Surface chemistry, friction and wear of Ni-Zn and Mn-Zn ferrites in contact with metals

X-ray photoelectron and Auger electron spectroscopy analysis were used in sliding friction experiments. These experiments were conducted with hot-pressed polycrystalline Ni-Zn and Mn-Zn ferrites, and single-crystal Mn-Zn ferrite in contact with various transition metals at room temperature in both vacuum and argon. The results indicate that Ni2O3 and Fe3O4 were present on the Ni-Zn ferrite surface in addition to the nominal bulk constituents, while MnO2 and Fe3O4 were present on the Mn-Zn ferrite surface in addition to the nominal bulk constituents. The coefficients of friction for the ferrites in contact with metals were related to the relative chemical activity of these metals. The more active the metal, the higher is the coefficient of friction. The coefficients of friction for the ferrites were correlated with the free energy of formation of the lowest metal oxide. The interfacial bond can be regarded as a chemical bond between the metal atoms and the oxygen anions in the ferrite surfaces. The adsorption of oxygen on clean metal and ferrite does strengthen the metal-ferrite contact and increase the friction. The ferrites exhibit local cracking and fracture with sliding under adhesive conditions. All the metals transferred to he surfaces of the ferrites in sliding.

Miyoshi, K.↗

Surface chemistry, friction, and wear of Ni-Zn and Mn-Zn ferrites in contact with metals

X-ray photoelectron and Auger electron spectroscopy analysis were used in sliding friction experiments. These experiments were conducted with hot-pressed polycrystalline Ni-Zn and Mn-Zn ferrites, and single-crystal Mn-Zn ferrite in contact with various transition metals at room temperature in both vacuum and argon. The results indicate that Ni2O3 and Fe3O4 were present on the Ni-Zn ferrite surface in addition to the nominal bulk constituents, while MnO2 and Fe3O4 were present on the Mn-Zn ferrite surface in addition to the nominal bulk constituents. The coefficients of friction for the ferrites in contact with metals were related to the relative chemical activity of these metals. The more active the metal, the higher is the coefficient of friction. The coefficients of friction for the ferrites were correlated with the free energy of formation of the lowest metal oxide. The interfacial bond can be regarded as a chemical bond between the metal atoms and the oxygen anions in the ferrite surfaces. The adsorption of oxygen on clean metal and ferrite does strengthen the metal-ferrite contact and increase the friction. The ferrites exhibit local cracking and fracture with sliding under adhesive conditions. All the metals transferred to the surfaces of the ferrites in sliding. Previously announced in STAR as N83-19901

Miyoshi, K.↗

In situ fabrication and characterization of cobalt ferrite nanorods/graphene composites

Cobalt ferrite nanorods/graphene composites were prepared by a one-step hydrothermal process using NaHSO{sub 3} as the reducing agent and 1-propyl-3-hexadecylimidazolium bromide as the structure growth-directing template. The reduction of graphene oxide and the in situ formation of cobalt ferrite nanorods were accomplished in a one-step reaction. The structure and morphology of as-obtained composites were characterized by field emission scanning electron microscopy, transmission electron microscopy, high resolution transmission electron microscopy, atomic force microscope, X-ray diffractometer, Fourier transform infrared spectra, X-ray photoelectron spectroscopy and Raman spectroscopy. Uniform rod-like cobalt ferrites with diameters of about 100 nm and length of about 800 nm were homogeneously distributed on the graphene sheets. The hybrid materials showed a saturation magnetization of 42.5 emu/g and coercivity of 495.1 Oe at room temperature. The electromagnetic parameters were measured using a vector network analyzer. A minimum reflection loss (RL) of − 25.8 dB was observed at 16.1 GHz for the cobalt ferrite nanorods/graphene composites with a thickness of 2 mm, and the effective absorption frequency (RL < − 10 dB) ranged from 13.5 to 18.0 GHz. The composites exhibited better absorbing properties than the cobalt ferrite nanorods and the mixture of cobalt ferrite nanorods and graphene. - Highlights: • Reduction of GO and formation of ferrites were accomplished in a one-step reaction. • Ionic liquid was used to control 1D growth of ferrite nanorods for the first time. • Cobalt ferrite nanorods/graphene composites showed dielectric and magnetic loss. • Cobalt ferrite nanorods/graphene composites exhibited better absorbing properties.

