Spherical Indentation and Implementation of S 3 /P for yield stress determination of brittle materials

Here, a mathematically transparent and robust experimental method has been developed to estimate the yield stress of brittle materials through the analysis of depth-sensing spherical indentation. Employing Hertzian contact mechanics, an elastically invariant ratio based on the simple equation S 3 / P = 6RE r 2 , (where S and P are contact stiffness and indentation load, respectively) has been derived that enables more accurate and confident determination of the transition from elastic to inelastic deformation; a transition that the yield stress dictates and represents. Using two diamond spheres with radii of 3.2 and 8.6 μm, the indentation test method and analyses are applied to two vitreous silicates: Corning's HPFS 7980® fused silica and Vitro's Starphire® soda lime silicate. The estimated yield strengths are 8.15 GPa ± 2.5% for the fused silica and 6.1 GPa ± 3.3% for the soda-lime silicate, and both were independent of indenter radius. Verification of this new experimental method is demonstrated with an as-drawn titanium by showing equivalence of measured yield stress by its spherical indentation and that from uniaxial compression testing. This method will enable easier and more confident estimation of yield stress in brittle materials - a property that historically has been elusive to measure for these materials using common laboratory mechanical test methods.

36 MATERIALS SCIENCE↗

Evolution of global and local deformation in additively manufactured octet truss lattice structures

Additively manufactured lattice truss structures, often referred to as architected cellular materials, present significant advantages over conventional structures due to their unique characteristics such as high strength-to-weight ratios and surface area-to-volume ratios. These geometrically complex structures, however, come with concomitant challenges for qualification and inspection. In this study, compression testing interrupted with micro-computed tomography inspection was conducted to monitor the evolution of global and local deformation throughout the loading process of 304L stainless steel octet truss lattice structures. Both two- and three-dimensional image analysis techniques were leveraged to characterize geometric heterogeneities resulting from the laser powder bed fusion manufacturing process as well as track the structure throughout deformation. Variations from model-predicted behavior resulting from these heterogeneities are considered relative to the predicted and actual responses of the structures during compression to better understand, model, and predict the octet truss lattice structure compression response.

36 MATERIALS SCIENCE↗

CHIPFoam Modification to Allow for Modelling SWIFT Foams

SWIFT (Silicon-water in Familiar Template) foams are silicone foams that have a continuous porosity without having any obvious spherical or ellipsoidal pore shapes. Like other foamed rubber, SWIFT foams can experience large reversible deformations. Because of their microstructure, SWIFT foams have a stiffering behavior in compression that is very abrupt compared to most other foamed rubbers. Work by Benedikt reported by Miller showed that fitting compressive test data with the CHIPFoam model in its current form is impractical and inaccurate. This report describes an extension made to CHIPFoam to allow the modeling of SWIFT foams. While the extension allows the modeling of SWIFT foams, it also extends the range of porosity of foams that can be modelled with CHIPFoam to include very high porosity (>99%) foamed rubber. The previous model was unstable for porosities greater than 70%. The changes made to CHIPFoam include the introduction of a critical porosity at which the compressible Danielsson strain energy function that couples volumetric and deviatoric mechanical behavior begins to increase with compression. This new feature also required the introduction of a third term in the multiplicative decomposition of the relative volume, J . The organization of this report is described here. The first section, SWIFT Foam Structure and Mechanical Behavior, describes the structure of SWIFT foams as contrasted to other foamed rubbers. It also contrasts the mechanical behavior of SWIFT foams to other more traditional foamed rubbers. The second section, CHIPFoam Modifications, describes the specific modifications done to be able to modify the delayed rapid compressive stiffening seen in SWIFT foams. The third section, Results, demonstrates the use of the modified model to fit compressive loading response data from a SWIFT foam sample. The fourth section, Conclusions and Further Work, puts the work in perspective and presents likely further work.

