Ordered CoPt oxygen reduction catalyst with high performance and durability

A high-performance and durable polymer electrolyte membrane fuel cell cathode catalyst composed of an ordered L10–CoPt core and a thin Pt shell was designed and prepared. Under practical fuel cell membrane electrode assembly testing conditions, the cathode catalyst showed an outstanding initial mass activity of 0.6 A/mgPt, which satisfies the U.S. Department of Energy performance target while also meeting the durability target of less than 40% loss in mass activity after 30,000 accelerated stress test voltage cycles. The high structural stability of the L10–CoPt@Pt-shell catalyst was confirmed by postmortem materials characterization, and the origin of this robustness was revealed by density functional theory calculations, where the barriers for diffusion of Co atoms were observed to be significantly increased in the ordered intermetallic core.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Membrane Pretreatment and Cell Conditioning for Proton Exchange Membrane Water Electrolysis

As the research community studying proton exchange membrane water electrolysis (PEMWE) grows, it is important to develop methods that achieve transparent, reproducible research. Reproducibility of performance and durability is a challenge facing the PEMWE field, as the published literature includes a wide spread of results obtained with nominally similar materials. Prior round-robin performance benchmarking efforts [1] have identified inadequate cell conditioning as a major source of variation in apparent cell performance. Inadequate pre-treatment and conditioning can lead to instability in initial performance and adds ambiguity to durability measurements. However, excessively prolonged conditioning procedures limit the throughput of testing and the pace of research. Pretreatment and conditioning methods vary significantly across the research literature, but little systematic investigation is available into the mechanisms of these procedures or how procedural differences may impact results. This presentation will discuss investigations into the effects of membrane pre-treatment and operating procedures during cell conditioning on initial performance and catalyst-specific accelerated stress tests, with the aim of recommending procedures to enable clear, reproducible, and high-throughput research. Methods investigated include the use of hydrogen peroxide, acids, and hydration at elevated temperature for membrane pretreatment, and conditioning procedures such as current or voltage holds and cycling. The investigations cover both the impacts of these procedures on cell performance and stability as well as underlying mechanisms and processes taking place in the cell materials.

cell↗

Pt–Co truncated octahedral nanocrystals: a class of highly active and durable catalysts toward oxygen reduction

We report a facile and scalable synthesis of Pt–Co truncated octahedral nanocrystals (TONs) by employing Pt(acac) 2 and Co(acac) 2 as precursors, together with CO molecules and Mn atoms derived from the decomposition of Mn 2 (CO) 10 as a reductant and a {111} facet-directing agent, respectively. Both the composition and yield of the Pt–Co TONs could be varied through the introduction of CHCl 3 . When tested at 80 °C using membrane electrode assembly (MEA), the 4 nm Pt 2.6 Co TONs gave a mass activity of 294 A g Pt –1 at beginning-of-life (BOL) and it increased to 384 A g Pt –1 during recovery cycles. The mass activity at BOL only dropped by 24% after 30 000 voltage cycles at end-of-life (EOL) in a metal dissolution accelerated stress test. The Pt 2.6 Co/C catalyst outperformed the commercial TKK Pt 3 Co/C (230 A g Pt –1 at BOL and 40% loss after 30 000 cycles at EOL) in terms of both activity and durability. Our systematic analysis suggested that the enhancement in activity can be attributed to the combination of small, uniform size and well-defined {111} facets. This new class of catalysts holds promise for applications in proton-exchange membrane fuel cells.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Catalyst and Catalyst Layer Composition on Catalyst Support Durability

Polymer electrolyte membrane fuel cells (PEMFCs) are efficient, zero-emission engines for the automotive sector. However, cost and durability are major barriers for the commercialization of PEMFCs. Degradation of the carbon support in the cathode catalyst layer due to high potential excursions caused by unmitigated events like H 2 starvation, or start-up/shutdown are still a major durability issue in PEMFCs. Catalyst support durability was studied by accelerated stress tests (ASTs) that included repeated potential cycling from 1.0 to 1.5 V. The effect of catalyst layer composition on carbon corrosion was studied using membrane electrode assemblies with different catalysts (Pt, PtCo), catalyst composition (catalyst wt.%, supports), ionomer composition (loading, and equivalent weights). The corrosion of the carbon support is similar between Pt and PtCo catalysts. However, the performance degradation rate is higher for the alloy catalysts due to differences in catalyst particle size and the transition metal’s leaching accelerating the performance degradation. The carbon loss is lower for catalysts with lower initial carbon loading (or higher catalyst wt.%), which is better for durability. However, the cumulative loss of carbon is identical for electrodes with the same catalyst support irrespective of catalyst and ionomer composition in the catalyst layer.

