Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Low Creep”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Development of a Compact, Low Cost Test Fixture to Evaluate Creep in High Strength Softgoods Materials under Constant Environmental Control

Space exploration is typically driven by two key factors: cost and payload mass. Therefore creating relatively low cost, low mass space hardware is critical. With the advancement of new high-strength flexible materials, a new chapter is opening in the evolution of pressurized space structures. Space-rated inflatable structures are attractive due to their low mass, compact stowage, and capability of performing as well, or better than, their rigid counterparts for applications such as habitats and airlocks. The lifetime properties of materials used for inflatable structures are not as well characterized as heritage composite and metallic materials; therefore, they require extensive testing to increase the level of confidence in their use. Creep testing is one method of evaluating the expected lifetime of materials that may be under constant load for many years in operational use. Conventional creep testing of high-strength softgoods webbings or cordage requires a large, temperature-controlled facility, with structural frames capable of supporting large dead weights, weighing thousands of pounds on each specimen. This is expensive and takes up a significant amount of volume in a facility for a long time. This paper describes the design and analysis of a low-cost, low-volume creep test stand that can be locally environmentally controlled, so that smaller, cheaper facilities can be used for characterizing the creep life of the softgoods materials used in inflatable space structures.

Softgoods↗

Effect of composition and grain size on slow plastic flow properties of NiAl between 1200 and 1400 K

A series of about 15-micron diameter polycrystalline B2 crystal structure NiAl alloys ranging in composition from 43.9 to 52.7 Al (at. pct) have been compression tested at constant velocities in air between 1200 and 1400 K. All materials were fabricated via powder metallurgy techniques with hot extrusion as the densification process. Seven intermediate compositions were produced by blending various amounts of two master heats of prealloyed powder; in addition, a tenth alloy of identical composition, 48.25 Al, as one of the blended materials, was produced from a third master heat. Comparison of the flow stress-strain rate behavior for the two 48.25 Al alloys revealed that their properties were identical. The creep strength of materials for Al/Ni not above 1.03 was essentially equal, and deformation could be described by a single stress exponent and activation energy. Creep at low temperatures and faster strain rates is independent of grain sizes and appears to be controlled by a subgrain mechanism. However, at higher temperatures and slower strain rates, diffusional creep seems to contribute to the overall deformation rate.

Whittenberger, J. Daniel↗

Increased Mechanical Properties Through the Addition of Zr to GRCop-84

GRCop-84 (Cu-8 at.% Cr-4 at.% Nb) has shown exceptional mechanical properties above 932 F (773 K). However, its properties below 932 F (773 K) are inferior to precipitation strengthened alloys such as Cu-Cr, Cu-Zr and Cu-Cr-Zr when they are in the fully aged, hard-drawn condition. It has been noted that the addition of small amounts of Zr, typically 0.1 wt.% to 0.5 wt.%, can greatly enhance the mechanical properties of copper-based alloys. Limited testing was conducted upon GRCop-84 with an addition of 0.4 wt.% Zr to determine its tensile, creep and low cycle fatigue (LCF) properties. Very large increases in strength (up to 68%) and ductility (up to 123%) were observed at both room temperature and 932 F (773 K). Creep properties at 932 F (773 K) demonstrated more than an order of magnitude decrease in the creep rate relative to unmodified GRCop-84 with a corresponding order of magnitude increase in creep life. Limited LCF testing showed that the modified alloy had a comparable LCF life at room temperature, but it was capable of sustaining a much higher load. While more testing and composition optimization are required, the addition of Zr to GRCop-84 has shown clear benefits to mechanical properties.

Ellis, David L.↗

AN INITIAL ASSESSMENT OF THE CREEP-RUPTURE STRENGTHS FOR WELDMENTS WITH ALLOY 800H BASE METAL AND ALLOY 617 FILLER METAL

In Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Alloy 800H is qualified for elevated-temperature nuclear construction for temperatures up to 760°C (1,400°F) and a maximum service life of 300,000 hours. There are two permissible filler metals for Alloy 800H weldments specified in Division 5: ENiCrFe-2 (Alloy A) and ERNiCr-3 (Alloy 82). Low creep-rupture strengths of these weldments at the upper limits of the qualified temperatures and service lives may restrict the design envelope for elevated-temperature nuclear construction with Alloy 800H. As a result, an alternative filler metal is desired to improve the creep-rupture strengths of Alloy 800H weldments for the qualified temperatures and service lives. This work investigates an overmatched filler metal. Specifically, a weldment with Alloy 800H base metal and Alloy 617 filler metal fabricated by semiautomated gas tungsten arc welding is investigated. A scoping creep-rupture test program was conducted of cross-weld specimens at temperatures ranging from 750 to 1,000°C (1,292 to 1,832°F). Preliminary results on the creep-rupture strengths of the Alloy 800H weldment with Alloy 617 filler metal do not show significant improvement compared to the filler metals currently qualified in Division 5 for Alloy 800H weldments. Consequently, work is in progress to investigate a matching filler metal.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Stress versus temperature dependent activation energies in creep

