Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STEELS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 883 records · Page 49

Circular economy pathways for decarbonizing aluminum and steel automotive body sheet components in the United States

Decarbonizing vehicle production is essential to reducing automotive sector emissions. This study quantifies greenhouse gas (GHG) emissions from aluminum and steel auto-body sheet components produced in the US. It evaluates the effectiveness of circular economy (CE) strategies (greater closed-loop recycling of pre-consumer scrap, post-consumer scrap, and increased manufacturing yields) to reduce supply chain emissions across different process technology and electricity grid decarbonization pathways. We combine dynamic material flow analysis (2025–2050) with cradle-to-gate life-cycle modeling to assess production emissions and the potential reductions associated with the CE strategies under frozen, moderate, and aggressive technology and grid decarbonization scenarios. Current emissions intensities are estimated at approximately 12.3 kg.CO₂eq/kg of aluminum and 4.3 kg.CO₂eq/kg of steel sheet embedded in the vehicle. Under the frozen decarbonization scenario and current levels of circularity, annual emissions attributable to US aluminum and steel auto-body sheet supply chains could rise by 54 % and 18 % respectively by 2050. Rapid deployment of the CE strategies can cut these annual emissions in 2050 by 52 % for aluminum and 44 % for steel. However, scrap quality constraints lead to saturation points, limiting these benefits unless addressed. Aggressive deployment of low-carbon production technologies and a low-carbon grid reduces the relative benefit of implementing the CE strategies; however, even under the aggressive technology and grid decarbonization scenario, the CE strategies reduce annual emissions by a further 23 %-54 % by 2050. These findings highlight the urgent need to integrate CE strategies into the sheet metal supply chain to support decarbonization efforts and help meet climate targets.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Figure the impact of steel microstructure and heat treatment on the formation of white etching cracks

White etching crack (WECs) associated macro-pitting is a dominant mode of damage within wind turbine gearbox bearings. This damage is characterized by broadly branching crack networks surrounded by local regions of microstructural alterations. The definitive cause of WECs in the field is unknown; therefore, the implementation of effective mitigation techniques has proven difficult. The current work utilized an accelerated benchtop testing technique in order to quantify differences in performance between through-hardened AISI 52100 steel and carburized AISI 3310 steel. It was found that the carburized AISI 3310 steel demonstrated a more than twofold increase in the time elapsed until WEC macro-pitting damage occurred compared to the through-hardened AISI 52100 steel samples.

36 MATERIALS SCIENCE↗

Surface Processes Control the Fate of Reactive Oxidants Generated by Electrochemical Activation of Hydrogen Peroxide on Stainless-Steel Electrodes

Low-cost stainless-steel electrodes can activate hydrogen peroxide (H 2 O 2 ) by converting it into a hydroxyl radical ( • OH) and other reactive oxidants. At an applied potential of +0.020 V, the stainless-steel electrode produced • OH with a yield that was over an order of magnitude higher than that reported for other systems that employ iron oxides as catalysts under circumneutral pH conditions. Decreasing the applied potential at pH 8 and 9 enhanced the rate of H 2 O 2 loss by shifting the process to a reaction mechanism that resulted in the formation of an Fe(IV) species. Significant metal leaching was only observed under acidic pH conditions (i.e., at pH <6), with the release of dissolved Fe and Cr occurring as the thickness of the passivation layer decreased. Despite the relatively high yield of • OH production under circumneutral pH conditions, most of the oxidants were scavenged by the electrode surface when contaminant concentrations comparable to those expected in drinking water sources were tested. The stainless-steel electrode efficiently removed trace organic contaminants from an authentic surface water sample without contaminating the water with Fe and Cr. With further development, stainless-steel electrodes could provide a cost-effective alternative to other H 2 O 2 activation processes, such as those by ultraviolet light.

42 ENGINEERING↗

Hybrid Grid-Renewable Strategies for Green Steel Production under Electricity Market Uncertainty

Volatility in grid spot prices is expected to rise with climate change-driven demand pressures and the intermittency of renewable generation. This volatility poses financial risks for green hydrogen-based steel production. The Direct Reduced Iron− Electric Arc Furnace (H 2 -DRI-EAF) is a promising pathway to decarbonize steel, which accounts for ∼8% of global GHG emissions. This study assesses how increased grid spot price volatility influences the optimal sizing and operation of H2-DRIEAF plants under three operational scenarios: grid-connected, fully behind-the-meter (islanded), and mixed-mode (semi-islanded). Our analysis identifies the semi-islanded configuration as the most cost-effective solution, achieving a Levelized Cost of Steel (LCOS) 10−35% lower than sourcing energy solely from the grid. Modeling also shows hydrogen storage or selective electricity purchases at high prices (>$1000/MWh) generally outperform battery storage, except under extreme volatility. Additionally, the study explores cost reduction strategies to strengthen the economic viability and sustainability of green steel production.

