Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “IRON COMPOUND”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 883 records · Page 49

Experimental Study on the Activities of Al and Ca in Ferrosilicon

Experiments were carried out to determine the activities of Al and Ca in liquid ferrosilicon (with about 50 wt pct Si) at 1823 K (1550 °C) in their dilution ranges. Liquid FeSi50 and SiO{sub 2}-Al{sub 2}O{sub 3}-CaO slag were stirred mechanically in a graphite crucible to enhance the transfer of Al and Ca between the two phases. The stirring time for the two phases to reach equilibrium was studied. It was found that a time of 45 minutes was long enough to reach the slag–metal equilibrium. The activities of Al and Ca in the ferrosilicon alloy were calculated based on the compositions of the two liquid phases. The activity coefficients obtained for Al and Ca in the liquid FeSi50 at 1823 K (1550 °C) were found to be nearly constant in the composition range studied.

36 MATERIALS SCIENCE↗

Duplex Heterogeneous Nucleation Behavior of Precipitates in C-Mn Steel Containing Sn

The two successive heterogeneous nucleation behaviors of FeSn{sub 2}-MnS-Al{sub 2}O{sub 3} complex precipitates in ultrahigh Sn-bearing steel were investigated. First, Al{sub 2}O{sub 3} was the nucleation site of the MnS at the end of solidification. Then, FeSn{sub 2} nucleated heterogeneously on the MnS particles that nucleated on the Al{sub 2}O{sub 3} particles. The formation sequence of the precipitated phase caused the duplex heterogeneous nucleation to occur consecutively at most twice.

36 MATERIALS SCIENCE↗

Damring Formation During Rotary Kiln Chromite Pre-reduction: Effects of Pulverized Carbonaceous Fuel Selection and Partial Pellet Melting

Electricity consumption is the largest cost contributing factor in the production of ferrochrome. Currently the pelletized chromite pre-reduction process (solid-state reduction of chromite) is the process option with the lowest specific electricity consumption (MWh/ton). In this process, pelletized chromite is fed into a rotary kiln at 1573 K (1300 °C), where partial pre-reduction takes place. Damring formation (material build-up) in the rotary kiln causes routine shutdowns, resulting in loss of revenue. The damring formation is possibly caused by melting of the ash of the pulverized coal used to fire the kiln and/or the partial melting of the chromite pellets. Ash fusion temperatures of twenty different samples were evaluated to assess the temperature at which the pulverized coal ash will start to contribute to damring formation. Sessile drop tests were used to assess the softening behavior of different ore types (e.g., UG2, MG, and LG metgrade), as well as softening of composite chromite pellets made from these ores. Actual damrings were also analyzed using scanning electron microscopy with energy dispersive X-ray spectroscopy. Results indicate that it is mainly the pulverized coal ash that will contribute to damring formation, and not ore or pellet softening. Multiple-linear regression was used to derive equations to predict the ash fusion temperatures of the pulverized coal ash, which can be used by ferrochrome producers to optimize pulverized coal selection.

36 MATERIALS SCIENCE↗

Non-isothermal Reduction Kinetics of Iron During Vacuum Carbothermal Reduction of Ilmenite Concentrate

The non-isothermal reduction kinetics and mechanism of iron during vacuum carbothermal reduction of ilmenite concentrate were investigated by X-ray diffraction, backscattered electron imaging, and energy-dispersive X-ray spectroscopy at temperatures from 1273 K to 1673 K (1000 °C to 1400 °C). The pressure dropped and the increasing trend of mass loss and metallization ratios slowed down when the temperature was higher than 1573 K (1300 °C). The reaction products were iron, Ti{sub 2}O{sub 3}, and silicate. Iron was mainly obtained by carbothermal reduction of FeTiO{sub 3} and FeTi{sub 2}O{sub 5}. The irons continued to nucleate, aggregate, and grow during the reduction process. Comprehensive consideration of Šatava–Šesták method and Coats–Redfern method, the apparent activation energy of the reduction process was 587.4 ± 2.98 kJ/mol, and the forms of both integral and differential for the mechanism function were G(a)= [(1−a){sup −1/3}−1]{sup 2} and f(a) = 3/2(1−a){sup 4/3}[(1−a)−{sup 1/3}−1]{sup −1}, respectively.

