Model 9975 O Ring Fixture Long-Term Leak Performance (FY2024 Status Report)
Leak testing experiments to monitor the aging performance of Viton ® GLT and GLT-S O-rings used in the model 9975 shipping package have been ongoing since 2004 at Savannah River National Laboratory. Seventy tests using mock-up 9975 primary containment vessels (PCVs) with GLT O-rings were assembled and heated to temperatures ranging from 200 to 450 °F. Due to material substitution, fourteen tests with GLT-S O-rings were initiated in 2008 and heated to temperatures ranging from 200 to 400 °F. The conditioning temperatures are elevated compared to the calculated maximum O-ring temperature in a 9975 package in storage, 158 °F, to accelerate aging and enable observations of O-ring failures in a reasonable time frame. The mock-up PCV fixtures are leak tested periodically, and all GLT O-ring fixtures aging at 350 °F or above have failed to maintain a leak-tight seal. Eight GLT O-ring fixtures aging at 300 °F have failed after 2.8 to 5.7 years at temperature while the remaining fixtures at 300 °F were retired from testing following more than five years of aging without failure. Two of these retired fixtures were returned to testing and heated to 350 °F to evaluate the impact of additional heating at higher temperature for aged O-rings. Fixture #20 failed after 3 months of testing while fixture #18 remained leak tight. These O-rings demonstrated that aged and in-service O-rings can continue to be used, even at higher temperatures, after being in storage, and their leak performance are consistent with other samples at 350 °F.