Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “GAS WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

The Effect of Ar and N 2 Shielding Gas on Laser Weld Porosity in Steel, Stainless Steel, and Nickel

Complete, or near complete, elimination of porosity in 304L stainless steel keyhole laser welds was observed when using N2 instead of Ar shielding gas. Partial penetration autogeneous welds made at intermediate power levels of 2-4 kW using a CW fiber laser at travel speeds of 8-11 mm/s where porosity often occurs when using inert shielding gas. To investigate this effect further, laser welds were made in N 2 and Ar gas on three additional metals (A36 steel, 21-6-9 stainless steel, and pure nickel) that have varying properties and degrees of reactivity and solubilities with the shielding gasses. Optical metallography, x-ray radiography, and x-ray computed tomography were used to characterize the porosity levels in the welds. Results show that high levels of porosity occurred in nickel, regardless of shielding gas type, while low levels or no porosity was observed in 21-6-9 for either shielding gas. However, A36 and 304L exhibited porosity in all of the welds made with Ar, and very low or no porosity when made with N2. Computed tomography was used to quantify the porosity in selected welds, showing that the pore sizes are distributed in a monotonically decreasing trend that can be described by a two parameter Weibull relationship (β=0.5429, α=0.0366). Based on the results, it is believed that the reactivity of N 2 with alloying elements, and/or its solubility in the liquid weld pool, play a significant role in reducing the amount of retained porosity in unstable keyhole welds as they solidify and cool to room temperature.

Steel↗

Properties of a thick-section narrow-gap gas tungsten arc weld of cast Haynes 282

Abstract A 50.8-mm-deep gas tungsten arc weld was made with matching filler metal in cast Haynes 282 alloy. The narrow-gap joint was filled with 104 weld beads. Visual and dye-penetrant inspection of cross-weld specimens indicated that the cast base metal contained numerous casting defects. No visible indications of physical defects were found in the weld deposit. The weld heat-affected zone was characterized by microcracking and localized recrystallization. The cause of the cracking could not be determined. Hardness testing showed that a softened region in the as-welded heat-affected zone was nearly eliminated by post-weld heat treatment. Tensile testing up to 816 °C showed that cross-weld specimen strengths ranged from 57 to 79% of the cast base metal tensile strength. The stress-rupture strengths of cross-weld specimens are within 20% of base metal reference data. Failures of both tensile and stress-rupture specimens occurred in the base metal.

282↗

Considerations on repeated repairing of weldments in Inconel 718 alloy

The effects of repeated weld repairs on the metallurgical characteristics, high cycle fatigue (HCF), and tensile properties of Inconel 718 butt weld joints were determined. A 1/4 in thick plate and a 1/2 in thick plate were used as well as tungsten inert gas welding, and Inconel 718 filler wire. Weld panels were subjected to 2, 6, and 12 repeated repairs and were made in a highly restrained condition. Post weld heat treatments were also conducted with the welded panel in the highly restrained condition. Results indicate that no significant metallurgical anomaly is evident as a result of up to twelve repeated weld repairs. No degradation in fatigue life is noted for up to twelve repeated repairs. Tensile results from specimens which contained up to twelve repeated weld repairs revealed no significant degradation in UTS and YS. However, a significant decrease in elongation is evident with specimens (solution treated and age hardened after welding) which contained twelve repeated repairs. The elongation loss is attributed to the presence of a severe notch on each side (fusion line) of the repair weld bead reinforcement.

Bayless, E. O.↗

Characterization of fusion welded ceramics in the SiC-ZrB 2 -ZrC system

Various SiC-ZrB 2 -ZrC ceramics were joined by fusion welding to determine the maximum silicon carbide content that could be joined. Commercial powders were hot pressed, machined, and preheated to 1450 °C before joining with a tungsten inert gas welding torch at 160–200 A. Resulting welds were cross-sectioned and analyzed to determine which compositions were weldable and to characterize microstructural evolution in welded samples. As compositions approached the ternary eutectic, the welds had smaller SiC grains and exhibited better weldability. Penetration depth of welds was controlled by a combination of current input and welding speed. Here, the ternary eutectic in the system was found at 36.9 ± 1.3 vol% SiC, 42.7 ± 1.5 vol% ZrB 2 , and 20.4 ± 1.9 vol% ZrC and its melting temperature was 2330 ± 23 °C. A ternary phase diagram for the SiC-ZrB 2 -ZrC was constructed and proposed via microstructural analysis of arc melted pellets on binary joins between each binary eutectic and the ternary eutectic in the system.

