Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “bulk modulus”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 883 records · Page 49

Semiempirical formulae for elastic moduli and brittleness of diamondlike and zinc-blende covalent crystals

In the present work, semiempirical formulae for both bulk B and shear G moduli of diamondlike and zinc-blende covalent crystals are elaborated in terms of bond length and ionicity fraction of the bonding. The resulting expressions can be applied to a broad selection of covalent materials and their modulus predictions are in good agreement with the experimental data and those from ab initio calculations. Furthermore, the correlation between the ratio G/B and the aforementioned bonding parameters was investigated. The analysis of this relationship demonstrates that compared to the ionicity fraction, the bond length is the predominant parameter responsible for the brittle features of covalent materials.

36 MATERIALS SCIENCE↗

Nanostructured cobalt powders synthesised by polyol process and consolidated by Spark Plasma Sintering: Microstructure and mechanical properties

Bulk nanostructured cobalt was processed using a bottom-up strategy. Nanostructured particle agglomerates of about 50 and 240 nm in diameter were synthesised using a polyol route and subsequently consolidated by Spark Plasma Sintering (SPS). The microstructure of the starting powders and of the processed bulk samples was studied and characterised by X-ray diffraction (XRD) and transmission electron microscopy (TEM). The XRD patterns of the as-prepared powders showed predominantly a face centred cubic (fcc) crystalline phase, whereas both fcc and hexagonal close packed (hcp) phases were found within the consolidated samples. A sample with the highest relative mass density (94.5%) was obtained from the small powder particles. TEM observations revealed a lamellar substructure with a high density of nanotwins and stacking faults in every grain in the sample with the highest density. Brillouin light scattering (BLS) and quasistatic compression tests were used to investigate the mechanical properties of the consolidated samples. The two techniques yielded Young modulus values of 168 GPa and 130 GPa, respectively, in the sample with the highest density. This sample also exhibited a yield stress higher than 1 GPa after the compression test, which is mainly attributed to the lamellar-like structure occurring in almost every grain of the polycrystalline aggregate. - Highlights: Black-Right-Pointing-Pointer Cobalt nanoparticles produced by the polyol process present mainly the fcc metastable phase. Black-Right-Pointing-Pointer Bulk nanostructured cobalt is obtained from the nano-particles by Spark Plasma Sintering consolidation. Black-Right-Pointing-Pointer Nanotwins and stacking faults are present in every grain of the more dense sample. Black-Right-Pointing-Pointer Yield strength and plastic domain may be varied depending on the nanoparticle size and the porosity of the consolidated material.

36 MATERIALS SCIENCE↗

Investigation of specimen size effects by in-situ microcompression of equal channel angular pressed copper

Here, micropillar compression testing was implemented on Equal Channel Angular Pressed copper samples ranging from 200 nm to 10 µm in side length in order to measure the mechanical properties yield strength, first load drop during plastic deformation at which there was a subsequent stress decrease with increasing strain, work hardening, and strain hardening exponent. Several micropillars containing multiple grains were investigated in a 200 nm grain sample. The effective pillar diameter to grain size ratios, D/d , were measured to be between 1.9 and 27.2. Specimens having D/d ratios between 0.2 and 5 were investigated in a second sample that was annealed at 200 °C for 2 h with an average grain size of 1.3 µm. No yield strength or elastic modulus size effects were observed in specimens in the 200 nm grain size sample. However work hardening increases with a decrease in critical ratios and first stress drops occur at much lower stresses for specimens with D/d ratios less than 5. For comparison, bulk tensile testing of both samples was performed, and the yield strength values of all micropillar compression tests for the 200 nm grained sample are in good agreement with the yield strength values of the tensile tests.

36 MATERIALS SCIENCE↗

Interdigital Capacitance Local Non-Destructive Examination of Nuclear Power Plant Cable for Aging Management Programs

This Pacific Northwest National Laboratory milestone report describes progress to date on the investigation of non-destructive test methods focusing on local cable insulation and jacket testing using an interdigital capacitance (IDC) approach. Earlier studies have assessed a number of non-destructive examination (NDE) methods for bulk, distributed, and local cable tests. A typical test strategy is to perform bulk assessments of the cable response using dielectric spectroscopy, Tan , or partial discharge followed by distributed tests like time domain reflectometry or frequency domain reflectometry to identify the most likely defect location followed by a local test that can include visual inspection, indenter modulus tests, or Fourier Transform Infrared Spectroscopy (FTIR) or Near Infrared Spectroscopy FTIR (FTNIR). If a cable is covered with an overlaying jacket, the jacket’s condition is likely to be more severely degraded than the underlying insulation. None of the above local test approaches can be used to evaluate insulation beneath a cable jacket. Since the jacket’s function is neither structural nor electrical, a degraded jacket may not have any significance regarding the cable’s performance or suitability for service. IDC measurements offer a promising alternative or complement to these local test approaches including the possibility to test insulation beneath an overlaying jacket.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Simulated Adhesive Response to Aging (CRADA 453 Final Report)

