Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STRESS CORROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 883 records · Page 49

PV encapsulant formulations and stress test conditions influence dominant degradation mechanisms

Polyethylene-based poly(ethylene-co-vinyl acetate) (EVA), polyolefin elastomer (POE), and thermoplastic polyolefin (TPO) are common polymer candidates for photovoltaic (PV) module encapsulants. The choice of encapsulant must be carefully considered in novel module designs, such as bifacial glass/glass laminates, to limit performance degradation through loss of optical transmittance, mechanical integrity, and corrosion - as well as potential-induced degradation. Encapsulant quality and resilience against environmental stressors are readily influenced by the additives in the encapsulant formulation. Here, we show that, the changes in optical transmittance after UV aging result from the discoloration caused by interactions between additives, and optical scattering from changes in the polymer crystal structure. We observed competing cross-linking and chain scission mechanisms, with their kinetics influenced by the presence of oxygen and elevated temperatures. Increasing chamber temperatures from 55 °C to 85 °C during the UV stress test amplified encapsulant discoloration and promoted polymer cross-linking, causing severe, irreversible damage that remains to be proven field relevant. Damp heat aging was found to be insufficient to produce significant encapsulant degradation; however, combining stress tests sequentially allowed detection of further degradation beyond the limitations of the damp heat test alone. Appropriate degradation screening methods are necessary to uncover potential encapsulant weaknesses.

14 SOLAR ENERGY↗

Fracture toughness and corrosion resistance of semisolid AlSi5 alloy

The aim of this work was to investigate fracture toughness and corrosion resistance of semisolid AlSi5 castings, compared to samples obtained from conventional casting operations. In order to have a semisolid microstructure, the melt alloy was treated by means of ultrasound during solidification and then poured into permanent moulds. Mechanical properties of semisolid and conventional castings were compared by means of ultimate tensile strength (R{sub m}), yield stress (Rp{sub 02}) and hardness (HV) measurements. Fracture mechanics tests were carried out on Single Edge Notched Bend (SENB) specimens, machined from castings, and pre-cracked by fatigue. These tests were performed to determine the effect of the microstructure on the J-Integral resistance (J-R) behavior and to deeply understand the ductile fracture behaviour of semisolid parts. The J-Integral versus spaced crack extension (J-{Delta}a) curves showed an improved resistance of the semisolid microstructure, due to the higher ductility. Finally, the corrosion behaviour of semisolid samples was compared to that of castings coming from solidification of fully liquid alloy by means of electrochemical potentiodynamic polarization tests. It was observed that the globular microstructure offers better quality, in terms of higher mechanical properties, as a consequence of a more uniform distribution of the solute.

36 MATERIALS SCIENCE↗

Anion transport as a target of adaption to perchlorate in sulfate-reducing communities

Inhibitors can be used to control the functionality of microbial communities by targeting specific metabolisms. The targeted inhibition of dissimilatory sulfate reduction limits the generation of toxic and corrosive hydrogen sulfide across several industrial systems. Sulfate-reducing microorganisms (SRM) are specifically inhibited by sulfate analogs, such as perchlorate. Previously, we showed pure culture SRM adaptation to perchlorate stress through mutation of the sulfate adenylyltransferase, a central enzyme in the sulfate reduction pathway. Here, we explored adaptation to perchlorate across unconstrained SRM on a community scale. We followed natural and bio-augmented sulfidogenic communities through serial transfers in increasing concentrations of perchlorate. Our results demonstrated that perchlorate stress altered community structure by initially selecting for innately more resistant strains. Isolation, whole-genome sequencing, and molecular biology techniques allowed us to define subsequent genetic mechanisms of adaptation that arose across the dominant adapting SRM. Changes in the regulation of divalent anion:sodium symporter family transporters led to increased intracellular sulfate to perchlorate ratios, allowing SRM to escape the effects of competitive inhibition. Thus, in contrast to pure-culture results, SRM in communities cope with perchlorate stress via changes in anion transport and its regulation. Finally, this highlights the value of probing evolutionary questions in an ecological framework, bridging the gap between ecology, evolution, genomics, and physiology.

