Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “EUTECTICS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 883 records · Page 49

Effects of high magnetic field on the evolutions of constituent phases in 7085 aluminum alloy during homogenization

The evolutions of coarse constituent phases in homogenized 7085 aluminum alloy at different conditions with or without the application of 12 T high magnetic field were examined by using differential scanning calorimetry, scanning electronic microscope, energy dispersive spectroscopy and X-ray diffraction. It is found that the main constituent phases including quaternary phase T(AlZnMgCu), Al{sub 7}Cu{sub 2}Fe, and AlTiCuFeSi are present in as-cast 7085 alloy. During homogenization, {alpha} + T eutectics become discontinuous and spheroidized, and Al{sub 2}CuMg phase nucleates and grows along {alpha} + T eutectics. High magnetic field significantly accelerates the melting of quaternary phase T and Al{sub 2}CuMg phase. When the alloy homogenized at 460 Degree-Sign C/10 h + 480 Degree-Sign C/8 h with 12 T magnetic field, the least amount of constituent phases is obtained. - Highlights: Black-Right-Pointing-Pointer Most of published reports of magnetic field are focused on ferrous alloys. Black-Right-Pointing-Pointer Effect of magnetic field on microstructure of 7085 during homogenization is studied. Black-Right-Pointing-Pointer Magnetic field accelerates the melting of AlZnMgCu and S phase.

36 MATERIALS SCIENCE↗

Real time synchrotron X-ray observations of solidification in hypoeutectic Al–Si alloys

This paper demonstrates how recent advances in synchrotron technology have allowed for the real-time X-ray imaging of solidification in Al–Si alloys, despite the small difference in atomic number of these elements. The experiments performed at the SPring-8 synchrotron, involved imaging the solidification of Al–1wt.%Si and Al–4wt.%Si alloys under a low-temperature gradient and a cooling rate of around 0.3 °C/s. The nucleation and growth of the primary aluminum grains as well as the onset of eutectic solidification were clearly observed. In the alloys containing Al–4wt.%Si, contrast was sufficient to characterize the nucleation rate and growth velocity of the aluminum grains. The importance of improving observation of solidification in the Al–Si system by increasing the time resolution during critical events is discussed. - Highlights: • A synchrotron technique was used to observe solidification of Al-Si alloys. • Nucleation, coarsening, and the onset of eutectic solidification were observed. • Images captured are suitable for quantitative analysis. • The resolution that was obtained should be possible for most aluminum alloys.

36 MATERIALS SCIENCE↗

Effect of re-melting on particle distribution and interface formation in SiC reinforced 2124Al matrix composite

The interface between metal matrix and ceramic reinforcement particles plays an important role in improving properties of the metal matrix composites. Hence, it is important to find out the interface structure of composite after re-melting. In the present investigation, the 2124Al matrix with 10 wt.% SiC particle reinforced composite was re-melted at 800 °C and 900 °C for 10 min followed by pouring into a permanent mould. The microstructures reveal that the SiC particles are distributed throughout the Al-matrix. The volume fraction of SiC particles varies from top to bottom of the composite plate and the difference increases with the decrease of re-melting temperature. The interfacial structure of re-melted 2124Al–10 wt.%SiC composite was investigated using scanning electron microscopy, an electron probe micro-analyzer, a scanning transmission electron detector fitted with scanning electron microscopy and an X-ray energy dispersive spectrometer. It is found that a thick layer of reaction product is formed at the interface of composite after re-melting. The experimental results show that the reaction products at the interface are associated with high concentration of Cu, Mg, Si and C. At re-melting temperature, liquid Al reacts with SiC to form Al{sub 4}C{sub 3} and Al–Si eutectic phase or elemental Si at the interface. High concentration of Si at the interface indicates that SiC is dissociated during re-melting. The X-ray energy dispersive spectrometer analyses confirm that Mg- and Cu-enrich phases are formed at the interface region. The Mg is segregated at the interface region and formed MgAl{sub 2}O{sub 4} in the presence of oxygen. The several elements identified at the interface region indicate that different types of interfaces are formed in between Al matrix and SiC particles. The Al–Si eutectic phase is formed around SiC particles during re-melting which restricts the SiC dissolution. - Highlights: • Re-melted composite shows homogeneous particle distribution • Thick reaction products are observed at the interface • Carbide is identified at interface due to SiC dissolution at high temperature • Reaction products are also Si enrich phase • Mg and Cu segregated and formed MgAl{sub 2}O{sub 4}, CuMgAl{sub 2} phase at grain boundary.