The goal of this project was to develop a suite of molecular models to investigate adhesive performance as a result of the presence of different levels of moisture. These different levels of moisture are accepted in the adhesives community to represent different states of aging. First, our team modeled the adhesive’s crosslinked structure. Next, we modeled adding water to the crosslinked structure and used high performance computing resources to simulate water diffusion through the bulk adhesive and possible sites for chain scission. Finally, we modeled the response of the simulated adhesive to tensile loads at various levels of moisture content. These simulations were validated by experimental characterization by the industry partner. We found that the Young’s modulus of the adhesive decreased by about 30% when the water content increased to 3 wt.%. Our simulations also identified the likely site where the polymer chain could break. Our integration of molecular level simulations and mechanical property predictions using high performance computing with experimental studies of a hydrated epoxy system has yielded fundamental insights that will help industry advance lightweight joining technologies.

36 MATERIALS SCIENCE↗

Low-Velocity Impact Wear Behavior of Ball-to-Flat Contact Under Constant Kinetic Energy

The impact tests were conducted on metallic materials with different bulk hardness and Young’s moduli. Analysis of the dynamics response during the tribological process showed that the tested materials had similar energy absorption, where the peak contact force increased as the tests continued. Moreover, wear volume decreased with the increase in Young’s modulus of metals, except for Cr with a relatively low hardness. Wear rate was gradually reduced to a steady stage with increasing cycles, which was attributed to the decrease in contact stress and work-hardening effect. The main wear mechanism of impact was characterized by delamination, and the specific surface degradation mechanisms were depending on the mechanical properties of materials. The absorbed energy was used to the propagation of micro-cracks in the subsurface instead of plastic deformation, when resistance of friction wear and plastic behavior was improved. Hence, both the hardness and Young’s modulus played important roles in the impact wear of metallic materials.

36 MATERIALS SCIENCE↗

In Situ TEM Microcompression Pillar Size Effects in Fe-9Cr ODS

The objective of this paper is to ascertain the existence of a specimen size threshold, below which the material no longer exhibits bulk mechanical behavior when tested using in situ transmission electron microscopic (TEM) micro-compression pillars. In this work, sub-micron sized pillars of a model Fe-9Cr oxide dispersion strengthened (ODS) alloy were compressed in TEM in situ at room temperature, and attempts have been made to quantify the resulting data. Results are compared to mechanical property values in the archival literature, and a discussion on the validity of quantitative in situ TEM micro-compression data for ODS steel is included. In situ TEM mechanical testing is a relatively new technique enabling concurrent TEM imaging and mechanical testing of sub-micron-sized electron-transparent specimens. Due to limited sample volume of many nuclear materials, in situ TEM mechanical testing holds great promise for advancing our understanding of deformation phenomena. But it is well known that the dramatically reduced specimen size required for in situ testing can affect quantitative and qualitative deformation behaviors. However, Kiener, et al. used in situ TEM micro-compression pillars on irradiated and unirradiated single-crystal copper. They observed size independence in the irradiated material, while the unnirradiated material displayed a size threshold below which the mechanical properties deviated from those of bulk Cu. They assert that the more densely-spaced obstacles in irradiated Cu allow it to display bulk properties even in specimens having ∼ 100 nm dimensions. Similar to Kiener's findings, we hypothesize that unirradiated ODS will demonstrate a size threshold, but the in situ TEM micro-compression technique can be extended from single crystal materials to engineering alloys. An Fe-9Cr model ODS alloy was chosen for this study because of the broad interest in ODS for advanced nuclear reactors. ODS alloys exhibit high irradiation tolerance and high temperature creep resistance. New insight into deformation processes gained through in situ TEM mechanical testing could be valuable for the validation of ODS alloys for next generation nuclear reactors. The fact that the compressive yield stress and elastic modulus do not follow distinct trends as a function of specimen size is likely due to the high density of obstacles to dislocation motion. The ODS microstructure contains such obstacles as oxide nanoparticles, a fine grain structure, a high density of dislocation lines, and carbide precipitates. Since the deformation behavior is governed by the minimum separation distance between obstacles [1], it is plausible that the high obstacle density enables ODS alloy micropillars to exhibit bulk-like mechanical properties even prior to irradiation. Future work will focus on: (1) developing finite element models to help explain the difference in elastic moduli between bulk and micropillar tests, (2) understanding the spread in yield stress measurements at fixed micropillar volumes, and (3) extending this study to irradiated ODS. (authors)