59 BASIC BIOLOGICAL SCIENCES↗

Disposal of High-Level Nuclear Waste in Deep Horizontal Drillholes

Spent nuclear fuel and high-level radioactive waste can be disposed in deep horizontal drillholes in sedimentary, metamorphic or igneous rocks. Horizontal drillhole disposal has safety, operational and economic benefits: the repository is deep in the brine-saturated zone far below aquifers in a reducing environment of formations that can be shown to have been isolated from the surface for exceedingly long times; its depth provides safety against inadvertent intrusion, earthquakes and near-surface perturbations; it can be placed close to the reactors and interim storage facilities, minimizing transportation; disposal costs per ton of waste can be kept substantially lower than for mined repositories by its smaller size, reduced infrastructure needs and staged implementation; and, if desired, the waste could be retrieved using “fishing” technology. In the proposed disposal concept, corrosion-resistant canisters containing unmodified fuel assemblies from commercial reactors would be placed end-to-end in up to 50 cm diameter horizontal drillholes, a configuration that reduces mechanical stresses and keeps the temperatures below the boiling point of the brine. Other high-level wastes, such as capsules containing 137 Cs and 90 Sr, can be disposed in small-diameter horizontal drillholes. We provide an overview of this novel disposal concept and its technology, discuss some of its safety aspects and compare it to mined repositories and the deep vertical borehole disposal concept.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

040226_AnnularFuel_FuelPerformance_LRSv2

This slide deck summarizes a comparative fuel performance assessment of four annular fuel concepts for pressurized water reactor applications against a reference 17×17 fuel design. Overall, annular fuel geometry improves several key thermal-mechanical performance metrics, with the large-annulus configuration providing the most favorable balance of benefits. Relative to the reference design, annular fuel reduces peak fuel temperature by lowering thermal resistance through a thinner fuel pellet and smaller heat-conduction path. At the same time, the reduced fuel volume raises local burnup and correspondingly increases fission gas release. Despite this, rod internal pressure at end of life decreases because the annular geometry provides greater internal void volume. Annular designs also tend to delay fuel-cladding gap closure, although this advantage diminishes in thin-gap configurations where the smaller initial gap accelerates closure. Similarly, hoop stress and hoop strain are generally reduced for annular fuel, but both increase as the initial gap becomes smaller, indicating a potential cladding integrity concern for thin-gap designs. Corrosion performance shows no meaningful variation among the concepts considered. Taken together, the results indicate that annular fuel can offer significant performance advantages in a PWR environment, with large-annulus designs emerging as the strongest candidate while thin-gap geometries introduce more challenging mechanical margins.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Design and life-cycle considerations for unconventional-reservoir wells

This paper provides an overview of design and life-cycle considerations for certain unconventional-reservoir wells. An overview of unconventional-reservoir definitions is provided. Well design and life-cycle considerations are addressed from three aspects: upfront reservoir development, initial well completion, and well-life and long-term considerations. Upfront-reservoir-development issues discussed include well spacing, well orientation, reservoir stress orientations, and tubular metallurgy. Initial-well-completion issues include maximum treatment pressures and rates, treatment diversion, treatment staging, flowback and cleanup, and dewatering needs. Well-life and long-term discussions include liquid loading, corrosion, refracturing and associated fracture reorientation, and the cost of abandonment. These design considerations are evaluated with case studies for five unconventional-reservoir types: shale gas (Barnett shale), tight gas (Jonah feld), tight oil (Bakken play), coalbed methane (CBM) (San Juan basin), and tight heavy oil (Lost Hills field). In evaluating the life cycle and design of unconventional-reservoir wells, 'one size' does not fit all and valuable knowledge and a shortening of the learning curve can be achieved for new developments by studying similar, more-mature fields.

