Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CORROSION PROTECTION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 883 records · Page 49

Severe Hot Corrosion of the Superalloy IN718 in Mixed Salts of Na{sub 2}SO{sub 4} and V{sub 2}O{sub 5} at 700 °C

This study presents hot corrosion behavior of the superalloy IN718 in 100 wt.% NaCl (salt S) and in salt mixtures of 60 wt.% Na{sub 2}SO{sub 4} + 40 wt.% V{sub 2}O{sub 5} (SM1) and 75 wt.% Na{sub 2}SO{sub 4} + 15 wt.% NaCl + 10 wt.% V{sub 2}O{sub 5} (SM2), deposited separately by spray gun technique, at elevated temperature of 700 °C. The weight gain per unit area at 700 °C was increased by 49% for salt S, 153% for the dual salt mixture SM1, and only 8% for the triple salt mixture SM2, in comparison with that observed earlier at 600 °C. The marked increase in the severity of corrosion at 700 °C is attributed to formation of the highly damaging compound NaVO{sub 3} that significantly enhances the oxygen activity, in the SM1 coated samples. The effect of surface roughness and dislocation density on corrosion behavior at 700 °C, however, is found to be similar to that at 600 °C. Ultrasonic shot peening, a novel technique of surface modification, is found to enhance the hot corrosion resistance in the salt mixture SM1 at 700 °C appreciably due to extensive grain refinement to nanoscale and formation of highly protective Cr{sub 2}O{sub 3} layer in the surface region.

36 MATERIALS SCIENCE↗

Nanoscale Chemical Imaging of Zinc Oxide Nanowire Corrosion

Nanoscale chemical images of individual bare and alumina-coated zinc oxide nanowires (NWs) were recorded using tip-enhanced second harmonic generation (SHG) spectroscopy before and after exposure to carbon dioxide and water vapor. The NWs were exposed for 0, 2, 4 and 6 days, and images were collected for the same bare nanowire after each two-day exposure period. Corrosion of the bare ZnO NW to zinc carbonate was evident from far-field and near-field SHG images and simultaneously recorded AFM data. The expected zinc carbonate corrosion product is SHG inactive. The AFM profile of the NW showed vertical and lateral expansion in different regions of the nanowire. The lower resolution far-field SHG signal decreased gradually and uniformly. The near-field SHG signal provided a profile of the evolving NW under investigation with a spatial resolution of ~100 nm which is in agreement with the AFM results. In contrast, alumina-coated ZnO NWs that were exposed in the same gas environment showed reduced, but still observable, degradation. The 3-nm thick alumina protective layer may have been insufficient to fully protect the NW, or the coating may have been incomplete. Thicker coatings preclude the tip-enhanced method. Nevertheless, the ability to monitor corrosion on a nanometer scale is a powerful tool for a fundamental understanding of surface chemical processes and should lead to the discovery of protective layers to prevent or delay degradation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Geometric Optimization of an Electrochemical Purification Cell to Prevent Corrosion in CSP Plants During Operation

When exposed to moisture or oxygen, molten chloride salts produce corrosive impurities which degrade containment alloys. This can significantly decrease the lifetime and increase costs of molten-salt-based systems. To overcome this barrier, we designed and modeled an electrochemical purification cell to remove the corrosive impurity MgOH+. Various reactor architectures, including continuous stirred tank reactors (CSTRs) and plug flow reactors (PFRs) were investigated. Steady-state thermoelectric properties were evaluated using analytical methods, allowing assessment of the effects of structure and design parameters such as flow rate, cell length, and cross-sectional area of molten salt. The results suggest that our design could most effectively increase reliability and decrease costs of molten-chloride-salt-based systems by protecting them during continuous operation using an annular plug flow reactor.

analytical modeling↗

Compatibility of Type 304H Stainless Steel in Static Molten FLiBe for Inertial Confinement Fusion Reactors: Role of Impurities and Redox Control