Batteries↗

Impact of nitrogen on lithium-induced corrosion and cracking of RAFM steel

The emergence of private fusion enterprises, combined with advancements in U.S. and EU ITER-TBM as well as EU DEMO liquid breeder blanket concepts, has renewed focus on the materials challenges. This study examines the compatibility of reduced activation ferritic/martensitic (RAFM) steel in liquid Lithium (Li) containing various Nitrogen (N) concentrations, tested at 600 and 700 °C for 500 and 1000 h under static conditions. Microstructural characterization revealed the corrosion-induced dissolution and precipitation in Li containing 0.082 and 0.17 wt.% N at 600 °C, while limited dissolution and precipitation were observed in N-gettered Li using zirconium (Zr) and titanium (Ti) foils at 600 °C. Tensile testing at room temperature after Li exposure revealed a decrease in strength and ductility of the RAFM steel as a function of N content in Li. Severe embrittlement was observed after 500 h in Li containing 0.17 wt.% N at 600 °C and after 500 h in hot-gettered Li at 700 °C. Chromium (Cr) depletion from the steel matrix was observed, leading to the formation of M6C-type carbides on the surface identified by electron microscopy (SEM), X-ray diffraction (XRD), in agreement with thermodynamic calculations. These findings highlight the critical materials challenges posed by liquid Li breeder blanket concepts, emphasizing the need for improved strategies to address Li-induced dissolution, precipitation, and steel embrittlement due to N contamination of the coolant.

Romedenne, Marie [ORNL] (ORCID:0000000317936561)↗

Atomic-scale decoration for improving the pitting corrosion resistance of austenitic stainless steels

Stainless steels are susceptible to the localized pitting corrosion that leads to a huge loss to our society. Studies in the past decades confirmed that the pitting events generally originate from the local dissolution in MnS inclusions which are more or less ubiquitous in stainless steels. Although a recent study indicated that endogenous MnCr 2 O 4 nano-octahedra within the MnS medium give rise to local nano-galvanic cells which are responsible for the preferential dissolution of MnS, effective solutions of restraining the cells from viewpoint of electrochemistry are being tantalizingly searched. Here we report such a galvanic corrosion can be greatly resisted via bathing the steels in Cu 2+ -containing solutions. This chemical bath generates Cu 2–δ S layers on the surfaces of MnS inclusions, invalidating the nano-galvanic cells. Our study provides a low-cost approach via an atomic scale decoration to improve the pitting corrosion resistance of stainless steels in a volume-treated manner.

36 MATERIALS SCIENCE↗

Microstructure-dependent particulate populations in ODS steels revealed by single-particle ICP-TOF-MS

In this work, we evaluated the ability of single-particle inductively coupled plasma time-of-flight mass spectrometry (SP-ICP-TOF-MS) to characterize particulates generated from 300 series stainless steels and oxide dispersion–strengthened (ODS) steels. Particulates were produced using two different rotary tools (cutting disk and grinding bit) to assess the influence of particle generation on effluent particulates. Across all materials and preparation techniques, SP-ICP-TOF-MS detected a substantial population of particles containing the expected constituent elements, with average compositions closely matching the nominal alloy values. A secondary population of Y-bearing particles was evident in ODS steels; their formation is strongly favored in particulates generated using the grinding bit. Specifically, in PM2000, Y-bearing particles were predominantly colocated with Al, whereas in 14YWT, Y-bearing particles were less frequently Fe-free but showed stronger colocation with Ti. These trends are consistent with the known microstructural differences between Y–Al–O oxide particles in PM2000 and finer Y–Ti–O nanoclusters in 14YWT. Together, these results demonstrate that SP-ICP-TOF-MS can resolve distinct particulate populations in complex, multicomponent steels at the femtogram mass scale, enabling particle-resolved insight into microstructure-driven phase separation and preparation-dependent particle generation.

