Development of Ambient Temperature Lithium-Ion Cells

Four types of materials have been evaluated as anodes for Li-ion cell fabrication. Among the materials evaluated, graphite and magnasium silicide were identified to be suitable candidate anode materials.

Li alloys Lithium-Ion↗

Anode-less Solid-State Li–S Batteries Enabled by Fe-Stabilized Polysulfides

Anode-less solid-state lithium-sulfur batteries (SSLSBs) with lithium sulfide (Li 2 S) as the cathode promise a high energy density and ease of manufacturing. However, Li 2 S is plagued by poor conductivity, sluggish activation kinetics, and a poor cycle life. Here, in this study, we report an FeCl 3 -activated Li 2 S (FLS) cathode with solid-state polysulfide intermediates generated through a redox reaction between FeCl 3 and Li 2 S. This strategy is shown to boost the electrical conductivity of Li 2 S by 7 orders of magnitude and lower the activation barrier. During cycling, Fe plays a significant role in stabilizing the highly active polysulfide species, contributing to the exceptional electrochemical performance. The FLS cathode achieves 80% capacity retention over 500 cycles with >99% Li 2 S utilization. Furthermore, a Li-metal-free (anode-less) full cell retained over 80% of its initial capacity after 240 cycles. This work underscores the promise of leveraging Fe-stabilized polysulfides in enabling high-energy, long-lasting, solid-state Li-S batteries.

25 ENERGY STORAGE↗

Engineering the Si Anode Interface via Particle Surface Modification: Embedded Organic Carbonates Lead to Enhanced Performance

Si nanoparticles (SiNPs) are recognized as a promising anode material for next-generation high-energy lithium-ion batteries. However, due to the more stringent requirements resulting from severe volume change, the solid-electrolyte interphase (SEI) on SiNPs plays a critical role in determining their cycling performance. Engineering the interface for higher stability has become an effective yet challenging approach to accommodate the deterioration of the silicon anode from the repeated lithiation/delithiation process. Herein, we report a novel approach of engineering a covalently bonded organic monolayer of ethylene carbonates onto the surface of the SiNPs that can help form a sturdy SEI. Finally, this molecule-level surface modification provides an effective approach to enable high-energy lithium-ion batteries with Si anodes.

25 ENERGY STORAGE↗

Impacts of Dissolved Ni 2+ on the Solid Electrolyte Interphase on a Graphite Anode

Transition metal (e.g. Ni) ions dissolved from layered-structured Ni-rich cathodes can migrate to the anode side and accelerate the failure of lithium-ion batteries. The investigations of the impact and distribution of Ni species on the solid electrolyte interphase (SEI) on the anode are crucial to understand the failure mechanism. Herein, we used time-of-flight secondary ion mass spectroscopy (TOF-SIMS) coupled with multivariate curve resolution (MCR) analysis to intuitively characterize the distribution of Ni species in the SEI. We find that the SEI on the graphite electrode using an EC-based electrolyte exhibits a multi-stratum structure. During accelerated aging of the LiNi 0.88 Co 0.08 Mn 0.04 O 2 /graphite full cell, the dissolution of Ni aggravates significantly upon cycling. A strong correlation between the dissolved-Ni and organic species in the SEI on graphite is illustrated. Here, the ion-exchange reaction between Ni 2+ and Li + ions in the SEI is demonstrated to be the main reason for the increase of SEI resistivity.

25 ENERGY STORAGE↗

Performance and properties of arsenic passivated lithium-titanium disulfide cells

In order to inhibit chemical degradation associated with the lithium-electrolyte interaction in ambient temperature lithium cells, an attempt was made to synthetically passivate the anode via ion implantation of arsenic. Solvent reduction is reduced although salt reaction with lithium is still present. The performance of the Li-TiS2 cell differs from those with standard electrodes, but further work is necessary to clarify the efficacy of this mode of passivation.

Yen, S. P. S.↗

Fracture Dynamics in Silicon Anode Solid-State Batteries

Solid-state batteries (SSBs) with silicon anodes could enable improved safety and energy density compared to lithium-ion batteries. However, degradation arising from the massive volumetric changes of silicon anodes during cycling is not well understood in solid-state systems. Here, we use operando X-ray computed microtomography to reveal micro- to macro-scale chemo-mechanical degradation processes of silicon anodes in SSBs. Mud-type channel cracks driven by biaxial tensile stress form across the electrode during delithiation. We also find detrimental cracks at the silicon/ solid electrolyte interface that form due to local reaction competition between neighboring domains of different sizes. Continuum phase-field damage modeling quantifies stress-driven channel cracking and shows that the lithiated silicon stress state is critical for determining the extent of interfacial fracture. This work reveals the mechanisms that govern SSBs compared to conventional lithium-ion batteries and provides guidelines for engineering chemomechanically resilient electrodes for high-energy batteries.