36 MATERIALS SCIENCE↗

Investigation into the Wear and Dent Resistance of Ni/Ti Nanolaminates and Superelastic NiTi Coating

Metallic wear-resistant coatings, such as chromium based, are desired to prevent premature failure of working parts and are widely used in the oil and gas and aerospace industries. These coatings are extremely hard; however, researchers have found that an optimal coating will also be resilient. Bulk NiTi possesses a superelasticity effect that can provide wear resistance to parts that will experience impact, wear, and erosion daily. Yet, NiTi as a surface coating has not been fully exploited in industrial applications. Bulk NiTi production presents significant challenges, such as poor formability and machinability. This study attempts to fabricate NiTi through a heat treatment process of sputter-deposited alternating nanosized Ni and Ti layers. After annealing, the nanolaminate coatings contained the austenitic NiTi phase. The elastic modulus to hardness ratio and wear resistance showed that the nanolaminate annealed at 650 °C is comparable to the sputtered superelastic NiTi coating. The annealed nanolaminate coating is found to exhibit higher hardness than the monolayered NiTi, as well as, comparable elastic modulus to hardness values and dent resistance. The findings in this study reveal the superiority of 650 °C annealed nanolaminate NiTi coating over the monolayer NiTi.

36 MATERIALS SCIENCE↗

The mechanical behavior of metal-halide perovskites: Elasticity, plasticity, fracture, and creep

Wide ranging mechanical properties — elasticity, plasticity, fracture, and creep — most relevant to the mechanical reliability of perovskite solar cells (PSCs) are systematically investigated. High quality bulk single-crystals of the commonly studied metal-halide perovskites (MHPs) relevant to PSCs are fabricated and studied: CH 3 NH 3 PbBr 3 (MAPbBr 3 ) and CH 3 NH 3 PbI 3 (MAPbI 3 ). The first direct measurement of MHP Young's modulus (E) using uniaxial compression reveals E <100> of 13.1 ± 1.3 and 10.6 ± 1.0 GPa for MAPbBr 3 and MAPbI 3 , respectively. Further, the Vickers micro-hardness H (100) of MAPbBr 3 and MAPbI 3 is 0.54±0.02 GPa and 0.76±0.05 GPa, respectively. The Vickers micro-indentation fracture toughness K IC of MAPbBr 3 and MAPbI 3 is estimated at 0.20±0.03 MPa∙m 0.5 and 0.18±0.03 MPa∙m 0.5 , respectively. The stress-exponent, n, extracted from nanoindentation creep data is ~8 and ~10 for MAPbBr 3 and MAPbI 3 , respectively. The trends in these properties are discussed. These properties are best estimates and are recommended for use in future mechanical behavior and reliability analyses of MHPs and PSCs.

36 MATERIALS SCIENCE↗

A Broadband Laboratory Study of the Seismic Properties of Cracked and Fluid-Saturated Synthetic Glass Media

In this paper, for better understanding of frequency dependence (dispersion) of seismic wave velocities caused by stress-induced fluid flow, broadband laboratory measurements were performed on a suite of synthetic glass media containing both equant pores and thermal cracks. Complementary forced oscillation, resonant bar, and ultrasonic techniques provided access to millihertz-hertz frequencies, ~1 kHz frequency, and ~1 MHz frequency, respectively. The wave speeds or effective elastic moduli and associated dissipation were measured on samples under dry, argon- or nitrogen-saturated, and water-saturated conditions in sequence. The elastic moduli, in situ permeability, and crack porosity inferred from in situ X-ray computed tomography all attest to strong pressure-induced crack closure for differential (confining-minus-pore) pressures <30 MPa, consistent with zero-pressure crack aspect ratios <4 × 10 -4 . The low permeabilities of these materials allow access to undrained conditions, even at subhertz frequencies. The ultrasonically measured elastic moduli reveal consistently higher shear and bulk moduli upon fluid saturation—diagnostic of the saturated-isolated regime. For a glass rod specimen, containing cracks but no pores, saturated-isolated conditions apparently persist to subhertz frequencies—requiring in situ aspect ratios (minimum/maximum dimension) <10 -5 . In marked contrast, the shear modulus measured at subhertz frequencies on a cracked glass bead specimen of 5% porosity, is insensitive to fluid saturation, consistent with the Biot-Gassmann model for the saturated-isobaric regime. Finally, the measured dispersion of the shear modulus approaches 10% over the millihertz-megahertz frequency range for the cracked and fluid-saturated media—implying that laboratory ultrasonic data should be used with care in the interpretation of field data.

