Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MAGNETRON SPUTTERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Microstructural, optical, and electrical properties of Ni–Al co-doped ZnO films prepared by DC magnetron sputtering

Graphical abstract: - Highlights: • Ni–Al co-doped ZnO (NiAl:ZnO) composite thin films were deposited by DC magnetron sputtering at room temperature. • All films showed a highly preferential (0 0 2) c-axis orientation. • XPS revealed the presence of metallic Ni, NiO, and Ni{sub 2}O{sub 3} states, and Ni atoms were successfully doped in the NiAl:ZnO films. • NiAl:ZnO (3 wt% Ni) film showed the lowest electrical resistivity of 2.59 × 10{sup −3} Ω cm. • Band gap widening (4.18 eV) was observed in the NiAl:ZnO films with 5 wt% Ni. - Abstract: Ni–Al co-doped ZnO (NiAl:ZnO) films with fixed Al content at 2 wt% and different Ni contents (2.5, 3, and 5 wt%) were deposited by DC magnetron sputtering in an argon atmosphere at room temperature. X-ray diffraction revealed that all films showed a highly preferential (0 0 2) c-axis orientation. XPS revealed the presence of metallic Ni, NiO, and Ni{sub 2}O{sub 3} states, and Ni atoms were successfully doped in NiAl:ZnO films, which did not result in a change in ZnO crystal structure and orientation. The electrical resistivity of NiAl:ZnO film was decreased to 2.59 × 10{sup −3} Ω cm at a Ni doping concentration of 3 wt% compared with undoped Al-doped ZnO film (5.58 × 10{sup −3} Ω cm). The mean optical transmittance in the visible range was greater than 80% for all films. Band gap widening (4.18 eV) was observed in the NiAl:ZnO films with 5 wt% Ni, attributed to the Burstein–Moss shift due to the increase of carrier concentration.

36 MATERIALS SCIENCE↗

Electrochemical and microstructural characterization of magnetron-sputtered ATO thin films as Li–ion storage materials

Highlights: • Nano-structured ATO thin films prepared by RF magnetron sputtering at 25 °C, 100 °C and 200 °C, respectively. • ATO thin films show a high reversible capacity and high rate performance. • Electrochemical reaction mechanism of the ATO thin film was revealed by transmission electron microscopy. - Abstract: Sb-doped SnO{sub 2} (ATO) nanostructured thin films were prepared by using radio frequency magnetron sputtering at the substrate temperatures of 25 °C, 100 °C and 200 °C, respectively. All the ATO thin films have the similar redox characteristics in the cyclic voltammetry measurements. The ATO thin film sputtered at 200 °C shows the lowest charge transfer resistance and best electrochemical performance, and has a high reversible capacity of 679 mA h g{sup −1} at 100 mA g{sup −1} after 200 charge–discharge cycles and high rate performance of 483 mA h g{sup −1} at 800 mA g{sup −1}. The electrochemical mechanisms were investigated by analyzing the phase evolution of the ATO electrodes that had been electrochemically induced at various stages. The results reveal that the ATO underwent reversible lithiation/delithiation processes during the electrochemical cycles, i.e., the SnO{sub 2} reacted with Li{sup +} to produce metallic Sn and followed by the formation of the Li{sub x}Sn alloys during discharge process, and then Li{sub x}Sn alloys de-alloyed, Sn reacted with Li{sub 2}O, and even partially formed SnO{sub 2} during charge process.

36 MATERIALS SCIENCE↗

Compression and strong rarefaction in high power impulse magnetron sputtering discharges

Gas compression and strong rarefaction have been observed for high power impulse magnetron sputtering (HIPIMS) discharges using a copper target in argon. Time-resolved ion saturation currents of 35 probes were simultaneously recorded for HIPIMS discharges operating far above the self-sputtering runaway threshold. The argon background pressure was a parameter for the evaluation of the spatial and temporal development of the plasma density distribution. The data can be interpreted by a massive onset of the sputtering flux (sputter wind) that causes a transient densification of the gas, followed by rarefaction and the replacement of gas plasma by the metal plasma of sustained self-sputtering. The plasma density pulse follows closely the power pulse at low pressure. At high pressure, the relatively remote probes recorded a density peak only after the discharge pulse, indicative for slow, diffusive ion transport.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Negative oxygen ion formation in reactive magnetron sputtering processes for transparent conductive oxides