Brubaker, Zach E. [Oak Ridge National Laboratory (↗

Friction stir scribe welding technique for dissimilar joining of aluminium and galvanised steel

Friction stir scribe technology, a derivative of friction stir welding, was applied for the dissimilar lap welding of an aluminum alloy and galvanized mild steel sheets. During the process, the rotating tool with a cobalt steel scribe first penetrated the top material — aluminum — and then the scribe cut the bottom material — steel. The steel was displaced into the upper material to produce a characteristic hook feature. Lap welds were shear tested, and their fracture paths were studied. Welding parameters affected the welding features including hook height, which turned out to be highly related to fracture position. Therefore, in this paper, the relationships among welding parameters, hook height, joint strength and fracture position are presented. In addition, influence of zinc coating on joint strength was also studied. Keywords: friction stir scribe technology; dissimilar material welding; zinc coating; hook height; joint strength; fracture position

Aluminum↗

Effect of hook characteristics on the fracture behaviour of dissimilar friction stir welded aluminium alloy and mild steel sheets

Under tensile shear loading, fracture modes of dissimilar lap welds produced by friction stir scribe technology were studied. Three fracture modes were observed. For zone A fracture, the initial crack was restrained, and the joint ultimately fractured in the base mild steel. For zone B fracture, the initial crack progressed through the aluminium sheet just above the Al/steel interface. For zone C fracture, the initial crack proceeded along the steel hook to the aluminium sheet surface. Fracture mode and joint strength were greatly influenced by steel hook size, and the steel hook size was affected by welding parameters and tool scribe height. In this study, the experimental joint strength achieved the calculated joint load limit.

Wang, Tianhao↗

On High-Fluence Irradiation Hardening of Nine RPV Surveillance Steels in the UCSB ATR-2 Experiment: Implications for Extended-Life Embrittlement Predictions

Nine archival reactor pressure vessel (RPV) surveillance steels from commercial nuclear power plants were irradiated in the University of California, Santa Barbara Advanced Test Reactor 2 (ATR-2) experiment to evaluate irradiation embrittlement under low-flux surveillance capsule versus higher flux test reactor (ATR-2) conditions. The postirradiation measurements of irradiation hardening, measured as increases in yield stress (Δσy), and corresponding conversions of Δσy to Charpy V-notch 41-J transition temperature shifts (ΔTc) are compared with various embrittlement trend curve (ETC) model predictions for the nine steels. Tensile and converted shear punch and microhardness measurements of Δσy generally show a continuing increase between intermediate and high ATR-2 fluences. The Eason-Odette-Nanstad-Yamamoto and ASTM E900 ETC models underpredict embrittlement at the ATR-2 irradiation condition: irradiation temperature (Ti) of 292°C, neutron fluence (ϕt) of 1.4 × 1020 n/cm2 (E > 1 MeV), and neutron flux (ϕ) of 3.68 × 1012 n/cm2-s. On average, the French FIS and Japanese JAEC ETCs slightly overpredict the ATR-2 data. The increase in Δσy with higher fluence is primarily due to Ni-Mn-Si precipitates, which slowly evolve in both nearly copper-free and copper-bearing steels. Finally, a new Odette-Wells-Almirall-Yamamoto embrittlement model is shown that yields good predictions for the nine steels at high fluences (ϕt > 5.5 × 1019 n/cm2).

Nanstad, Randy K.↗

The impact of temperature, chlorides and sulfate-reducing bacteria on the corrosion of steel in soil

Here, this investigation aimed to study the corrosion performance of low-carbon steel in a soil environment at different temperatures. The steel specimens in the soil were treated at three temperatures: 5, 25 and 60°C. The specimens were embedded in chloride-free soil for 21 days, and then 3.5% (by weight) sodium chloride (NaCl) was added to the soil. The specimens were then kept in the chloride-contaminated soil for 54 days. The results of electrochemical experiments showed superior corrosion performance of the specimens at 60°C, which had the lowest corrosion activity, followed by the specimens at 5 and 25°C. The slow nature of the kinetics of the corrosion reactions at 5°C compared with that at ambient temperature was the reason for this improvement at 5°C. The lower number of microorganisms, including sulfate-reducing bacteria, in the soil at 60°C compared with that at the other temperatures was attributed to the lower corrosion activity of steel in the soil at 60°C compared with the corrosion activity of steel in the soil at other temperatures.