Molten fluoride salts, such as FLiBe (LiF-BeF2), are promising candidates for tritium breeding and heat transfer in fusion reactors, but corrosion of structural materials remains a major challenge. This study investigates the corrosion behavior of austenitic stainless steel 304H in purified and NiF2-containing FLiBe at 500°C and 600°C, focusing on the effects of impurities and redox control. Exposure to purified FLiBe resulted in the concurrent depletion of Cr, Mn, and Fe, with corrosion at 500 °C dominated by the combined oxide formation and elemental dissolution, while at 600°C elemental depletion was predominant. The addition of a controlled NiF2 impurity significantly accelerated corrosion at both temperatures, demonstrating the sensitivity of 304H to the salt redox state. Beryllium additions were effective in mitigating corrosion for both baseline and NiF2-containing FLiBe; minimal depletion of Cr, Mn, and Fe occurred with Be additions as low as 2.5 mg (147 wppm), and no NiBe intermetallics formed at 5 mg (294 wppm), indicating that small Be inventories can provide substantial protection without deleterious phase formation. Thermodynamic equilibrium and coupled thermodynamic-kinetic analyses at the salt-alloy interface suggested low corrosion rates in systems with limited hydrogen fluoride (HF) generation, highlighting the importance of salt redox control. Estimates for a Be addition rate were calculated for the HYLIFE-II fusion reactor that can mitigate corrosion-induced degradation, assuming complete conversion of tritium to tritium fluoride (TF). Overall, 304H shows reasonable compatibility with FLiBe under optimized redox conditions. These results provide quantitative guidance for material selection and salt management in fusion blanket and heat exchanger systems and motivate validation under flowing, nonisothermal, and irradiated conditions.

Pillai, Rishi [ORNL] (ORCID:0000000243688197)↗

Effect of Microadding Amine Surfactant on Erosion-Corrosion Wear of Structural Steel in NPP

Corrosion processes, specifically, erosion-corrosion, are one of the causes of damage occurring in NPP equipment during operation. Measures are taken to prevent erosion-corrosion wear of thermal-power equipment and pipelines. One such measure is the development and adoption of water chemistry regimes that are capable of forming a protective fi lm on a metal surface. Octadecylamine is one such reagent. The results of laboratory tests and industrial experiments studying the effect of octadecylamine on the development of erosion-corrosion wear of NPP equipment are presented. The octadecylamine-hydrazine water chemistry regime at octadecylamine concentration 0.5 mg/dm{sup 3} reduces the rate of erosion-corrosion wear by about 15-fold. The positive effect of micro-additions of octadecylamine is confirmed by direct erosion-corrosion studies performed at the Kola NPP.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Corrosion in Supercritical Carbon Dioxide: Materials, Environmental Purity, Surface Treatments, and Flow Issues (Project No. 10-872)

The supercritical CO 2 Brayton cycle is gaining importance for power conversion in the Generation IV fast reactor system because of its high conversion efficiencies. When used in conjunction with a sodium fast reactor, the supercritical CO 2 cycle offers additional safety advantages by eliminating potential sodium-water interactions that may occur in a steam cycle. In power conversion systems for Generation IV fast reactors, supercritical CO 2 temperatures could be in the range of 30°C to 650°C, depending on the specific component in the system. Materials corrosion primarily at high temperatures will be an important issue. Therefore, the corrosion performance limits for materials at various temperatures must be established. The proposed research will have four objectives centered on addressing corrosion issues in a high-temperature supercritical CO 2 environment: Task 1: Evaluation of corrosion performance of candidate alloys in high-purity supercritical CO 2 : The following alloys will be tested: Ferritic-martensitic Steels NF616 and HCM12A, austenitic alloys Incoloy 800H and 347 stainless steel, and two advanced concept alloys, AFA (alumina forming austenitic) steel and MA754. Supercritical CO 2 testing will be performed at 450°C, 550°C, and 650°C at a pressure of 20 MPa, in a test facility that is already in place at the proposing university. High purity CO 2 (99.9998%) will be used for these tests. Task 2: Investigation of the effects of CO, H 2 O, and O 2 impurities in supercritical CO 2 on corrosion: Impurities that will inevitably present in the CO 2 will play a critical role in dictating the extent of corrosion and corrosion mechanisms. These effects must be understood to identify the level of CO 2 chemistry control needed to maintain sufficient levels of purity to manage corrosion. The individual effects of important impurities CO, H 2 O, and O 2 will be investigated by adding them separately to high purity CO 2 . Task 3: Evaluation of surface treatments on the corrosion performance of alloys in supercritical CO 2 : Surface treatments can be very beneficial in improving corrosion resistance. Shot peening and yttrium and aluminum surface treatments will be investigated. Shot peening refines the surface grain sizes and promotes protective Cr-oxide layer formation. Both yttrium and aluminum form highly stable oxide layers (Y 2 O 3 and Al 2 O 3 ), which can get incorporated in the growing Fe-oxide layer to form an impervious complex oxide to enhance corrosion resistance. Task 4: Study of flow-assisted corrosion of select alloys in supercritical CO 2 under a selected set of test conditions: To study the effects of flow-assisted corrosion, tests will be conducted in a supercritical CO 2 flow loop. An existing facility used for supercritical water flow studies at the proposing university will be modified for use in this task. The system is capable of flow velocities up to 10 m/s and can operate at temperatures and pressures of up to 650°C and 20 MPa, respectively. All above tasks will be performed in conjunction with detailed materials characterization and analysis using scanning electron microscopy/energy dispersive spectroscopy (SEM-EDS), x-ray diffraction (XRD), Auger electron spectroscopy (AES) techniques, and weight change measurements. Inlet and outlet gas compositions will be monitored using gas chromatography-mass spectrometry (GCMS).