36 MATERIALS SCIENCE↗

Effects of gas to melt ratio on the microstructure of an Al–10.83Zn–3.39Mg–1.22Cu alloy produced by spray atomization and deposition

Various gas to melt ratios (GMR) that govern the cooling rate of spray forming can be achieved through controlling the atomizer form and the atomization pressure. The effect of the GMR on microstructures of an Al–10.83Zn–3.39Mg–1.22Cu alloy produced through spray forming has been studied using electron microscopy. When the GMR is high at 3.5, dendritic structure and quasi-crystalline i-Mg{sub 32}(AlZn){sub 49} particles inherited from the original powders can be observed. Spray forming at medium GMR of 2.3 produces equiaxed α-Al grains and MgZn{sub 2} phase that discontinuously distributes along the grain boundaries and within the grains as small particles. The low GMR of 1.4 corresponds to low cooling rate. Coarse and equiaxed α-Al grains together with eutectic structure consisting of b.c.c.-Mg{sub 32}(AlZn){sub 49} and α-Al phases along the grain boundaries are obtained. - Highlights: • At high GMR, the broken fragments and i-Mg{sub 32}(AlZn){sub 49} quasicrystal are observed. • At medium GMR, microstructure consists of α-Al equiaxed grains and MgZn{sub 2} phase. • At low GMR, the coarsened α-Al grains and bcc-Mg{sub 32}(AlZn){sub 49} eutectic appear.

36 MATERIALS SCIENCE↗

A comparative study of quantitative microsegregation analyses performed during the solidification of the Ni-base superalloy CMSX-10

Quantitative microsegregation analyses were systematically carried out during the solidification of the Ni-base superalloy CMSX-10 to clarify the methodological effect on the quantification of microsegregation and to fully understand the solidification microstructure. Three experimental techniques, namely, mushy zone quenching (MZQ), planar directional solidification followed by quenching (PDSQ), and random sampling (RS), were implemented for the analysis of microsegregation tendency and the magnitude of solute elements by electron probe microanalysis. The microprobe data and the calculation results of the diffusion field ahead of the solid/liquid (S/L) interface of PDSQ samples revealed that the liquid composition at the S/L interface is significantly influenced by quenching. By applying the PDSQ technique, it was also found that the partition coefficients of all solute elements do not change appreciably during the solidification of primary γ. All three techniques could reasonably predict the segregation behavior of most solute elements. Nevertheless, the RS approach has a tendency to overestimate the magnitude of segregation for most solute elements when compared to the MZQ and PDSQ techniques. Moreover, the segregation direction of Cr and Mo predicted by the RS approach was found to be opposite from the results obtained by the MZQ and PDSQ techniques. This conflicting segregation behavior of Cr and Mo was discussed intensively. It was shown that the formation of Cr-rich areas near the γ/γ′ eutectic in various Ni-base superalloys, including the CMSX-10 alloy, could be successfully explained by the results of microprobe analysis performed on a sample quenched during the planar directional solidification of γ/γ′ eutectic. - Highlights: • Methodological effect on the quantification of microsegregation was clarified. • The liquid composition at the S/L interface was influenced by quenching. • The segregation direction of Cr varied depending on the experimental techniques. • Cr and Mo segregation in Ni-base superalloys was fully understood.

36 MATERIALS SCIENCE↗

The use of a directional solidification technique to investigate the interrelationship of thermal parameters, microstructure and microhardness of Bi–Ag solder alloys