36 MATERIALS SCIENCE↗

Microstructure and mechanical performance of welded joint between a novel heat-resistant steel and Inconel 617 weld metal

Highlights: • MGBs were suspected as the DDC crack source during high-temperature tensile test. • Microhardness variations in different passes of joint denote grain refinement effect induced by the multi-pass welds. • After tensile test, changes in microhardness can be attributed to the extent of deformation and amount of precipitation. - Abstract: In the present study, the microstructure and mechanical performance of a tungsten inert gas welded joint between a novel heat-resistant austenitic steel and Inconel 617 weld metal were examined. Migrated grain boundaries were discovered more frequently in the lower portion of the weld metal that solidifies in austenite type. Ti-rich precipitates were observed in weld metal and Cr-rich and Nb-rich precipitates were observed in base metal. The fusion boundary area had the lowest impact toughness due to the large non-homogeneity of the microstructure. Microhardness profiles of the joint were obtained and the backing passes were found to produce the highest microhardness values, which was caused by the grain refinement effect. Ductile failure with slipping separation occurred in those joints ruptured after tensile tests at both room temperature and 923 K. In addition, multiscale precipitates in the joint after high-temperature tensile tests were inspected, where it was found that nanoscale particles contributed to the high-temperature resistance of the joint. Furthermore, microhardness changes in the joint after tensile tests were analysed according to the precipitation and strain-hardening mechanism.

36 MATERIALS SCIENCE↗

Mechanical properties of fusion welded ceramics in the $\mathrm{SiC-ZrB}$ 2 and $\mathrm{SiC-ZrB}$ 2 -$\mathrm{ZrC}$ systems

Mechanical properties of welded SiC-ZrB 2 and SiC-ZrB 2 -ZrC ceramics were measured up to 1700 °C. Commercial powders were hot pressed, machined into coupons, and preheated to 1600 °C before joining the ceramics using either tungsten inert gas welding or plasma arc welding. Toughness of the parent materials was 3–4 MPa*m 1/2 which decreased after welding to 2–2.5 MPa*m 1/2 . Strength of the SiC-ZrB 2 -ZrC parent material was ~700 MPa at 25 °C, ~300 MPa at 1700 °C, and retained 40–60% of this strength once welded. Strength of the SiC-ZrB2 parent material was ~600 MPa at 25 °C and 1700 °C and retained 20–30% of this strength once welded. Griffith analysis indicated that the strength in the parent materials was controlled by the size of SiC clusters while strength of welds was controlled by the size of pores in fusion zones. Therefore, removal of pores in produced fusion zones should be investigated to improve strength of future ceramic welds.

36 MATERIALS SCIENCE↗

Improved Assembly for Gas Shielding During Welding or Brazing

An improved assembly for inert-gas shielding of a metallic joint is designed to be useable during any of a variety of both laser-based and traditional welding and brazing processes. The basic purpose of this assembly or of a typical prior related assembly is to channel the flow of a chemically inert gas to a joint to prevent environmental contamination of the joint during the welding or brazing process and, if required, to accelerate cooling upon completion of the process.

Gradl, Paul↗

Microstructure and Wear Resistance of FeCrBSi Plasma-Sprayed Coating Remelted by Gas Tungsten Arc Welding Process

Herein, an FeCrBSi coating was fabricated via plasma spray on AISI1045 steel, and subsequently, a gas tungsten arc welding (GTA) process was employed to remelt the coating. The microstructure, microhardness, fracture toughness and surface roughness of the coating before and after remelting were investigated, as well as the wear resistance was tested by a UMT-3-type sliding wear apparatus. The results showed that, upon remelting, most defects in the as-sprayed coating were effectively eliminated, the surface roughness decreased by 43%, and the coating–substrate interface bonding changed from mechanical to metallurgical. The phase composition of the as-sprayed coating was primarily α-Fe and a small amount of hard Fe{sub 3}B phase, while the remelted coating consisted of α-Fe and (Fe,Cr){sub 23}C{sub 6} and a small quantity of CrB. In addition, remelting the coating was found to induce a 287.6% increase in the fracture toughness, a 33.4% increase in the average microhardness, and a 47.5% decrease in the wear volume, while the failure mechanism changed from abrasive wear to fatigue wear upon remelting. Therefore, GTA remelting of plasma-sprayed coating was found to be a feasible method to obtain a coating with good wear resistance.