01 COAL, LIGNITE, AND PEAT↗

Cold Spray NDE for Porosity and Other Process Anomalies

This paper describes a technology review of non-destructive examination (NDE) methods that can be applied to cold spray coatings. Cold spray is a process for depositing metal powder at high velocity so that it bonds to the substrate metal without significant heating that would be likely to cause additional residual tensile stresses. Coatings in the range from millimeters to centimeters are possible at relatively high deposition rates. Cold spray coatings that may be used for hydroelectric components that are subject to erosion, corrosion, wear, and cavitation damage are of interest. The topic of cold spray NDE is treated generally however and may be considered applicable to virtually any cold spray application except where there are constraints of the hydroelectric component application that bear special consideration. Hydroelectric turbine components are primarily made from low carbon and austenitic stainless steels. They are typically very large components that are partially assembled on-site. Transport of these components within the hydroelectric facility and away from the hydroelectric facility is challenging due to the component’s size and weight, high cost of disassembly, and the confined space of the dam. One method for prolonging component life is application of cold spray and thermal powder metal coatings to the components most susceptible to erosion, corrosion, cracking, and mechanical wear. Process controls and visual inspections have historically been applied to cold spray application; however, quantitative NDE could detect anomalies not readily apparent from such a visual examination. Optical profilometry, Eddy current, ultrasound, and hardness tests are shown for one set of good, fair, and poor Nickle-Chrome (NiCr) on 304 stainless steel (304SS) cold spray samples to demonstrate inspection possibilities. The primary indicator of cold spray quality is the cold spray porosity that is most directly measured with witness-sample destructive examinations (DE) – mostly photo-micrographs. These DE generated porosity values are correlated with optical profilometry, eddy current, ultrasound, and hardness test NDE methods to infer the porosity and other Information of interest. These parameters of interest primarily include: • Porosity primarily caused by improper process conditions (temperature, gas velocity, spray standoff, spray angle, powder size, condition, surface cleanliness, surface oxide, etc.). • Presence/absence of the cold spray coating including possible over-sprayed voids • Coating thickness Optical profilometry measurements of surface roughness trended with porosity plus if compared with a reference measurement or reference drawing would provide information on the coating thickness. Ultrasound could provide similar surface profile information plus attenuation measurements trended with porosity. The ultrasound measurements however may be limited to geometries where the substrate back-wall is normal to the cold spray surface and not too thick. Eddy current showed a strong correlation with porosity. Eddy currents can also be sensitive to cracks and do not need fluid coupling to make measurements. Eddy currents however are not sensitive to coating thicknesses in most cases. Vickers hardness measurements also tracked well with porosity. These types of hardness measurements however are also not sensitive to coating thickness. An NDE program may include multiple measurements. Acknowledgement: This work is sponsored by Bonneville Power Administration (BPA) under their technology innovation project program. Such support does not constitute BPA endorsement of views expressed in this work.

Glass, Samuel W.↗

The challenge of acquiring a satisfactory EBSD result of CWSR Zircaloy-4 cladding tube

This article presents a methodology combining SEM, EDS, conventional EBSD, and transmission-EBSD to analyse a recrystallised Zircaloy-4 sheet and cold-worked stress-relieved (CWSR) Zircaloy-4 cladding in unprecedented detail. Second-phase precipitates (SPPs) in Zircaloy-4 specimens were revealed after chemical polishing using a solution containing hydrofluoric acid (HF). Pitting corrosion of Zircaloy-4 specimens was revealed after electropolishing using an electrolyte containing HClO4. A zirconium coupon without SPPs was used to confirm the chemical response of SPPs on surface morphology. Intrinsic features of cold-worked Zircaloy-4 such as relatively small grain sizes, high dislocation density, and complex microstructure make it significantly more difficult to collect excellent EBSD results compared to recrystallised Zircaloy-4. The fine hydride structure of as-hydrided CWSR Zircaloy-4 cladding further increases the level of challenge on EBSD analysis.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Thermo-mechanical and neutron lifetime modeling and design of Be pebbles in the neutron multiplier for the LIFE engine