36 MATERIALS SCIENCE↗

High-Fidelity Mock Development for the Insensitive High Explosive TATB

Due to the violent reaction potential of high explosives, in tests where a reaction is not desired, it can be safe and convenient to use an inert mock that can mimic relevant properties of the associated explosive. Use of mock materials is well-established in explosives work, but most existing mocks are generally meant to mimic only one or two properties of a given explosive, potentially failing to match the explosive in other critical ways. Recently, there has been interest in developing robust thermomechanical mocks for many common explosives. Here, eleven materials are systematically chosen and investigated as potential thermomechanical mocks for TATB, the explosive component of PBX 9502. DSC, nanoindentation, and compression testing are used to narrow down to most appropriate mocks and identify their advantages and limitations. Hardness and elastic modulus are reported for the first time for the molecular crystals iodoanthranilic acid, hexamine, melamine, and trithiolane dioxide, and the crystal structure is reported for the first time for the molecular crystals iodoanthranilic acid and iodosalicylic acid.

36 MATERIALS SCIENCE↗

An Investigation of Nanoindentation as Quality Control [Slides]

Nanoindentation Continuous Stiffness Measurement (CSM) mapping, and Strain Rate Jump Testing (SRJT) proved effective to highlight and visualize the extent of property differences between the samples. From the analysis, Lot A has a significant dead zone at its center, especially when compared with the cross section of Lot B. Quick identification of property issues from one of the two feed stocks, both of which fit the specification. Mechanical performance was connected to the microstructure. Thus, using the structure-property results, it is noted that the processing of Lot A may have been insufficient. Nanoindentation allows for the sampling of quality control variables such as hardness and modulus in a short time span at high resolution, which is cheaper and faster than traditional strength experiments (tension and compression tests).

36 MATERIALS SCIENCE↗

Microstructural Coarsening Kinetics and Mechanical Property Changes in Long-Term Aged Sn–Pb–Sb Solder Joints

Tin-lead-antimony (50Sn–47Pb–3Sb wt.%) soldered assemblies were mechanically tested approximately 30 years after initial production and found to have solder joints of reduced strength. The microstructure of this solder alloy exhibits a ternary eutectic structure with Sn-rich, Pb-rich, and SnSb phases. Accelerated aging was performed to evaluate solder microstructural coarsening and associated strength of laboratory solder joints to correlate these properties to the “naturally aged” solder joints. Isothermal aging was conducted at room temperature, 55, 70, 100, and 135 °C and aging times that ranged from 0.1 to 365 days. The coarsening kinetics of the Pb-rich phase were determined through optical microscopy and image analysis methods established in previous studies on binary Sn–Pb solder. A kinetic equation was developed with time exponent n of 0.43 and activation energy of 24000 J/mol, suggesting grain boundary diffusion or other fast diffusion pathways controlling the microstructural evolution. Compression testing and Vickers microhardness showed significant strength loss within the first 20–30 days after soldering; then, the microstructure and mechanical properties changed more slowly over long periods of time. Further, by combining accelerated aging data and the microstructure-based kinetics, strength predictions were made that match well with the properties of the actual soldered assemblies naturally aged for 30 years. However, aging at the highest temperature of 135 °C produced anomalous behavior suggesting that extraneous aging mechanisms are active. Therefore, data obtained at this temperature or higher should not be used. Overall, the combined microstructural and mechanical property methods used in this study confirmed that the observed reduction in strength of ~ 30-year-old solder joints can be accounted for by the microstructural coarsening that takes place during long-term solid-state aging.

36 MATERIALS SCIENCE↗

High-strength, lightweight nano-architected silica

Continuous nanolattices are an emerging class of mechanical metamaterials that are highly attractive due to their superior strength-to-weight ratios, which originate from their spatial architectures and nanoscale-sized elements possessing near-theoretical strength. Rational design of frameworks remains challenging below 50 nm because of limited methods to arrange small elements into complex architectures. Here, we fabricate silica frameworks with ~4- to 20-nm-thick elements using self-assembly and silica templating of DNA origami nanolattices and perform in situ micro-compression testing to examine the mechanical properties. We observe strong effects of lattice dimensions on yield strength (σ $\mathcal{y}$ ) and failure mode. Silica nanolattices are found to exhibit yield strengths higher than those of any known engineering materials with similar mass density. The robust coordination of the nanothin and strong silica elements leads to the combination of lightweight and high-strength framework materials offering an effective strategy for the fabrication of nanoarchitected materials with superior mechanical properties.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Evolution of Microstructure and Surface Characteristics of FeCrAl alloys when Subjected to Flow Boiling Testing