36 MATERIALS SCIENCE↗

Corrosion behavior of magnetic ferrite coating prepared by plasma spraying

Graphical abstract: The saturation magnetization (M{sub s}) of the ferrite coating is 34.417 emu/g while the M{sub s} value of the ferrite powder is 71.916 emu/g. It can be seen that plasma spray process causes deterioration of the room temperature soft magnetic properties. - Highlights: • Spinel ferrite coatings have been prepared by plasma spraying. • The coating consists of nanocrystalline grains. • The saturation magnetization of the ferrite coating is 34.417 emu/g. • Corrosion behavior of the ferrite coating was examined in NaCl solution. - Abstract: In this study, spray dried spinel ferrite powders were deposited on the surface of mild steel substrate through plasma spraying. The structure and morphological studies on the ferrite coatings were carried out using X-ray diffraction, scanning electron microscope and Raman spectroscopy. It was showed that spray dried process was an effective method to prepare thermal spraying powders. The coating showed spinel structure with a second phase of LaFeO{sub 3}. The magnetic property of the ferrite samples were measured by vibrating sample magnetometer. The saturation magnetization (M{sub s}) of the ferrite coating was 34.417 emu/g. The corrosion behavior of coating samples was examined by electrochemical impedance spectroscopy. EIS diagrams showed three corrosion processes as the coating immersed in 3.5 wt.% NaCl solution. The results suggested that plasma spraying was a promising technology for the production of magnetic ferrite coatings.

36 MATERIALS SCIENCE↗

Nanosized copper ferrite materials: Mechanochemical synthesis and characterization

Nanodimensional powders of cubic copper ferrite are synthesized by two-steps procedure of co-precipitation of copper and iron hydroxide carbonates, followed by mechanochemical treatment. X-ray powder diffraction, Moessbauer spectroscopy and temperature-programmed reduction are used for the characterization of the obtained materials. Their catalytic behavior is tested in methanol decomposition to hydrogen and CO and total oxidation of toluene. Formation of nanosized ferrite material is registered even after one hour of milling time. It is established that the prolonging of treatment procedure decreases the dispersion of the obtained product with the appearance of Fe{sub 2}O{sub 3}. It is demonstrated that the catalytic behavior of the samples depends not only on their initial phase composition, but on the concomitant ferrite phase transformations by the influence of the reaction medium. -- Graphical abstract: It is demonstrated that the catalytic behavior of the obtained copper ferrites depends not only on their initial phase composition, but on the concomitant phase transformations by the influence of the reaction medium. Display Omitted Highlights: {yields} Two-step co-precipitation-ball-milling procedure for copper ferrites preparation. {yields} The phase composition of ferrites depends on the milling duration. {yields} Ferrites transforms under the reaction medium, which affects their catalytic behavior. {yields} Ferrites decompose to magnetite and carbides during methanol decomposition. {yields} Agglomeration and further crystallization of ferrite occur during toluene oxidation.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

The influence of fine ferrite formation on the γ/α interface, fine bainite and retained austenite in a thermomechanically-processed transformation induced plasticity steel

We subjected a Fe–0.26C–1.96Si–2Mn with 0.31Mo (wt%) steel to a novel thermomechanical processing route to produce fine ferrite with different volume fractions, bainite, and retained austenite. In two types of fine ferrites were found to be: (i) formed along prior austenite grain boundaries, and (ii) formed intragranularly in the interior of austenite grains. An increase in the volume fraction of fine ferrite led to the preferential formation of blocky retained austenite with low stability, and to a decrease in the volume fraction of bainite with stable layers of retained austenite. Moreover, the difference in the morphology of the bainitic ferrite and the retained austenite after different isothermal ferrite times was found to be responsible for the deterioration of the mechanical properties. The segregation of Mn, Mo, and C at distances of 2–2.5 nm from the ferrite and retained austenite/martensite interface on the retained austenite/martensite site was observed after 2700 s of isothermal hold. Finally, it was suggested that the segregation occurred during the austenite-to-ferrite transformation, and that this would decrease the interface mobility, which affects the austenite-to-ferrite transformation and ferrite grain size.