36 MATERIALS SCIENCE↗

Examining Graphite Degradation in Molten Salt Environments: A Chemical, Physical, and Material Analysis

Molten-salt reactors (MSRs) are Generation IV nuclear reactors that use liquid salt as a coolant and/or fuel. In several MSR designs, graphite serves as a moderator and/or reflector. However, due to limited experimental data and operational experience, our understanding of graphite behavior in molten salt environments remains incomplete. This report aims to identify the degradation mechanisms of nuclear graphite in MSRs, detail the mechanisms of each factor, and provide an initial assessment of their impact on the structural integrity of graphite components. This assessment is based on an extensive literature review and insights from subject matter experts. Furthermore, given the limited data, a modeling strategy using existing Grizzly software is proposed for a more thorough analysis where appropriate. Additionally, it presents mitigation strategies where applicable. The report covers physical degradation mechanisms such as infiltration, erosion, and abrasion, as well as chemical degradation mechanisms including fluorination, intercalation, corrosion, and oxidation. Molten salt can infiltrate the porous structure of graphite, leading to several detrimental effects. Entrapment of fissile products within the graphite pores can cause radiation damage and could pose challenges in the handling and disposal of contaminated components. The differential thermal expansion between the infiltrated salt and graphite, along with internal stress from pressurized molten salt and volumetric heating, can compromise the structural integrity of graphite. To mitigate these effects, employing ultra-fine graphite grades and applying sealants and coatings are effective strategies. A computational model based on coupled solid mechanics and heat transfer phenomena could be used to predict the internal stresses using Grizzly software. In pebble-bed MSRs, graphite fuel pebbles can cause abrasion against reactor components due to friction and wear. The severity of wear is influenced by various factors such as temperature, environment, and the presence of lubricants. Tribological studies reveal that higher temperatures and molten salt environments, such as FLiBe, significantly reduce wear rates compared to dry conditions. Additionally, the chemical composition of the salt can further optimize graphite's tribological performance. Long-term wear effects can be modeled by incorporating surface defects into the geometry and predict stresses under thermal and radiation effects using Grizzly software. Chemical degradation of graphite in a molten salt environment can occur through fluorination and intercalation. Fluorination can occur via replacement of hydrogen or oxygen atoms, or at the active sites, but does not cause structural degradation. Intercalation, on the other hand, can lead to exfoliation, where layers of graphite separate and peel away, damaging the graphite. Protective coatings can enhance graphite's resistance to intercalation. Graphite generally exhibits good chemical stability in molten salt environments, though it can corrode under specific conditions, particularly in the presence of impurities or oxidants. Studies have shown that protective coatings, such as plasma-sprayed partially stabilized zirconia (PSZ), can effectively prevent such degradation. Corrosion behavior varies significantly with different graphite grades and coating applications, underscoring the need for detailed studies on uncoated and coated graphite to understand and mitigate corrosion mechanisms in MSRs. Research indicates that the presence of oxidants and impurities can accelerate graphite degradation in molten salts, making it essential to explore acceptable impurity limits. Oxidation is another critical degradation mechanism, leading to weight loss and structural damage due to the formation of CO and CO 2 from the reaction of carbon atoms with oxygen. This process creates new porosity and compromises graphite's integrity. While extensive research on graphite oxidation has been conducted for gas-cooled reactors, studies specific to MSRs are limited. Findings from the coal industry suggest that molten alkali metal salts can significantly accelerate graphite oxidation, a hypothesis worth exploring for fluoride salts in MSRs. Understanding oxidation behavior in MSRs is vital for developing protective measures. The analysis of post-irradiated graphite from the MSRE experiment demonstrated exceptional chemical compatibility with molten fluoride salt, suggesting that the extent of chemical attack on graphite largely depends on the salt's infiltration capability. Therefore, the use of ultra-fine grade graphite could help mitigate chemical degradation effects. Existing oxidation modeling capabilities in Grizzly, which use reaction-diffusion equations to model graphite-air interactions, could be adapted to simulate the chemical degradation effects of graphite in molten salt environments.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Growth of Cr-Nitrides on commercial Ni–Cr and Fe–Cr base alloys to protect PEMFC bipolar plates