FeCrAl alloys are candidate materials for manufacturing accident-tolerant fuel (ATF) cladding intended for light water reactors to increase fuel reliability and safety during design-basis and beyond-design-basis accident scenarios. The evolution of the materials' surface characteristics, microstructure, and mechanical properties when exposed to the Critical Heat Flux (CHF) in flow boiling testing is crucial for safety analysis while providing insights into their thermal-hydraulic performance in nuclear reactors. After CHF, the surface chemistry of two FeCrAl alloys, APMT and C26M, was studied to understand their evolution at the early stage of high-temperature excursions in short time periods. The results indicated a thin layer composed of oxides and hydroxides of Al, Cr, and Fe with varying proportions at different depths in the layer, as indicated by X-ray photoelectron spectroscopy (XPS) and depth profiling. The cross-sections prepared by focused ion beam (FIB) revealed the growth of an oxide layer, in the range of 90-180 nm thick, on the alloys' surfaces. The evolution of the materials' surface chemistry also led to a noticeable post CHF excursion increase in their wettability, with a slight increase in roughness. Further, the investigation of the materials' mechanical properties indicated a modest increase in hardness by 10-15% as well as an increase in their yield strength, as evidenced by the microindentation and ring compression tests conducted before and after CHF testing. Scanning electron Microscopy (SEM) and X-ray diffraction (XRD) were used to investigate microstructural features of the materials and their changes after CHF treatment.

36 MATERIALS SCIENCE↗

Development of Ti 3 SiC 2 MAX phase tubular structures for solar receiver applications

Solar receiver tubes are key components of concentrating solar-thermal power (CSP) systems that harvest solar energy. For better efficiency, the Gen3 CSP receivers, which collect heat into a heat transfer fluid, require a temperature exceeding 700 °C during operation and need to perform under extreme conditions of high temperature and high thermal stress. Operators are seeking CSP designs using new high-temperature structural materials with high thermal conductivity and high creep resistance to achieve a design life of 30 years and thus help recover the plant capital cost sooner. MAX phase materials, which consist of an early transition metal element, an A-group element, and carbon or nitrogen, are expected to exhibit high creep resistance as well as high fracture toughness. Here, in this paper, we describe fabricating both (1) dense Ti 3 SiC 2 MAX phase disks and (2) short-length tubes using field-assisted sintering technology (FAST). First, the disk samples that we fabricated are fully dense and contain ≈90 % Ti 3 SiC 2 MAX phase materials and ≈10 % TiC phase materials. We determined a flexure strength of 519 ± 32 MPa by conducting a four-point bending test at room temperature with rectangular bar samples of ≈100 % density. The thermal conductivity of the Ti 3 SiC 2 MAX phase samples, measured by light flashing analysis, decreases linearly from a value of 41 W . m -1 . K -1 at room temperature to a value of 36 W . m -1 . K -1 at 650 °C. A solar reflectance measurement of the Ti 3 SiC 2 MAX phase revealed that, temperature increases from 400 to 1400 °C, thermal emittance increases from 0.39 to 0.49, while selectivity decreases from 1.8 to 1.4, respectively. Whereas the surface oxidized MAX phase samples after 100 h exposure to air at 1000 °C exhibit that of SiC. Next, we discuss fabrication of the crack-free Ti 3 SiC 2 MAX phase tubular structures accomplished by using FAST processing in graphite bedding. A Ti 3 SiC 2 MAX phase content of > 95 % with traceable ≈3% remaining TiC phase and ≈15 % porosity were demonstrated after high-temperature annealing. An average fracture strength of ≈250 MPa was determined with Ti 3 SiC 2 MAX phase tubes of ≈85 % density by diametral compression testing at room temperature. Our work demonstrated that using FAST processing to produce Ti 3 SiC 2 MAX phase tubular structures for CSP receiver applications is a viable approach.