Concept designs for the laser-initiated fusion/fission engine (LIFE) include a neutron multiplication blanket containing Be pebbles flowing in a molten salt coolant. These pebbles must be designed to withstand the extreme irradiation and temperature conditions in the blanket to enable a safe and cost-effective operation of LIFE. In this work, we develop design criteria for spherical Be pebbles on the basis of their thermomechanical behavior under continued neutron exposure. We consider the effects of high fluence/fast flux on the elastic, thermal and mechanical properties of nuclear-grade Be. Our results suggest a maximum pebble diameter of 30 mm to avoid tensile failure, coated with an anti-corrosive, high-strength metallic shell to avoid failure by pebble contact. Moreover, we find that the operation temperature must always be kept above 450 C to enable creep to relax the stresses induced by swelling, which we estimate to be at least 16 months if uncoated and up to six years when coated. We identify the sources of uncertainty on the properties used and discuss the advantages of new intermetallic beryllides and their use in LIFE's neutron multiplier. To establish Be-pebble lifetimes with improved confidence, reliable experiments to measure irradiation creep must be performed.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Response of bentonite microbial communities to stresses relevant to geodisposal of radioactive waste

Microbes have been isolated previously from bentonite materials that may be used as barriers for the disposal of radioactive waste. Actively respiring microbes in such barrier materials, within a repository environment, have the potential to adversely affect waste container corrosion rates. Additionally, they could potentially alter the properties of the bentonite barrier itself. This is of significance, since the integrity of the waste container and properties of the bentonite barrier are required to fulfil defined safety functions. Furthermore to help identify the critical factors that affect microbial activity in bentonite materials, this study examines the impact of a range of parameters that could affect microbial metabolism in a geodisposal environment. Several bentonites from different sources (bentonite mined from locations in Spain and the USA, along with commercially-sourced bentonite) were subjected to increased pressure (74 MPa, 30 s), heat (90 °C, 24 h), and irradiation (1000 Gy, 24.17 Gy min –1 ), before incubation in growth media selective for sulfate-reducing bacteria (SRB) or iron-reducing bacteria (IRB).

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fatigue Testing and Characterization of Pre-hydrided Zircaloy-4 Cladding Tubes

The solubility of hydrogen in Zircaloy-4 (Zry-4) at the cladding operating temperature is near 100 wt. ppm. Above this solubility limit, excess hydrogen precipitates as δ-hydride platelets in the cladding material. Because of the effect of the thermal gradient across the cladding thickness on the migration and precipitation of hydrogen, hydride rims are often observed at the cladding outer surface; under excessive corrosion conditions hydride blisters are possible. It is well known that the fatigue of metal alloys, especially high cycle fatigue, is sensitive to the status of surface including the microstructure, roughness, and residual stress. Thus, the question considered herein, is whether excessive hydrogen pickup modifies the microstructure such that it has a degradation effect on the fatigue performance of cladding during operation. This report describes the evaluation of fatigue performance of a pre-hydrided Zry-4 cladding. A commercial Zry-4 was polished and pre-hydrided to 800 ppm and 1300 ppm H contents. The fatigue testing was conducted under strain control at 5 Hz with fully-reversed bending by using a cyclic integrated reversible bending fatigue tester (CIRFT). Six specimens with 1300 ppm and one specimen with 800 ppm were tested. Significant variation in test results were observed. While two of the 1300 ppm specimens failed with less than 1 ×10 5 cycles (at 0.32% and 0.41%), the four other samples did not fail over the strain amplitude range of 0.25% to 0.38%. Interestingly, the fracture initiation site of the failed samples was on the outside diameter (OD) surface rather than on the inside diameter (ID) surface as is typical for the as-polished cladding. This suggested a degrading effect of the hydriding process. Subsequently, three of the unfailed specimens were then further tested at ~0.43% to observe where failure initiation occurred. Significant variation was also observed in these three specimens. One specimen failed at ~9000 cycles while the two others failed at 43000 and 1.06 ×10 5 cycles. The performance here correlated to the location of failure initiation; failure initiated on the OD in the sample that failed after 9000 cycles while it initiated on the ID in the sample that failed after 43000 and 1.06 ×10 5 cycles. Flat features at the OD initiation sites suggest a brittle hydride feature on the surface of those samples was the cause of the degradation in fatigue performance, though the overall hydrogen levels in all samples was similar. A summary of all the observations is provided below: • The un-failed specimens with 1300 ppm H were cycled to failure with a higher amplitude near 0.43%. In addition, the fatigue-treated specimen tended to have a longer fatigue at the same induced amplitude. • Fractography revealed a mixed failure mode for the pre-hydrided specimen. Particularly, the specimen with fracture initiation site (FIS) located on the outer diameter surface of tube tended to have a shorter fatigue life than that of FIS on the inner diameter surface. • Etched cross section was shown to have hydride platelets aligned with tube longitudinal axis as expected, and the density of hydrides is at the similar level as in literature data. Meanwhile, a LECO procedure was applied for hydrogen concentration measurement, which showed the measured hydrogen contents are close to the nominal value. • With the polished cladding tube as baseline, O’Donnell-Lager (O-L) analysis showed that a decrease of about 50% in reduction-of-area (RA) would be needed for the O-L fitting to the fatigue data of 1300 ppm cladding. The suggestion for the next steps is provided.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Mechanisms Underpinning Degradation of Protective Oxides and Thermal Barrier Coatings in High Hydrogen Content (HHC) - Fueled Turbines

