Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Oxidation behavior”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Thermal and Oxidation Behavior of CoCrFeMnNi Alloy with and Without Yttrium Oxide Particle Dispersion

The equiatomic CoCrFeMnNi alloy is currently one of the most studied high-entropy alloys. In our previous work, a new grade of CoCrFeMnNi high-entropy alloy with yttria-based particle dispersion was introduced showing improved mechanical properties, especially high-temperature strength and creep rate. In this study, a detailed analysis of room to high-temperature thermal properties was performed, as it is important for defining the future application of the alloy and opening the discussion on tailoring the thermal response. Thermal properties are not well known for the original CoCrFeMnNi alloy or for CoCrFeMnNi with yttria dispersion. As a result of the analysis, thermal properties of both alloys and the effect of the oxide dispersion are discussed. Most of the thermal properties remain unchanged. However, it was found that the presence of 0.3% yttria influences the oxidation rate of CoCrFeMnNi alloy at the initial and intermediate oxidation times. The onset of the oxidation is described in detail. Yttria nano-oxide dispersion and related grain refinement also reduce the microstructural degradation caused by the formation of voids due to outward Mn diffusion.

36 MATERIALS SCIENCE↗

Oxidation behavior of nickel-chromium-aluminum-yttrium - Magnesium oxide and nickel-chromium-aluminum-yttrium - zirconate type of cermets

The 1100 and 1200 C cyclic oxidation resistance of dense Ni-Cr-Al-Y - MgO, Ni-Cr-Al-Y - CaZrO3, Ni-Cr-Al-Y - SrZrO3, Ni-Cr-Al-Y - MgZro3 cermets and a 70 percent dense Ni-Cr-Al-Y developmental material was determined. The cermets contained 60 and 50 volume percent of Ni-Cr-Al-Y which formed a matrix with the oxide particles imbedded in it. The cermets containing MgO were superior to cermets based on zirconates and to the porous Ni-Cr-Al-Y material.

Zaplatynsky, I.↗

High-Temperature Oxidation Behavior of FeCoCrNi+(Cu/Al)-Based High-Entropy Alloys in Humid Air

Previous studies showed some transition metal high-entropy alloy (HEA) compositions can have good oxidation resistance in air up to 800 °C. Four equiatomic HEAs have been developed based on FeCoCrNi with additions of Mn, Cu, Al or Al+Cu. The oxidation behavior of these HEAs was compared in humid (10 vol.% H2O) air at 800 °C for 100–500 h to investigate the influence of water vapor on the oxidation mechanisms. The Cu- and Al-containing alloys exhibited improved oxidation resistance over the Mn composition. For the Cu-containing alloy, a local attack of the Cu-rich phase was observed, which formed an Fe/Ni/Co/Cr spinel that was surrounded by Cr2O3. This oxide was thicker for the humid air atmosphere when compared to dry air, and the transition of the Cu oxide to the spinel was accelerated. The Al-containing HEA formed a thin Al2O3 scale with humidity suppressing AlN formation and forming a smoother oxide layer. The Al+Cu composition had the highest overall oxidation resistance (minimal local attack, no nitridation) and also showed a smooth oxide scale topography under humid air oxidation as opposed to a plate-like, rougher scale under dry air.

Crystallography↗

High-Temperature Oxidation Behavior of Wrought and Additive Manufactured Ni-based Alloys in Direct-Fired Supercritical CO2 Power Cycle Environments

Materials selection is a key concern for corrosion resistance in elevated temperature and pressure direct-fired supercritical CO2 (sCO2) power cycles. Herein, the wrought product form of alloy H282, as well as several additional nickel-based commercial alloys (230, 263, 617, 625, 740H), were exposed to direct-fired supercritical CO2 conditions (95CO2 – 4H2O – 1O2) at 750 °C and 20 MPa for over 2,000 h. Additionally, additive manufactured (AM) 282 produced by laser powder bed fusion (LPBF) were also included in the exposures. This paper focuses primarily on the differences observed in the degradation behavior of the wrought and additively manufactured materials. AM samples in the as-printed state were found to form less protective oxide scales resulting in higher oxidation rates compared to wrought samples. However, applying a 600 grit surface finish to the AM samples modified the oxidation behavior to closely resemble that of the wrought material. The AM samples formed Mo-rich carbides in the alloy beneath the oxide following sCO2 exposure, implying potentially higher levels of carbon uptake relative to the wrought material. Conversely, the AM samples seemed to be less affected by water-assisted oxide volatilization compared to the wrought material. The results are discussed in terms of the potential compatibility issues that may arise when using Ni-based alloys in the hot portions of direct-fired sCO2 power cycles, particularly in the case of thin-walled components.