Nitridation of Cr-bearing alloys can yield low interfacial contact resistance (ICR), electrically conductive and corrosion-resistant CrN or Cr2N base surfaces of interest for a range of electrochemical devices, including fuel cells, batteries, and sensors. This paper presents results of exploratory studies of the nitridation of commercially available, high Cr (30–35 wt%) Ni–Cr alloys and a ferritic high Cr (29 wt%) stainless steel for proton exchange membrane fuel cell (PEMFC) bipolar plates. A high degree of corrosion resistance in sulfuric acid solutions designed to simulate bipolar plate conditions and low ICR values were achieved. Oxygen impurities in the nitriding environment were observed to play a significant role in the nitrided surface structures that formed, with detrimental effects for the Ni–Cr base alloys, but beneficial effects for the stainless steel alloy. Positive results from single-cell fuel cell testing are also presented.

30 DIRECT ENERGY CONVERSION↗

Intercalated hybrid graphite fiber composite

The invention is directed to a highly conductive lightweight hybrid material and methods of producing the same. The hybrid composite is obtained by weaving strands of a high strength carbon or graphite fiber into a fabric-like structure, depositing a layer of carbon onto the structure, heat treating the structure to graphitize the carbon layer, and intercalating the graphitic carbon layer structure. A laminate composite material useful for protection against lightning strikes comprises at least one layer of the hybrid material over at least one layer of high strength carbon or graphite fibers. The composite material of the present invention is compatible with matrix compounds, has a coefficient of thermal expansion which is the same as underlying fiber layers, and is resistant to galvanic corrosion in addition to being highly conductive. These materials are useful in the aerospace industry, in particular as lightning strike protection for airplanes.

Gaier, James R.↗

Effect of Sulfide Concentration on the Corrosion and Cavitation Erosion Behavior of a Manganese-Aluminum Bronze in 3.5% NaCl Solution

The effect of sulfide concentration on the corrosion and cavitation erosion behavior of a cast manganese-aluminum bronze (MAB) alloy in 3.5% NaCl solution was investigated. The electrochemical results showed that when the sulfide concentration exceeded 50 ppm, hydrogen evolution reaction dominated the cathodic process because of the very negative corrosion potential of MAB, and the formation of a copper sulfide film on MAB was a diffusion-controlled process. The mass loss rate of MAB after longer-term immersion was ordered by the sulfide concentration as: 20/50 ppm > 100 ppm > zero > 200 ppm. In the 200 ppm sulfide solution, the mass loss rate of MAB was the lowest, because of the formation of a thin and homogeneous copper sulfide film. In the other sulfide solutions, the formation of a less-protective film with both oxides and sulfides resulted in higher mass loss rate of MAB. Moreover, selective phase corrosion occurred at the β and κ phases in solutions with sulfide addition less than 100 ppm. For all solutions, it was the mechanical attack that dominated cavitation erosion degradation. The cavitation erosion–corrosion synergy was lower in high sulfide solutions, because the corrosion products on MAB could reduce the mechanical impact under cavitation erosion.