25 ENERGY STORAGE↗

Coaxial Nanowire Electrodes Enable Exceptional Fuel Cell Durability

Polymer-electrolyte-membrane fuel cells (PEMFCs) hold great promise for applications in clean energy conversion, but cost and durability continue to limit commercialization. This work presents a new class of catalyst/electrode architecture that does not rely on Pt particles or carbon supports, eliminating the primary degradation mechanisms in conventional electrodes, and thereby enabling transformative durability improvements. The coaxial nanowire electrode (CANE) architecture consists of an array of vertically aligned nanowires, each comprising an ionomer core encapsulated by a nanoscale Pt film. This unique design eliminates the triple-phase boundary and replaces it with two double-phase boundaries, increasing Pt utilization. It also eliminates the need for carbon support and ionomer binder, enabling improved durability and faster mass transport. Fuel cell membrane electrode assemblies based on CANEs demonstrate extraordinary durability in accelerated stress tests (ASTs), with only 2% and 5% loss in performance after 5000 support AST cycles and 30000 catalysts AST cycles, respectively. The high-power density and extremely high durability provided by CANEs can enable a paradigm shift from random electrodes based on unstable platinum nanoparticles dispersed on carbon to ordered electrodes based on durable Pt nanofilms, facilitating rapid deployment of fuel cells in transportation and other clean energy applications.

25 ENERGY STORAGE↗

Creating Favorable Pt/Co Interfaces via a Two‐Step Approach for Constructing Highly Durable PtCo Intermetallic Fuel Cell Catalysts

Structurally ordered PtCo intermetallics are one of the most promising oxygen-reduction catalysts in proton exchange membrane fuel cells (PEMFCs) due to their intrinsically improved catalytic activity and stability relative to PtCo solid-solution alloys. However, increasing the heating temperature to achieve a desirable high degree of ordering results in severe particle agglomeration and low mass activity and stability. Herein, a two-step synthesis approach is developed to create an L1 2 -Pt 3 Co intermetallic structure with an increased ordering degree and well-dispersed ultrafine particles. The first step of the synthesis yields ultrafine Pt nanoparticles that are well-dispersed on the ZIF-8-derived carbon support. The second adsorption step enables us to fine-tune the Pt and Co interfaces, assisted by optimal amino acids, to establish a favorable Co-rich environment around fine Pt nanoparticles, facilitating Co diffusion into the Pt crystalline under mild thermal conditions (<800 °C). In conclusion, this two-step ordered L1 2 -Pt 3 Co catalyst is systematically evaluated using membrane electrode assemblies under heavy-duty vehicle (HDV) conditions and demonstrated exceptional performance and durability, retaining 1.35 A cm -2 only a 7% loss in current density at 0.7 V after an extensive accelerated stress test of 150,000 voltage cycles.

30 DIRECT ENERGY CONVERSION↗

Mapping of Heterogeneous Catalyst Degradation in Polymer Electrolyte Fuel Cells

Pt catalysts in polymer electrolyte fuel cells degrade heterogeneously as the catalyst particles are exposed to local variations throughout the catalyst layer during operation. State-of-the-art analytical techniques for studying degradation of Pt catalysts do not possess fine spatial resolution to elucidate such non-uniform degradation behavior at a large electrode level. A new methodology is developed to spatially resolve and quantify the heterogeneous Pt catalyst degradation over a large area (several cm ) of aged MEAs based on synchrotron X-ray microdiffraction. PEFC single cells are aged using voltage cycling as an accelerated stress test and the degradation heterogeneity at a micrometer length scale is visualized by mapping Pt catalyst particle size after voltage cycling. It is demonstrated in detail that the Pt catalyst particle size growth is non-uniform and follows the flow field geometry. The Pt particle size growth is greater in the area under the flow field land, while it is minimal in the area under the flow field channel. Additional non-uniformity is observed with the Pt particle size increasing more rapidly at the air outlet area than the Pt particle size at the inlet area.