58 GEOSCIENCES↗

Microstructural and bulk property changes in hardened cement paste during the first drying process

This paper reports the microstructural changes and resultant bulk physical property changes in hardened cement paste (hcp) during the first desorption process. The microstructural changes and solid-phase changes were evaluated by water vapor sorption, nitrogen sorption, ultrasonic velocity, and {sup 29}Si and {sup 27}Al nuclear magnetic resonance. Strength, Young's modulus, and drying shrinkage were also examined. The first drying process increased the volume of macropores and decreased the volume of mesopores and interlayer spaces. Furthermore, in the first drying process globule clusters were interconnected. During the first desorption, the strength increased for samples cured at 100% to 90% RH, decreased for 90% to 40% RH, and increased again for 40% to 11% RH. This behavior is explained by both microstructural changes in hcp and C–S–H globule densification. The drying shrinkage strains during rapid drying and slow drying were compared and the effects of the microstructural changes and evaporation were separated.

36 MATERIALS SCIENCE↗

EGS Collab Testbed 1: Baseline Cross-well Seismic

As part of the geophysical characterization suite for the first EGS Collab tesbed, here are the baseline cross-well seismic data and resultant models. The campaign seismic data have been organized, concatenated with geometry and compressional (P-) & and shear (S-) wave picks, and submitted as SGY files. P-wave data were collected and analyzed in both 2D and 3D, while S-wave data were collected and analyzed in 2D only. Inversion models are provided as point volumes; the volumes have been culled to include only the points within source/receiver array coverage. The full models space volumes are also included, if relevant. An AGU 2018 poster by Linneman et al. is included that provides visualizations/descriptions of the cross-well seismic characterization method, elastic moduli calculations, and images of model inversion results.

15 GEOTHERMAL ENERGY↗

Mechanically induced self-propagating reaction and consequent consolidation for the production of fully dense nanocrystalline Ti{sub 55}C{sub 45} bulk material

We employed a high-energy ball mill for the synthesis of nanograined Ti{sub 55}C{sub 45} powders starting from elemental Ti and C powders. The mechanically induced self-propagating reaction that occurred between the reactant materials was monitored via a gas atmosphere gas-temperature-monitoring system. A single phase of NaCl-type TiC was obtained after 5 h of ball milling. To decrease the powder and grain sizes, the material was subjected to further ball milling time. The powders obtained after 200 h of milling possessed spherical-like morphology with average particle and grain sizes of 45 μm and 4.2 nm, respectively. The end-products obtained after 200 h of ball milling time, were then consolidated into full dense compacts, using hot pressing and spark plasma sintering at 1500 and 34.5 MPa, with heating rates of 20 °C/min and 500 °C/min, respectively. Whereas hot pressing of the powders led to severe grain growth (∼ 436 nm in diameter), the as-spark plasma sintered powders maintained their nanograined characteristics (∼ 28 nm in diameter). The as-synthesized and as-consolidated powders were characterized, using X-ray diffraction, high-resolution electron microscopy, and scanning electron microscopy. The mechanical properties of the consolidated samples obtained via the hot pressing and spark plasma sintering techniques were characterized, using Vickers microhardness and non-destructive testing techniques. The Vickers hardness, Young's modulus, shear modulus and fracture toughness of as-spark plasma sintered samples were 32 GPa, 358 GPa, 151 GPa and 6.4 MPa·m{sup 1/2}, respectively. The effects of the consolidation approach on the grain size and mechanical properties were investigated and are discussed. - Highlights: • Room-temperature synthesizing of NaCl-type TiC • Dependence on the grain size on the ball milling time • Fabrication of equiaxed nanocrystalline grains with a diameter of 4.2 nm • Fabrication of nanocrystalline bulk TiC material by SPS with minimal grain growth • Dependence of improved mechanical properties on the consolidation techniques.