99 - GENERAL AND MISCELLANEOUS↗

Developing Fatigue Pre-crack Procedure to Evaluate Fracture Toughness of Pipeline Steels Using Spiral Notch Torsion Test

The spiral notch torsion test (SNTT) has been utilized to investigate the crack growth behavior of X52 steel base and welded materials used for hydrogen infrastructures. The X52 steel materials are received from a welded pipe using friction stir welding techniques. Finite element models were established to study the crack growth behavior of steel SNTT steel samples, which were assumed to be isotropic material. A series SNTT models were set up to cover various crack penetration cases, of which the ratios between crack depth to diameter (a/D ratio) ranging from 0.10 to 0.45. The evolution of compliance and energy release rates in the SNTT method have been investigated with different cases, including different geometries and materials. Indices of characteristic compliance and energy release rates have been proposed. Good agreement has been achieved between predictions from different cases in the same trend. These work shed lights on a successful protocol for SNTT application in wide range of structural materials. The further effort needed for compliance function development is to extend the current developed compliance function to the deep crack penetration arena, in the range of 0.55 to 0.85 to effectively determine fracture toughness for extremely tough materials.

fracture toughness↗

Crack Growth Rate and Fracture Toughness Tests on Irradiated Cast Stainless Steels

Cast austenitic stainless steels are used in the cooling system of light water reactors for components with complex shapes, such as pump casings, valve bodies, and coolant piping. In the present study, crack growth rate and fracture toughness JR curve tests were performed on irradiated cast stainless steels in low-corrosion-potential environments (low-dissolved-oxygen high-purity water or simulated pressurized water reactor environment) at 320°C. Both as received and thermally aged materials were included to investigate the combined effect of thermal aging and irradiation embrittlement on the fracture behavior of cast stainless steels. The samples were irradiated to approximately 0.08 dpa at the Halden reactor. Good resistance to corrosion fatigue and stress corrosion cracking was observed for all samples. Thermal aging had little effect on the crack growth behavior at this dose level. Cleavage-like fracture was the dominant cracking morphology during the crack growth rate tests, and the ferrite phase was deformed to a lesser extent compared with the surrounding austenite phase. The fracture toughness results showed a dominant effect of neutron irradiation, and the fracture resistances were decreased considerably for all cast specimens regardless of their thermal aging conditions. The reduction in fracture toughness was more significant in the unaged than thermally aged materials. Nonetheless, the fracture toughness values of thermally aged specimens were about 30% lower than their unaged counterparts, suggesting a combined effect of thermal aging and neutron irradiation in cast stainless steel.

Chen, Y.↗

HYDROGEN-ASSISTED FRACTURE IN FORGED TYPE 304L AUSTENITIC STAINLESS STEEL

Austenitic stainless steels generally have good resistance to hydrogen-assisted fracture; however, structural designs for high-pressure gaseous hydrogen are constrained by the low strength of this class of material. Forging is used to increase the low strength of austenitic stainless steels, thus improving the efficiency of structural designs. Hydrogen-assisted racture, however, depends on microstructural details associated with manufacturing. In this study, hydrogen-assisted fracture of forged type 304L austenitic stainless steel is investigated. Microstructural variation in multi-step forged 304L was achieved by forging at different rates and temperatures, and by process annealing. High internal hydrogen content in forged type 304L austenitic stainless steel is achieved by thermal precharging in gaseous hydrogen and results in as much as 50% reduction of tensile ductility.