36 MATERIALS SCIENCE↗

Effect of Deformation Temperature on Dynamic Recrystallization and CSL Grain Boundary Distribution of Fe-36%Ni Invar Alloy

This paper investigated the effect of deformation temperatures on microstructure evolution and grain boundary character distribution (GBCD) of Fe-36%Ni Invar alloy during hot compression tests. The isothermal hot deformation tests were carried out in a temperature range of 850-1100 °C and a strain rate of 0.01 s{sup −1}. The grain boundary character distribution was based on the Σ3{sup n} (n = 1, 2, 3,…) coincidence site lattice (CSL) boundaries. The experimental results show that the extent of dynamic recrystallization significantly expanded at the strain rate of 0.01 s{sup −1} with the increase in temperature and this phenomenon was consistent with the evolution tendency of Σ3{sup n} boundaries. To some degree, the increasing proportion of typical low-ΣCSL boundaries, especially the increasing trend of Σ3, positively promoted the wider process of dynamic recrystallization.

36 MATERIALS SCIENCE↗

Effect of Hot Deformation on Texture and Microstructure in Fe-Mn Austenitic Steel During Compression Loading

Hot compression tests of a new high-Mn austenitic steel were carried out at deformation temperatures of 700, 800, 900, and 1000 °C under strain rate of 0.01 s{sup −1}. The hot deformation behavior was investigated by the analyses of flow curves, texture, and deformed microstructures. Microstructures of the deformed specimens and macrotexture were examined using electron backscatter diffraction and x-ray diffraction methods, respectively. The results showed that the flow stress depended strongly on the deformation temperature and decreased by increasing deformation temperature. The microstructural evidence indicated that the dynamic recrystallization (DRX) process of experimental steel was initiated at 800 °C with necklace structure. The volume fraction of DRX grains was considerably increased by increasing deformation temperature to 1000 °C. Texture of the DRX grains tended to become a weak texture and was associated with the formation of Goss and R-Cube components. Meanwhile, martensitic transformation was detected in the hot-deformed austenite. The martensitic transformation was the most difficult in the DRX grains because of the effect of small grain size. The tendency of transformation was decreased after compression at 1000 °C.

36 MATERIALS SCIENCE↗

Formation and Decomposition Process of the Filled Skutterudite Sm{sub y}(Fe{sub x}Ni{sub 1−x}){sub 4}Sb{sub 12} (0.40 ≤ x ≤ 1) as Revealed by Differential Thermal Analysis

Filled skutterudites are among the most promising thermoelectric materials, and the obtainment of monophasic samples is crucial for the study of their transport properties. In this work, a differential thermal analysis study was performed on samples belonging to the Sm{sub y}(Fe{sub x}Ni{sub 1-x}){sub 4}Sb{sub 12} system with the aim to determine the most proper annealing temperature to possibly obtain skutterudite monophasic samples, and to study the effect of Sm addition on the thermodynamics of the Fe-Ni-Sb system. Samples were prepared through the traditional procedure consisting in melting–quenching–annealing the starting elements. DTA analyses were carried out on annealed samples, and results were interpreted using the Fe{sub 25}Sb{sub 75}-Ni{sub 25}Sb{sub 75} pseudobinary phase diagram taken from the literature as a starting point. They reveal that 870 K is the best annealing temperature, being the formation of a liquid phase just above this point; moreover, the Sm introduction results in widening the one-phase skutterudite stability region toward both higher temperatures and higher Fe concentrations compared with the Sm-free system.