Carney, Casey↗

Ferritic stainless steel interconnects for protonic ceramic electrochemical cell stacks: Oxidation behavior and protective coatings

Protonic ceramic fuel or electrolysis cells (PCFC/PCEC) have shown promising performance at intermediate temperatures. However, these technologies have not yet been demonstrated in a stack, hence the oxidation behavior of the metallic interconnect under relevant operating environments is unknown. In this work, ferritic stainless steels 430 SS, 441 SS, and Crofer 22 APU were investigated for their use as interconnect materials in the PCFC/PCEC stack. Specifically, the bare metal sheets were exposed to a humidified air environment in the temperature range from 450 °C to 650 °C, to simulate their application in a PCFC cathode or PCEC anode. Breakaway oxidation with rapid weight gain and Fe outward diffusion/oxidation was observed on all the selected stainless steel materials. A protective coating is deemed necessary to prevent the metallic interconnect from oxidizing. To mitigate the observed breakaway oxidation, state-of-the-art protective coatings, Y 2 O 3 , Ce 0.02 Mn 1.49 Co 1.49 O 4 , CuMn 1.8 O 4 and Ce/Co, were applied to the stainless steel sheets and their oxidation resistance was investigated. Dual atmosphere testing further validated the effectiveness of the protective coatings in realistic PCFC/PCEC environments, with a hydrogen gradient across the interconnect. Several combinations of metal and coating material were found to be viable for use as the interconnect for PCFC/PCEC stacks.

25 ENERGY STORAGE↗

Microstructures and oxidation behavior of some Molybdenum based alloys

The advent of Ni based superalloys revolutionized the high temperature alloy industry. These materials are capable of operating in extremely harsh environments, comprising of temperatures around 1050 C, under oxidative conditions. Demands for increased fuel efficiency, however, has highlighted the need for materials that can be used under oxidative conditions at temperatures in excess of 1200 C. The Ni based superalloys are restricted to lower temperatures due to the presence of a number of low melting phases that melt in the 1250 - 1450 C, resulting in softening of the alloys above 1000 C. Therefore, recent research directions have been skewed towards exploring and developing newer alloy systems. This thesis comprises a part of such an effort. Techniques for rapid thermodynamic assessments were developed and applied to two different systems - Mo-Si alloys with transition metal substitutions (and this forms the first part of the thesis) and Ni-Al alloys with added components for providing high temperature strength and ductility. A hierarchical approach towards alloy design indicated the Mo-Ni-Al system as a prospective candidate for high temperature applications. Investigations on microstructures and oxidation behavior, under both isothermal and cyclic conditions, of these alloys constitute the second part of this thesis. It was seen that refractory metal systems show a marked microstructure dependence of oxidation.

36 MATERIALS SCIENCE↗

Burst and oxidation behavior of Cr-coated Zirlo during simulated LOCA testing

We report Cr-coated Zr-alloys are a near-term cladding concept to improve reactor safety during accident scenarios. Burst and steam oxidation behavior of bare and Cr-coated Zirlo claddings were examined under simulated loss-of-coolant accident conditions. The 4.4 µm coating had no substantial effect on ballooning or opening geometry but did increase burst temperatures at higher pressures. The coating reduced steam oxidation of the cladding compared to bare specimens, but in regions of high strain, the coating developed through-cracks allowing rapid underlying zirconia formation.

36 MATERIALS SCIENCE↗

High-Temperature Oxidation Behavior of Iridium-Rhenium Alloys

The life-limiting mechanism for radiation-cooled rockets made from iridium-coated rhenium (Ir/Re) is the diffusion of Re into the Ir layer and the subsequent oxidation of the resulting Ir-Re alloy from the inner surface. In a previous study, a life model for Ir/Re rockets was developed. It incorporated Ir-Re diffusion and oxidation data to predict chamber lifetimes as a function of temperature and oxygen partial pressure. Oxidation testing at 1540 deg C suggested that a 20-wt percent Re concentration at the inner wall surface should be established as the failure criterion. The present study was performed to better define Ir-oxidation behavior as a function of Re concentration and to supplement the data base for the life model. Samples ranging from pure Ir to Ir-40 wt percent Re (Ir-40Re) were tested at 1500 deg C, in two different oxygen environments. There were indications that the oxidation rate of the Ir-Re alloy increased significantly when it went from a single-phase solid solution to a two-phase mixture, as was suggested in previous work. However, because of testing anomalies in this study, there were not enough dependable oxidation data to definitively raise the Ir/Re rocket failure criterion from 20-wt percent Re to a Re concentration corresponding to entry into the two-phase region.