Reactive d.c. magnetron sputtering in Ar/O{sub 2} gas mixtures has been investigated with energy-resolved mass spectrometry. Different metal targets (Mg, Ti, Zn, In, InSn, and Sn), which are of importance for transparent conductive oxide thin film deposition, have been used to study the formation of negative ions, mainly high-energetic O{sup -}, which are supposed to induce radiation damage in thin films. Besides their energy distribution, the ions have been particularly investigated with respect to their intensity in comparison of the different target materials. To realize the comparability, various calibration factors had to be introduced. After their application, major differences in the negative ion production have been observed for the target materials. The intensity, especially of O{sup -}, differs by about two orders of magnitude. It is shown that this difference results almost exclusively from ions that gain their energy in the target sheath. Those may gain additional energy from the sputtering process or reflection at the target. Low-energetic negative ions are, however, less affected by changes of the target material. The results concerning O{sup -} formation are discussed in term of the sputtering rate from the target and are compared to models for negative ion formation.

36 MATERIALS SCIENCE↗

Deposition rates of high power impulse magnetron sputtering: Physics and economics

Deposition by high power impulse magnetron sputtering (HIPIMS) is considered by some as the new paradigm of advanced sputtering technology, yet this is met with skepticism by others for the reported lower deposition rates, if compared to rates of more conventional sputtering of equal average power. In this contribution, the underlying physical reasons for the rate changes are discussed, including (i) ion return to the target and self-sputtering, (ii) the less-than-linear increase in the sputtering yield with increasing ion energy, (iii) yield changes due to the shift of species responsible for sputtering, (iv) changes due to greater film density, limited sticking, and self-sputtering on the substrate, (v) noticeable power losses in the switch module, (vi) changes in the magnetic balance and particle confinement of the magnetron due to self-fields at high current, and (vii) superposition of sputtering and sublimation/evaporation for selected materials. The situation is even more complicated for reactive systems where the target surface chemistry is a function of the reactive gas partial pressure and discharge conditions. While most of these factors imply a reduction in the normalized deposition rate, increased rates have been reported for certain conditions using hot targets and less poisoned targets. Finally, some points of economics and HIPIMS benefits are considered.

36 MATERIALS SCIENCE↗

Ion-energy distributions at a substrate in reactive magnetron sputtering discharges in Ar/H{sub 2}S from copper, indium, and tungsten targets

Ion-energy distributions from copper, indium, and tungsten targets were measured during reactive sputtering in argon-hydrogen sulfide (H{sub 2}S) mixtures, since reactive magnetron sputtering of sulfides from metallic targets is of increasing interest, especially for photovoltaic applications (buffer and absorber layers, i.e., CuInS{sub 2}, In{sub 2}S{sub 3}, or WS{sub 2}). The mass spectra of the ions show a wide range of molecules H{sub x}S{sub n} derived from H{sub 2}S by plasma-assisted attachment both for positive (n{<=}9) and for negative (n{<=}6) ions. From the copper and the indium targets metallic ions (Cu{sup +}, In{sup +}) could be detected. While tungsten and indium sulfur compounds were found, copper does not form compounds with sulfur, caused by its lower chemical reactivity. Positive (Ar{sup +}, S{sup +}, W{sup +}, Cu{sup +}, In{sup +}, etc.) as well as negative ions (S{sup -}, InS{sup -}, WS{sub 3}{sup -}) were measured for dc and rf (27 MHz) plasma excitations. The positive ions originate mainly from the plasma in front of the substrate and exhibit energies of about 12 eV for the dc and 18 eV for the rf discharge for the substrate at floating potential. The energy difference is caused by the higher electron temperature in the rf compared to the dc discharge. The ion-energy distributions of negative ions exhibit two distinct peaks. The high-energetic peak can be attributed to ions accelerated in the cathode dark space to a high energy (up to more than 400 eV) corresponding to the cathode (target) voltage. The second peak has its maximum at zero energy decreasing steeply up to energies of about 100 eV. These ions are generated by charge-exchange collisions of energetic species from the target (reflected neutral argon, negative sulfur ions, etc.) on their passage from the target to the substrate caused by the high charge-exchange cross section. rf magnetron sputtering leads to significantly lower energies of negative ions from the target, caused by the lower discharge voltages, which could be advantageous for the deposition of active semiconducting sulfide films.

