dendritic arm spacings for both ternary Sn–Bi–Cu and Sn–Bi–Ag alloys examined. - Highlights: • Dendritic growth prevailed for the ternary Sn–Bi–Cu and Sn–Bi–Ag solder alloys. • Bi precipitates within Sn-rich dendrites were shown to be unevenly distributed. • Morphology and preferential region for the Ag{sub 3}Sn growth depend on Ag content and Ṫ{sub L}. • Rappaz-Boettinger model reasonably estimated the experimental scatter of λ{sub 2}.

36 MATERIALS SCIENCE↗

Thermomechanical fatigue resistance of low temperature solder for multiwire interconnects in photovoltaic modules

Novel interconnect technologies leveraging low melting temperature solders, such as multiwire interconnects, are being deployed in photovoltaic (PV) modules for improved reliability through interconnect redundancy and lower thermal loads during interconnection and lamination. However, the equivalency of standardized accelerated testing to field conditions has not yet been established for these emerging technologies. In this study, the thermomechanical fatigue resistance of low temperature solder alloys is investigated and compared to that of conventional SnPb to assess the acceleration behavior of these alloys. While InSn is shown to have sufficient thermomechanical fatigue resistance on the order of that of SnPb, these results indicate Sn–Bi alloys may have poor thermomechanical fatigue resistance at field conditions. The results also show that Sn–Bi alloys have thermal cycling acceleration factors of less than one. This indicates that the standardized accelerated thermal cycling test, such as that in IEC 61215, will produce misleading results for Sn–Bi alloys and that unique testing is required for this PV module architecture. Though accelerated thermal cycling may be a meaningful qualification test for SnPb solder joints, these results suggest that mechanical loading may be a more appropriate test for Sn–Bi multiwire interconnects. This is due to the distinct processing and geometry of multiwire interconnects which may allow for mechanical, rather than strictly metallurgical interconnections.

14 SOLAR ENERGY↗

Generalized soldering of {+-}2 helicity states in D=2+1

The direct sum of a couple of Maxwell-Chern-Simons gauge theories of opposite helicities {+-}1 does not lead to a Proca theory in D=2+1, although both theories share the same spectrum. However, it is known that by adding an interference term between both helicities we can join the complementary pieces together and obtain the physically expected result. A generalized soldering procedure can be defined to generate the missing interference term. Here, we show that the same procedure can be applied to join together {+-}2 helicity states in a full off-shell manner. In particular, by using second-order (in derivatives) self-dual models of helicities {+-}2 (spin-2 analogues of Maxwell-Chern-Simmons models) the Fierz-Pauli theory is obtained after soldering. Remarkably, if we replace the second-order models by third-order self-dual models (linearized topologically massive gravity) of opposite helicities, after soldering, we end up exactly with the new massive gravity theory of Bergshoeff, Hohm, and Townsend in its linearized approximation.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

The Influence of PV Module Materials and Design on Solder Joint Thermal Fatigue Durability

Finite element model (FEM) simulations have been performed to elucidate the effect of flat plate photovoltaic (PV) module materials and design on PbSn eutectic solder joint thermal fatigue durability. The statistical method of Latin Hypercube sampling was employed to investigate the sensitivity of simulated damage to each input variable. Variables of laminate material properties and their thicknesses were investigated. Using analysis of variance, we determined that the rate of solder fatigue was most sensitive to solder layer thickness, with copper ribbon and silicon thickness being the next two most sensitive variables. By simulating both accelerated thermal cycles (ATCs) and PV cell temperature histories through two characteristic days of service, we determined that the acceleration factor between the ATC and outdoor service was independent of the variables sampled in this study. This result implies that an ATC test will represent a similar time of outdoor exposure for a wide range of module designs. This is an encouraging result for the standard ATC that must be universally applied across all modules.

14 SOLAR ENERGY↗

Reliability Implications of Solder in Multiwire Modules under Dynamic Mechanical Loading

Two generations of multiwire modules were studied under dynamic mechanical loading (DML) with in-situ differential conductance (dG) and electroluminescence (EL) imaging. Energy-dispersive x-ray spectroscopy (EDS) was used to identity the solder alloys. The earlier generation module was found to use an In-based solder alloy, and the current generation a Bi-based alloy. The earlier generation module degraded significantly under DML with increasing resistance, while the current generation module did not demonstrate degradation under DML. Atomic force microscopy scratch testing was used to probe the wear resistance of each solder alloy. These results indicate that current multiwire designs may have higher mechanical durability than earlier generations.

atomic force microscopy↗

A high-speed micro-impact testing system for evaluating the properties of lead-free solder joints

ConclusionThis study presents a novel high-speed micro-impact testing system for evaluating the shear strength and energy absorbance properties of lead-free solder ball joints under impact velocities of 0.3–1.0 m/s. The test method can examine the failure mode transition from ductile failure to brittle failure based on the failure mode distribution percentage. The load—displacement curves can distinguish between different failure modes. Notably, the values of peak load and the energy-to-peak load at various impact speeds can be used as indices for determining solder ball under impact loading conditions. Thus, the proposed method is a suitable technique for evaluating the mechanical response of solder ball joints used in typical semiconductor packages and, therefore, represents a simple and effective technique for optimizing the chip-level reliability of portable consumer electronic products.