36 MATERIALS SCIENCE↗

Properties of ferrites important to their friction and wear behavior

Environmental, chemical and crystallographical effects on the fundamental nature on friction and wear of the ferrites in contact with metals, magnetic tapes and themselves are reviewed. The removal of adsorbed films from the surfaces of ferrites results in very strong interfacial adhesion and high friction in ferrite to metal and ferrite to magnetic tape contacts. The metal ferrite bond at the interface is primarily a chemical bond between the metal atoms and the large oxygen anions in the ferrite surface, and the strength of these bonds is related to the oxygen to metal bond strength in the metal oxide. The more active the metal, the higher is the coefficient of friction. Not only under adhesive conditions, but also under abrasive conditions the friction and wear properties of ferrites are related to the crystallographic orientation. With ferrite to ferrite contact the mating of highest atomic density (most closely packed) direction on matched crystallographic planes, that is, 110 directions on /110/planes, results in the lowest coefficient of friction.

Miyoshi, K.↗

A New Grain Refiner for Ferritic Steels

A new grain refiner, LaB{sub 6}, was identified for ferritic steels based on the crystallographic calculation using the edge-to-edge matching model. Addition of 0.5 wt pct LaB{sub 6} led to a reduction of the average grain size from 765 to 92 μm and the proportion of the columnar structure from 35 to 8 pct in an as-cast Fe-4Si ferritic alloy. Although LaB{sub 6} was supposed to act as an active inoculant for δ-ferrite, thermodynamic calculation indicated that LaB{sub 6} is not thermodynamically stable in the melt of the Fe-4Si alloy. It was subject to decompose into La and B solutes. Consequently, both La and B reacted with Fe, O and S, forming different compounds. Microstructural examination at room temperature observed La{sub 2}SO{sub 2} and La{sub 2}O{sub 3} particles within the ferrite grains and Fe{sub 2}B along the grain boundaries in the samples. Through EBSD analysis, a reproducible orientation relationship between ferrite and La{sub 2}SO{sub 2} was identified. In addition, the edge-to-edge matching calculation also predicted the high potency for La{sub 2}SO{sub 2} to be an effective nucleant for δ-ferrite. It was considered that the grain refinement of LaB{sub 6} was attributed to the enhanced heterogeneous nucleation of δ-ferrite by La{sub 2}SO{sub 2}, and the solute effect of B due to the high Q-value in ferrite.

36 MATERIALS SCIENCE↗

Magnetic properties of superparamagnetic, nanocrystalline cobalt ferrite thin films deposited at low temperature

Bulk cobalt ferrite, being a hard ferrite, shows high magnetization, high resistivity and high coercivity. If thin films of cobalt ferrite can be deposited at a low enough temperature and if its coercivity can be reduced, cobalt ferrite will make a very good candidate for use as a magnetic core of an integrated inductor in RF-CMOS ICs. Though polycrystalline and epitaxial thin films of cobalt ferrite have been made by various techniques, there are no reports of thin films of superparamagnetic cobalt ferrite. In this work, nanocrystalline cobalt ferrite thin films, which are superparamagnetic as deposited, have been prepared in the solution medium at ~190 °C, using microwave irradiation. The as-prepared films have a saturation magnetization (M S ) of 401 emu/cc and coercivity (H C ) of 19 Oe at room temperature for a crystallite size of 2 nm. The cobalt ferrite powder obtained as a by-product during the same process has M S of 50 emu/g and H C of 5 Oe at room temperature, making it superparamagnetic. The as-prepared films were annealed in air at 300 °C for 5 min and 10 min. Annealing for 10 min results in an increase in crystallite size to 36 nm, M S increases from 401 emu/cc to 545 emu/cc, and H C increases from 19 Oe to 860 Oe. In conclusion, the change in magnetic properties can be directly associated with change in the crystallite size and degree of crystallographic inversion, as determined by neutron diffraction and deduced from X-ray photoelectron spectroscopy.

