Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CRACKS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 883 records · Page 49

A Self-Healing, Flowable, Yet Solid Electrolyte Suppresses Li-Metal Morphological Instabilities

In this article, lithium metal (Li 0 ) solid-state batteries encounter implementation challenges due to dendrite formation, side reactions, and movement of the electrode–electrolyte interface in cycling. Notably, voids and cracks formed during battery fabrication/operation are hot spots for failure. Here, a self-healing, flowable yet solid electrolyte composed of mobile ceramic crystals embedded in a reconfigurable polymer network is reported. This electrolyte can auto-repair voids and cracks through a two-step self-healing process that occurs at a fast rate of 5.6 µm h -1 . A dynamical phase diagram is generated, showing the material can switch between liquid and solid forms in response to external strain rates. The flowability of the electrolyte allows it to accommodate the electrode volume change during Li 0 stripping. Simultaneously, the electrolyte maintains a solid form with high tensile strength (0.28 MPa), facilitating the regulation of mossy Li 0 deposition. The chemistries and kinetics are studied by operando synchrotron X-ray and in situ transmission electron microscopy (TEM). Solid-state NMR reveals a dual-phase ion conduction pathway and rapid Li + diffusion through the stable polymer-ceramic interphase. This designed electrolyte exhibits extended cycling life in Li 0 –Li 0 cells, reaching 12 000 h at 0.2 mA cm -2 and 5000 h at 0.5 mA cm -2 . Furthermore, owing to its high critical current density of 9 mA cm -2 , the Li 0 –LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) full cell demonstrates stable cycling at 5 mA cm -2 for 1100 cycles, retaining 88% of its capacity, even under near-zero stack pressure conditions.

25 ENERGY STORAGE↗

Heterogeneity of the Dominant Causes of Performance Loss in End-of-Life Cathodes and Their Consequences for Direct Recycling

Recycling Li-ion batteries from electric vehicles is critical for reducing costs and supporting the development of a domestic battery supply chain. Direct recycling of cathodes, like LiNixMnyCozO2 (NMC), is attractive due to its low cost, energy use, and emissions compared to traditional recycling techniques. However, a comprehensive understanding of the active material properties at end-of-life is needed to guide direct recycling processes and the performance-dependent reuse applications. Here, NMC material from an end-of-life commercial pouch cell is characterized and bench-marked against pristine non-cycled counterparts with respect to capacity, impedance, crystallography, morphology, and microstructure to identify major degradation modes and understand variability in the end-of-life material. The spatial heterogeneity of each property throughout the cell is also quantified. While the degraded material demonstrated similar capacity as the pristine, its impedance and rate capability are severely diminished. Furthermore, samples from the periphery of the electrode layers showed more severe performance loss compared to samples extracted from central regions. The dominant culprit of performance loss is the material microstructure, where the magnitude of particle cracking showed the strongest correlation to the impedance components that are most unfavorably impacted. This work suggests severe cracks in cathode active materials are the primary challenge that direct recycling methods must overcome.

25 ENERGY STORAGE↗

Enhanced Reactivity of Accessible Protons in Sodalite Cages of Faujasite Zeolite

Abstract Faujasite (FAU) zeolites (with Si/Al ratio of ca. 1.7) undergo mild dealumination at moderate ion exchange conditions (0.01 to 0.6 M of NH 4 NO 3 solutions) resulting in protons circumscribed by sodalite cages becoming accessible for reaction without conspicuous changes to bulk crystallinity. The ratio of protons in sodalite cages (H SOD ) to supercages (H SUP ) can be systematically manipulated from 0 to ca. 1 by adjusting ammonium concentrations used in ion exchange. The fraction of accessible protons in the sodalite cages is assessed by virtue of infrared spectra for H‐D exchange of deuterated propane based on the band area ratio of OD 2620 /OD 2680 (OD SOD /OD SUP ). Protons in sodalite cages (H SOD ) show higher rate constants of propane dehydrogenation ( k D ) and cracking ( k C ) than protons in supercages (H SUP ) plausibly due to confinement effects being more prominent in smaller voids. Rate constants of dehydrogenation and cracking including k D / k C ratios are also augmented as the fraction of accessible protons in the sodalite cages is enhanced. These effects of accessibility and reactivity of protons in sodalite cages hitherto inconspicuous are revealed herein via methods that systematically increase accessibility of cations located in sodalite cages.