The overarching goal of this research program has been to evaluate the potential impacts of coal-derived syngas and high-hydrogen content fuels on the degradation of turbine hot-section components through attack of protective oxides and thermal barrier coatings. The primary focus of this research program has been to explore mechanisms underpinning the observed degradation processes, and connections to the combustion environments and characteristic non-combustible constituents. Based on the mechanistic understanding of how these emerging fuel streams affect materials degradation, the ultimate goal of the program is to advance the goals of the Advanced Turbine Program by developing materials design protocols leading to turbine hot-section components with improved resistance to service lifetime degradation under advanced fuels exposures. This research program has been focused on studying how: (1) differing combustion environments – relative to traditional natural gas fired systems – affect both the growth rate of thermally grown oxide (TGO) layers and the stability of these oxides and of protective thermal barrier coatings (TBCs); and (2) how low levels of fuel impurities and characteristic non-combustibles interact with surface oxides, for instance through the development of molten deposits that lead to hot corrosion of protective TBC coatings. The overall program has been comprised of six inter-related themes, each comprising a research thrust over the program period, including: (i) evaluating the role of syngas and high hydrogen content (HHC) combustion environments in modifying component surface temperatures, heat transfer to the TBC coatings, and thermal gradients within these coatings; (ii) understanding the instability of TBC coatings in the syngas and high hydrogen environment with regards to decomposition, phase changes and sintering; (iii) characterizing ash deposition, molten phase development and infiltration, and associated corrosive/thermo-chemical attack mechanisms; (iv) developing a mechanics-based analysis of the driving forces for crack growth and delamination, based on molten phase infiltration, misfit upon cooling, and loss of compliance; (v) understanding changes in TGO growth mechanisms associated with these emerging combustion product streams; and (vi) identifying degradation resistant alternative materials (including new compositions or bi-layer concepts) for use in mitigating the observed degradation modes. To address the materials stability concerns, this program integrated research thrusts aimed at: (1) Conducting tests in simulated syngas and HHC environments to evaluate materials evolution and degradation mechanisms; assessing thermally grown oxide development unique to HHC environmental exposures; carrying out high-resolution imaging and microanalysis to elucidate the evolution of surface deposits (molten phase formation and infiltration); exploring thermo-chemical instabilities; assessing thermo-mechanical drivers and thermal gradient effects on degradation; and quantitatively measuring stress evolution due to enhanced sintering and thermo-chemical instabilities induced in the coating. (2) Executing experiments to study the melting and infiltration of simulated ash deposits, and identifying reaction products and evolving phases associated with molten phase corrosion mechanisms; utilizing thermal spray techniques to fabricate test coupons with controlled microstructures to study mechanisms of instability and degradation; facilitating thermal gradient testing; and developing new materials systems for laboratory testing; (3) Correlating information on the resulting combustion environments to properly assess materials exposure conditions and guide the development of lab-scale simulations of material exposures; specification of representative syngas and high-hydrogen fuels with realistic levels of impurities and contaminants, to explore differences in heat transfer, surface degradation, and deposit formation; and facilitating combustion rig testing of materials test coupons.