36 MATERIALS SCIENCE↗

Structure evolution of magnetron sputtered TiO{sub 2} thin films

The structure evolution of TiO{sub 2} thin films deposited by rf and dc magnetron sputtering onto nonintentionally heated, floating, glass and Si (100) substrates was investigated. As the total pressure was varied from 0.15 to 4.0 Pa, corresponding to the pressure-distance product values from 10.5 to 280 Pa mm, rutile, anatase, and a mixture thereof were deposited. The pressure-distance induced changes in ion energy were quantified by probing the ion energy distribution functions. The ion energy during synthesis was additionally varied by applying a substrate bias potential ranging from floating to -100 V revealing a similar phase formation characteristic. While the structure evolution of the TiO{sub 2} thin films reported in the literature exhibits a rather complex dependence on the process parameters, a simple correlation between the structure evolution and the ratio between the ion energy flux and the deposition flux was identified here. Phase pure anatase films were grown below 540 eV/Ti atom and phase pure rutile films were grown above 1000 eV/Ti atom. The here presented data suggest that the ratio between the ion energy flux and the deposition flux ratio defines the phase formation of TiO{sub 2} thin films during magnetron sputtering.

36 MATERIALS SCIENCE↗

Formation of pyrite (FeS{sub 2}) thin films by thermal sulfurization of dc magnetron sputtered iron

Iron films deposited by direct current magnetron sputtering onto glass substrates were converted into FeS{sub 2} films by thermal sulfurization. Experiments were carried out to optimize the sulfurization process, and the formation of FeS{sub 2} thin films was investigated under different annealing temperatures and times. High quality FeS{sub 2} films were fabricated using this process, and single phase pyrite films were obtained after sulfurization in a sulfur and nitrogen atmosphere at 450 deg. C for 1 h. Film crystallinity and phase identification were determined by using x-ray diffraction. The cubic phase pyrite films prepared were p-type, and scanning electron microscopy studies exhibited a homogeneous surface of pyrite. The authors have found that the best Ohmic contact for their pyrite thin films, using inexpensive metals, was Ni. The following were chosen for the study: Al, Mo, Fe, and Ni, and the one that led to the lowest resistance, 333 {Omega}, was Ni.

36 MATERIALS SCIENCE↗

Microstructural evaluation of NiTi-based films deposited by magnetron sputtering

Shape memory alloy films belonging to the NiTi-based systems were deposited on heated and unheated substrates, by magnetron sputtering in a custom made system, and their structure and composition was analyzed using electron microscopy. Several substrates were used for the depositions: glass, Cu-Zn-Al, Cu-Al-Ni and Ti-NiCu shape memory alloy ribbons and kapton. The composition of the Ti-Ni-Cu films showed limited differences, compared to the one of the target and the microstructure for the DC magnetron sputtering revealed crystallized structure with features determined on peel off samples from a Si wafer. Both inter and transcrystalline fractures were observed and related to the interfacial stress developed on cooling from deposition temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of oxygen on the optical and electrical properties of magnetron-sputtered indium tin oxide thin films at ambient temperature

Indium Tin Oxide (ITO) thin films are commonly used as transparent conductive layers in the production of solar cells. ITO films are typically heat-treated at temperatures exceeding 200 °C after magnetron sputtering to optimize the physical, optical, and electrical characteristics for photovoltaic devices. Here, this high temperature heating procedure greatly limits the use of potential substrates, particularly those comprised of low-temperature-rated polymers. Herein, we examine the physical, optical, and electrical transport effects of oxygen:argon plasmas during radio frequency magnetron sputtering of ITO on glass and flexible polymer surfaces without subsequent heat treatment. ITO thin films were characterized via sheet resistance testing, UV-Vis spectroscopy, X-ray diffraction, and scanning electron microscopy imaging. Sheet resistance measurements revealed an increase in surface resistance with increasing oxygen concentration during sputtering. UV-Vis optical transmittance measurements demonstrated an improvement in optical transmittance with an increase in oxygen concentration reaching a maximum transmittance at an oxygen concentration of 1-2 %. Most importantly, it was discovered that producing bilayers of ITO with pure argon sputtered plasmas followed by oxygen:argon plasmas produced ITO thin films with suitable resistance and transmittance without the need for high temperature post annealing. These results highlight a methodology for the deposition of ITO thin films on temperature sensitive substrates for flexible photovoltaics and low-cost module production.

36 MATERIALS SCIENCE↗

Confinement in PbSe wires grown by rf magnetron sputtering

Lead selenide (PbSe) nanowires were grown by magnetron sputtering on silicon with silicon dioxide (SiO{sub 2}/Si) substrates, and characterized by scanning electron microscopy, x-ray diffraction, Fourier transform infrared spectroscopy, photoluminescence, and x-ray photoelectron spectroscopy. Closely packed PbSe nanowires of approximately 100 nm diameter grew in the <111> rock-salt cubic structure orientation. These large wires showed a large blueshift in the luminescence and absorption compared to the bulk crystal, demonstrating quantum confinement. This is attributed to a strong built-in field due to surface states, band bending, and a depletion layer which confines the carrier states.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Measurements of sputtered neutrals and ions and investigation of their roles on the plasma properties during rf magnetron sputtering of Zn and ZnO targets