36 MATERIALS SCIENCE↗

Probing Heterogeneous Degradation of Catalyst in PEM Fuel Cells under Realistic Automotive Conditions with Multi-Modal Techniques

The heterogeneity of polymer electrolyte fuel cell catalyst degradation is studied under varied relative humidity and types of feed gas. Accelerated stress tests (ASTs) are performed on four membrane electrode assemblies (MEAs) under wet and dry conditions in an air or nitrogen environment for 30 000 square voltage cycles. The largest electrochemically active area loss is observed for MEA under wet conditions in a nitrogen gas environment AST due to constant upper potential limit of 0.95 V and significant water content. The mean Pt particle size is larger for the ASTs under wet conditions compared to dry conditions, and the Pt particle size under land is generally larger than under the channel. Observations from ASTs in both conditions and gas environments indicate that water content promotes Pt particle size growth. ASTs under wet conditions and an air environment show the largest difference in Pt particle size growth for inlet versus outlet and channel versus land, which can be attributed to larger water content at outlet and under land compared to inlet and under channel. From X-ray fluorescence experiments Pt particle size increase is a local phenomenon as Pt loading remains relatively uniform across the MEA.

25 ENERGY STORAGE↗

A Three–Dimensional Nanoscale View of Electrocatalyst Degradation in Hydrogen Fuel Cells

The loss of platinum (Pt) electrochemically active surface area (ECSA) is a critical degradation mode that often becomes a limiting factor for heavy-duty proton exchange membrane fuel cell vehicles. High surface area carbon supports have been shown to improve Pt dispersion and limit detrimental ionomer-electrocatalyst interactions due to their large interior pore volume. Here, in this work, using automated scanning transmission electron tomography, the degradation of nanoparticles located on the interior versus exterior surfaces of the carbon support is compared following a catalyst-specific accelerated stress test (AST) of 90,000 voltage cycles between 0.6 V to 0.95 V. The results reveal a notable increase in median particle size for both interior and exterior Pt catalyst particles, with a slightly higher increase in particle size distribution and loss of specific surface area for the particles located on the exterior carbon surface. The fraction of Pt nanoparticles that reside within the interior of the carbon support also increased following the AST test, accompanied by evidence of an increase in average carbon mesopore size. Here, the results shed light on the degradation mechanisms affecting electrochemical properties and the enhanced particle accessibility at lower relative humidity.

08 HYDROGEN↗

Probing Electrode Transformation under Dynamic Operation for Alkaline Water Electrolysis

Alkaline water electrolyzers (AWEs) play a pivotal role in the realm of large-scale hydrogen production. However, AWEs face significant challenges in electrode degradation particularly under dynamic operating conditions, induced by reverse current phenomenon during frequent startup/shutdown. Herein, this study aims to rationalize the degradation mechanisms of AWEs under these conditions. A three-electrode membrane electrode assembly (MEA) setup is first utilized to decouple polarization behaviors of anode and cathode in AWEs. Following a proposed accelerated stress testing protocol, the setup allows for tracking individual electrode performance transformations during frequent reverse current operation. Integrating operando cell studies with in situ and post-mortem characterizations, it is showed that continuous formation of highly active species, nickel (oxy)hydroxides, improves the anode performance for oxygen evolution reaction. On the contrary, irreversible oxidation of nickel to β-nickel hydroxide results in a severe degradation of cathode, leading to material dissolution, poor electrical conductivity and loss of catalytic activity for hydrogen evolution reaction. These results provide insights in nickel-based electrode transformation mechanisms for alkaline water electrolysis and indicate that cathode with higher redox reversibility can potentially improve durability of AWEs under dynamic conditions.

08 HYDROGEN↗

Durability of Pt-Alloy Catalyst for Heavy-Duty Polymer Electrolyte Fuel Cell Applications under Realistic Conditions

As an emerging technology, polymer electrolyte fuel cells (PEFCs) powered by clean hydrogen can be a great source of renewable power generation with flexible utilization because of high gravimetric energy density of hydrogen. To be used in real-life applications, PEFCs need to maintain their performance for long-term use under a wide range of conditions. Therefore, it's important to understand the degradation of the PEFC under protocols that are closely related to the catalyst lifetime. Alloying Pt with transitional metal improves catalyst activity. It is also crucial to understand Pt alloys degradation mechanisms to improve their durability. To study durability of Pt alloys, accelerated stress tests (ASTs) are performed on Pt-Co catalyst supported on two types of carbon. Two different AST protocols were being studied: Membrane Electrolyte Assembly (MEA) AST based on the protocol introduced by the Million Mile Fuel Cell Truck consortium in 2023 and Catalyst AST, adopted from the U.S. Department of Energy (DoE).