36 MATERIALS SCIENCE↗

Corrosion Behavior of Sm{sub y}(Fe{sub x}Ni{sub 1−x}){sub 4}Sb{sub 12} (0.40 ≤ x ≤ 0.80) in NaCl Solutions Studied by Electron Microscopy and ICP-AES

Filled skutterudites are currently studied as thermoelectric materials to be used in the automotive and nautical field; the study of their resistance to a saline environment is therefore mandatory. To this purpose, the corrosion behavior of several compositions belonging to the Sm{sub y}(Fe{sub x}Ni{sub 1−x}){sub 4}Sb{sub 12} skutterudites system was investigated by immersing samples in differently concentrated (0.1 and 0.5 M) NaCl solutions. The effect of the treatment was analyzed both by SEM–EDS on the sample surface and at fixed times by ICP-AES on the solution. The formation of an oxide layer was observed on the surface of all the samples: the film results uniformly grown on specimens treated in NaCl at the lower concentration, while it is cracked and not spread over the whole surface in the other samples. Relying on the oxide layer thickness, the oxidation resistance results to increase with increasing the Fe content; correspondingly, the Sb concentration in the more diluted solution decreases at each time considered with increasing the Fe amount, pointing at a strict correlation between the cationic release and the oxide formation, and suggesting a possible mechanism for the growth of the protective film.

36 MATERIALS SCIENCE↗

Dynamic Recrystallization and Grain Refinement of Fe-P-C-Si and Fe-P-C-Si-N Steels

Grain refinement is an effective technique to improve the mechanical properties of steels. In the present work, single-pass hot compression experiments have been conducted on two different compositions of high phosphorous steels to study the microstructural evolution and ferrite grain refinement at various strain rates and deformation temperatures, i.e., 0.01-10 s{sup −1} and 750-1050 °C, respectively. Optical metallography has been employed to understand the physical processes that take place during hot deformation process. The results indicate that when these compositions of high phosphorous steels are worked at relatively low temperatures in the intercritical regions, a ferrite grain size of 5-7 µm is obtained. It is observed that the grain size decreases with an increase in strain rate and with the decrease in deformation temperature. Based on the values of stress exponent (n) obtained in the present work, dislocation creep is identified as the deformation mechanism. The activation energies for deformation of these two types of high phosphorous steels have been calculated. The effect of the alloying elements on the stress–strain curve, microstructure, and grain refinement has been discussed.

36 MATERIALS SCIENCE↗

Effect of Plane Strain Compression and Subsequent Recrystallization Annealing on Microstructures and Phase Transformation of NiTiFe Shape Memory Alloy

The effect of plane strain compression and subsequent recrystallization annealing on microstructures and phase transformation of NiTiFe shape memory alloy (SMA) is investigated. Inhomogeneous plastic deformation at various deformation degrees occurs in NiTiFe SMA during plane strain compression. Nanocrystalline phase and amorphous phase increase as the deformation degree increases. B2 austenite, B19′ martensite, nanocrystalline and amorphous phases coexist in the NiTiFe samples subjected to large plastic strain. The static recrystallization mechanisms depend on the microstructures of the deformed NiTiFe samples. The static recrystallization mechanisms deal with nucleation and growth of the recrystallized grains, growth of nanocrystalline phase and crystallization of amorphous phase. Grain size, subgrain boundaries, geometrically necessary dislocation density and Schmid factor are captured on the basis of electron backscattered diffraction data. The process of recrystallization annealing cannot eliminate the deformation texture completely. The slip direction [110] is the most favorable slip direction in the recrystallized NiTiFe sample. Plane strain compression along with subsequent recrystallization annealing changes the phase transformation path of as-rolled NiTiFe SMA, and it results in the decreasing martensite transformation start temperature. The three annealed NiTiFe samples exhibit the similar phase transformation behavior since complete recrystallization annealing leads to the similar microstructures.

36 MATERIALS SCIENCE↗

On the Steel–Aluminum Hybrid Casting by Sand Casting

Hybrid casting is a well-known technology to join steel inserts and aluminum. In order to achieve a high-performance material-based joining between steel and aluminum, a new PVD Al-Si-(Fe) coating, which consists of two sub-layers, has been successfully developed for high-pressure die casting. This coating system has been investigated further in this work for the sand casting process. By extending the sand casting process to the plaster casting process with preheating possibilities for the coated steel inserts, a material-based connection between steel and aluminum with a tensile shear strength of 7.7 MPa could be created. The ductility of this connection is decreased comparing with the connection manufactured by die casting. SEM and EDS analysis and diffusion experiments show that the difference of mechanical properties between plaster and die casting is caused by the extensive diffusion and the corresponding layer growth at plaster casting. The edge separation in plaster casting is a result of the edge stresses due to the different thermal expansion of steel and aluminum which can be suppressed at high-pressure die casting. To improve the joining properties at sand casting, it is necessary to control the layer diffusion by adding other alloy elements such as Mn into the Al-Si-(Fe) coating layer.