Langmuir probe and optical absorption spectroscopy measurements were used to determine the line-integrated electron density, electron temperature, and number density of Ar atoms in metastable {sup 3}P{sub 2} and {sup 3}P{sub 0} levels in a 5 mTorr, rf magnetron sputtering plasmas used for the deposition of ZnO-based thin films. While the average electron energy and density of Ar atoms in {sup 3}P{sub 2} and {sup 3}P{sub 0} excited states were fairly independent of self-bias voltage, the Ar {sup 3}P{sub 2}-to-electron number density ratio decreased by approximately a factor of 5 when going from −115 V to −300 V. This decrease was correlated to an increase by about one order of magnitude of the number density of sputtered Zn atoms determined by absolute actinometry measurements on Zn I using either Ar or Xe as the actinometer gas. These results were also found to be in excellent agreement with the predictions of a global model accounting for Penning ionization of sputtered Zn particles. The importance of the latter reactions was further confirmed by plasma sampling mass spectrometry showing a double peak structure for Zn ions: a low-energy component ascribed to thermalized ions created in the gas phase (by direct electron impact and by Penning ionization) and a high-energy tail due to ions ejected from the target and reaching quasi-collisionlessly the substrate surface.

36 MATERIALS SCIENCE↗

Plasma potential mapping of high power impulse magnetron sputtering discharges

Pulsed emissive probe techniques have been used to determine the plasma potential distribution of high power impulse magnetron sputtering (HiPIMS) discharges. An unbalanced magnetron with a niobium target in argon was investigated for pulse length of 100 μs at a pulse repetition rate of 100 Hz, giving a peak current of 170 A. The probe data were taken with a time resolution of 20 ns and a spatial resolution of 1 mm. It is shown that the local plasma potential varies greatly in space and time. The lowest potential was found over the target’s racetrack, gradually reaching anode potential (ground) several centimeters away from the target. The magnetic pre-sheath exhibits a funnel-shaped plasma potential resulting in an electric field which accelerates ions toward the racetrack. In certain regions and times, the potential exhibits weak local maxima which allow for ion acceleration to the substrate. Knowledge of the local E and static B fields lets us derive the electrons’ E×B drift velocity, which is about 105 m/s and shows structures in space and time.

36 MATERIALS SCIENCE↗

Ion-enhanced oxidation of aluminum as a fundamental surface process during target poisoning in reactive magnetron sputtering

Plasma deposition of aluminum oxide by reactive magnetron sputtering (RMS) using an aluminum target and argon and oxygen as working gases is an important technological process. The undesired oxidation of the target itself, however, causes the so-called target poisoning, which leads to strong hysteresis effects during RMS operation. The oxidation occurs by chemisorption of oxygen atoms and molecules with a simultaneous ion bombardment being present. This heterogenous surface reaction is studied in a quantified particle beam experiment employing beams of oxygen molecules and argon ions impinging onto an aluminum-coated quartz microbalance. The oxidation and/or sputtering rates are measured with this microbalance and the resulting oxide layers are analyzed by x-ray photoelectron spectroscopy. The sticking coefficient of oxygen molecules is determined to 0.015 in the zero coverage limit. The sputtering yields of pure aluminum by argon ions are determined to 0.4, 0.62, and 0.8 at 200, 300, and 400 eV. The variation in the effective sticking coefficient and sputtering yield during the combined impact of argon ions and oxygen molecules is modeled with a set of rate equations. A good agreement is achieved if one postulates an ion-induced surface activation process, which facilitates oxygen chemisorption. This process may be identified with knock-on implantation of surface-bonded oxygen, with an electric-field-driven in-diffusion of oxygen or with an ion-enhanced surface activation process. Based on these fundamental processes, a robust set of balance equations is proposed to describe target poisoning effects in RMS.