36 MATERIALS SCIENCE↗

Prediction of External Corrosion for Steel Cylinders--2007 Report

Depleted uranium hexafluoride (DUF{sub 6}) is stored in over 62,000 containment cylinders at the Paducah Gaseous Diffusion Plant (PGDP) in Paducah, Kentucky, and at the Portsmouth Gaseous Diffusion Plant (PORTS) in Portsmouth, Ohio. Over 4,800 of the cylinders at Portsmouth were recently moved there from the East Tennessee Technology Park (ETTP) in Oak Ridge, Tennessee. The cylinders range in age up to 56 years and come in various models, but most are 48-inch diameter 'thin-wall'(312.5 mil) and 'thick-wall' (625 mil) cylinders and 30-inch diameter '30A' (including '30B') cylinders with 1/2-inch (500 mil) walls. Most of the cylinders are carbon steel, and they are subject to corrosion. The United States Department of Energy (DOE) manages the cylinders to maintain them and the DUF{sub 6} they contain. Cylinder management requirements are specified in the System Requirements Document (LMES 1997a), and the activities to fulfill them are specified in the System Engineering Management Plan (LMES 1997b). This report documents activities that address DUF{sub 6} cylinder management requirements involving measuring and forecasting cylinder wall thicknesses. As part of these activities, ultrasonic thickness (UT) measurements are made on samples of cylinders. For each sampled cylinder, multiple measurements are made in an attempt to find, approximately, the minimum wall thickness. Some cylinders have a skirt, which is an extension of the cylinder wall to protect the head (end) and valve. The head/skirt interface crevice is thought to be particularly vulnerable to corrosion, and for some skirted cylinders, in addition to the main body UT measurements, a separate suite of measurements is also made at the head/skirt interface. The main-body and head/skirt minimum thickness data are used to fit models relating minimum thickness to cylinder age, nominal thicknesses, and cylinder functional groups defined in terms of plant site, storage yard, top or bottom row storage positions, etc. These models are then used to compute projections of numbers of cylinders expected to fail various minimum wall thickness criteria. The minimum wall thickness criteria are as follows. For thin-wall cylinders: 0 (breach), 62.5, and 250 mils. For thick-wall cylinders: 0, 62.5, and 500 mils. For 30A cylinders: 0, 62.5, and 100 mils. Each of these criteria triplets are based respectively on (1) loss of DUF{sub 6} (breaching), (2) safe handling and stacking operations, and (3) ANSI N14.1 standards for off-site transport and contents transfer. This report complements and extends previous editions of the cylinder corrosion report by Lyon (1995, 1996, 1997, 1998, 2000), by Schmoyer and Lyon (2001, 2002, 2003), and by Schmoyer (2004). These reports are based on UT data collected in FY03 and before. In this report UT data collected after FY03 but before FY07 is combined with the earlier data, and all of the UT data is inventoried chronologically and by the various functional groups. The UT data is then used to fit models of maximum pit depth and minimum wall thickness, statistical outliers are investigated, and the fitted models are used to extrapolate minimum thickness estimates into the future and in turn to compute projections of numbers of cylinders expected to fail various thickness criteria. A model evaluation is performed comparing UT measurements made after FY05 with model-fitted projections based only on data collected in FY05 and before. As in previous reports, the projections depend on the treatment of outliers.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Wear and Corrosion Behavior of Graphene-Nanoplate-Reinforced Copper Matrix Composites Prepared Through Electrostatic Self-Assembly

Synthesis of graphene nanoplates (GNPs)/copper (Cu) composites is one of the key challenges in the uniform dispersion of GNPs in the Cu matrix because of their density difference. In this work, GNPs/Cu composites are synthesized through electrostatic self-assembly and spark plasma sintering. The GNPs are uniformly dispersed in the Cu matrix. The graphene protective films are formed in the composites to protect the Cu matrix. The antifriction performance of the GNPs/Cu composites is investigated using a ball-on-disk apparatus. The corrosion resistance of the GNPs/Cu composites is estimated using potentiodynamic polarization curves. Wear and corrosion mechanisms are analyzed through scanning electron microscopy with energy-dispersive spectroscopy. The antifriction performance and corrosion resistance of the composites can be significantly improved by adding GNPs.