The activation energy for creep at low stresses and elevated temperatures is lattice diffusion, where the rate controlling mechanism for deformation is dislocation climb. At higher stresses and intermediate temperatures, the rate controlling mechanism changes from that of dislocation climb to one of obstacle-controlled dislocation glide. Along with this change, there occurs a change in the activation energy. It is shown that a temperature-dependent Gibbs free energy does a good job of correlating steady-state creep data, while a stress-dependent Gibbs free energy does a less desirable job of correlating the same data. Applications are made to copper and a LiF-22 mol. percent CaF2 hypereutectic salt.

Freed, A. D.↗

Stress versus temperature dependence of activation energies for creep

The activation energy for creep at low stresses and elevated temperatures is associated with lattice diffusion, where the rate controlling mechanism for deformation is dislocation climb. At higher stresses and intermediate temperatures, the rate controlling mechanism changes from dislocation climb to obstacle-controlled dislocation glide. Along with this change in deformation mechanism occurs a change in the activation energy. When the rate controlling mechanism for deformation is obstacle-controlled dislocation glide, it is shown that a temperature-dependent Gibbs free energy does better than a stress-dependent Gibbs free energy in correlating steady-state creep data for both copper and LiF-22mol percent CaF2 hypereutectic salt.

Freed, A. D.↗

Rapid Bayesian High Entropy Alloy Designs Fabricated via Wire Arc Additive Manufacturing

Purpose: This project seeks to demonstrate a new high-throughput (rapid) alloy design technique applied to creating new high entropy alloys (HEAs) for extreme environments. High entropy alloys shift the design paradigm from being focused on a single principal element (e.g. nickel-based alloys) to target alloys that include high atomic fractions (X >10%) of multiple elements. These HEA materials can exhibit sluggish diffusion and enhanced corrosion resistance, ideal for potential applications in advanced ultra supercritical (A-USC) steam cycles for power generation. Scope: The addition of multiple elements in high atomic fractions creates an enormous design space that cannot easily be investigated by traditional material design strategies such as designed of experiments (DOE). This project utilizes a Bayesian machine learning algorithm that has been modified to work with calculation of phase diagrams (CALPHAD) software. This Bayesian algorithm reduces manual inputs and increase the likelihood of achieving an optimal solution. Compositional inputs to this algorithm will be assessed using existing material property models for high temperature strength and corrosion resistance. The target for alloy performance will be a 15% (~100 ⁰C) increase in allowable service temperature beyond heat-resistant stainless steels while maintaining or improving alloy cost and corrosion resistance. Haynes 230 was selected as a baseline, which is 57 wt% Ni with 22 wt% Cr 14 wt% W, and 2 wt% Mo as solid solution strengtheners. In addition to rapid design via Bayesian machine learning, the alloys were rapidly fabricated using a multi-wire arc additive manufacturing (mWAAM) technique which allows for precise control of alloy composition and assessing of alloy design “windows” to study composition effects. Build speeds for wire-arc additive processes are among the highest for additive technologies enabling rapid and reliable sample fabrication when compared to conventional methods such as arc button melting. The mWAAM samples will be rapidly characterized via instrumented indentation for room temperature modulus and strength and for elevated temperature strength via hot hardness tests. After being screened with hardness testing, potential alloys will be further evaluated with conventional microscopy techniques including scanning electron microscopy (SEM) and transmission electron microscopy (TEM) to assess agreement with modeling results. The most promising compositions will also be evaluated by printing full sized tensile specimens for mechanical behavior tests at elevated temperatures. Results: Bayesian machine learning of a single performance function was initially used to optimize five performance metrics: 1) single phase stability, 2) yield strength, 3) creep resistance (low diffusion coefficient), 4) freezing range (weldability), and 5) material cost. The single performance function was suboptimal as assumptions had to be made about the results while formulating the optimization. A goal-oriented Bayesian optimization strategy (Hanaoka, 2021) was implemented with CALPHAD for use with the five metrics above. This multi-objective Bayesian optimization (MOBO) enabled the design of NiCrCoFe alloys with V and W additions. A base composition of NiCoCr was selected as Ni provides a stable FCC matrix, Cr aids corrosion/oxidation resistance, and Co is a solid-solutions strengthener that also improves creep by increasing the activation energy. Fe helps reduce diffusion coefficients and cost. Finally, V and W were selected for their reasonable solubility and high atomic misfit to aid in solid solution strengthening. Cracking of the mWAAM specimens was an early issue, and the Easton solidification cracking model (Easton et al., 2014a) was selected for addition to the MOBO function. High performing alloys fabricated by mWAAM included Ni 28 Cr 25 Co 26 Fe 15 V 8 and Ni 62 Cr 18 Co 1 Fe 3 W 15 . It was observed that even after adapting the mWAAM process for W, the W did not fully dissolve. To fully evaluate the Ni 62 Cr 18 Co 1 Fe 3 W 15 composition, a cored wire (80-20 NiCr sheath/powder core) was manufactured and printed via WAAM, and HIP’ing was utilized to homogenize and densify the printed alloy. The V and W alloys produced met metrics 1 (solid solution), 4 (solidification cracking), and 5 (cost). However, an unmodeled mechanism of thermal stress cracking was identified in the WAAM produced materials, perhaps exacerbated by the lack of grain boundary strengthening elements (B, C). Conclusions & Recommendations: A high-throughput (rapid) alloy design technique was applied to designing and manufacturing new high entropy alloys (HEAs) for extreme environments utilizing MOBO and mWAAM. The developed process was rapid and effective in addressing the mechanisms included in the model. The lack of grain boundary strengthening element additions (e.g., B, C) was a simplification that likely produced thermal stress cracking that turned into a large part of the investigation. Additions on the order of 0.005 wt% B and 0.05 wt% C likely would have minimized thermal stress grain boundary cracking. Overall, the high throughput design strategy is promising for rapid design of metrics-driven alloys for advanced ultra supercritical (A-USC) steam cycles for power generation. The MOBO and mWAAM process could be commercialized to accelerate metrics-driven alloy design. In addition, the cored-wire process utilized for scale-up is a promising high-volume process for WAAM alloy development and scale-up.