36 MATERIALS SCIENCE↗

Reliability Implications of Solder in Multiwire Modules under Dynamic Mechanical Loading: Preprint

Two generations of multiwire modules were studied under dynamic mechanical loading (DML). The earlier generation module was found to use an In-based solder alloy, and the current generation a Bi-based alloy. The earlier generation module degraded significantly under DML with increasing resistance, while the state-of-the-art module did not demonstrate degradation under DML. The degradation in the earlier module was attributed to damage at the solder-gridline interfaces. Atomic force microscopy scratch testing estimated the wear resistance of each solder alloy to assess susceptibility to degradation. Bi-based alloys appear to be more wear resistant than In-based alloys, consistent with the DML results. These results indicate that current multiwire designs may have higher mechanical durability than earlier generations.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Experimental Determination of the Sn-Cu-Ni Phase Diagram for Pb-Free Solder Applications

The rapid increase of scrapped electrical products disposed in landfill sites is significantly influencing the environment because of the composition of the associated components. This situation has been the stimulus for the international community to issue a directive to prohibit the use of Pb-containing solders in electronic devices and effectively ban such products on the market. The Sn-Cu-Ni has become increasingly significant as it is used in several solder alloys and more generally both Cu and Ni are common substrates that interact with Sn-based solders in microelectronic applications. However, there is currently an insufficient understanding of the phase equilibria and the associated phase diagrams of many Sn alloys. The present work implemented an experimental methodology to obtain high accuracy results for the phase equilibria between one liquid and one or two intermetallic compounds. The Sn-Cu-Ni and the associated Sn-Cu and Sn-Ni binary systems have been re-evaluated and compared with the literature. The liquidus and the invariant lines were determined for the Sn-Cu-Ni ternary at the temperatures ranges of between 240 °C and 270 °C. The result will contribute to filling phase equilibria data gaps in the Sn-rich corner of the Sn-Cu-Ni alloy system.

36 MATERIALS SCIENCE↗

Corrosion and Electrochemical Behavior of Sn-2Ag-0.5Cu Lead-Free Solders Solidified with Magnet Stirring

In this study, permanent magnet stirring (PMS) was applied to modify the crystallographic texture and corrosion resistance of Sn-2Ag-0.5Cu (SAC205) solders. The results indicate that PMS transforms the lamellar structure into equiaxed grains. Following the initiation corrosion process, the crystallographic texture shows a new class of grains that consists of single-crystal morphology with {111}{sub Sn} facets before applying PMS. This could result in severe corrosion of β-Sn crystals with non-uniform corrosion rate caused by the orientation effect of (111). The corrosion rate for SAC205 solder, measured by immersion tests in 3.5% NaCl solution at 25 °C, was significantly decreased from 31 to 8 mpy after applying PMS. This change in corrosion resistance of SAC205 solder can be attributed to the improved anodic and cathodic reaction activities caused by the modification of microstructure and crystallographic texture. The mechanism of pitting and sequential corrosion events is fully explained and discussed.

36 MATERIALS SCIENCE↗

Superconducting properties of commercially available solders for low-field applications

Solders with superconducting transitions around 4K are useful in low magnetic field environments for AC current leads or in electrical and mechanical bonds. Accurate knowledge of these solders’ superconducting properties is essential for improving high precision experiments. We have measured the electrical resistance of five commercially-available eutectic or near-eutectic solders: 50%Sn-50%Pb, 60%Sn-40%Pb, 60%Sn-40%Pb-0.3%Sb, 52%In-48%Sn, and 96.5%Sn-3.5%Ag, down to 2.3K and in applied magnetic fields from 0 to 0.1 T . We report critical temperatures T c (B), 90%–10% transition widths ΔT c , and zero-temperature critical fields B c,0 . Our best candidate for low-loss AC current wiring in low fields is 50%Sn-50%Pb, which has a zero-field T c,0 = 7.1K (with ΔT c = 0.6 K), and remained high at T c (0.1 T) = 6.9K (ΔT c = 0.6K ). We also report, for the first time, T c and B c of 60%Sn-40%Pb-0.3%Sb and B c,0 of 96.5%Sn-3.5%Ag. Our T c,0 - 3.31K (ΔT c = 0.08K) for 96.5%Sn-3.5%Ag disagrees with a widely adopted value.

Hickman, C. [North Carolina State University, Rale↗