Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Nickel”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Electrolyte Management Considerations in Modern Nickel Hydrogen and Nickel Cadmium Cell and Battery Designs

This paper reviews three general areas where the potassium ion content can impact the performance and life of nickel hydrogen and nickel cadmium cells. Sample calculations of the concentration or volume changes that can take place within operating cells are presented. With the aid of an accurate model of an operating cell or battery, the impact of changes of potassium ion content within a potential cell design can be estimated. All three of these areas are directly related to the volume tolerance and pore size engineering aspects of the components used in the cell or battery design.

Thaller, Lawrence H.↗

High–Nickel NMA: A Cobalt–Free Alternative to NMC and NCA Cathodes for Lithium–Ion Batteries

High-nickel LiNi 1–x–y Mn x Co y O 2 (NMC) and LiNi 1–x–y Co x Al y O 2 (NCA) are the cathode materials of choice for next-generation high-energy lithium-ion batteries. Both NMC and NCA contain cobalt, an expensive and scarce metal generally believed to be essential for their electrochemical performance. Herein, a high-Ni LiNi 1–x–y Mn x Al y O 2 (NMA) cathode of desirable electrochemical properties is demonstrated benchmarked against NMC, NCA, and Al–Mg-codoped NMC (NMCAM) of identical Ni content (89 mol%) synthesized in-house. Despite a slightly lower specific capacity, high-Ni NMA operates at a higher voltage by ≈40 mV and shows no compromise in rate capability relative to NMC and NCA. In pouch cells paired with graphite, high-Ni NMA outperforms both NMC and NCA and only slightly trails NMCAM and a commercial cathode after 1000 deep cycles. Further, the superior thermal stability of NMA to NMC, NCA, and NMCAM is shown using differential scanning calorimetry. Here, considering the flexibility in compositional tuning and immediate synthesis scalability of high-Ni NMA very similar to NCA and NMC, this study opens a new space for cathode material development for next-generation high-energy, cobalt-free Li-ion batteries.

25 ENERGY STORAGE↗

Crossover Effects in Batteries with High–Nickel Cathodes and Lithium–Metal Anodes

It is well understood that cathode-to-anode crossover, especially of transition-metal ions, can significantly impact the long-term cycling of lithium-ion batteries. The dissolved transition-metal ions in lithium-ion cells deposit on the graphite anode, disrupt the solid-electrolyte interphase (SEI), and catalyze further side reactions. Meanwhile, crossover effects in lithium-metal batteries have rarely been studied. This study is the first to investigate crossover effects in lithium-metal batteries with high-nickel layered-oxide cathodes. It is shown that the crossover of transition-metal ions from LiNi 0.9 Mn 0.05 Co 0.05 O 2 has minimal effect on the lithium-metal anode (LMA) due to the following reasons. The catalytic transition metals 1) have less effect on an inherently reactive LMA, 2) are diluted in a thicker SEI, and 3) are produced in overall lower quantity due to the limited cycle life of the LMA. Conversely, the LMA generates soluble decomposition products that cross over to the cathode even during early cycling. This crossover accelerates impedance growth and capacity fade at the cathode and is partially responsible for the mismatch between the performance of half and full-cells with layered-oxide cathodes. Finally, this study highlights the need for better battery design with LMA, potentially including electrolyte or cell modifications.

25 ENERGY STORAGE↗

Long-Life, Ultrahigh-Nickel Cathodes with Excellent Air Storage Stability for High-Energy Density Lithium-Based Batteries

With increased energy density and cost advantage, ultrahigh-nickel layered oxides (LiNi x M 1-x O 2 , x = 0.9 - 1.0) are becoming front-runner as cathodes for next-generation lithium-based batteries, yet their commercialization is blocked both by severe capacity fade and exponentially aggravated air degradation. Thus, it is imperative to find effective solutions to address these issues simultaneously. Here, a significant enhancement in both the cycling and air storage stability of the ultrahigh-Ni cathode LiNi 0.94 Co 0.06 O 2 is achieved via a distinctive phosphoric acid treatment strategy. The modified cathode displays remarkably improved capacity retention (from 36 % to 80 % after 1,000 cycles) and rate capability (from 0 to 105 mA h g -1 at 30C rate) in pouch cells. Impressively, the modified cathode, after air storage for 450 days, maintains the morphology and 92% of the initial capacity of the fresh sample with excellent cyclability. Comprehensive interphase and structural analyses reveal that the enhanced electrochemical performance is due to a highly stabilized electrode/electrolyte interphase that suppresses electrode corrosion and lattice reconstruction. The excellent air stability results from an adsorption-buffering effect enabled by phosphoric acid to air attack. Finally, the study demonstrates an engineering pathway to improve the cycling and air stability, facilitating the practical viability of high-capacity, affordable, ultrahigh-Ni cathodes in lithium-based batteries.