36 MATERIALS SCIENCE↗

Synthesis and Structural Characterization of Sb-Doped TiFe{sub 2}Sn Heusler Compounds

Ternary Heusler compounds form a numerous class of intermetallics, which include two families with general compositions ABC and AB{sub 2}C, usually referred to as half- and full-Heusler compounds, respectively. Given their tunable electronic properties, made possible by adjusting the chemical composition, these materials are currently considered for the possible use in sustainable technologies such as solar energy and thermoelectric conversion. According to theoretical predictions, Sb substitution in the TiFe{sub 2}Sn full-Heusler compound is thought to yield band structure modifications that should enhance the thermoelectric power factor. In this work, we tested the phase stability and the structural and microstructural properties of such heavily doped compounds. We synthesized polycrystalline TiFe{sub 2}Sn{sub 1−x}Sb{sub x} samples, with x = 0, 0.1, 0.2 and 1.0 by arc melting, followed by an annealing treatment. The structural characterization, performed by x-ray powder diffraction and microscopy analyses, confirmed the formation of the pseudo-ternary Heusler structure (cF16, Fm-3m, prototype: MnCu{sub 2}Al) in all samples, with only few percent amounts of secondary phases and only slight deviations from nominal stoichiometry. With increasing Sb substitution, we found a steady decrease in the lattice parameter, confirming that the replacement takes place at the Sn site. Quite unusually, the as-cast samples exhibited a higher lattice contraction than the annealed ones. The fully substituted x = 1.0 compound, again adopting the MnCu{sub 2}Al structure, does not form as stoichiometric phase and turned out to be strongly Fe deficient. The physical behavior at room temperature indicated that annealing with increasing temperature is beneficial for electrical and thermoelectrical transport. Moreover, we measured a slight improvement in electrical and thermoelectrical properties in the x = 0.1 sample and a suppression in the x = 0.2 sample, as compared to the undoped x = 0 sample.

36 MATERIALS SCIENCE↗

Pulsed TIG Welding–Brazing of Aluminum–Stainless Steel with an Al-Cu Twin Hot Wire

A TIG welding–brazing process with a twin aluminum hot wire technique was utilized to control the heat input, improve the joint formation, suppress the interfacial intermetallic compounds (IMCs) and increase the joint strength, thereby creating reliable joints between an aluminum alloy and stainless steel with an ER2319 filler. Twin wires with reasonable diameters and filling modes led to a satisfactory weld of parent metals with varying thicknesses. By the hot wire technique, the reasonable range of the welding current was extended and the thickness of the interfacial IMC at the seam bottom was reduced. In addition, both the tensile strength and stability of the joints increased compared with a cold wire. The IMC consisted of θ-(Fe,Cu){sub 4}Al{sub 13} and minor Cr{sub 0.7}Fe{sub 0.3}Al{sub 6}, and the precipitated phases in the weld were Al{sub 2}Cu and Al{sub 2}CuMg. With an increasing welding current, the IMC thickness significantly increased, while the joint strength decreased. The fracture positions of the joints varied with the corresponding welding currents.