36 MATERIALS SCIENCE↗

Fire extinguishment and inhibition in spacecraft environments

It was concluded that it is essential that NASA develop a comprehensive approach to fire extinguishment and inerting in spacecraft environments. Electronic equipment might be easily protected through use of an onboard inert gas generating system. The use of Halon 1301 presents serious technological challenges for agent cleanup and removal of the toxic and corrosive products of combustion. Nitrogen pressurization, while effective, probably presents a serious weight penality. The use of liquid water sprays appears to be the most effective approach to general purpose spacecraft fire protection.

Deris, John↗

Neutron irradiation and high temperature effects on amorphous Fe-based nano-coatings on steel – A macroscopic assessment

Here, this study revealed that loss of ductility in an amorphous Fe-alloy coating on a steel substrate composite structure was essentially prevented from occurring, following radiation with modest neutron doses of ~2 x 10 18 n/cm 2 . At the higher neutron dose of ~2 x 10 19 , macroscopic stress-strain analysis showed that the amorphous Fe-alloy nanostructured coating, while still amorphous, experienced radiation-induced embrittlement, no longer offering protection against ductility loss in the coating-substrate composite structure. Neutron irradiation in a corrosive environment revealed exemplary oxidation/corrosion resistance of the amorphous Fe-alloy coating, which is attributed to the formation of the Fe 2 B phase in the coating. To establish the impact of elevated temperatures on the amorphous-to-crystalline transition in the amorphous Fe-alloy, electron microscopy was carried out which confirmed the radiation-induced suppression of crystallization in the amorphous Fe-alloy nanostructured coating.

36 MATERIALS SCIENCE↗

Application of Field Protective Coatings over Pipeline Girth Welds

This document provides guidance for the application of two types of field protective coating on a pipeline during construction, after completion of girth weld, to mitigate external corrosion. Steel alloy B9 is applied using electric arc welding and aluminum alloy 5356 is applied using thermal spray.

03 NATURAL GAS↗

Advanced Rankine and Brayton cycle power systems: Materials needs and opportunities

Conceptual advanced potassium Rankine and closed Brayton power conversion cycles offer the potential for improved efficiency over steam systems through higher operating temperatures. However, for utility service of at least 100,000 hours, materials technology advances will be needed for such high temperature systems. Improved alloys and surface protection must be developed and demonstrated to resist coal combustion gases as well as potassium corrosion or helium surface degradation at high temperatures. Extensions in fabrication technology are necessary to produce large components of high temperature alloys. Long time property data must be obtained under environments of interest to assure high component reliability.

Grisaffe, S. J.↗

Advanced Rankine and Brayton cycle power systems - Materials needs and opportunities

Conceptual advanced potassium Rankine and closed Brayton power conversion cycles offer the potential for improved efficiency over steam systems through higher operating temperatures. However, for utility service of at least 100,000 hours, materials technology advances will be needed for such high temperature systems. Improved alloys and surface protection must be developed and demonstrated to resist coal combustion gases as well as potassium corrosion or helium surface degradation at high temperatures. Extensions in fabrication technology are necessary to produce large components of high temperature alloys. Long-time property data must be obtained under environments of interest to assure high component reliability.

Grisaffe, S. J.↗

The effect of NaCl/g/ on the Na2SO4-induced hot corrosion of NiAl

Studies have been performed to examine the effect of NaCl vapor on the Na2SO4-induced hot corrosion of the alumina former NiAl. In the incubation period associated with such hot corrosion, NaCl(g) has been shown to be effective in removing aluminum from below the protective alumina scale and redepositing it as Al2O3 whiskers on the surface of the Na2SO4-coated sample. Similar effects seen in simple oxidation are associated with isothermal rupturing of the protective alumina scale.

Smeggil, J. G.↗