36 MATERIALS SCIENCE↗

Elastic properties of suspended multilayer WSe{sub 2}

We report the experimental determination of the elastic properties of suspended multilayer WSe{sub 2}, a promising two-dimensional (2D) semiconducting material combined with high optical quality. The suspended WSe{sub 2} membranes have been fabricated by mechanical exfoliation of bulk WSe{sub 2} and transfer of the exfoliated multilayer WSe{sub 2} flakes onto SiO{sub 2}/Si substrates pre-patterned with hole arrays. Then, indentation experiments have been performed on these membranes with an atomic force microscope. The results show that the 2D elastic modulus of the multilayer WSe{sub 2} membranes increases linearly while the prestress decreases linearly as the number of layers increases. The interlayer interaction in WSe{sub 2} has been observed to be strong enough to prevent the interlayer sliding during the indentation experiments. The Young's modulus of multilayer WSe{sub 2} (167.3 ± 6.7 GPa) is statistically independent of the thickness of the membranes, whose value is about two thirds of other most investigated 2D semiconducting transition metal dichalcogenides, namely, MoS{sub 2} and WS{sub 2}. Moreover, the multilayer WSe{sub 2} can endure ∼12.4 GPa stress and ∼7.3% strain without fracture or mechanical degradation. The 2D WSe{sub 2} can be an attractive semiconducting material for application in flexible optoelectronic devices and nano-electromechanical systems.

36 MATERIALS SCIENCE↗

Elasticity of Amorphous Zirconium Tungstate at High Pressure

Compressional (VP) and shear wave (VS) velocities of the amorphous phase of ZrW2O8 have been measured up to 10.4 GPa at room temperature using ultrasonic interferometry in conjunction with synchrotron x radiation. The pressure-density relation is determined using the measured velocities. Both VP and VS, as well as the adiabatic bulk and shear moduli, exhibit monotonic increase with increasing pressure. The pressure derivatives of the bulk and shear moduli are determined to be KS0'=7.3(1) and G0'=1.8(1), with bulk and shear moduli KS0=61.7(5) GPa and G0=35.0(2) GPa. Comparing with the a phase, VP, VS, KS0, E, Tac, and s of the amorphous phase decrease by 14.8%, 10.0%, 17.2%, 2.9%, 1.2%, and 15.5%, along with 28% and 3.2% increase in density and shear modulus, respectively.

43 PARTICLE ACCELERATORS↗

Acoustic velocities, elasticity, and pressure-induced elastic softening in compressed neodymium

For the first time, the acoustic velocities and elasticity of double hexagonal close-packed neodymium (Nd) were measured at high pressure using ultrasonic interferometry in conjunction with synchrotron X-ray techniques. Here, both the compressional and shear wave velocities increased with an increase in pressure of up to ~5.4 GPa before they exhibited almost constant values upon further compression. This pressure-induced elastic wave velocity softening can be attributed to the structural instability in dhcp-Nd. From the current sound velocities and density data, we obtained new bulk and shear moduli as well as their pressure dependence for polycrystalline dhcp-Nd, yielding $B_0$=33.2(9) GPa, $G_0$=14.1(5) GPa, $\partial$$B/$$\partial$$P$ = 3.6 (4) and $\partial$$=G/$$\partial$$P$ = 1.3 (2) while other elasticity-related/mechanical properties, including Young's modulus, Debye temperature, Poisson's ratio, and Grüneisen parameter, which are important parameters for the application of Nd in extreme environments, were also derived.

36 MATERIALS SCIENCE↗

Diameter-Dependent Modulus and Melting Behavior in Electrospun Semicrystalline Polymer Fibers

Confinement of the semicrystalline polymers, poly(ethylene-co-vinyl acetate) (PEVA) and low-density polyethylene (LDPE), produced by electrospinning has been observed to produce fibers with large protrusions, which have not been previously observed in fibers of comparable diameters produced by other methods. SAXS spectra confirmed the crystalline structure and determined that the lamellar spacing was almost unchanged from the bulk. Measurement of the mechanical properties of these fibers, by both shear modulation force microscopy (SMFM) and atomic force acoustic microscopy (AFAM), indicates that the modulii of these fibers increases with decreasing diameter, with the onset at {approx}10 {micro}m, which is an order of magnitude larger than previously reported. Melting point measurements indicate a decrease of more than 7% in T{sub m}/T{sub 0} (where T{sub m} is the melting point of semicrystalline polymer fibers and T{sub 0} is the melting point of the bulk polymer) for fibers ranging from 4 to 10 {micro}m in diameter. The functional form of the decrease followed a universal curve for PEVA, when scaled with T{sub 0}.

36 MATERIALS SCIENCE↗