36 MATERIALS SCIENCE↗

Dry Sliding Wear Behavior and Mechanism of a Hot-Dip Aluminized Steel as a Function of Sliding Velocity

Fe-Al intermetallic coatings were prepared on AISI 1045 steel by hot-dip aluminizing and subsequent high-temperature diffusion. The dry sliding wear tests were performed for the aluminized steel with various substrate hardnesses in the velocity range of 0.75-4 m/s on a pin-on-disk configuration. The dry sliding wear behavior and mechanisms of the aluminized steel under various velocities were explored. It was found that the wear rate decreased substantially with an increase in sliding velocity from 0.75 to 1.5 and then slightly varied in the velocity range of 1.5-4 m/s. The wear behavior and mechanisms of the aluminized steel were noticed to be closely related with tribo-layers. As tribo-layers contained more oxides with Fe{sub 2}O{sub 3}, the wear resistance of the aluminized steel was markedly improved because of their protective function. The substrate hardness also changed the wear behavior of the aluminized steel by affecting the stability of tribo-layers because the substrate hardness was inversely proportional to the thermal stability of the substrate structure. Under a low velocity of 0.75 m/s, adhesive wear and abrasive wear prevailed owing to the metal-on-metal contact, resulting in a higher wear rate. At 1.5-4 m/s, mild oxidative wear prevailed due to the stable existence of tribo-oxides layers. However, at 1.5 and 4 m/s for the substrate hardness of 45 HRC, the wear rate was slightly increased because the protection of tribo-layers was weakened by a double-layered structure or more cracks in tribo-layers and coatings.

36 MATERIALS SCIENCE↗

Effect of Different Heat Treatments on the Microstructural Evolution and Mechanical Properties of Ni-Cr-Si Alloy Fabricated by Laser Additive Manufacturing

Ni-Cr-Si alloy samples were fabricated on mild steel via laser additive manufacturing technology. The microstructural evolution and mechanical properties of the samples were studied systematically in as-deposited conditions and under three different types of heat-treated conditions. The scanning electron microscopy, energy-dispersive x-ray spectroscopy and x-ray diffraction results showed that the structures of the as-deposited samples were mainly dendritic matrices of γ(Ni, Fe), continuous interdendritic eutectics of γ + Ni{sub 3}B and discrete Cr-rich carbides and borides. After solid solution treatment, carbides (Cr{sub 7}C{sub 3}) and borides (CrB) precipitated on the boundary of the eutectic structure, distributing discretely in the matrix. In the solution plus aging heat-treated conditions, the interdendritic eutectics formed Ni{sub 3}Fe intermetallic compounds with a layered distribution. After annealing, the grains were refined, and the hard phases (CrB) were uniformly dispersed along the grain boundary. Among the tested samples, the as-deposited specimens exhibited the highest microhardness and good wear ability at room temperature; however, the wear resistance of the as-deposited sample obviously decreased at 250 °C. The mechanical properties of the specimens were not greatly improved by solution treatment or solution plus aging treatment. The sample subjected to annealing treatment exhibited excellent wear resistance both at room temperature and at a service temperature of 250 °C.

36 MATERIALS SCIENCE↗

The corrosion pattern of reinforcement and its influence on serviceability of reinforced concrete members in chloride environment

This paper deals with two corroded reinforcement concrete beams, which have been stored under sustained load in a chloride environment for 14 and 23 years respectively. The evolution of corrosion pattern of reinforcement and its influence on serviceability are studied. In chloride-induced corrosion process, corrosion cracking affects significantly the corrosion pattern. During the corrosion cracking initiation period, only local pitting corrosion occurs. At early stage of cracking propagation, localized pitting corrosion is still predominant as cracks widths are very small and cracks are not interconnected, but a general corrosion slowly develops as the cracks widen. At late cracking stage, interconnected cracking with wide width develops along large parts of the beam leading to a general corrosion pattern. Macrocells and microcells concepts are used for the interpretation of the results. Mechanical experiments and corrosion simulation tests are performed to clarify the influence of this corrosion pattern evolution on the serviceability of the beams (deflection increase). Experimental results show that, when the corrosion is localized (early cracking stage), the steel-concrete bond loss is the main factor affecting the beams serviceability. The local cross-section loss resulting from pitting attack does not significantly influence the deflection of the beam. When corrosion is generalized (late cracking stage), as the steel-concrete bond is already lost, the generalized steel cross-section reduction becomes the main factor affecting the beams serviceability. But, at this stage, the deflection increase is slower due to the low general corrosion rate.