Li, Xinyu↗

Damage of prismatic lithium‐ion cells subject to bending: Test, model, and detection

Abstract The mechanically induced internal short circuit (ISC) is one of the major safety concerns of lithium‐ion batteries. Mechanical abuse tests are often performed to evaluate the integrity and safety of lithium‐ion batteries under mechanical loadings. Except for the widely explored compression‐dominated indentation tests, bending is another typical real‐world loading condition that is tension‐dominated. To investigate the mechanical damage and ISC behavior of batteries under bending, we carried out controlled three‐point bending tests in four progressive steps on prismatic battery cells with maximum deflections ranging from 38% to 76% of the cell thickness. None of the tested cells experienced an ISC. We then conducted 3D X‐ray computed tomography (CT) scanning on the bent cells after unloading. X‐ray CT images showed three out of the four tested cells have extensive cracking in the electrode layers at the bottom side (opposite to the loading head). This indicates that cracking does not necessarily lead to an ISC under bending. Electrochemical impedance spectroscopy was also measured on the bent cells and substantial changes were observed. Both the bulk resistance and charge‐transfer resistance increased significantly after bending, which could influence the battery performance and lifespan. We then developed a detailed finite (FE) element model to further investigate the mechanical deformation and failure mechanisms. The FE model successfully predicts the load–displacement response and reproduces the deformation patterns. The findings and the FE model developed in the present study provide useful insights and tools for the battery structure and crash safety design. image

25 ENERGY STORAGE↗

A micromorphic filter for determining stress and deformation measures from direct numerical simulations of lower length scale behavior

A micromorphic filter is presented for the extraction of stress and deformation measures from underlying direct numerical simulation (DNS) of microstructural mechanical response. The filter is consistent with the micromorphic continuum theory of Eringen and Suhubi (1964), and allows the interrogation of a DNS to generate higher order constitutive models. The filter adopts aspects of the overlap coupling techniques for atomistic-continuum scale-bridging in order to update the nodal degrees of freedom of the finite-element-based filter. Here, two methods for the extraction of quantities of interest from the underlying DNS are presented. The first is a least squares fitting technique which is appropriate for finite-element-style macro-scale domains, and the second is a variationally based approach which generalizes the method to any macro-scale domain which has a variational form. No restrictions on the form of the micro-scale simulation are inherent to the approach, provided that the required quantities (stress, position, etc.) can be provided. The filter is applied to a simple homogeneous medium undergoing homogeneous deformation to demonstrate the recovery of a classical continuum response, what we call the null case. We then apply the framework to the same homogeneous medium with a central and edge penny-shaped crack to show micromorphic effects. We demonstrate that varying the size of the filter causes the micromorphic behaviors to arise and then dissipate as the filter becomes smaller than the crack's length scale. Additionally we show the effect of filter size on a chiral element network along with a plate perforated with evenly spaced and perturbed holes through the thickness. The micromorphic effects are shown to be present for the chiral elements under any loading but become most pronounced when a single element is located within each averaging domain. Micromorphic effects become pronounced for the plate upon the onset of localization.

97 MATHEMATICS AND COMPUTING↗

Multiscale numerical investigation of ratchet growth damage effects in PBX 9502

This paper presents results of numerical experiments conducted on the high explosive PBX 9502 to investigate how recently observed grain-scale damage mechanisms of ratchet growth affect uniaxial compression measurements. Simulations are multiscale in the sense of directly resolving grains, pores, cracks, and grain-interfaces based upon scanning electron microscope (SEM) images of damaged and undamaged samples. The combined finite-discrete element method (FDEM) is utilized to resolve both grain-scale microfracture and elastoplastic deformation of solid grains. Pristine (undamaged) and damaged microstructures are compared in simulation of unconfined compression tests of the same material from the literature. Here, the simulation results show the observed microscale mechanisms of damage, specifically microfracture predominantly around and sometimes through grains and crack-associated pore growth, can well-explain the effective degradation of strength and stiffness observed in the laboratory measurements.

36 MATERIALS SCIENCE↗

Atomistic Mechanics of Torn Back Folded Edges of Triangular Voids in Monolayer WS 2

Triangular nanovoids in 2D materials transition metal dichalcogenides have vertex points that cause stress concentration and lead to sharp crack propagation and failure. Here, the atomistic mechanics of back folding around triangular nanovoids in monolayer WS 2 sheets is examined. Combining atomic-resolution images from annular dark-field scanning transmission electron microscopy with reactive molecular modelling, it is revealed that the folding edge formation has statistical preferences under geometric conditions based on the orientation mismatch. It is further investigated how loading directions and strong interlayer friction, interplay with WS 2 lattice's crack preference, govern the deformation and fracture pattern around folding edges. Finally, these results provide fundamental insights into the combination of fracture and folding in flexible monolayer crystals and the resultant Moiré lattices.