14 SOLAR ENERGY↗

Petrophysical and geomechanical properties of gas hydrate-bearing sediments recovered from Alaska North Slope 2018 Hydrate-01 Stratigraphic Test Well

Knowledge of petrophysical and geomechanical properties of gas hydrate-bearing sediments are essential for predicting reservoir response due to gas production from gas hydrate reservoirs. That information will be critical parameters for designing production well completion such as specification of depressurization pump, water storage tank, and mesh size of sand screen. In December 2018, Stratigraphic Test Well Hydrate-01 was drilled in the western part of the Prudhoe Bay Unit, Alaska North Slope as part of the technical planning effort for a future long-term production test by collaborative team of DOE/NETL, USGS, and MH21-S (Boswell et al., 2020, Collett et al., 2020, Okinaka et al., 2020). Data set of logging-while-drilling (LWD) were acquired (Haines et al., 2020, Suzuki et al., 2019) and core sampling depth was determined on-site.Side-wall pressure coring was conducted to recover gas hydrate-bearing sediments from two reservoir sections named Unit-B and Unit-D. A total of 34 cores were successfully recovered by 5 runs of a wire-line deployed pressure corer (CoreVault® System - Halliburton). Core analysis scheme of this project are shown in Figure 1. All cores were quenched in liquid nitrogen while at high pressure in the laboratory of Stratum Reservoir, LLC. at Anchorage (Figure 1, a)). And the cores were removed from the pressure corer autoclave with temperature support of dry ice and stored under liquid nitrogen at atmospheric pressure. 19 damaged cores were processed to index property measurements directly such as grain size, grain density. 4 of another 17 cores were depressurized and trimmed for making a plug to analyze petrophysical properties of host sediments. Unsteady-state permeability test was conducted to obtain relative water permeability to gas and core scale NMR T2 distribution measurement was performed for evaluating pore size distribution at Houston (Figure 1, b)). Remained high quality 13 cores were preserved with gas hydrate for advanced laboratory analysis. National Institute of Advanced Industrial Science and Technology, as a part of the Japanese National Hydrate Research Program (MH21-S, funded by Ministry of Economy, Trade and Industry), received the samples at Sapporo, Japan for advanced core analysis. High-resolution X-ray CT was used to analyze the quality of the samples, which showed undisturbed lithological layers. Cores were lathed into cylindrical shape and distributed for multi property measurements (Figure 1, c)).<p>As a result, sediment from Unit-D is categorized as silty sand at ~37% porosity with ~80% gas hydrate saturation. An average hydration number n = 6.16 was measured by Raman spectroscopy. An average intrinsic permeability of ~400 mD and in situ effective permeability (with hydrate) on the order of ~10 mD. The Unit B recovered cores consisted of well sorted sand at ~40% porosity with ~95% gas hydrate saturation. An average intrinsic permeability of ~1 Darcy and in situ effective permeability on the order of ~30 mD was measured for the Unit B cores. There was a small permeability reduction due to porosity loss with increasing effective stress that simulated consolidation behavior along with depressurization in the highly permeable sandy sediment. The apparent minimum change in porosity and permeability may be caused by the low compressibility of quartz sand grains in the recovered cores. XRD and thermal conductivity analysis also suggested high quartz content. Triaxial compression tests established internal friction angles based on the Mohr-Coulomb's failure criterion, which are 40° for hydrate-bearing sediment and 29.8° for hydrate free sediment.</p>

Yoneda, Jun↗

Microstructure and mechanical behavior of laser remelted amorphous Al-Ni-La welds

To explore the feasibility of using laser powder bed fusion systems to print bulk amorphous Al alloys, a single autogenous weld produced by laser remelting on a cast Al-5La-9Ni (at.%) alloy was studied for its microstructure and mechanical behavior. The solidification rates experienced by material within the welds were high enough to produce entirely amorphous regions within the welds. Welds were characterized using SEM, STEM, and APT and were found to contain Ni-rich amorphous clusters. Micropillar compression tests were used to assess mechanical properties of the welds and found that all of the amorphous regions exhibited yield strengths around 1 GPa. In conclusion, these results are discussed in the context of diffusivity of Ni and rare earth elements in liquid, glass forming ability, thermodynamic driving force for phase formation during solidification, free volume concentrations in bulk metallic glasses, and cluster-related softening.