Bi–Ag alloys have been stressed as possible alternatives to replace Pb-based solder alloys. Although acceptable melting temperatures and suitable mechanical properties may characterize such alloys, as referenced in literature, there is a lack of comprehension regarding their microstructures (morphologies and sizes of the phases) considering a composition range from 1.5 to 4.0 wt.%Ag. In order to better comprehend such aspects and their correlations with solidification thermal parameters (growth rate, v and cooling rate, T-dot), directional solidification experiments were carried out under transient heat flow conditions. The effects of Ag content on both cooling rate and growth rate during solidification are examined. Microstructure parameters such as eutectic/dendritic spacing, interphase spacing and diameter of the Ag-rich phase were determined by optical microscopy and scanning electron microscopy. The competition between eutectic cells and dendrites in the range from 1.5 to 4.0 wt.%Ag is explained by the coupled zone concept. Microhardness was determined for different microstructures and alloy Ag contents with a view to permitting correlations with microstructure parameters to be established. Hardness is shown to be directly affected by both solute macrosegregation and morphologies of the phases forming the Bi–Ag alloys, with higher hardness being associated with the cellular morphology of the Bi-2.5 and 4.0 wt.%Ag alloys. - Highlights: • Asymmetric zone of coupled growth for Bi–Ag is demonstrated. • Faceted Bi-rich dendrites have been characterized for Bi–1.5 wt.%Ag alloy. • Eutectic cells were shown for the Bi-2.5 and 4.0 wt.%Ag solder alloys. • Interphase spacing relations with G × v are able to represent the experimental scatters. • Hall-Petch type equations are proposed relating microstructural spacings to hardness.

36 MATERIALS SCIENCE↗

The sequence of intermetallic formation and solidification pathway of an Al–13Mg–7Si–2Cu in-situ composite

The phase transformation sequence and solidification behaviour of an Al–13Mg–7Si–2Cu in-situ composite was examined using a combination of computer-aided cooling curve thermal analysis and interrupted quenching techniques. Five different phases were identified by analysing the derivative cooling curves, the X-ray diffraction profile, optical and scanning electron microscopy images and the corresponding energy dispersive spectroscopy. It has been found that the solidification of this alloy begins with primary Mg{sub 2}Si precipitation and continues with the formation of eutectic Al–Mg{sub 2}Si, followed by Al{sub 5}FeSi and simultaneous precipitation of Al{sub 5}Cu{sub 2}Mg{sub 8}Si{sub 6} and Al{sub 2}Cu complex intermetallic phases. The formation of the last three intermetallic compounds changes the solidification behaviour of these composites remarkably due to their complex eutectic formation reactions. The solidification of the alloy, calculated using the Factsage thermochemical analysis software, has demonstrated a good agreement with the experiments in terms of compound prediction, their weight fractions and reaction temperatures. - Highlights: • Solidification path of a commercial Al-13Mg-7Si-2Cu composite was characterized. • Five different phases were identified and then confirmed with EDS and XRD results. • Mg{sub 2}Si, Al-Mg{sub 2}Si,Al{sub 5}FeSi (β),Al{sub 5}Cu{sub 2}Mg{sub 8}Si{sub 6} (Q) and Al{sub 2}Cu(θ) precipitated respectively. • Solidification was predicted using the Factsage thermochemical analysis software.

36 MATERIALS SCIENCE↗

Effects of W on microstructure of as-cast 28 wt.%Cr–2.6 wt.%C–(0–10)wt.%W irons

Microstructures of as-cast 28 wt.%Cr–2.6 wt.%C irons containing (0–10)wt.%W with the Cr/C ratio about 10 were studied and related to their hardness. The experimental irons were cast into dry sand molds. Microstructural investigation was performed by light microscopy, X-ray diffractometry, scanning electron microscopy, transmission electron microscopy and energy-dispersive X-ray spectrometry. It was found that the irons with 1 to 10 wt.%W addition was hypereutectic containing large primary M{sub 7}C{sub 3}, whereas the reference iron without W addition was hypoeutectic. The matrix in all irons was austenite, partly transformed to martensite during cooling. The volume fractions of primary M{sub 7}C{sub 3} and the total carbides increased, but that of eutectic carbides decreased with increasing the W content of the irons. W addition promoted the formation of W-rich M{sub 7}C{sub 3}, M{sub 6}C and M{sub 23}C{sub 6}. At about 4 wt.%W, two eutectic carbides including M{sub 7}C{sub 3} and M{sub 6}C were observed together with primary M{sub 7}C{sub 3}. At 10 wt.%W, multiple carbides including primary M{sub 7}C{sub 3}, fish-bone M{sub 23}C{sub 6}, and M{sub 6}C were observed. M{sub x}C where x = 3 or less has not been found due possibly to the high M/C ratio in the studied irons. W distribution to all carbides has been determined increasing from ca. 0.3 to 0.8 in mass fraction as the W content in the irons was increased. W addition led to an increase in Vickers macro-hardness of the irons up to 671 kgf/(mm){sup 2} (HV30/15) obtained from the iron with 10 wt.%W. The formation of primary M{sub 7}C{sub 3} and aggregates of M{sub 6}C and M{sub 23}C{sub 6} were the main reasons for hardness increase, indicating potentially improved wear performance of the as-cast irons with W addition. - Highlights: • W addition at 1 up to 10 wt.%W to Fe–28Cr–2.6C produced “hypereutectic” structure. • W addition promoted the formation of W-rich M{sub 7}C{sub 3}, M{sub 6}C and M{sub 23}C{sub 6}. • M{sub 23}C{sub 6} has higher Fe/Cr and W/Cr atm% ratios than those in M{sub 7}C{sub 3}. • Si content and high W content over about 11 atm% are characteristics of M{sub 6}C. • Primary M{sub 7}C{sub 3} and aggregates of M{sub 6}C and M{sub 23}C{sub 6} increased the alloy macro-hardness.