36 MATERIALS SCIENCE↗

Effects of Vacuum Ultraviolet Radiation on Thin Polyimide Films Evaluated

NASA anticipates launching the Next Generation Space Telescope (NGST) mission-- whose purpose is to examine the origins of our universe by making measurements in the infrared portion of the spectrum--in 2009. So that the telescope can operate at very low temperatures (less than 100 K), a halo orbit about the second Lagrangian point (L2) is being considered because it is far from Earth and its reflected sunlight. The Sun-Earth L2 point is located 1.53 10(exp 6) km from the Earth in the direction away from the Sun. This mission presents new challenges in many areas of technology, including the development of a multilayer insulation sunshield for the telescope. This sunshield is required to be large (proposed dimensions of approximately 33 by 14 m), storable, deployable, and lightweight. In addition, its polymer film layers must be seamable, foldable, and resistant to tearing and creep, with low outgassing. The sunshield must maintain its structural integrity and its Sun-facing side must maintain a low solar absorptance to thermal emittance ratio (alpha/epsilon) over the planned 10-yr mission duration including over 80,000 hr facing constant sunlight.

Dever, Joyce A.↗

Evaluation of Increased Peak Temperatures for Spent Fuel Cladding Performance during Dry Storage (Rev.1)

NUREG-2214, “Managing Aging Processes in Storage (MAPS) Report,” (2019) documents the technical basis for age-related degradation mechanisms on spent nuclear fuel assemblies during dry storage operations. The technical bases have been reviewed, and hoop cladding stress calculations were conducted using the Fuel Analysis under Steady-state and Transients (FAST) code at elevated normal condition temperatures of 425°C and 450°C, and at an off-normal and accident conditions temperature of 600°C. The NUREG-2214 conclusions are substantiated by the referenced literature. The calculations demonstrate that the aging mechanisms primarily driven by hoop stress such as hydride reorientation, delayed hydride cracking, thermal and athermal (low-temperature) creep, and localized mechanical overload are either not credible or do not compromise the fuel assembly’s performance for increased peak normal condition temperatures of 425°C or 450°C during the up to 60-year dry storage period. Other aging mechanisms considered are also not credible for compromising the fuel assembly’s performance during 60-year dry storage with a peak temperature of 400ºC as specified in ISG – 11 Rev. 3, and the same is indicated for the increased peak normal condition temperatures of 425°C or 450°C.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Stress analysis, thermomechanical fatique evaluation, and root subcomponent testing of gamma/gamma prime-delta eutectic alloy