Mumm, Daniel↗

Operando carbon corrosion measurements in fuel cells using boron-doped carbon supports

Carbonaceous materials are the most common catalyst supports in proton exchange membrane fuel cell (PEMFCs), yet their corrosion is one of the limiting factors in achieving high durability. Herein, we doped carbon supports with boron (B) to increase the corrosion-resistance of the support. Two types of B-doped carbons were synthesized and studied as platinum support materials. Further, they varied in their morphologies, surface areas, and the types of boron species. The durability of Pt/B-doped carbon catalysts was investigated using the US-DOE catalysts’ supports accelerated stress test (AST) and a mass-spectrometer connected to the fuel cell effluent stream to quantify the mass of corroded carbon support in operando. The addition of boron to the carbon increased the stability of Pt catalysts in long-term usage of PEMFC. After 4000 AST cycles, more than 50% of initial current density was preserved for the boron-containing systems, while less than 30% of it remained with Vulcan carbon (Pt/V). Also, the Pt/B-doped carbon samples demonstrated better electrochemical active surface area (ECSA) stability when compared to Pt/V. Carbon loss measurements showed that B-doped carbons have higher resistance to electrochemical corrosion than unmodified carbon. Specifically, the substitutional boron-doped carbon demonstrated an extremely high stability and low corrosion rate.

25 ENERGY STORAGE↗

Microstructural and Oxidation Effects of Nb Additions to U3Si2

U3Si2 is a long term, accident-tolerant nuclear fuel candidate for light-water reactors because of its superior thermal conductivity and increased uranium density when compared to traditional uranium dioxide (UO2). While reducing internal thermal stresses and increasing efficiency, U3Si2 exhibits energetic oxidation during certain off-normal and accident scenarios, which include coolant or steam exposure. To mitigate this, Nb is investigated as an alloy constituent to enhance corrosion resistance and increase mechanical strength. The work presented investigates the response of Nb-alloyed U3Si2 to steam atmospheres. A thermogravimetric analysis is conducted in flowing steam to T > 1000 °C to assess oxidation resistance. The phase characterization of as-melted, thermally annealed and post-oxidation compositions with up to 12 vol% Nb by powder X-ray diffraction, scanning electron microscopy, and energy dispersive spectroscopy is reported.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Bison Modeling of SiC/SiC Cladding Including Fuel-Pellet Interaction

SiC/SiC composites are considered leading candidates for accident tolerant fuel cladding in light water reactors. However, when SiC-based materials are exposed to neutron irradiation, they experience significant changes in dimensions and physical properties. In the extreme nuclear reactor environment, SiC-based fuel cladding will see neutron damage, significant heat flux, as well as a corrosive environment. In this report, we evaluate the effect of non-uniform changes in the dimensions caused by neutron irradiation with variable temperatures, along with the closing of the fuel – clad gap, on the stress development in the clad over the course of time. To ensure reliable and safe operation of accident tolerant fuel cladding concepts such as SiC-based materials, it is important to assess its thermo-mechanical performance under in-reactor conditions of irradiation and realistic temperature distributions. In this work, we have used the BISON fuel performance modeling code to perform the thermo-mechanical analysis of SiC/SiC cladding. A constitutive model is constructed and solved numerically to predict the stress distribution and variation in the cladding under normal operating conditions. The dependence of dimensions and physical properties variation with irradiation and temperature has been incorporated. These initial results from the analyses provides insights about the stress distribution and variation with time in the cladding as well as the interaction of fuel pellet with the cladding under different conditions of initial fuel pellet-cladding gap and steady state power levels.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Design of a Supercritical Carbon Dioxide Corrosion Test Rig for Tube-to-Tubesheet Joint and High Temperature Insulation Testing