36 MATERIALS SCIENCE↗

Precipitates in a quasicrystal-strengthened Al–Mn–Be–Cu alloy

In this work, an Al–Mn–Be–Cu alloy was studied containing a primary and eutectic icosahedral quasicrystalline phase in the as-cast microstructure. Special attention was given to a transmission electron microscopy investigation of precipitates formed within the aluminium solid solution (Al{sub ss}) at different temperatures. At 200 °C, only binary Al–Cu precipitates (θ′) were formed. At 300 °C, icosahedral quasicrystalline (IQC) precipitates prevailed with a crystallographic orientation relationship with the Al{sub ss.} The rods of the T-phase (Al{sub 20}Mn{sub 3}Cu{sub 2}) which were precipitated above 400 °C, also had a specific orientation relationship with the Al{sub ss}. The primary and eutectic IQC microstructural constituent started to transform rapidly to the T-phase and Be{sub 4}Al(Mn,Cu) at 500 °C. - Highlights: • In a quasicrystal-strengthened Al-alloy several types of precipitates can form. • At 200 °C, only binary Al–Cu precipitates formed (Al{sub 2}Cu-θ′). • The icosahedral quasicrystalline (IQC) precipitates prevailed at 300 °C. • T-phase (Al{sub 20}Mn{sub 3}Cu{sub 2}) precipitated at temperatures above 400 °C. • The precipitation of different phases did not have a strong effect on hardness.

36 MATERIALS SCIENCE↗

Study of formation mechanism of incipient melting in thixo-cast Al–Si–Cu–Mg alloys

Mechanical properties of thixo-cast Al–Si–Cu–Mg alloys can be enhanced by T61 heat treatment. Copper and magnesium atoms in aluminum matrix can form homogeneously distributed precipitations after solution and aging treatment which harden the alloys. However, microsegregation of these alloying elements could form numerous tiny multi-compound phases during solidification. These phases could cause incipient melting defects in subsequent heat treatment process and degrade the macro-mechanical properties of productions. This study is to present heterogeneous distribution of Cu, Si, and Mg elements and formation of incipient melting defects (pores). In this study, incipient melting pores that occurred during solution treatment at various temperatures, even lower than common melting points of various intermetallic phases, were identified, in terms of a method of investigating the same surface area in the samples before and after solution treatment in a vacuum environment. The results also show that the incipient melting mostly originates at the clusters with fine intermetallic particles while also some at the edge of block-like Al{sub 2}Cu. The fine particles were determined being Al{sub 2}Cu, Al{sub 5}Cu{sub 2}Mg{sub 8}Si{sub 6} and Al{sub 8}Mg{sub 3}FeSi{sub 2}. Tendency of the incipient melting decreases with decreases of the width of the clusters. The formation mechanism of incipient melting pores in solution treatment process was discussed using both the Fick law and the LSW theory. Finally, a criterion of solution treatment to avoid incipient melting pores for the thixo-cast alloys is proposed. - Highlights: • In-situ comparison technique was used to analysis the change of eutectic phases. • The ralationship between eutectic phase size and incipient melting was studied. • Teat treatment criterion for higher incipient melting resistance was proposed.