36 MATERIALS SCIENCE↗

Strain Field Around Individual Dislocations Controls Failure

Understanding material failure on a fundamental level is a key aspect in the design of robust structural materials, especially for metals and alloys capable to undergo plastic deformation. In the last decade, significant progress is made in quantifying the stresses associated with failure in both experiments and simulations. Nonetheless, the processes occurring on the most essential level of individual dislocations that govern semi-brittle and ductile fracture are still experimentally not accessible, limiting the failure prediction capabilities. Therefore, in the present work, a one-of-a-kind nanoscale fracture experiment is conducted on a single crystalline Cr bending beam in situ in the transmission electron microscope and for the first time quantify the transient strains around individual dislocations, as well as of the whole dislocation network during crack opening. The results reveal the importance of both pre-existing and newly emitted dislocations for crack-tip shielding via their intrinsic strain field and provide guidelines to design more damage tolerant materials.

36 MATERIALS SCIENCE↗

Assessment of Dynamic Fracture in Ultra-High Performance Concrete Using Synchrotron X-ray Source

Ultra-high-performance concretes (UHPCs) retain higher ultimate (compressive) strengths and greater durability relative to traditional concrete materials. As a result, they are enabling construction materials for blast resistant structures, where a higher capacity for energy absorption is required. In past investigations, the strength of UHPCs was shown to retain a dependency on strain rate. Still, the failure mechanisms which govern this rate dependency have yet to be completely elucidated. In the current study, the dynamic fracture behavior of Cor-tuf UHPC was assessed, in-situ, using a Synchrotron X-ray source in phase contrast imaging (PCI) mode. Prior to testing, the material’s morphology was characterized using X-ray computed tomography (CT) and scanning electron microscopy (SEM). A polychromatic pulsed X-ray source, high-speed camera and Kolsky bar apparatus were used in tandem, to observe the transient failure modes. A pin was placed at the end of the incident bar to control the location of damage initiation, and tests were performed at a constant velocity of ~6 m/s. These test conditions were observed to yield cracks with median and/or cone like geometries. Despite the variation in the crack paths, a significant difference in peak load was not observed. The failure mode was also observed to depend on the microstructure of the concrete samples.

Kolsky bar↗

Exploring the Microstructure-Property Relationship of Mg-Al-Mn alloys enhanced via Friction Stir Processing

Friction Stir Processing (FSP) is a solid-state thermomechanical processing technique that enables local grain refinement, densification, and homogenization of microstructure in metallic components. Here, FSP is applied to thin sheets of high-pressure die cast AM60 to address the porosity and heterogeneities inherent to the casting process. In this work, microstructure characterization is correlated to improvements in the static mechanical properties of the Mg-Al-Mn alloy system at various FSP processing conditions. Notably, there is a significant increase in the ductility and ultimate tensile stress of system following FSP. The dominant deformation mechanisms for the as-cast material and the FSP material are investigated. Finally, the fatigue life improvement is correlated to microstructure modifications that may lead to distinct behavior in crack initiation and crack propagation for the as-cast and FSP material.

Garcia, David↗

Joining of High Strength Low Ductility AA7055 by Friction Self-piercing Rivet

High strength aluminum (Al) alloy is one of higher specific strength materials for decarbonization in transportation industries. Because of low ductility at room temperature, conventional mechanical fastening such as self-piercing riveting produces cracks at the joint. In this work, we applied friction self-piercing riveting to join Al alloy (AA) 7055. No cracks were observed in the joints because of the improved local ductility of Al alloy by the generated frictional heat during joining step. Numerical modeling of joining process was applied to guide rivet geometry design and rivet material strength. Mechanical integrity of the AA7055 joints was assessed by lap shear tensile and cross-tension testing. Metallurgical characterizations revealed solid-state bonding formed not only between the rivet and surround Al materials, but also upper and lower Al sheets at the joint interface. Both solid-state bonding and mechanical interlocking between the flared rivet and bottom AA7055 sheet were the major joint mechanisms.