APT↗

Strain localization criteria for viscoplastic geomaterials

This report presents a viscoplastic localization criterion to detect quasi-instantaneous (i.e., load-induced) and delayed (creep-induced) strain localization in rate-dependent solids. The study is based on the theory of controllability and a viscoplastic description of the mechanical response. Analytical precursors of unstable states are defined through systems of ordinary differential equations (OEDs). The use of the proposed criteria is illustrated at the material point level through a set of strain localization analyses simulating active strain localization of a porous rock. In addition, full-field finite element simulations of compression tests conducted under various pressures are reported to demonstrate the role of local unstable viscoplasticity in the spontaneous propagation of deformation bands under stationary boundary conditions. The study shows that the viscoplastic localization criterion maintains a negative sign as long as the behavior is unstable, that is, the rate of deformation is accelerating. The sign switch coincides with the transition to decelerating deformation. The analyses revealed that pulses of overstress always emerge in correspondence with the growth of unstable behavior, and the peak matches the transition to stable behavior. The local responses recovered from full-field analyses were consistent with those observed in analyses at material point level and the predictions of the presented theory.

36 MATERIALS SCIENCE↗

Multiscale numerical investigation of ratchet growth damage effects in PBX 9502

This paper presents results of numerical experiments conducted on the high explosive PBX 9502 to investigate how recently observed grain-scale damage mechanisms of ratchet growth affect uniaxial compression measurements. Simulations are multiscale in the sense of directly resolving grains, pores, cracks, and grain-interfaces based upon scanning electron microscope (SEM) images of damaged and undamaged samples. The combined finite-discrete element method (FDEM) is utilized to resolve both grain-scale microfracture and elastoplastic deformation of solid grains. Pristine (undamaged) and damaged microstructures are compared in simulation of unconfined compression tests of the same material from the literature. Here, the simulation results show the observed microscale mechanisms of damage, specifically microfracture predominantly around and sometimes through grains and crack-associated pore growth, can well-explain the effective degradation of strength and stiffness observed in the laboratory measurements.

36 MATERIALS SCIENCE↗

Microstructural, Oxidation, and Mechanical Behavior of NbTi-Based Refractory Alloys with 5 to 10 Pct Co, Cr, and Ni Additions

NbTi-based refractory alloys with additions of Co, Cr, and Ni represent an interesting medium-entropy alloy system with potential for protective oxide film formation, high strength, and ductility. This study investigates the microstructural evolution, oxidation behavior, and mechanical properties of NbTi-based alloys containing 5 to 10 at. pct Co, Cr, and Ni. CALPHAD predictions suggest that this composition range can be heat treated to obtain a predominantly body-centered cubic matrix phase. Mechanical properties, including microhardness, yield strength, maximum strength, and specific strength are evaluated through isothermal compression tests conducted between room temperature and 800 °C. The oxidation kinetics of these alloys are assessed through discontinuous oxidation tests. Parabolic oxidation kinetics were observed for NbTi–10Ni and NbTi–5Co, while linear oxidation kinetics were found for NbTi–10Cr and NbTi–10(CoCrNi). Microstructures and oxide layers are characterized using X-ray diffraction, electron backscatter diffraction, energy-dispersive X-ray spectroscopy, and scanning electron microscopy. All alloys exhibit significant mechanical softening between room temperature and 800 °C, with elastic-perfectly plastic flow observed at 800 °C. The addition of 10 pct Cr to NbTi resulted in two BCC phases up to 1050 °C, conflicting with CALPHAD predictions of a single-phase solid solution at this temperature, and resulting in higher flow stress at 800 °C. NbTi–10(CoCrNi) exhibited the lowest flow stress at 800 °C despite having more ‘cocktail effect’ potential and insufficient molar fractions of Co, Cr, or Ni to form a desirable protective oxide film.