36 MATERIALS SCIENCE↗

3D study of intermetallics and their effect on the corrosion morphology of rheocast aluminium alloy

In the present study, the effect of heat treatment T6.1 on the microstructure and corrosion behaviour of rheocast aluminium alloy A356 is investigated on the basis of 2D/3D characterization techniques and electrochemical and SKPFM measurements. Heat treatment strengthens the α-Al matrix, modifies the intermetallic particles and spheroidizes eutectic Si. These changes do not modify significantly the corrosion behaviour of the alloy. 3D SEM-Tomography clearly shows that the corrosion advances in the shape of narrow paths between closely spaced intermetallics without a major influence of eutectic Si. - Highlights: • T6.1 spheroidizes Si, strengthens the matrix and modifies the intermetallics. • Electrochemical behaviour of untreated and heat-treated alloys is similar. • 3D SEM-Tomography provides additional information on the corrosion morphology. • Corrosion advances as paths between intermetallics with little influence of Si.

36 MATERIALS SCIENCE↗

Cooling thermal parameters and microstructure features of directionally solidified ternary Sn–Bi–(Cu,Ag) solder alloys

Low temperature soldering technology encompasses Sn–Bi based alloys as reference materials for joints since such alloys may be molten at temperatures less than 180 °C. Despite the relatively high strength of these alloys, segregation problems and low ductility are recognized as potential disadvantages. Thus, for low-temperature applications, Bi–Sn eutectic or near-eutectic compositions with or without additions of alloying elements are considered interesting possibilities. In this context, additions of third elements such as Cu and Ag may be an alternative in order to reach sounder solder joints. The length scale of the phases and their proportions are known to be the most important factors affecting the final wear, mechanical and corrosions properties of ternary Sn–Bi–(Cu,Ag) alloys. In spite of this promising outlook, studies emphasizing interrelations of microstructure features and solidification thermal parameters regarding these multicomponent alloys are rare in the literature. In the present investigation Sn–Bi–(Cu,Ag) alloys were directionally solidified (DS) under transient heat flow conditions. A complete characterization is performed including experimental cooling thermal parameters, segregation (XRF), optical and scanning electron microscopies, X-ray diffraction (XRD) and length scale of the microstructural phases. Experimental growth laws relating dendritic spacings to solidification thermal parameters have been proposed with emphasis on the effects of Ag and Cu. The theoretical predictions of the Rappaz-Boettinger model are shown to be slightly above the experimental scatter of secondary dendritic arm spacings for both ternary Sn–Bi–Cu and Sn–Bi–Ag alloys examined. - Highlights: • Dendritic growth prevailed for the ternary Sn–Bi–Cu and Sn–Bi–Ag solder alloys. • Bi precipitates within Sn-rich dendrites were shown to be unevenly distributed. • Morphology and preferential region for the Ag{sub 3}Sn growth depend on Ag content and Ṫ{sub L}. • Rappaz-Boettinger model reasonably estimated the experimental scatter of λ{sub 2}.

36 MATERIALS SCIENCE↗

Influence of phase composition on microstructure and properties of Mg-5Al-0.4Mn-xRE (x = 0, 3 and 5 wt.%) alloys

The microstructure and mechanical properties investigations of two AME503 and AME505 experimental alloys in as-cast conditions were presented. The investigated materials were fabricated on the basis of the AM50 commercial magnesium alloy with 3 and 5 wt.% cerium rich mischmetal. In the as-cast condition, both experimental alloys were mainly composed of α-Mg, Al{sub 11}RE{sub 3} and Al{sub 10}RE{sub 2}Mn{sub 7} intermetallic phases. Additionally, due to non-equilibrium solidification conditions, a small amount of α + γ divorced eutectic and Al{sub 2}RE intermetallic phase were revealed. The obtained results also show a significant influence of rare earth elements on Brinell hardness, tensile and compression properties at ambient temperature and especially on creep properties at 473 K. Improved alloy properties with a rise in rare earth elements mass fraction results from an increase in Al{sub 11}RE{sub 3} phase volume fraction and suppression of α + γ eutectic volume fraction in the alloy microstructure. Additionally, the influence of rare earth elements on the dendrite arm space value was discussed. The presented results also proved the thermal stability of the intermetallic phases during creep testing. - Highlights: • Two different Mg-5Al-0.4Mn alloys containing 3 and 5 wt.% of rare earth elements were fabricated. • Addition of rare earth elements leads to a reduction of dendrite arm spaces. • Mechanical properties depend on the phase composition of the alloys. • The increase of the rare earth elements content causes rise of the creep resistance.