Lim, Yong Chae↗

An adaptive space-time phase field formulation for dynamic fracture of brittle shells based on LR NURBS

Here, we present an adaptive space-time phase field formulation for dynamic fracture of brittle shells. Their deformation is characterized by the Kirchhoff–Love thin shell theory using a curvilinear surface description. All kinematical objects are defined on the shell’s mid-plane. The evolution equation for the phase field is determined by the minimization of an energy functional based on Griffith’s theory of brittle fracture. Membrane and bending contributions to the fracture process are modeled separately and a thickness integration is established for the latter. The coupled system consists of two nonlinear fourth-order PDEs and all quantities are defined on an evolving two-dimensional manifold. Since the weak form requires C 1 -continuity, isogeometric shape functions are used. The mesh is adaptively refined based on the phase field using Locally Refinable (LR) NURBS. Time is discretized based on a generalized-α method using adaptive time-stepping, and the discretized coupled system is solved with a monolithic Newton–Raphson scheme. Finally, the interaction between surface deformation and crack evolution is demonstrated by several numerical examples showing dynamic crack propagation and branching.

42 ENGINEERING↗

Interpreting test temperature and loading rate effects on the fracture toughness of polymer-metal interfaces via time–temperature superposition

Here, in this letter, we present interfacial fracture toughness data for a polymer-metal interface where tests were conducted at various test temperatures T and loading rates $\dot{δ}$. An adhesively bonded asymmetric double cantilever beam (ADCB) specimen was utilized to measure toughness. ADCB specimens were created by bonding a thinner, upper adherend to a thicker, lower adherend (both 6061 T6 aluminum) using a thin layer of epoxy adhesive, such that the crack propagated along the interface between the thinner adherend and the epoxy layer. The specimens were tested at T from 25 to 65 °C and $\dot{δ}$ from 0.002 to 0.2 mm/s. The measured interfacial toughness Γ increased as both T and $\dot{δ}$ increased. For an ADCB specimen loaded at a constant $\dot{δ}$, the energy release rate G increases as the crack length a increases. For this reason, we defined rate effects in terms of the rate of change in the energy release rate $\dot{G}$. Although not rigorously correct, a formal application of time–temperature superposition (TTS) analysis to the Γ data provided useful insights on the observed dependencies. In the TTS-shifted data, Γ decreased and then increased for monotonically increasing $\dot{G}$. Thus, the TTS analysis suggests that there is a minimum value of Γ. This minimum value could be used to define a lower bound in Γ when designing critical engineering applications that are subjected to T and $\dot{δ}$ excursions.

36 MATERIALS SCIENCE↗

Neutron and x-ray computed tomography of a natural uranium tristructural isotropic (TRISO) fuel compact

A natural uranium-based, unirradiated tristructural isotropic (TRISO) fuel compact was nondestructively imaged using both X-ray (XCT) and neutron computed tomography (nCT). While XCT of compacts can provide information on fuel kernels, imaging artifacts preclude examination of the graphite matrix. In this work, nCT was used for the first time on a TRISO compact to examine the graphite matrix. A crack was clearly resolved within the graphite matrix, proving that nCT is a viable tool for nondestructive volumetric examination of the matrix material in TRISO fuel compacts. The XCT and nCT data were then fused together to create a more comprehensive dataset containing both matrix and fuel kernels.

36 - MATERIALS SCIENCE↗

Effects of a Pressurized Water Treatment on Internal Gelation Sol-Gel Microspheres

Based on previous observations that a pressurized water treatment (PWT) prevented cracking of sol-gel microspheres, we investigated the effects of a PWT on microsphere crystallinity, density, and specific surface area (SSA). Results were used to determine how a PWT alters the properties of microspheres upon drying and heating. Microspheres with diameters near 100-200 µm were prepared with and without a PWT and measured using x-ray diffraction (XRD), transmission electron microscopy (TEM), nitrogen adsorption (BET), and pycnometry. Properties of air-dried microspheres processed with and without a PWT are compared. Additionally, the properties of microspheres processed using a PWT are reported after heating to 150 °C, 450 °C, 750 °C, 1050 °C, and 1350 °C. X-ray diffraction measurements indicate that the PWT step improves the crystallinity of air-dried microspheres. XRD data was also used to calculate crystallite size, which increases with higher heat treatment temperatures. TEM images support crystallite size calculations from XRD data and provide an indication of the range of crystallite sizes, particularly for samples processed at higher temperatures where crystallite sizes are too large for estimation using the Scherrer formula. Density and SSA measurements performed as a function of heat treatment temperature indicate that a PWT increases the density of air-dried microspheres, creates a pore network, and that significant densification occurs between 450 - 750 °C. These results may be used to inform decisions on internal gelation flowsheet parameters to optimize the microsphere formation and gelation step, prevent microsphere cracking, and produce microspheres suitable for subsequent coating operations or pressing into pellets.