Reed, Brian D.↗

Water vapor oxidation behaviors of nuclear graphite IG-110 for a postulated accident scenario in high temperature gas-cooled reactors

Water leakage in accidental conditions of high temperature gas-cooled reactors is one of the most critical problems that can compromise the integrity of different nuclear components. In this study, oxidation behaviors of nuclear graphite IG-110 in water ingress accidental conditions were investigated. Mass loss and oxidation rates were evaluated after oxidation tests at temperatures up to 1400 °C in an Ar-20 vol% H 2 O mixed atmosphere. The activation energy decreased from 318.6 to 148.9 kJ/mol with temperature, indicating two different oxidation regimes. The cross-sections of the oxidized samples were systematically characterized. The corresponding logarithmic porosity profiles showed a temperature dependency. Pore formation moved toward near-surface regions with increasing temperature and preferential binder oxidation, with filler particle degradation. Furthermore, oxidant concentration profiles and oxidation depths were estimated using a theoretical model and compared with the experimental results. This work provides important benchmark data and safety analysis guidance for the accident scenario in high temperature gas-cooled reactors.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Microstructure and thermal oxidation behavior of yttria-stabilized hafnia nanostructured coatings deposited on alumina

Nanostructured yttria-stabilized hafnia (YSH) coatings were grown on α-Al2O3 substrates with variable coating thickness in a wide range of ~50 nm to 1 μm. Microstructure and thermal oxidation behavior of the grown YSH coatings were studied employing X-ray diffraction (XRD), Rutherford backscattering spectrometry (RBS), scanning electron microscopy (SEM) and isothermal furnace oxidation testing. The effect of coating thickness on the crystal structure, surface/interface morphology and thermal oxidation was investigated. X-ray diffraction analyses revealed the formation of monoclinic phase for relatively thin coatings (b100 nm) indicating that the interfacial phenomena play a dominant role in phase stabilization. The evolution towards stabilized cubic phase with increasing coating thickness is observed. The SEM results indicate the dense, columnar structure of YSH coatings as a function of thickness. Thermal oxidation measurements indicate the enhanced hightemperature oxidation resistance of cubic YSH coatings.

36 MATERIALS SCIENCE↗

The oxidation behavior of a model molybdenum/tungsten-containing alloy in air alone and in air with trace levels of NaCl(g)

Thermogravimetric, metallographic, and X-ray studies of a model alloy, Ni-(17 a/o)Al-(10 a/o)Mo+W, oxidized in dry air at 600-1200 C and in air with 10 ppm NaCl gas at 900 C, are reported. The alloy was melted under Ar and pretreated in flowing H2 for 24 h at 1300 C. Polished 1.3 x 1.3 x 0.2-cm specimens were washed and degreased prior to oxidation in a quartz tube within a furnace for up to 120 hr. The oxidation activation energy of the alloy is determined to be about 30 kcal/mole. The specimens oxidized at 900 C and hotter exhibited oxidized and nitrided phases covered by complex NiMoO4, NiWO4, and NiAl2O4 scales and a porous, nonprotective outer layer of NiO. The oxidation behavior is found to be determined by the formation and growth of the scale, especially the (Mo,W)O2 component. Al2O3 scale layers were not formed, and further runs with pure O2 or Ar-(20 percent)O2 ruled out an explanation of this phenomenon based on aluminum nitride formation. The oxidation was accelerated by the addition of NaCl gas, a finding attributed to the reaction of NaCl with external locally protective Al2O3 scales and with the internal(Mo, W)O2 layers.

Smeggil, J. G.↗

10,000-Hour Cyclic Oxidation Behavior at 982 C (1800 F) of 68 High-Temperature Co-, Fe-, and Ni-Base Alloys

Sixty-eight high temperature Co-, Fe-, and Ni-base alloys were tested for 10-one thousand hour cycles in static air at 982 C (1800 F). The oxidation behavior of the test samples was evaluated by specific weight change/time data, x-ray diffraction of the post-test samples, and their final appearance. The gravimetric and appearance data were combined into a single modified oxidation parameter, KB4 to rank the cyclic oxidation resistance from excellent to catastrophic. The alloys showing the 'best' resistance with no significant oxidation attack were the alumina/aluminate spinel forming Ni-base turbine alloys: U-700, NASA-VIA and B-1900; the Fe-base ferritic alloys with Al: TRW-Valve, HOS-875, NASA-18T, Thermenol and 18SR; and the Ni-base superalloy IN-702.