36 MATERIALS SCIENCE↗

Improved the microstructures and properties of M3:2 high-speed steel by spray forming and niobium alloying

The microstructures and properties of spray formed (SF) high-speed steels (HSSs) with or without niobium (Nb) addition were studied. Particular emphasis was placed on the effect of Nb on the solidification microstructures, decomposition of M{sub 2}C carbides, thermal stability and mechanical properties. The results show that spray forming can refine the cell size of eutectic carbides due to the rapid cooling effect during atomization. With Nb addition, further refinement of the eutectic carbides and primary austenite grains are obtained. Moreover, the Nb addition can accelerate the decomposition of M{sub 2}C carbides and increase the thermal stability of high-speed steel, and also can improve the hardness and bending strength with slightly decrease the impact toughness. The high-speed steel made by spray forming and Nb alloying can give a better tool performance compared with powder metallurgy M3:2 and commercial AISI M2 high-speed steels. - Highlights: • Spray forming can effectively refine the microstructure of M3:2 steel. • Niobium accelerates the decomposition of M{sub 2}C carbides. • Niobium increases the hardness and bending strength of spray formed M3:2 steel. • Spray-formed niobium-containing M3:2 steel has the best tool performance.

36 MATERIALS SCIENCE↗

Influence of severe plastic deformation on intermetallic particles in Mg-12 wt.%Zn alloy investigated using transmission electron microscopy

The in-depth microstructural characterization of intermetallic particles in an Mg-12 wt.%Zn binary alloy subjected to a severe plastic deformation is presented. The alloy was processed by four passes via equal channel angular pressing with an applied back pressure at a gradually decreasing temperature and analyzed using transmission electron microscopy techniques to observe the influence of processing on intermetallic particles. The results are compared with the initial state of the material prior to severe plastic deformation. The microstructural evolution of the α-Mg matrix and the Mg{sub 21}Zn{sub 25}, Mg{sub 51}Zn{sub 20} and MgZn{sub 2} was analyzed using bright field imaging, selected area electron diffraction, high-resolution transmission electron microscopy and high-angle annular dark field imaging in scanning mode. The plastic deformation process influenced the α-Mg matrix and each type of intermetallic particle. The α-Mg matrix consisted of two types of areas. The first type of area had a highly deformed structure, and the second type of area had a partially recrystallized structure with an average grain size of approximately 250 nm. The Mg{sub 21}Zn{sub 25} microparticles exhibited distinct forms in the α-Mg matrix that were characterized as a single-crystalline form, a nano-crystalline form and a broken up form. No evidence of Mg{sub 51}Zn{sub 20} nanoparticles within the α-Mg matrix was found in the microstructure, which indicates their dissolution or phase transformation during the deformation process. MgZn{sub 2} nanoparticles exhibited different behavior in both types of α-Mg matrix. Two orientation relationships toward the highly deformed α-Mg matrix were observed; however, there was no relationship toward the partially recrystallized α-Mg matrix. Additionally, the growth of the MgZn{sub 2} nanoparticles was different in the two types of α-Mg matrix. The Mg{sub 51}Zn{sub 20} nanoparticles inside Mg{sub 21}Zn{sub 25} microparticles exhibited a distinct behavior within the single-crystalline or nano-crystalline form of the parent Mg{sub 21}Zn{sub 25} microparticles. The Mg{sub 21}Zn{sub 25} + Mg{sub 51}Zn{sub 20} eutectic compound was confirmed for both forms of the parent Mg{sub 21}Zn{sub 25} microparticles, and the growth of Mg{sub 51}Zn{sub 20} nanoparticles is discussed. - Highlights: •Comprehensive microstructure characterization of Mg-12 wt.%Zn alloy after ECAP-BP •TEM analysis of changes of intermetallic phases caused by SPD •Mg{sub 21}Zn{sub 25} particles exhibit nano-crystalline regions with grain size below 100 nm. •MgZn{sub 2} preserved its orientation relationship toward highly deformed α-Mg after SPD. •Existence of Mg{sub 21}Zn{sub 25} + Mg{sub 51}Zn{sub 20} eutectic remained for each Mg{sub 21}Zn{sub 25} particle form.