Supercritical carbon dioxide (S-CO{sub 2}) Brayton cycles are attractive for thermal power generation since they offer highly efficient means of power generation (thermal solar, coal, nuclear, etc.) with a compact footprint, resulting in potential cost savings. The University of California, Berkeley (UCB) is developing an S-CO{sub 2}- Brayton Cycle design for advanced reactors using sodium and molten salt coolants. Coiled tube gas heaters (CTGH) made from 316L stainless steel are presently foreseen to transfer heat from a sodium or molten salt coolant at atmospheric pressure (approximately 0.1 MPa) to an S-CO{sub 2} power conversion fluid at very high pressure (approximately 20 MPa or more). CTGHs operate at temperatures of 400 to 700 deg. C where time-dependent creep is an important design issue. Given the high external pressure conditions and compressive stress, the highest stresses and creep rates in CTGH are expected to occur at the tube-to-tubesheet joints. UCB has developed different diffusion bonding techniques to fabricate 316L stainless steel tube-to-tubesheet joint dummies representative of the final design: press fitting and diffusion bonding, tube expansion and diffusion bonding as well as hybrid friction diffusion bonding. High pressure/temperature testing of such joints in an S-CO{sub 2} environment is important prior to deployment and will be foreseen with the corrosion test rig introduced in this work. This summary provides a brief overview of an Innovative S-CO, creep corrosion test rig for tube-to-tube sheet joint testing currently under construction at UCB. In contrast to other comparable test rigs, the design (1) makes the samples an active part of the pressure barrier and (2) uses internal insulation to reduce the temperature at the vessel wall, allowing the vessel to be manufactured from commercial carbon steel. (authors)

42 ENGINEERING↗

EXPERIMENTAL-BASED DISCUSSION FOR THE SEPARATION OF RESIDUAL STRESSES AND COLD WORK IN SHOT PEENED IN718 USING HIGH FREQUENCY EDDY CURRENT SPECTROSCOPY

Typical aero engine alloys, such as IN718, can be surface-treated by shot peening to induce near-surface compressive strains. To calculate the remaining operation time for those critical aero engine components, a quantitative nondestructive determination of near-surface strain gradients has to be developed. We have demonstrated in the past, that it is possible to obtain a characteristic depth profile (surface and sub-surface) of the electrical conductivity of shot peened specimen by using high-frequency eddy current techniques. The measured conductivity profile is resulting from residual stresses, cold work, surface roughness, and the microstructure of the material. The objective is to measure residual stresses (separately from other material properties) in such components after a defined life time. It can be assumed, that surface roughness and microstructure remain unchanged in IN718 materials over their lifetime, but cold work and residual stresses can change independently. Consequently, there is a need to clearly separate the information from both material properties of received eddy current conductivity signals in order to obtain specific information related to residual stresses. This paper presents results acquired from different experiments, conducted to separate both effects by using the eddy current technique on shot peened IN718 materials. We present different physical approaches and illustrate the experiments to solve them. In addition, we will demonstrate that there is a need to use additional techniques, for example ultrasonic time-of-flight measurements, to separate the effects of residual stresses from compound (mixed) signals obtained on cold work samples.

36 MATERIALS SCIENCE↗

Field‐Relevant Degradation Mechanisms in Metal Halide Perovskite Modules

Field testing, failure analysis, and understanding of degradation mechanisms are essential to advancing metal halide perovskite (MHP) photovoltaic (PV) technology toward commercialization. Here, we present performance data from up to 1 year of outdoor testing of MHP modules in Golden, Colorado. The module encapsulation architecture and encapsulant materials have a significant impact on module reliability, with modules containing a polyolefin elastomer (POE) in addition to a desiccated polyisobutylene (PIB) edge seal outlasting modules with only a PIB edge seal or PIB blanket. Nondestructive and destructive characterization of the field-tested modules points to module scribes and interfaces as areas of potential mechanical weakness and chemical migration, resulting in shunt pathways and increased series resistance. Finally, indoor accelerated stress testing with light and elevated temperatures is performed, demonstrating failure with similar scribe degradation signatures as compared to the field-tested modules. In conclusion, under both outdoor testing and light and elevated temperature conditions, electrochemical corrosion between the copper electrode and the mobile iodine ions appeared dominant, with a significant progression at the scribes that is speculated to result from an interplay between the initial laser damage and joule heating from enhanced ion diffusion under bias.

14 SOLAR ENERGY↗