36 MATERIALS SCIENCE↗

Coupling Thermomechanical Processing and Alloy Design to Improve Textures in Mg-Zn-Ca Sheet Alloys

Abstract The effect of Ca and Zn additions on the microstructure and texture evolution during thermomechanical processing of Mg-Zn-Ca sheet alloys was systematically investigated and quantified. Plane strain compression testing in a Gleeble thermomechanical simulator was used to physically simulate a 10-pass rolling schedule, while allowing for careful control and monitoring of the processing parameters. Textures in the as-deformed ternary alloy samples demonstrate a weak maximum basal intensity and spreading in the transverse direction. Increasing the Zn content to 3.2 wt.% in the ternary alloys resulted in samples that exhibited weak textures in the as-deformed state. Importantly, static recrystallization (SRX) during post-deformation annealing of these alloys promoted a desirable annular texture, with the c -axis tipped from the normal direction and a lower basal texture intensity. The evolution in texture during SRX is associated with as-deformed microstructures with broad grain orientation spreads and a low degree of recrystallization.

36 MATERIALS SCIENCE↗

In-Situ X-Ray Imaging High Strain Rate Compression of Laminate Al-Graphene Composite and Mechanical Property Characterization

Owing to the opaque nature of the laminated structures, traditional high-speed optical camera cannot be used to detect the dynamic process of sub-surface deformation. In this article, we report a study of using high speed X-ray imaging to study the high strain rate deformation in laminated Al structures. We used a Kolsky bar apparatus to apply dynamic compression and a high-speed synchrotron X-ray phase contrast imaging (PCI) setup to conduct the in situ X-ray imaging study. The in situ X-ray imaging captures the shock wave propagation in the laminated structures. After shock compression, we characterized the microstructures by using transmission electron microscopy (TEM), which demonstrates an increase of dislocation density. In conclusion, the micro-pillar compression tests show that the yield strength at 0.2% offset of laminated Al-graphene composite has a significant increase of 67%, from 30 to 50 MPa, compared to laminate Al after shock loading.

36 MATERIALS SCIENCE↗

Probing the Mechanical Performance of Micro-architected Porous Structures Through In Situ Characterization and Analysis

Micropores play critical roles in both natural and man-made materials. Such pores take on a variety of shapes and sizes ranging from spherical to irregular sphere-like voids with diameters spanning from the nanometer to millimeter scales. When porous structures are mechanically loaded, the pores direct the stress around their free surfaces, altering the material’s mechanical response relative to fully dense materials. In this study, for the first time, we create micro-architected porous samples using nanolithography and investigate the role of pore morphology by conducting a series of in situ micropillar compression tests in scanning electron microscopy. The findings demonstrate that porosity is the primary factor influencing the mechanical response of these micro-architected materials, as often seen on a macroscopic level. Additionally, we observed that pore geometry had a significant impact on Young’s modulus, yield stress, and strain energy density as a secondary parameter. Then, the extracted Young’s modulus was compared to macroscopic empirical models and determined the analytical models sufficiently described the impact of porosity in the microscopic scale but failed to capture the impact of second-order parameters. Furthermore, these results suggest how porous materials can be tailored to achieve desired mechanical properties based on the engineering applications of interest.

36 MATERIALS SCIENCE↗

Laboratory-Based Micro-X-ray Computed Tomography of Energy Materials at Idaho National Laboratory

Abstract The Idaho National Laboratory (INL) has implemented laboratory-based micro-X-ray computed tomography in a laboratory equipped for the examination of highly radioactive samples. This capability provides nondestructive three-dimensional volumetric information on samples to inform subsequent traditional destructive examinations as well as real-world inputs for high-fidelity scientific modeling. Samples can be imaged with spatial resolutions ranging from several hundred nm/voxel up to ~ 100 µm/voxel. The best usable spatial resolution achieved to date is 384 nm/voxel with this instrument, while the highest radiological dose rate of a sample imaged is ~ 60 R/h β/γ on contact. Advanced data analysis, including custom tomographic reconstruction and segmentation methods, have also been developed to support this capability. In addition to traditional digital X-ray radiography and tomography, this instrument is also able to visualize in situ tensile and compression testing as well as perform diffraction contrast tomography. This work describes the X-ray computed tomography post-irradiation examination capabilities at INL, as well as detailing a variety of applications this instrument has examined.

36 MATERIALS SCIENCE↗