36 MATERIALS SCIENCE↗

Effects of Si on microstructure and phase transformation at elevated temperatures in ferritic white cast irons

The effects of Si on microstructure and phase transformation at elevated temperature of ferritic 31wt.%Cr-1.1wt.%C white cast irons with up to 3wt.%Si have been studied. Applications of these irons include parts requiring heat resistance at elevated temperature. The irons were produced by sand casting. The microstructure in as-cast condition and after being subjected to high temperature (700 to 1000 °C) was investigated by light microscopy, X-ray diffraction, and electron microscopy. The results revealed that the as-cast microstructure consisted mainly of primary ferrite dendrites and eutectic (ferrite + M{sub 7}C{sub 3}). Si promotes M{sub 7}C{sub 3}-to-M{sub 23}C{sub 6} transformation in the irons subjected to transformation at elevated temperature, but no sigma phase was found. The extent of M{sub 7}C{sub 3}-to-M{sub 23}C{sub 6} transformation increases proportional to the increasing transformation temperature, holding time and Si content in the irons. For the iron with 1.0wt.%Si content after holding at elevated temperatures, martensite was also found, which could be attributed to carbon accretion effects in eutectic ferrite. Si was incorporated in M{sub 23}C{sub 6} such that M{sub 23}C{sub 6} containing Si can show darker contrast under SEM-BEI as compared to M{sub 7}C{sub 3}; this is the opposite to what has been observed for the cases of typical M{sub 23}C{sub 6} and M{sub 23}C{sub 6} containing Mo or W. The results obtained are important to understand the change in properties of ferritic, high chromium irons containing Si subjected to elevated temperature.

36 MATERIALS SCIENCE↗

Lead Coolant Test Facility - Design Concept and Requirements

The Idaho National Laboratory prepared a preliminary technical and functional requirements (T&FR), thermal hydraulic design and cost estimate for a lead coolant test facility. The purpose of this small scale facility is to simulate lead coolant fast reactor (LFR) coolant flow in an open lattice geometry core using seven electrical rods and liquid lead or lead-bismuth eutectic. Based on review of current world lead or lead-bismuth test facilities and research need listed in the Generation IV Roadmap, five broad areas of requirements are identified in this paper: (1) Develop and Demonstrate Feasibility of Submerged Heat Exchanger; (2) Develop and Demonstrate Open-lattice Flow in Electrically Heated Core; (3) Develop and Demonstrate Chemistry Control; (4) Demonstrate Safe Operation; and (5) Provision for Future Testing Across these five broad areas are supported by twenty-one specific requirements. The purpose of this facility is to focus the lead fast reactor community domestically on the requirements for the next unique state of the art test facility. The facility thermal hydraulic design is based on the maximum simulated core power using seven electrical heater rods of 420 kW; average linear heat generation rate of 300 W/cm. The core inlet temperature for liquid lead or Pb/Bi eutectic is 4200C. The design includes approximately seventy-five data measurements such as pressure, temperature, and flow rates. The preliminary estimated cost of construction of the facility is $3.7M (in 2006 $). It is also estimated that the facility will require two years to be constructed and ready for operation.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Lead Coolant Test Facility Systems Design, Thermal Hydraulic Analysis and Cost Estimate

The Idaho National Laboratory prepared a preliminary technical and functional requirements (T&FR), thermal hydraulic design and cost estimate for a lead coolant test facility. The purpose of this small scale facility is to simulate lead coolant fast reactor (LFR) coolant flow in an open lattice geometry core using seven electrical rods and liquid lead or lead-bismuth eutectic coolant. Based on review of current world lead or lead-bismuth test facilities and research needs listed in the Generation IV Roadmap, five broad areas of requirements were identified as listed: (1) Develop and Demonstrate Feasibility of Submerged Heat Exchanger; (2) Develop and Demonstrate Open-lattice Flow in Electrically Heated Core; (3) Develop and Demonstrate Chemistry Control; (4) Demonstrate Safe Operation; and (5) Provision for Future Testing. This paper discusses the preliminary design of systems, thermal hydraulic analysis, and simplified cost estimate. The facility thermal hydraulic design is based on the maximum simulated core power using seven electrical heater rods of 420 kW; average linear heat generation rate of 300 W/cm. The core inlet temperature for liquid lead or Pb/Bi eutectic is 4200 C. The design includes approximately seventy-five data measurements such as pressure, temperature, and flow rates. The preliminary estimated cost of construction of the facility is $3.7M (in 2006 $). It is also estimated that the facility will require two years to be constructed and ready for operation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