36 MATERIALS SCIENCE↗

Magnetron sputtered nanostructured cadmium oxide films for ammonia sensing

Nanostructured cadmium oxide (CdO) films were deposited on to glass substrates by reactive dc magnetron sputtering technique. The depositions were carried out for different deposition times in order to obtain films with varying thicknesses. The CdO films were polycrystalline in nature with cubic structure showing preferred orientation in (1 1 1) direction as observed by X-ray diffraction (XRD). Field-emission scanning electron microscope (FE-SEM) micrographs showed uniform distribution of grains of 30–35 nm size and change in morphology from spherical to elliptical structures upon increasing the film thickness. The optical band gap value of the CdO films decreased from 2.67 to 2.36 eV with increase in the thickness. CdO films were deposited on to interdigitated electrodes to be employed as ammonia (NH{sub 3}) gas sensor. The fabricated CdO sensor with thickness of 294 nm has a capacity to detect NH{sub 3} as low as 50 ppm at a relatively low operating temperature of 150 °C with quick response and recovery time. - Highlights: • Nanostructured CdO films were deposited on to glass substrates using magnetron sputtering. • Deposition time was varied in order to obtain films with different thicknesses. • The CdO films were polycrystalline in nature with preferred orientation along (1 1 1) direction. • The optical bandgap values of the films decreased on increasing the thickness of the films. • CdO films with different thickness such as 122, 204, 294 nm was capable to detect NH{sub 3} down to 50 ppm at operating temperature of 150 °C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Radio-frequency magnetron sputter deposition of ultrathick boron carbide films

The deposition of thick B 4 C films with low residual stress by conventional direct-current magnetron sputtering is accompanied by the formation of dust particulates contaminating the target, chamber, and substrates and leading to the formation of nodular defects in films. Here, we demonstrate that the formation of particulates is greatly reduced during radio-frequency magnetron sputtering (RFMS). We systematically study properties of B 4 C films deposited by RFMS with a substrate temperature of 330 °C, a target-to-substrate distance of 10 cm, Ar working gas pressure in the range of 4.5–12.0 mTorr (0.6–1.6 Pa), and substrate tilt angles of 0°–80°. All films are x-ray amorphous. A columnar structure develops with increasing either Ar pressure or substrate tilt. For columnar films, the column tilt angle decreases with increasing Ar pressure, which we attribute to a corresponding increase in the width of the distribution of impact angles of deposition flux. In contrast to the Keller–Simmons rule, the deposition rate increases with increasing Ar pressure, which suggests a better coupling of the RF energy to the plasma processes that lead to target sputtering at higher pressures. There is a critical substrate tilt angle above which the total residual stress is close to zero. This critical substrate tilt angle is ~0° for an Ar pressure of 12 mTorr (1.6 Pa). The lower residual stress state, necessary for depositing ultrathick films, is characterized by a larger concentration of nanoscale inhomogeneities and decreased mechanical properties. Based on these results, RFMS deposition of 60-μm-thick B 4 C films is demonstrated.

36 MATERIALS SCIENCE↗

Effects of sample bias on adhesion of magnetron sputtered Cr coatings on SiC

Swelling of SiC at 300 C due to in-service neutron irradiation causes tensile residual stresses in coatings which are expected to adversely affect the performance of coated SiC composite fuel cladding for light water reactors. Matching the coating swelling with the substrate, a solution common for thermal expansion, is not practical in the case of neutron irradiation. Biasing samples during magnetron sputtering deposition induces compressive residual stress which may counteract this. In this study, chromium coatings were deposited on SiC by DC magnetron sputtering with no external heating at bias voltages of –50V, –75V, and –100V. The effects of the bias voltage on morphology, residual stress, microstrain, texture, and adhesion are shown. The low deposition temperature resulted in the coating microstructure evolution following an energetic particle bombardment dominated trend. Additionally, at the two lower bias voltages knock-on implantation dominated increasing the residual stress and microstrain while at the highest bias voltage, thermal spike migration allowed for defect relaxation. When the knock-on induced compressive residual stress exceeded 0.8 GPa microcrack formation in the SiC substrate decreased coating adhesion. While no microcracks formed at the lowest bias voltage, insufficient atomic mobility during coating growth lead to voids forming in the coating. A balance is needed to form void-free coatings that have high compressive residual stress.

36 MATERIALS SCIENCE↗

Influence of plasma-generated negative oxygen ion impingement on magnetron sputtered amorphous SiO{sub 2} thin films during growth at low temperatures

Growth of amorphous SiO{sub 2} thin films deposited by reactive magnetron sputtering at low temperatures has been studied under different oxygen partial pressure conditions. Film microstructures varied from coalescent vertical column-like to homogeneous compact microstructures, possessing all similar refractive indexes. A discussion on the process responsible for the different microstructures is carried out focusing on the influence of (i) the surface shadowing mechanism, (ii) the positive ion impingement on the film, and (iii) the negative ion impingement. We conclude that only the trend followed by the latter and, in particular, the impingement of O{sup -} ions with kinetic energies between 20 and 200 eV, agrees with the resulting microstructural changes. Overall, it is also demonstrated that there are two main microstructuring regimes in the growth of amorphous SiO{sub 2} thin films by magnetron sputtering at low temperatures, controlled by the amount of O{sub 2} in the deposition reactor, which stem from the competition between surface shadowing and ion-induced adatom surface mobility.

36 MATERIALS SCIENCE↗