36 MATERIALS SCIENCE↗

Irradiation response in weldment and HIP joint of reduced activation ferritic/martensitic steel, F82H

This work investigates irradiation response in the joints of F82H employed for a fusion breeding blanket. The joints, which were prepared using welding and diffusion welding, were irradiated up to 6 dpa in the High Flux Isotope Reactor at the Oak Ridge National Laboratory. Post-irradiation tests revealed hardening in weldment (WM) and base metal (BM) greater than 300 MPa. However, the heat affected zones (HAZ) exhibit about half that of WM and BM. Therefore, neutron irradiation decreased the strength of the HAZ, leaving it in danger of local deformation in this region. Further the hardening in WM made with an electron beam was larger than that in WM made with tungsten inert gas welding. However the mechanical properties of the diffusion-welded joint were very similar to those of BM even after the irradiation.

Hirose, Takanori↗

Study of Radiographic Linear Indications and Subsequent Microstructural Features in Gas Tungsten Arc Welds of Inconel 718

This study presents examples and considerations for differentiating linear radiographic indications produced by gas tungsten arc welds in a 0.05-in-thick sheet of Inconel 718. A series of welds with different structural features, including the enigma indications and other defect indications such as lack of fusion and penetration, were produced, radiographed, and examined metallographically. The enigma indications were produced by a large columnar grain running along the center of the weld nugget occurring when the weld speed was reduced sufficiently below nominal. Examples of respective indications, including the effect of changing the x-ray source location, are presented as an aid to differentiation. Enigma, nominal, and hot-weld specimens were tensile tested to demonstrate the harmlessness of the enigma indication. Statistical analysis showed that there is no difference between the strengths of these three weld conditions.

Walley, J. L.↗

Microstructural response to heat affected zone cracking of prewelding heat-treated Inconel 939 superalloy

The microstructural response to cracking in the heat-affected zone (HAZ) of a nickel-based IN 939 superalloy after prewelding heat treatments (PWHT) was investigated. The PWHT specimens showed two different microstructures: 1) spherical ordered {gamma} Prime precipitates (357-442 nm), with blocky MC and discreet M{sub 23}C{sub 6} carbides dispersed within the coarse dendrites and in the interdendritic regions; and 2) ordered {gamma} Prime precipitates in 'ogdoadically' diced cube shapes and coarse MC carbides within the dendrites and in the interdendritic regions. After being tungsten inert gas welded (TIG) applying low heat input, welding speed and using a more ductile filler alloy, specimens with microstructures consisting of spherical {gamma} Prime precipitate particles and dispersed discreet MC carbides along the grain boundaries, displayed a considerably improved weldability due to a strong reduction of the intergranular HAZ cracking associated with the liquation microfissuring phenomena. - Highlights: Black-Right-Pointing-Pointer Homogeneous microstructures of {gamma} Prime spheroids and discreet MC carbides of Ni base superalloys through preweld heat treatments. Black-Right-Pointing-Pointer {gamma} Prime spheroids and discreet MC carbides reduce the intergranular HAZ liquation and microfissuring of Nickel base superalloys. Black-Right-Pointing-Pointer Microstructure {gamma} Prime spheroids and discreet blocky type MC carbides, capable to relax the stress generated during weld cooling. Black-Right-Pointing-Pointer Low welding heat input welding speeds and ductile filler alloys reduce the HAZ cracking susceptibility.

36 MATERIALS SCIENCE↗

Materials and technological processes for High-Gradient accelerating structures: new results from mechanical tests of an innovative braze-free cavity.

Pure oxygen-free high-conductivity copper is a widely used material for manufacturing accelerating cavities working at room temperature. Several studies attempted to explain limitations associated with the maximum allowed field gradients and the behaviour of vacuum RF breakdown in copper accelerating structures through generation and movement of dislocations under stresses associated with RF electric and magnetic fields. Pure copper and also copper alloys undergo mechanical and thermal treatments to be hardened and strengthened during manufacturing, although their mechanical properties significantly change after heating above 590°C. High temperature brazing and diffusion bonding are assembly methods widely used to manufacture ultra-high vacuum accelerating devices. However, these processes, occurring at about 800–1000°C, significantly affect the mechanical properties of copper and copper alloys. We introduce here a novel Tungsten Inert Gas welding procedure, which is fast and keeps the high-gradient surfaces of the cavity and other components well below the copper annealing temperature. This process may be successfully used to manufacture copper-based accelerating components. This technology further preserves the hardness and cleanliness of copper in order to achieve the maximum accelerating gradient.