36 MATERIALS SCIENCE↗

Structural, Electrical, and Magnetic Properties of Ferrite-Reinforced PANI Composites

A Y-type hexagonal ferrite with chemical composition CaBaCo{sub 2}In{sub 0.5}Fe{sub 11.5}O{sub 22} was prepared by a sol-gel auto combustion technique. Y-ferrite/PANI nanocomposites were prepared by in situ polymerization of PANI with general formula CaBaCo{sub 2}In{sub 0.5}Fe{sub 11.5}O{sub 22} (1-x) + PANI (x) (x = 0.30, 0.50, 0.8, and 1) with nomenclature CF1, CF2, CF3, and P respectively. The samples were characterized by X-ray diffraction (XRD) and electrical and magnetic measurements. X-ray diffraction revealed that Y-type ferrite was successfully prepared in a single phase form. DC resistivity increases with increasing ferrite filler in nanocomposites due to large resistive behavior of ferrite in conducting polymer matrix. The dielectric constant, dielectric loss, and AC conductivity decreases with the increase of ferrite content. The dielectric is high due to interfacial polarization at low frequency, and it is low at high frequency following Maxwell-Wagner model. The coercivity increases with the decrease of ferrite filler content whereas saturation magnetization and remanence decreases which is due to random distribution of ferrite filler particles in PANI matrix. Due to large coercivity and low values of ε′ and ε″, the present samples may be useful in recording media and electromagnetic shielding.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Transmission electron microscopy investigation of acicular ferrite precipitation in {gamma}'-Fe{sub 4}N nitride

Acicular-shaped crystals precipitate from {gamma}'-Fe{sub 4}N nitride in an iron-nitrogen alloy and were identified by electron microdiffraction as {alpha}-ferrite. Acicular ferrite develops both the Nishiyama-Wassermann and the Kurdjumov-Sachs orientation relationships with {gamma}'-Fe{sub 4}N nitride. These orientation relationships were discussed in terms of the symmetry theory. The driving force for acicular ferrite formation was related to the increasing nitrogen content of {gamma}'-Fe{sub 4}N, in equilibrium with {alpha}-ferrite, with decreasing temperature. The passage from lamellar to acicular structure in Fe-N system was proposed. - Research Highlights: {yields} Acicular crystals precipitate from pearlitic{gamma}'-Fe{sub 4}N nitride in an iron-nitrogen alloy and were identified by electron microdiffraction as acicular ferrite. {yields} The crystal structure, orientation relationships with the matrix and morphologies of acicular ferrite, were studied by transmission electron microscopy. {yields} The driving force for the formation of acicular ferrite is related to the temperature dependence of nitrogen content of {gamma}'-Fe{sub 4}N, in equilibrium with ferrite. {yields} The passage from the pearlitic structure to the acicular structure in the present iron-nitrogen alloy was proposed.

36 MATERIALS SCIENCE↗

Carbon concentration measurements by atom probe tomography in the ferritic phase of high-silicon steels

Current studies using atom probe tomography (APT) show that bainitic ferrite formed at low temperature contains more carbon than what is consistent with the paraequilibrium phase diagram. However, nanocrystalline bainitic ferrite exhibits a non-homogeneous distribution of carbon atoms in arrangements with specific compositions, i.e. Cottrell atmospheres, carbon clusters, and carbides, in most cases with a size of a few nanometers. The ferrite volume within a single platelet that is free of these carbon-enriched regions is extremely small. Proximity histograms can be compromised on the ferrite side, and a great deal of care should be taken to estimate the carbon content in regions of bainitic ferrite free from carbon agglomeration. For this purpose, APT measurements were first validated for the ferritic phase in a pearlitic sample and further performed for the bainitic ferrite matrix in high-silicon steels isothermally transformed between 200 °C and 350 °C. Additionally, results were compared with the carbon concentration values derived from X-ray diffraction (XRD) analyses considering a tetragonal lattice and previous APT studies. In conclusion, the present results reveal a strong disagreement between the carbon content values in the bainitic ferrite matrix as obtained by APT and those derived from XRD measurements. Those differences have been attributed to the development of carbon-clustered regions with an increased tetragonality in a carbon-depleted matrix.