Thermomechanical fatigue (TMF) and root subcomponent tensile, creep, and low cycle fatigue (LCF) tests were conducted to determine the capability of a fully lamellar directionally solidified eutectic alloy to sustain the airfoil thermal fatigue and root attachment loads anticipated in advanced, hollow, high work turbine blades. A three dimensional finite element elastic stress analysis was performed on typical advanced hollow eutectic airfoil and root-platform designs to determine appropriate conditions for these tests. Results of TMF tests conducted on longitudinal specimens (stress axis parallel to the solidification direction) containing a simulated leading edge cooling hole pattern indicated the longitudinal TMF properties to be more than adequate for the particular advanced hollow blade analyzed, with the strain range for a 10,000 cycle life being more than 50% above the maximum strain range calculated for the advanced hollow blade.

Sheffler, K. D.↗

Cast iron-base alloy for cylinder/regenerator housing

NASACC-1 is a castable iron-base alloy designed to replace the costly and strategic cobalt-base X-40 alloy used in the automotive Stirling engine cylinder/generator housing. Over 40 alloy compositions were evaluated using investment cast test bars for stress-rupture testing. Also, hydrogen compatibility and oxygen corrosion resistance tests were used to determine the optimal alloy. NASACC-1 alloy was characterized using elevated and room temperature tensile, creep-rupture, low cycle fatigue, heat capacity, specific heat, and thermal expansion testing. Furthermore, phase analysis was performed on samples with several heat treated conditions. The properties are very encouraging. NASACC-1 alloy shows stress-rupture and low cycle fatigue properties equivalent to X-40. The oxidation resistance surpassed the program goal while maintaining acceptable resistance to hydrogen exposure. The welding, brazing, and casting characteristics are excellent. Finally, the cost of NASACC-1 is significantly lower than that of X-40.

Witter, Stewart L.↗

Affordable Fabrication and Properties of Silicon Carbide-Based Interpenetrating Phase Composites

An affordable processing technique for the fabrication of silicon carbide-based interpenetrating phase composites (IPCs) is presented. This process consists of the production of microporous carbon preforms and subsequent infiltration with liquid silicon or silicon-refractory metal alloys. The microporous preforms are made by the pyrolysis of a polymerized resin mixture for which methods to control pore volume and pore size have been established. The process gives good control of microstructure and morphology of silicon carbide-based composite materials. Room and high temperature mechanical properties (flexural strength, compressive strength, and flexural creep) of low and high silicon-silicon carbide composites will be discussed.

Singh, Mrityunjay↗

Characterizing Early Damage Evolution in CMCs

Silicon carbide / silicon carbide ceramic matrix composites (SiC/SiC CMCs) are structural ceramics that are well-suited for the extreme environment conditions of space and aerospace applications largely due to their low weight, creep resistance, damage tolerance, and high specific strength. In CMCs, the initiation and accumulation of damage depends on characteristics of the constituent landscape including porosity, interfacial properties, and geometric distribution of CMC constituents. In order to accurately predict the lifetimes of these advanced composites, it is critical to understand the evolution of damage and to characterize which early damage mechanisms subsequently lead to crack coalescence and macroscopic failure. In this study, SiC/SiC minicomposites are characterized through an experimental approach combining acoustic emission (AE) with tensile testing in-SEM (scanning electron microscope), in order to examine early damage initiation (below the proportional limit) and its evolution at room temperature. The approach provides insight into the relative activity of early damage mechanisms in CMCs at both the surface and subsurface levels and sheds light on the impact of fabrication choices on the evolution of damage to final failure. The potential application of this combined approach towards the characterization of damage in SiC/SiC CMCs under more complex testing conditions will also be discussed.