Barrett, Charles A.↗

Graphite Oxidation Behavior: NRC Graphite Behavior Model

Graphite microstructure and oxidation Graphite crystal structure and basal planes Reactive surface area sites Zig-zag and Arm-chair Pore microstructure effects Interconnectivity Reactivity and oxygen transport Oxygen-graphitereaction Not C-O reaction! Temperature effects Oxygen diffusion to graphite Diffusion into the microstructure High temperature vs low temperature diffusion Oxidation: It’s a gradient of factors

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Cyclic and isothermal oxidation behavior at 1100 and 1200 C of Ni-20Cr, Ni-20Cr-3Mn, Ni-20Cr-3Si, and Ni-40Cr alloys

Alloys of Ni-20Cr, Ni-20Cr-3Mn, Ni-20Cr-3Si, and Ni-40Cr were cyclically oxidized at 1100 and 1200 C for up to 100 hours. Oxidation behavior was judged by sample thickness and weight change, metallography, diffraction, and microprobe analysis. The least attacked were Ni-40Cr and Ni-20Cr-3Si. The alloy Ni-20Cr-3Mn was much less attacked than Ni-20Cr, but more than the other alloys. The formation of Cr2O3 accounted for the increased resistance of Ni-Cr and Ni-20Cr-3Si, and the formation of MnCr2O4 accounts for the improvement in Ni-20Cr-3mn over Ni-20Cr.

Lowell, C. E.↗

Cyclic Oxidation Behavior of HVOF Bond Coatings Deposited on La- and Y-doped Superalloys

One suggested strategy for improving the performance of thermal barrier coating (TBC) systems used to protect hot section components in gas turbines is the addition of low levels of dopants to the Ni-base superalloy substrate. To quantify the benefit of these dopants, the oxidation behavior of three commercial superalloys with different Y and La contents was evaluated with and without a NiCoCrAlYHfSi bond coating deposited by high velocity oxygen fuel (HVOF) spraying. Cyclic oxidation experiments were conducted in dry O{sub 2} at 1050, 1100 and 1150 C. At the highest temperature, the bare superalloy without La showed more attack due to its lower Al content but no difference in oxidation rate or scale adhesion was noted at lower temperatures. With a bond coating, the alumina scale was non-uniform in thickness and spalled at each temperature. Among the three coated superalloys, no clear difference in oxide growth rate or scale adhesion was observed. Evaluations with a YSZ top coat and a bond coating without Hf are needed to better determine the effect of superalloy dopants on high temperature oxidation performance.

36 MATERIALS SCIENCE↗

Effect of Layer-Graded Bond Coats on Edge Stress Concentration and Oxidation Behavior of Thermal Barrier Coatings

Thermal barrier coating (TBC) durability is closely related to design, processing and microstructure of the coating Z, tn systems. Two important issues that must be considered during the design of a thermal barrier coating are thermal expansion and modulus mismatch between the substrate and the ceramic layer, and substrate oxidation. In many cases, both of these issues may be best addressed through the selection of an appropriate bond coat system. In this study, a low thermal expansion and layer-graded bond coat system, that consists of plasma-sprayed FeCoNiCrAl and FeCrAlY coatings, and a high velocity oxyfuel (HVOF) sprayed FeCrAlY coating, is developed to minimize the thermal stresses and provide oxidation resistance. The thermal expansion and oxidation behavior of the coating system are also characterized, and the strain isolation effect of the bond coat system is analyzed using the finite element method (FEM). Experiments and finite element results show that the layer-graded bond coat system possesses lower interfacial stresses. better strain isolation and excellent oxidation resistance. thus significantly improving the coating performance and durability.

Zhu, Dongming↗

Effect of high temperature preoxidation treatment on the oxidation behavior of MoSi 2 - and WSi 2 –Al 2 O 3 composites

Composites of 30 vol% MoSi 2 -70 vol% Al 2 O 3 and 30 vol% WSi 2 -70 vol% Al 2 O 3 were prepared via sintering at 1600 °C in argon. The high-temperature preoxidation treatments were applied at 1000°-1200 °C for 10–120 min in air. The non-isothermal oxidation tests were conducted in air at temperatures ranging between 50° and 870 °C to study and understand the influence of the alumina phase and preoxidation process on the low-temperature oxidation behavior. The optical and scanning electron microscopy, X-ray diffraction, X-ray photoelectron and Raman spectroscopy were used to characterize the surface layers formed. The oxidation-induced mass gains were substantially reduced by 82.1–99.8%, implying their enhanced oxidation resistance. This was due to the formation of highly dense, protective surface layers with a sufficient thickness (3.1–14.2 μm). The structural and surface analyses revealed their complex chemistries, since the ternary (Mo–Si–Al, W–Si–Al) intermetallic, mullite, alumina and silica phases with high oxidation resistances were identified within these surface features. In addition, the high-temperature electrical properties of the composites were highly preserved after the preoxidation treatment, and their electrical conductivities were measured as 45.1–78.6 S/cm at 800 °C and 40.1–69.1 S/cm at 900 °C.

36 MATERIALS SCIENCE↗