36 MATERIALS SCIENCE↗

Optimization and testing results of Zr-bearing ferritic steels

The mission of the Nuclear Energy Enabling Technologies (NEET) program is to develop crosscutting technologies for nuclear energy applications. Advanced structural materials with superior performance at elevated temperatures are always desired for nuclear reactors, which can improve reactor economics, safety margins, and design flexibility. They benefit not only new reactors, including advanced light water reactors (LWRs) and fast reactors such as sodium-cooled fast reactor (SFR) that is primarily designed for management of high-level wastes, but also life extension of the existing fleet when component exchange is needed. Developing and utilizing the modern materials science tools (experimental, theoretical, and computational tools) is an important path to more efficient alloy development and process optimization. Ferritic-martensitic (FM) steels are important structural materials for nuclear reactors due to their advantages over other applicable materials like austenitic stainless steels, notably their resistance to void swelling, low thermal expansion coefficients, and higher thermal conductivity. However, traditional FM steels exhibit a noticeable yield strength reduction at elevated temperatures above ~500°C, which limits their applications in advanced nuclear reactors which target operating temperatures at 650°C or higher. Although oxide-dispersion-strengthened (ODS) ferritic steels have shown excellent high-temperature performance, their extremely high cost, limited size and fabricability of products, as well as the great difficulty with welding and joining, have limited or precluded their commercial applications. Zirconium has shown many benefits to Fe-base alloys such as grain refinement, improved phase stability, and reduced radiation-induced segregation. The ultimate goal of this project is, with the aid of computational modeling tools, to accelerate the development of a new generation of Zr-bearing ferritic alloys to be fabricated using conventional steelmaking practices, which have excellent radiation resistance and enhanced high-temperature creep performance greater than Grade 91.

36 MATERIALS SCIENCE↗

Intermetallic Strengthened Alumina-Forming Austenitic Steels for Energy Applications

In order to achieve energy conversion efficiencies of >50 % for steam turbines/boilers in power generation systems, the materials required must be strong, corrosion-resistant at high temperatures (>700°C), and economically viable. Austenitic steels strengthened with Laves phase and L1 2 precipitates, and alloyed with aluminum to improve oxidation resistance, are potential candidate materials for these applications. The creep resistance of these alloys is significantly improved through intermetallic strengthening (Laves-Fe 2 Nb + L1 2 -Ni 3 Al precipitates) without harmful effects on oxidation resistance. Microstructural and microchemical analyses of the recently developed alumina-forming austenitic (AFA) steels (Fe-14Cr-32Ni-3Nb-3Al-2Ti-based) indicated they are strengthened by Ni 3 Al(Ti) L1 2 , NiAl B 2 , Fe 2 Nb Laves phase and MC carbide precipitates. Different thermomechanical treatments (TMTs) were performed on these stainless steels in an attempt to further improve their mechanical properties. The thermo-mechanical processing produced nanocrystalline grains in AFA alloys and dramatically increased their yield strength at room temperature. Unfortunately, the TMTs didn’t increase the yield strengths of AFA alloys at ≥700ºC. At these temperatures, dislocation climb is the dominant mechanism for deformation of TMT alloys according to strain rate jump tests. After the characterization of aged AFA alloys, we found that the largest strengthening effect from L1 2 precipitates can be obtained by aging for less than 24 h. The coarsening behavior of the L1 2 precipitates was not influenced by carbon and boron additions. Failure analysis and post-mortem TEM analysis were performed to study the creep failure mechanisms of these AFA steels after creep tests. Though the Laves and B2-NiAl phase precipitated along the boundaries can improve the creep properties, cracks were still initiated and propagated along the boundaries, which suggests that the boundaries are still the weaker regions for causing fracture during creep, possibly due to the presence of a precipitatefree zone. The precipitate size distribution and kinetics of precipitate growth were quantified.

36 MATERIALS SCIENCE↗

Mechanical properties and microstructure characterization of unirradiated Eurofer-97 steel variants for the EUROfusion project

To understand the microstructure and mechanical property degradation of various Eurofer-97 steel variants being neutron irradiated at HFIR up to 2.5 and 20 dpa for the EUROfusion programme, it is necessary to develop a general understanding of these steels in non-irradiated form. In this context, room temperature mechanical property evaluation tests and multi-length scale microstructure characterization of the different Eurofer-97 steel variants: H, I, J, K, L, M, N, O, P and reference E series steels, was performed at ORNL. Mechanical tests consisted of Vickers hardness indentation measurements, uniaxial tensile tests and fracture toughness tests.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

The Effects on Non-Actinide Impurities from Aging Heat Source Plutonium in Stainless Steel Containers

Replacing the tantalum vials used for 238 PuO 2 sample collection and storage with stainless steel sample vials has several advantages. These advantages include a decreased cost, better material availability, and ease of fabrication. However, it must first be demonstrated that the alloying elements contained in stainless steel are not leached into the 238 PuO 2 such that product specifications are exceeded. In order to determine the suitability of stainless steel for this application, two seperate 238 PuO 2 fuel lots were investigated. These two fuel lots had been stored in stainless steel containers since their first sampling date of March of 2015, and were again sampled in February of 2019.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