25 ENERGY STORAGE↗

Effect of Commercial Gas Diffusion Layers on Catalyst Durability of Polymer Electrolyte Fuel Cells in Varied Cathode Gas Environment

Gas diffusion layers (GDLs) play a crucial role in heat transfer and water management of cathode catalyst layers in polymer electrolyte fuel cells (PEFCs). Thermal and water gradients can accelerate electrocatalyst degradation and therefore the selection of GDLs can have a major influence on PEFC durability. Currently, the role of GDLs in electrocatalyst degradation is poorly studied. Here, we perform electrocatalyst accelerated stress test studies on membrane electrode assemblies (MEAs) prepared using three most commonly used GDLs. The effect of GDLs on electrocatalyst degradation is evaluated in both nitrogen (non-reactive) and air (reactive) gas environments at 100% relative humidity. In situ electrochemical characterization and extensive physical characterization is performed to understand the subtle differences in electrocatalyst degradation and correlated to the use of different GDLs. Overall, no difference is observed in the electrocatalyst degradation due to GDLs based on polarization curves at the end of life. But interestingly, MEA with a cracked microporous layer (MPL) in the GDL exhibited a higher electrocatalyst loading loss, which resulted in a lower and more heterogeneous increase in the average electrocatalyst nanoparticle size.

25 ENERGY STORAGE↗

Operando carbon corrosion measurements in fuel cells using boron-doped carbon supports

Carbonaceous materials are the most common catalyst supports in proton exchange membrane fuel cell (PEMFCs), yet their corrosion is one of the limiting factors in achieving high durability. Herein, we doped carbon supports with boron (B) to increase the corrosion-resistance of the support. Two types of B-doped carbons were synthesized and studied as platinum support materials. Further, they varied in their morphologies, surface areas, and the types of boron species. The durability of Pt/B-doped carbon catalysts was investigated using the US-DOE catalysts’ supports accelerated stress test (AST) and a mass-spectrometer connected to the fuel cell effluent stream to quantify the mass of corroded carbon support in operando. The addition of boron to the carbon increased the stability of Pt catalysts in long-term usage of PEMFC. After 4000 AST cycles, more than 50% of initial current density was preserved for the boron-containing systems, while less than 30% of it remained with Vulcan carbon (Pt/V). Also, the Pt/B-doped carbon samples demonstrated better electrochemical active surface area (ECSA) stability when compared to Pt/V. Carbon loss measurements showed that B-doped carbons have higher resistance to electrochemical corrosion than unmodified carbon. Specifically, the substitutional boron-doped carbon demonstrated an extremely high stability and low corrosion rate.

25 ENERGY STORAGE↗

Highly durable fuel cell electrocatalyst with low-loading Pt-Co nanoparticles dispersed over single-atom Pt-Co-N-Graphene nanofiber

The limited durability of Pt electrocatalysis toward cathodic oxygen reduction reaction remains challenging, yet crucial for the development of Proton Exchange Membrane Fuel Cell. Here, we present a rational design of a robust catalyst consisting of PtCo nanoparticles supported on Pt-Co-N-graphene nanofiber prepared through electrospun Cobalt-Metal-Organic-Framework. The catalyst delivers unprecedented mass activity of 2.48 A·mgPt -1 , and retains 80% of initial value after 60,000 Accelerated-Stress-Test cycles. Operando X-ray absorption spectroscopies show that the electronic configurations of Pt sites in PtCo and Co sites in Co-N4 in the hybrid catalyst are modified toward high catalytic activities. Density Functional Theory unveils that the enhanced curvature of the substrate induced by the morphology engineering lowers the reaction thermodynamic barrier on Co-N4 sites, favoring the formation of H2O and suppressing that of H2O2. This result along with the strong affinity of PtCo nanoparticles to the Pt-Co-N-graphene fiber endows the catalyst an exceptional durability.