47 OTHER INSTRUMENTATION↗

Methodology for Estimating Thermal and Neutron Embrittlement of Austenitic Stainless Steel Welds During Service in Light Water Reactors

The effect of thermal aging on the degradation of fracture toughness and Charpy-impact properties of austenitic stainless steel (SS) welds has been characterized at reactor temperatures. The solidification behavior and the distribution and morphology of the ferrite phase in SS welds are described. Thermal aging of the welds results in moderate decreases in Charpy-impact strength and fracture toughness. The upper-shelf Charpy-impact energy of aged welds decreases by 50–80 J/cm2. The decrease in fracture toughness J-R curve, or JIc is relatively small. Thermal aging has minimal effect on the tensile strength. The fracture properties of SS welds are insensitive to filler metal; the welding process has a significant effect. The large variability in the data makes it difficult to establish the effect of the welding process on fracture properties of SS welds. Consequently, the approach used for evaluating thermal and neutron embrittlement of austenitic SS welds relies on establishing a lower-bound fracture toughness J-R curve for unaged and aged, and non-irradiated and irradiated, SS welds. The existing fracture toughness J-R curve data for SS welds have been reviewed and evaluated to define lower-bound J-R curve for submerged arc (SA)/shielded metal arc (SMA)/manual metal arc (MMA) welds and gas tungsten arc (GTA)/tungsten inert gas (TIG) welds in the unaged and aged conditions. At reactor temperatures, the fracture toughness of GTA/TIG welds is a factor of about 2.3 higher than that of SA/SMA/MMA welds. Thermal aging decreases the fracture toughness by about 20%. The potential combined effects of thermal and neutron embrittlement of austenitic SS welds are also described. Lower-bound curves are presented that define the change in coefficient C and exponent n of the power-law J-R curve and the JIc value for SS welds as a function of neutron dose. The potential effects of reactor coolant environment on the fracture toughness of austenitic SS welds are also discussed.

Chopra, O. K.↗

Crack Growth of D6 Steel in Air and High Pressure Oxygen

Fracture and subcritical flaw growth characteristics were experimentally deter­mined for electroless nickel plated D6 steel in dry air and high pressure oxygen environments as applicable to the Lunar Module/Environmental Control System (LM/ECS) descent gaseous oxygen (GOX) tank. The material tested included forgings, plate, and actual LM/ECS descent GOX tank material. Parent metal and TIG (tungsten inert gas) welds were tested. Tests indicate that proof testing the tanks at 4000 pounds per square inch or higher will insure safe operation at 3060 pounds per square inch. Although significant flaw growth can occur during proofing, subsequent growth of flaws during normal tank operation is negligible.

Bixler, W. D.↗

A technique for making clean holes in metallic piping and components

Testing was conducted to develop a technique of providing clean holes in process piping or in a metal surface accessible from one side only without disassembling the system. The method was performed on sample pieces of piping and worked successfully with no contaminants being found on the inside of the pipe. The materials tested were Inconel 600, 304 stainless steel, Hastelloy X, and ASTM-A53 black steel. The technique was developed such that it could be done in the field with hand-held power tools and a portable tungsten inert gas welding machine.

Hecker, T. P.↗

A fixed grid numerical methodology for phase change problems involving a moving heat source

A numerical method for solving phase change problems involving a moving heat source is presented and illustrated by a two-dimensional example. The method uses a fixed grid and does not require the implementation of the Stefan condition at the solid-liquid interface; the procedure can thus be easily implemented using existing fixed grid codes. The problem considered as an example involves natural convection flow in the molten metal during tungsten inert gas welding.

Prakash, C.↗

High-temperature containerless aircraft furnace experimentation in the microgravity environment aboard a KC-135 aircraft

This paper describes a materials processing research furnace, the High-Temperature Containerless Aircraft Furnace (HITCAF), which uses an electric arc to melt and resolidify materials in the microgravity environment aboard a KC-135 aircraft. The HITCAF is designed to process almost every electrically conductive material, including such high-melting-point materials as tungsten, within a 15 to 20 sec microgravity period. It operates on tungsten/inert gas welding principles, using an adapted commercially available tube welder. The HITCAF is fully operational and available for use by researchers representing the Government agencies, as well as industry and academia.

Poorman, Richard M.↗