36 MATERIALS SCIENCE↗

Ferrite Solutions for Electromagnetic Shock Lines

The goal of this work is to develop tools and test procedures for identifying ferrites suitable for use in shock line applications. Electromagnetic shocklines have been used to provide fast rising voltage pulses for many applications. In these applications a slow rising pulse is injected into the line where currents drive the ferrites into saturation leading to a fast rising output pulse. A shockline’s unique capabilities could be applied to new detonator configurations. A properly conditioned voltage pulse is critical for fire set applications. A carefully designed shockline could provide a passive solution to generating a fast rising voltage pulse for the fire set. Traditional circuits use ferrites operating in a linear regime. Shock lines push the ferrites well into the nonlinear regime where very few tools and data currently exist. Ferrite material is key to the operation of these shock lines, and tools for identifying suitable ferrites are critical. This report describes an experimental setup to that allows testing of ferrite samples and comparison to models with the goal of identifying optimal ferrites for shockline use.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Computational Design of Creep-Resistant Alloys and Experimental Validation in Ferritic Superalloys

A new class of ferritic superalloys containing B2-type zones inside parent L21-type precipitates in a disordered solid-solution matrix, also known as a hierarchical-precipitate strengthened ferritic alloy (HPSFA), has been developed for high-temperature structural applications in fossil-energy power plants. These alloys were designed by the addition of the Ti element into a previously-studied NiAl-strengthened ferritic alloy (denoted as FBB8 in this study). In the present research, systematic investigations, including advanced experimental techniques, first-principles calculations, and numerical simulations, have been integrated and conducted to characterize the complex microstructures and excellent creep resistance of HPSFAs. The experimental techniques include transmission-electron microscopy, scanningtransmission- electron microscopy, neutron diffraction, and atom-probe tomography, which provide detailed microstructural information of HPSFAs. Systematic tension/compression creep tests revealed that HPSFAs exhibit the superior creep resistance, compared with the FBB8 and conventional ferritic steels (i.e., the creep rates of HPSFAs are about 4 orders of magnitude slower than the FBB8 and conventional ferritic steels.) First-principles calculations include interfacial free energies, anti-phase boundary (APB) free energies, elastic constants, and impurity diffusivities in Fe. Combined with kinetic Monte- Carlo simulations of interdiffusion coefficients, and the integration of computational thermodynamics and kinetics, these calculations provide great understanding of thermodynamic and mechanical properties of HPSFAs. In addition to the systematic experimental approach and first-principles calculations, a series of numerical tools and algorithms, which assist in the optimization of creep properties of ferritic superalloys, are utilized and developed. These numerical simulation results are compared with the available experimental data and previous first-principles calculations, providing deep insight of creep mechanisms of the creep-resistant ferritic superalloys. With the above investigations, the HPSFA has been proved with superior creep resistance, and its microstructure, creep mechanism, and thermal/mechanical properties have been well studied and understood. In the future, HPSFAs with different additions and sizes of precipitates will be investigated and developed to further enhance the creep resistance of the ferritic superalloys and provide promising applications of the fossil-energy power plants.

Liaw, Peter↗

Humidity effects on adhesion of nickel-zinc ferrite in elastic contact with magnetic tape and itself

The effects of humidity on the adhesion of Ni-Zn ferrite and magnetic tape in elastic contact with a Ni-Zn ferrite hemispherical pin in moist nitrogen were studied. Adhesion was independent of normal load in dry, humid, and saturated nitrogen. Ferrites adhere to ferrites in a saturated atmosphere primarily from the surface tension effects of a thin film of water adsorbed on the ferrite surfaces. The surface tension of the water film calculated from the adhesion results was 48 times 0.00001 to 56 times 0.00001 N/cm; the accepted value for water is 72.7 x 0.00001 N/cm. The adhesion of ferrite-ferrite contacts increased gradually with increases in relative humidity to 80 percent, but rose rapidly above 80 percent. The adhesion at saturation was 30 times or more greater than that below 80 percent relative humidity. Although the adhesion of magnetic tape - ferrite contacts remained low below 40 percent relative humidity and the effect of humidity was small, the adhesion increased considerably with increasing relative humidity above 40 percent. The changes in adhesion of elastic contacts were reversible on humidifying and dehumidifying.