damage evolution↗

Characterizing Damage Accumulation in CMCs

Silicon carbide / silicon carbide ceramic matrix composites (SiC/SiC CMCs) are structural ceramics that are well-suited for the extreme environment conditions of aerospace applications largely due to their low weight, creep resistance, damage tolerance, and high specific strength. In CMCs, the initiation and evolution of damage is influenced by a number of factors including characteristics of the constituent landscape (porosity, interfacial properties, and geometric distribution of CMC constituents), thermo-mechanical loading parameters, and environmental conditions. However, much is still unknown about these factors and the interactions between them. In order to accurately predict the lifetimes of these advanced composites, it is critical to understand the evolution of damage and to characterize which early damage mechanisms (and their relationship to key microstructural features) subsequently lead to crack coalescence and macroscopic failure. This research focuses on the use of a multi-modal, experimental approach to examine the relative activity of surface and subsurface damage mechanisms in CMCs. The impact of fabrication choices on the evolution of damage to final failure, and the influence of constituent architecture on early damage mechanisms, are investigated. This approach combines acoustic emission (AE) with microscale deformation tracking via digital image correlation inside a scanning electron microscope (SEM-DIC). The potential application of this combined approach towards characterization of damage in SiC/SiC CMCs under more complex testing conditions is explored.

Swaminathan, Bhavana↗

GCR: Development of Improved Alloy 800H Weldment

In Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Alloy 800H is qualified for elevated-temperature nuclear construction for temperatures up to 760°C (1400°F) and a maximum service life of 300,000 hours. There are two permissible filler metals for Alloy 800H weldments specified in Division 5: ENiCrFe-2 (Alloy A) and ERNiCr-3 (Alloy 82). Low creep-rupture strengths of these weldments at the upper limits of the qualified temperatures and service lives may restrict the design envelope for elevated-temperature nuclear construction with Alloy 800H. As a result, an alternative filler metal is desired to improve the creep-rupture strengths of Alloy 800H weldments for the qualified temperatures and service lives. This work investigates an overmatched filler metal. Specifically, a weldment with Alloy 800H base metal and Alloy 617 filler metal fabricated by semiautomated gas tungsten arc welding is investigated. A scoping creep-rupture test program was conducted of cross-weld specimens at temperatures ranging from 750 to 1000°C (1292 to 1832°F). Preliminary results on the creep-rupture strengths of the Alloy 800H weldment with an Alloy 617 filler metal do not show significant improvement compared to the filler metals currently qualified in Division 5 for Alloy 800H weldments. Consequently, work is in progress to investigate a matching filler metal, UTP A 2133 Mn.

36 MATERIALS SCIENCE↗

Creep strength boosted by a high-density of stable nanoprecipitates in high-chromium steels

There is a need worldwide to develop materials for advanced power plants with steam temperatures of 700°C and above that will achieve long-term creep-rupture strength and low CO 2 emissions. The creep resistance of actual 9-12Cr steels is not enough to fulfil the engineering requirements above 600°C. In this paper, the authors report their advances in the improvement of creep properties of this type of steels by the microstructural optimization through nano-precipitation using two methodologies. 1) Applying a high temperature austenitization cycle followed by an ausforming step (thermomechanical treatment, TMT) to G91 steel, to increase the martensite dislocation density and, thus, the number density of MX precipitates (M = V,Nb; X = C,N) but at the expense of deteriorating the ductility. 2) Compositional adjustments, guided by computational thermodynamics, combined with a conventional heat treatment (no TMT), to design novel steels with a good ductility while still possessing a high number density of MX precipitates, similar to the one obtained after the TMT in G91. The microstructures have been characterized by optical, scanning and transmission electron microscopy, EBSD and atom probe tomography. The creep behaviour at 700°C has been evaluated under a load of 200 N using small punch creep tests.

36 MATERIALS SCIENCE↗

Creep-Fatigue Properties of Additional 316H PM-HIP Materials Fabricated from Different Powder Compositions and Processing Routes

The process of powder metallurgy (PM) hot isostatic pressing (HIP) works by consolidating powdered materials at relatively high temperature and pressure to form near-net-shaped components. Ideally, PM-HIP production methods can reduce component lead time and improve designs for high-temperature reactors and/or microreactors. To introduce PM-HIP into Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, it is necessary to show adequate material properties regarding creep, high-temperature low-cycle fatigue, and creep fatigue. However, prior work has shown that the creep-fatigue cycles to failure for PM-HIP 316H stainless steel are greatly reduced compared to the conventional, wrought product. This work continued creep-fatigue analysis on a 316H stainless steel with lower oxygen and nitrogen contents and at different HIP parameters than previously analyzed. The objective was to better understand what is causing the reduced PM-HIP 316H performance so improvements can be made PM-HIP 316H creep-fatigue lifetimes.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