25 ENERGY STORAGE↗

Solid State Li Ion Batteries Using Si Composite Anodes

Solid Power has teamed with Argonne National Laboratory (ANL) to develop an all solid-state lithium-ion battery (ASSB), enabled by a high-capacity Si anode and a solid state electrolyte (SSE). Replacing liquid electrolytes with solid electrolytes addresses the calendar life challenges that currently limit the widespread adoption of Si anodes. In this project, Si-SSE composite materials have been developed with a specific capacity >1500 mAh/g (at electrode level). A Si anode was coated by using a roll-to-roll process. All-solid-state NMC-Si pouch cells have been assembled and tested. Cycle life of 1100 at 100% DOD has been demonstrated in the solid state Si pouch cell. Excellent calendar life is achieved in the cell via a high temperature storage test.

25 ENERGY STORAGE↗

Investigation of electrode materials for alkaline batteries

A number of amalgam electrode systems were investigated for possible use as high rate anodes and cathodes. The systems examined include: lithium, sodium, and potassium in Group 1, magnesium, calcium, and barium in Group 2, aluminum in Group 3, lead in Group 4, copper in Group 1b, and zinc and cadmium in Group 2b. The K(Hg) and Na(Hg) anodes in 10 VF and 15 VF (an unambiguous expression of concentration that indicates the number of formula weights of solute dissolved in a liter of solution) hydroxide solutions have proven satisfactory; some of these have produced current densities of more than 8 A/sq cm. None of the amalgam cathodes have approached this performance although the TI(Hg) has delivered 1 A/sq cm. Se(Hg) and Te(Hg) cathodes have given very stable discharges. Zn(Hg) and Cd(Hg) electrodes did not show good high rate characteristics, 200 to 300 mA/sq cm being about the maximum current densities obtainable. Both anodes are charged through a two-step process in which M(Hg) is first formed electrochemically and subsequently reduces Zn(II or Cd(II) to form the corresponding amalgam. The second step is extremely rapid for zinc and very slow for cadmium.

Arcand, G. M.↗

Direct reuse of graphite and lithium nickel manganese cobalt oxide (NMC) recovered from ultrafast-laser ablation debris in Li-ion battery electrodes

Here we demonstrate that debris collected from the ultrafast-laser ablation of graphite anodes can be directly reused in a lithium-ion battery with little to no negative effects on electrochemical performance. Further, we show that while post-ablation NMC (LiNi 0.33 Mn 0.33 Co 0.33 O) cathode debris will require additional processing before being incorporated into an electrode, its critical materials (nickel, manganese, and cobalt) are not lost during ablation and can be recovered for recycling. Pre- and post-ablation materials are characterized with a suite of diagnostics, including SEM, TEM, X-ray CT, EDS, and XRD, to study changes in material morphology, composition and crystal structure. Graphite exhibited little to no morphological or compositional changes and a slight annealing of its crystal structure. NMC underwent profound morphological and crystallographic changes, but retained its elemental composition. Finally, post-ablation materials were re-manufactured into electrodes and cycled vs lithium metal. Graphite showed equal or better capacity and Coulombic efficiency compared to pre-ablation electrodes, while the post-ablation NMC exhibited severely reduced electrochemical performance. Furthermore, we discuss the outlook for application of this work to advanced manufacturing lines that produce next-generation, laser-patterned electrodes.

25 ENERGY STORAGE↗

Extreme fast charge aging: Correlation between electrode scale and heterogeneous degradation in Ni-rich layered cathodes

Extreme fast charging (XFC) is a key requirement for the adoption of battery-based electric vehicles by the transportation sector. However, XFC has been shown to accelerate degradation, causing the capacity, life, and safety of batteries to deteriorate. There are no systematic studies in the open literature regarding aging modes in Ni-rich Li y Ni 0.a Mn 0.b Co 0.c O 2 (NMCabc) cathodes caused by fast charging. Herein, we report the effects of cathode composition and electrode loading in pouch cells containing NMC532, 622 and 811 paired with graphite and cycled under XFC conditions. The relative anisotropic volume change in the unit cell increases with Ni content in low-loading cells, while it levels up for all three NMC cathodes in high-loading cells because of substantial Li plating. The amounts of lithium plating and heterogeneity on the anode, determined by crystallographic phase quantification, were found to be correlated with electrode loading and cathode heterogeneity. The concentrations of the transition metals deposited on the anodes depend on NMCabc composition in a complex way. More particle cracking and surface degradation was found in NMC811. Here, the findings in this work provide a new understanding of the failure mechanisms and their practical implications for compositional tuning of future high-Ni NMCabc cathode materials during fast charging.