acidic electrolyte↗

Durability of PGM catalyst MEAs of polymer electrolyte membrane fuel cells for heavy-duty vehicles

Polymer electrolyte membrane fuel cells (PEMFCs) are promising power sources for heavy-duty vehicles (HDVs) owing to cleanliness and efficiency. However, the degradation of membrane electrode assemblies (MEAs) under HDV conditions remains a huge challenge. Here, this work investigated MEA durability under HDV conditions using a US Department of Energy standard accelerated stress test for 180,000 cycles (equivalent to 1 million miles of HDV operation). Effects of catalyst Pt content on MEA durability were examined using homemade 30% Pt/C (H-Pt/C) and commercial 46% Pt/C (C-Pt/C) catalysts. Both MEAs experienced H 2 /air and H 2 /O 2 performance loss over cycles. Analysis with scanning transmission electron microscopy, X-ray diffraction, inductively coupled plasma mass spectrometry, and mercury intrusion porosimetry revealed severe degradation of Pt nanoparticles (NPs), support structures, and the catalyst layer. Two degradation stages for NPs were proposed: Ostwald ripening dominated the initial 60,000 cycles, followed by combined Ostwald ripening and particle migration. Measurements with ion chromatography, high-frequency resistance, and oxygen-diffusion resistance revealed degradation of membrane and ionomer, respectively.

25 ENERGY STORAGE↗

Current research in low temperature proton exchange membrane-based electrolysis and a necessary shift in focus

While hydrogen has limited use in energy markets today, significant growth is possible in grid storage and as an energy carrier in other sectors. Along with lower electricity prices, further hydrogen cost reduction can enable electrochemical water splitting, particularly as the use of intermittent, renewable power sources increases and the quantity and duration of storage requirements limit electrical storage options. With the improved viability of large-scale hydrogen production, research in low temperature electrolysis has dramatically increased. The overwhelming majority of research efforts within proton exchange membrane-based systems has focused on catalyst development, although a smaller set have developed transport layers as well. As proton exchange membrane-based electrolysis shifts into higher technology readiness levels, however, there is a growing need for work optimizing materials integration, developing component-specific and device-level accelerated stress tests, and addressing manufacturing considerations. These areas directly impact electrolyzer performance, durability, and cost, and are critical to advancing hydrogen’s value and electrochemical water splitting.

08 HYDROGEN↗

Status and challenges for the application of platinum group metal-free catalysts in proton-exchange membrane fuel cells

Platinum group metal-free (PGM-free) electrocatalysts are an important class of materials for the sustainable energy economy and significant effort has been made towards developing PGM-free catalysts to replace their costly Pt counterparts in fuel cell electric vehicles. The progress made in activity over the last decade is reviewed, along with synthesis strategies for more controlled active site formation and performance gains achieved through electrode engineering. The increased focus on durability, the growing understanding of degradation mechanisms, and the need for standard performance and accelerated stress test protocols are discussed.

25 ENERGY STORAGE↗

Carbon nanotubes decorated with Pt as a viable electrocatalyst system using electrochemical atomic layer deposition

Surface limited redox replacement (SLRR) is an electrochemical deposition method designed to deposit metal thin films, typically onto other metals, that are mere monolayers in thickness, where such low dimensions allows catalyst-support interactions to affect catalyst efficiency. Here we explore the growth of Pt, using iterative Cu-mediated SLRR cycles, directly onto carbon nanotubes (CNTs) which are potentially good candidates as electrocatalyst supports due to their electrical conductivity and chemical resistance. Here scanning electron microscope images showed that Pt grew as nanoparticles, and hydrogen underpotential deposition from cyclic voltammetry showed that the active surface area approached an asymptotic value around eight iterations. Catalytic activity, measured using the oxygen reduction reaction, reached a maximum at ten iterations. Both are shown to be influenced by the growth mode, but electrochemical modeling indicates that the trend in activity is also due to a change in activation energy, possibly due to changes in Pt electronic structure due to interactions with the CNTs. Durability cycling showed a greater than 85% retention of surface area for the first 10,000 cycles of accelerated stress testing but decayed steadily to about 50% after 30,000 cycles. This performance may be related to the phenomenon that limits surface area growth.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