Miyoshi, K.↗

Structural, Electrical and Dielectric Properties of Hexa-ferrite-Polyaniline Nano-composites

Ferrite-polyaniline (PANI) composites were prepared by in situ polymerization of polyaniline with the general formula (1 − x) ferrite + (x) PANI where x = 0, 0.25, 0.5, 0.75, 1. The samples were characterized by XRD, SEM, electrical resistivity, and dielectric measurements. X-ray diffraction reveals single phase formation of CaBaCo{sub 2}Al{sub 0.5}Fe{sub 11.5}O{sub 22} Y-type ferrite, whereas polyaniline exhibits an amorphous nature. At room temperature, the resistivity of nano-composites increases with the increase of ferrite filler contents from 3.17 × 10{sup 4} to 3.19 × 10{sup 7} Ω cm. Real and imaginary parts of the complex permittivity of the PANI-ferrite composites follow the Maxwell-Wagner model. Based on the Jonscher Law, the AC conductivity of PANI-ferrite composites experiences an increase with the increase in frequency. The exponent calculated from AC conductivity reveals that the hopping is the likely conduction mechanism. The activation energy obtained from temperature-dependent measurements is consistent with room temperature resistivity. Due to the light weight, low cost and flexibility of design, the ferrite-polymer composites are considered useful for microwave devices.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Precipitation of sigma and chi phases in δ-ferrite of Type 316FR weld metals

The decomposition behavior and kinetics of δ-ferrite are examined using aging treatments between 873 and 1073 K for Type 316FR stainless steel weld metals with different solidification modes (316FR AF, 316FR FA). The dominant precipitates are sigma, chi, and secondary austenite nucleated at δ-ferrite/austenite interfaces or in the interior of the ferrite grains. These precipitates consume all the ferrite during isothermal aging in both 316FR AF and FA weld metals. Differences in the precipitation behavior (precipitation initiation time and precipitation speed) between weld metals can be explained by i) the degree of Cr and Mo microsegregation within δ-ferrite or austenite near ferrite and ii) the nucleation sites induced due to the solidification mode (AF or FA), such as the ferrite amount. For both weld materials, a Johnson–Mehl-type equation can express the precipitation behavior of the sigma + chi phases and quantitatively predict the behavior at the service-exposure temperatures of a fast breed reactor. - Highlights: • Precipitation of σ and χ phase in Type 316FR welds (two solidification modes) • Different precipitation behaviors: precipitation initiation time and growth speed • Johnson-Mehl–type equation is the most applicable to the precipitation behaviors • Precipitation behaviors are predicted under service conditions of FBRs.

36 MATERIALS SCIENCE↗

Development of nano-structured duplex and ferritic stainless steels by pulverisette planetary milling followed by pressureless sintering

Nano-structured duplex and ferritic stainless steel powders are prepared by planetary milling of elemental Fe, Cr and Ni powder for 40 h and then consolidated by conventional pressureless sintering. The progress of milling and the continuous refinement of stainless steel powders have been confirmed by means of X-ray diffraction and scanning electron microscopy. Activation energy for the formation of duplex and ferritic stainless steels is calculated by Kissinger method using differential scanning calorimetry and is found to be 159.24 and 90.17 KJ/mol respectively. Both duplex and ferritic stainless steel powders are consolidated at 1000, 1200 and 1400 °C in argon atmosphere to study microstructure, density and hardness. Maximum sintered density of 90% and Vickers microhardness of 550 HV are achieved for duplex stainless steel sintered at 1400 °C for 1 h. Similarly, 92% sintered density and 263 HV microhardness are achieved for ferritic stainless steel sintered at 1400 °C. - Highlights: • Synthesized duplex and ferritic stainless steels by pulverisette planetary milling • Calculated activation energy for the formation of duplex and ferritic stainless steels • Studied the effect of sintering temperature on density, hardness and microstructure • Duplex stainless steel exhibits 90% sintered density and microhardness of 550 HV. • Ferritic stainless steel shows 92% sintered density and 263 HV microhardness.

36 MATERIALS SCIENCE↗