25 ENERGY STORAGE↗

Electrolyte Design for Silicon-Based Li-Ion Battery Guided by Chemical Reactivity of Solvents with a Model Silicon Anode

Here, the use of a model compound trimethylsilyllithium was demonstrated to study the chemical reactions of electrolyte with as a principal guide to design electrolyte for silicon-based Li-ion battery. Me 3 Si - anion initiates ring-opening polymerization of EC leading to the formation of poly(ethylene ether carbonate), which subsequently defragments into oligomers and dissolves in electrolyte. FEC was found to react differently, generating LiF and vinylene carbonate (VC). Further reaction of VC with Me 3 SiLi generated poly(hydroxymethylene), which is a nonsoluble polymer and the critical SEI component. The insights from this study have guided the new electrolyte design for the Si-based battery.

25 ENERGY STORAGE↗

Are There Opportunities To Re-Think How We Manufacture Synthetic Graphite?

This manuscript contributes a Viewpoint article to ACS Sustainable Resource Management and discusses the graphite supply chain, growing mismatch between graphite demand and global manufacturing capacity, current graphite manufacturing technologies, and different feedstocks.

alternative carbon feedstocks↗

Si-based materials for lithium-ion batteries I: Surface-modified Si/C powder

X-ray photoelectron spectroscopy was used to analyze Si/C powder obtained from Paraclete Energy, Inc. The spectra were obtained using incident monochromatic Al K α radiation at 1486.6 eV (0.834 01 nm). An initial survey spectrum together with O 1s, C 1s, and Si 2p are presented. A final survey spectrum was collected to ascertain the amount of beam-induced damage, which appears to be minimal. Finally, the spectra indicate the principal core level photoelectron and Auger electron signals and show the expected silicon-carbon species related to the surface modification process in addition to oxidized carbon and silicon due to atmospheric exposure.

25 ENERGY STORAGE↗

Si-based materials for lithium-ion batteries III: Surface-modified Si/C/polyvinylidine difluoride powder

X-ray photoelectron spectroscopy was used to analyze Si/C/polyvinylidine difluoride powder obtained from Paraclete Energy Inc. The spectra were obtained using incident monochromatic Al K α radiation at 1486.6 eV (0.834 01 nm). An initial survey spectrum together with F 1s, O 1s, C 1s, and Si 2p are presented. A final survey spectrum was collected to ascertain the amount of beam-induced damage, which appears to be minimal. Finally, the spectra indicate the principal core level photoelectron and Auger electron signals with only minor nitrogen signal and show the expected silicon-carbon and silicon-fluorine species related to the surface modification process in addition to oxidized carbon and silicon due to atmospheric exposure.

25 ENERGY STORAGE↗

Si-based materials for lithium-ion batteries V. n-SiO powder

X-ray photoelectron spectroscopy was used to analyze Si powders that have a native oxide surface, obtained from Paraclete Energy, Inc. The spectra were obtained using incident monochromatic Al K α radiation at 1486.6 eV (0.834 01 nm). An initial survey spectrum together with O 1s, C 1s, and Si 2p are presented. A final survey spectrum was collected to ascertain the amount of beam-induced damage, which appears to be minimal. Finally, the spectra indicate the principal core level photoelectron and Auger electron signals with only minor nitrogen signal and show the expected oxidized carbon and silicon species related to atmospheric exposure.

25 ENERGY STORAGE↗

Si-based materials for lithium-ion batteries VI. 15% surface-modified Si/C-graphite/carbon black/lithiated polyacrylic acid electrode

X-ray photoelectron spectroscopy was used to analyze a 15%Si/C-graphite/carbon black/lithiated polyacrylic acid electrode fabricated at the Cell Analysis, Modeling, and Prototyping Facility (CAMP), Argonne National Laboratory. The spectra were obtained using incident monochromatic Al K α radiation at 1486.6 eV (0.83 401 nm). An initial survey spectrum together with O 1s, C 1s, and Si 2p are presented. A final survey spectrum was collected to ascertain the amount of beam-induced damage, which appears to be minimal. The spectra indicate the principal core level photoelectron and Auger electron signals with only minor nitrogen and lithium signals and show the expected silicon-carbon species related to the surface modification process in addition to oxidized carbon and silicon due to atmospheric exposure as well contributions related to the binder material.

17 WIND ENERGY↗

Si-based materials for lithium-ion batteries VII. 70% surface-modified Si/C-carbon black/lithiated polyacrylic acid electrode

X-ray photoelectron spectroscopy (XPS) was used to analyze a 70% Si/C-carbon black/lithiated polyacrylic acid electrode fabricated at the Cell Analysis, Modeling, and Prototyping Facility (CAMP), Argonne National Laboratory. The spectra were obtained using incident monochromatic Al K α radiation at 1486.6 eV (0.834 01 nm). An initial survey spectrum together with O 1s, C 1s, and Si 2p are presented. A final survey spectrum was collected to ascertain the amount of beam-induced damage, which appears to be minimal. Finally, the spectra indicate the principal core level photoelectron and Auger electron signals with only minor copper, nitrogen, calcium, and lithium signals and show the expected silicon-carbon species related to the surface modification process in addition to oxidized carbon and silicon due to atmospheric exposure as well contributions related to the binder material.

25 ENERGY STORAGE↗