cerium oxide, TRISO, internal gelation, nuclear fu↗

Inhibition of Micro-pitting by Tribofilm-Forming ZrO 2 Nanocrystal Lubricant Additives: A Micro-pitting Rig and Transmission Electron Microscope Study

The drive to reduce fuel consumption in transportation has encouraged the emergence of low viscosity lubricants to reduce viscous losses in the engine, drivetrain, and other components. However, viscosity reduction increases the risk of surface damage, thus motivating the development of new anti-wear (AW) additives. Capped ZrO 2 nanocrystals (NCs) in base oils have been shown to form AW tribofilms within microscale sliding contacts. However, the potential of ZrO 2 NCs to protect surfaces subjected to rolling-sliding contact from macroscale damage, such as micro-pitting, remains unexplored. Here, we explore the ability of ZrO 2 NCs to form protective tribofilms under harsh conditions using a micro-pitting rig (MPR), consisting of a three ring-on-roller configuration. The experiments were conducted in polyalphaolephin (PAO) base oil, with and without 5 nm diameter ZrO 2 NCs, at two levels of slide-to-roll ratio (SRR) (30% and 0%) and at variable test durations up to long durations (119 h). MPR results showed the use of ZrO 2 NCs gives rise to the formation of a tribofilm covering the roller surfaces and decreases the initiation and propagation of micro-pits compared to tests in pure PAO base stock. Transmission electron microscopy (TEM) performed on focused ion beam (FIB) milled cross-sectional samples of the roller surfaces revealed the growth of dense and 50–100 nm thick ZrO 2 -based tribofilms independent of (SRR), indicating the potential for robust micro-pitting fatigue protection. Nevertheless, small cracks localized within the near surface region of the roller tested at the most severe conditions (30% SRR and 119 h) were observed. The initiation of these cracks was directly related to the presence of manganese sulphide (MnS) inclusions in the steel, revealed using TEM combined with energy dispersive spectroscopy (EDS). Furthermore, the results highlight the benefits of the protective tribofilms formed by ZrO 2 NCs and suggest approaches for further optimizing their use.

36 MATERIALS SCIENCE↗

Creep Behavior of a High-$\gamma^{\prime}$ Ni-Based Superalloy Fabricated via Electron Beam Melting

Additive manufacturing enables the fabrication of complex engineering components previously inaccessible through traditional processes. Nickel-base superalloys with large γ' volume fraction are typically considered non-weldable and therefore exhibit a propensity for cracking during the fusion process. These crack-prone materials, however, are of great importance in gas turbine engines due to their excellent high temperature creep resistance. In this study we investigate the creep behavior of IN738LC produced by the electron beam melting process. Here, we find that with appropriate post-build heat treatment the creep response of material oriented in the build direction exhibits deformation and rupture behavior comparable to that of conventionally cast IN738 & IN738LC. In the transverse direction properties fall below the expected cast behavior, however, we argue this is likely due to differences in grain scale and crystallographic texture. It may be possible to coarsen the grain morphology with appropriate process-parameter optimization in order to reduce the severity of intergranular fracture in the transverse direction. These results illustrate that high temperature properties exhibited by additively manufactured IN738LC are suitable for the hot section of gas turbine engines.

36 MATERIALS SCIENCE↗

Microstructure, Hardness, and Residual Stress of the Dissimilar Metal Weldments of SA508-309L/308L-304L

A dissimilar metal weldment consisting of SA508-309L-308L-304L is widely used in light-water nuclear reactors. These weldments demonstrate dissimilar susceptibility to stress corrosion cracking that are related to the microstructure, properties, and residual stress. In this work, microstructures, hardness, and the residual stress distribution of the dissimilar metal weldments were investigated, with the correlation of increased hardness in the heat-affected zone (HAZ) to the microstructure. 304L HAZ demonstrated similar grain morphology as the base material, and the increase in hardness was primarily attributed to the increased dislocation density. SA508 HAZ demonstrated a change of grain morphology resulting from the different peak temperatures and cooling rates. The increased hardness in the SA508 HAZ was attributed to the refined grain morphology, higher dislocation density, and higher number density of precipitates. A ~ 20–30-μm-wide martensitic zone formed at the fusion boundary of SA508-309L, where Cr-rich carbide precipitates were observed, with the average size and the number density of 44.1 ± 16.9 nm and 1.5 × 10 21 m ₋3 , respectively. In conclusion, residual stress results demonstrated the largest tensile stress at 309L butter, indicating its high cracking susceptibility.

36 MATERIALS SCIENCE↗