25 ENERGY STORAGE↗

Water-Fed Hydroxide Exchange Membrane Electrolyzer Enabled by a Fluoride-Incorporated Nickel–Iron Oxyhydroxide Oxygen Evolution Electrode

Here, we have developed a dissolved oxygen and galvanic corrosion method to synthesize vertically aligned fluoride-incorporated nickel–iron oxyhydroxide nanosheet arrays on a compressed Ni foam as an efficient self-supported oxygen evolution electrode. It is integrated with poly(aryl piperidinium) hydroxide exchange membrane and ionomers with high ion exchange capacity into a hydroxide exchange membrane electrolyzer fed with pure water, which achieves a performance of 1020 mA cm –2 at 1.8 V and prevents the detachment of catalysts during continuous operation (>160 h at 200 mA cm –2 ). Furthermore, this work provides a potential pathway for massively producing low-cost hydrogen using intermittent renewable energy sources.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Oxidation of TD nickel at 1050 C and 1200 C as compared with three grades of nickel of different purity

The isothermal oxidation of three nickels of different purity, Ni-200, Ni-270, and JM-Ni, was compared with that of TD-Ni in air at 1050 and 1200 C. The samples were oxidized as ground, as polished, or as annealed and polished. Weight change, metal loss, scale thickness, oxide morphology, and scale texture were determined. In degree of oxidation, TD-Ni was nearly the same as the higher purity materials, Ni-270 and JM-Ni; and less pure Ni-200 oxidized more than the others. However, in microstructure and scale texture the TD-Ni more closely resembled Ni-200. Grinding only charged the texture of the oxides of Ni_200 and TD-Ni.

Lowell, C. E.↗

Diffusion in thoriated and nonthoriated nickel and nickel-chromium alloys at 1260 C

Various solid-solid diffusion couples were assembled from thoriated and nonthoriated nickel-base alloys, welded, and diffusion annealed at 1260 C. Concentration profiles indicated that a thoria dispersion does not affect diffusion in Cr(alloy):Ni and Ni-4.8Al:Ni types of couples unless a fine grain structure is retained by the thoria particles. Metallography revealed the presence of thoria-free bands in the thoriated-Ni side of the diffusion zone. The bands contained grain boundaries and, in some cases, non-Kirkendall porosity. A mechanism based on the operation of vacancy sources is proposed to explain the thoria-free bands. In addition, a particular DS-NiCr:Ni couple had negligible Kirkendall porosity. This behavior was related to the grain structure of the particular lot of DS-NiCr.

Whittenberger, J. D.↗

Hot hardness of nickel-rich nickel-chromium-aluminum alloys

Rockwell A hardness of cast nickel-chromium-aluminum (NiCrAl) alloys was examined from ambient to 1150 K and compared to cast NiAl and IN-100. Alloy constitution was either gamma, gamma prime + gamma or gamma + beta + alpha + gamma prime. Below 1000 K beta containing NiCrAl alloys have hardnesses comparable to IN-100; above 1000 K they soften faster than IN-100. At 1150 K the hardness of beta-containing NiCrAl alloys decreases with increasing beta-content. The beta-containing NiCrAl alloys were harder than beta-NiAl. The ultimate tensile strengths of the NiCrAl alloys were estimated. The effects of NiCrAl coatings on strength and fatigue life of cooled turbine components were deduced.

Levine, S. R.↗

X-ray photoelectron spectroscopy study of nickel and nickel-base alloy surface alterations in simulated hot corrosion conditions with emphasis on eventual application to turbine blade corrosion

Research on the high temperature oxidation and Na2SO4 induced hot corrosion of some nickel base superalloys was accomplished by using ESCA to determine the surface composition of the oxidized or corroded samples. Oxidation was carried out at 900 or 1000 C in slowly flowing O2 for samples of B-1900, NASA-TRW VIA, 713C, and IN-738. Oxidation times ranged from 0.5 to 100 hr. Hot corrosion of B-1900 was induced applying a coating of Na2SO4 to peroxidized samples, the heating to 900 C in slowly flowing O2. For oxidized samples, the predominant type of scale formed by each superalloy was determined, and a marked surface enrichment of Ti was found in each case. For corroded samples, the transfer of significant amounts of material from the oxide layer to the surface of the salt layer was observed to occur long before the onset of accelerating weight-gain. Changes in surface composition were observed to coincide with the beginning of accelerating corrosion, the most striking of which was a tenfold decrease in the sulfur to sodium ration and an increase in the Cr(VI) ratio.

Mateescu, G. D.↗

Testing of the Eagle-Picher nickel-iron, the Globe ISOA lead-acid, and the Westinghouse nickel-iron battery subsystems in an electric-vehicle environment

Three full size developmental batteries were tested with electric vehicles; two nickel-iron batteries and a lead-acid battery. Constant speed and driving schedule tests were done on a chassis dynamometer. Several aspects of battery performance were evaluated for capacity, recharge efficiency, voltage response, and self discharge. Each of these three batteries exhibited some strengths and some weaknesses.

Hewitt, R.↗

Zinc-Doped High-Nickel, Low-Cobalt Layered Oxide Cathodes for High-Energy-Density Lithium-Ion Batteries

High-Ni layered oxides with Ni contents greater than 90% are promising cathode candidates for high-energy-density Li-ion batteries. However, drastic electrode-electrolyte reactions and mechanical degradation issues limit their cycle life and practical viability. We demonstrate here that LiNi 0.94 Co 0.04 Zn 0.02 O 1.99 (NCZ), obtained by incorporating 2 mol% Zn 2+ into an ultrahigh-Ni baseline cathode material LiNi 0.94 Co 0.06 O 2 (NC), delivers superior cell performance. NCZ retains 74% of the initial capacity after 500 cycles in full cell assembled with graphite anode, outperforming NC (62% retention). NCZ also possesses a higher average discharge voltage relative to NC with an outstanding average voltage retention of over 99% after 130 cycles in half cells. Bulk structural investigations unveil that Zn doping promotes a smoother phase transition, suppresses anisotropic lattice distortion, and maintains the mechanical integrity of cathode particles. Furthermore, NCZ shows an enhanced interphase stability after long-term cycling, in contrast to the seriously degraded surface chemistry in NC. Finally, this work provides a practically viable approach for designing higher-energy-density high-Ni layered oxide cathodes for lithium-ion batteries.

25 ENERGY STORAGE↗