36 MATERIALS SCIENCE↗

Concrete cover cracking with reinforcement corrosion of RC beam during chloride-induced corrosion process

This paper deals with the evolution of the corrosion pattern based on two beams corroded by 14 years (beam B1CL1) and 23 years (beam B2CL1) of conservation in a chloride environment. The experimental results indicate that, at the cracking initiation stage and the first stage of cracking propagation, localized corrosion due to chloride ingress is the predominant corrosion pattern and pitting corrosion is the main factor that influences the cracking process. As corrosion cracking increases, general corrosion develops rapidly and gradually becomes predominant in the second stage of cracking propagation. A comparison between existing models and experimental results illustrates that, although Vidal et al.'s model can better predict the reinforcement corrosion of beam B1CL1 under localized corrosion, it cannot predict the corrosion of beam B2CL1 under general corrosion. Also, Rodriguez's model, derived from the general corrosion due to electrically accelerated corrosion experiments, cannot match natural chloride corrosion irrespective of whether corrosion is localized or general. Thus, for natural general corrosion in the second stage of cracking propagation, a new model based on the parameter of average steel cross-section loss is put forward to predict steel corrosion from corrosion cracking.

36 MATERIALS SCIENCE↗

Role of structural Fe in nontronite NAu-1 and dissolved Fe(II) in redox transformations of arsenic and antimony

Oxidation state is a major factor affecting the mobility of arsenic (As) and antimony (Sb) in soil and aquatic systems. Metal (hydr)oxides and clay minerals are effective sorbents, and may also promote redox reactions on their surfaces via direct or indirect facilitation of electron transfer. Iron substituted for Al in the octahedral sites of aluminosilicate clay minerals has the potential to be in variable oxidation states and is a key constituent of electron transfer reactions in clay minerals. This experimental work was conducted to determine whether structural Fe in clays can affect the oxidation state of As and Sb adsorbed at the clay surface. Another goal of our study was to compare the reactivity of clay structural Fe(II) with systems containing Fe(II) present in dissolved/adsorbed forms. The experimental systems included batch reactors with various concentrations of As(III), Sb(III), As(V), or Sb(V) equilibrated with oxidized (NAu-1) or partially reduced (NAu-1-Red) nontronite, hydrous aluminum oxide (HAO) and kaolinite (KGa-1b) suspensions under oxic and anoxic conditions. The reaction times ranged from 0.5 to 720 h, and pH was constrained at 5.5 (for As) and at 5.5 or 8.0 (for Sb). The oxidation state of As and Sb in the liquid phase was determined by liquid chromatography in line with an inductively coupled plasma mass spectrometer, and in the solid phase by X-ray absorption spectroscopy. Our findings show that structural Fe(II) in NAu-1-Red was not able to reduce As(V)/Sb(V) under the conditions examined, but reduction was seen when aqueous Fe(II) was present in the systems with kaolinite (KGa-1b) and nontronite (NAu-1). The ability of the structural Fe in nontronite clay NAu-1 to promote oxidation of As(III)/Sb(III) was greatly affected by its oxidation state: if all structural Fe was in the oxidized Fe(III) form, no oxidation was observed; however, when the clay was partially reduced ({approx}20% of structural Fe was reduced to Fe(II)), NAu-1-Red promoted the most extensive oxidation under both oxic and anoxic conditions. Electron balance considerations suggest that structural Fe(III) in the NAu-1-Red was the sole oxidant in the anoxic setup, while dissolved O{sub 2} also contributes in oxic conditions. Long-term batch experiments revealed the complex dynamics of As aqueous speciation in anoxic and oxic systems when reduced arsenic was initially added: rapid disappearance of As(III) was observed due to oxidation to As(V) followed by a slow increase of aqueous As(III). This behavior is explained by two reactions: fast initial oxidation of As(III) by structural Fe(III) (anoxic) or Fe(III) and dissolved O2 (oxic) followed by the slow reduction of As(V) by dissolved Fe(II). The resulting re-mobilization of As due to As(V) reduction by aqueous Fe(II) occurs on time scales on the order of days. These reactions are likely significant in a natural soil or aquifer environment with seasonal cycling or slightly reducing conditions with an abundance of clay minerals and dissolved Fe(II).

36 MATERIALS SCIENCE↗