Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “alloy solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 865 records · Page 48

Role of spall in microstructure evolution during laser-shock-driven rapid undercooling and resolidification

We previously reported [Colvin et al., J. Appl. Phys. 101, 084906 (2007)] on the microstructure morphology of pure Bi metal subjected to rapid laser-shock-driven melting and subsequent resolidification upon release of pressure, where the estimated effective undercooling rates were of the order of 10{sup 9}-10{sup 10} K/s. More recently, we repeated these experiments, but with a Bi/Zn alloy (Zn atomic fraction of 2%-4%) instead of elemental Bi and with a change in target design to suppress spall in the Bi/Zn samples. We observed a similar microstructure morphology in the two sets of experiments, with initially columnar grains recrystallizing to larger equiaxed grains. The Bi samples, however, exhibited micron-scale dendrites on the spall surfaces, whereas there were no dendritic structures anywhere in the nonspalled Bi/Zn, even down to the nanometer scale as observed by transmission electron microscopy. We present the simulations and the interferometry data that show that the samples in the two sets of experiments followed nearly identical hydrodynamic and thermodynamic paths apart from the presence of (probably partially liquid) spall in pure Bi. Simulations also show that the spall occurs right at the moving phase front and, hence, the spall itself cuts off the principal direction for latent heat dissipation across the phase boundary. We suggest that it is the liquid spall itself that creates the conditions for dendrite formation.

36 MATERIALS SCIENCE↗

Study of formation mechanism of incipient melting in thixo-cast Al–Si–Cu–Mg alloys

Mechanical properties of thixo-cast Al–Si–Cu–Mg alloys can be enhanced by T61 heat treatment. Copper and magnesium atoms in aluminum matrix can form homogeneously distributed precipitations after solution and aging treatment which harden the alloys. However, microsegregation of these alloying elements could form numerous tiny multi-compound phases during solidification. These phases could cause incipient melting defects in subsequent heat treatment process and degrade the macro-mechanical properties of productions. This study is to present heterogeneous distribution of Cu, Si, and Mg elements and formation of incipient melting defects (pores). In this study, incipient melting pores that occurred during solution treatment at various temperatures, even lower than common melting points of various intermetallic phases, were identified, in terms of a method of investigating the same surface area in the samples before and after solution treatment in a vacuum environment. The results also show that the incipient melting mostly originates at the clusters with fine intermetallic particles while also some at the edge of block-like Al{sub 2}Cu. The fine particles were determined being Al{sub 2}Cu, Al{sub 5}Cu{sub 2}Mg{sub 8}Si{sub 6} and Al{sub 8}Mg{sub 3}FeSi{sub 2}. Tendency of the incipient melting decreases with decreases of the width of the clusters. The formation mechanism of incipient melting pores in solution treatment process was discussed using both the Fick law and the LSW theory. Finally, a criterion of solution treatment to avoid incipient melting pores for the thixo-cast alloys is proposed. - Highlights: • In-situ comparison technique was used to analysis the change of eutectic phases. • The ralationship between eutectic phase size and incipient melting was studied. • Teat treatment criterion for higher incipient melting resistance was proposed.

36 MATERIALS SCIENCE↗

Hot-Tearing Assessment of Multicomponent Nongrain-Refined Al-Cu Alloys for Permanent Mold Castings Based on Load Measurements in a Constrained Mold

The hot-tearing resistance of multicomponent Al-Cu alloys during permanent mold casting was investigated using a constrained permanent mold in which the load and temperature were measured. The nominal Cu composition was varied from 5 to 8 wt pct. Casting experiments were conducted without adding any grain-refining inoculants. The following variables, which were obtained from the measured load data during casting, were considered to assess the hot-tearing resistance of the Al-Cu multicomponent alloys: “V”-like signature in the load rate variation, load at solidus point, and load rate average over the freezing range. In addition, a hot-tearing criterion based on the variation of the fraction of solid in the late stages of solidification was used. It was found that all criteria considered can accurately predict the alloys with the lowest and highest hot-tear resistance, respectively. It was found that the rate of measured load during casting could be used to indicate substantial hot tearing. However, the load rate variation could not be used to detect when small hot tears were present. Among all the criteria considered, the load at the solidus point shows an excellent agreement with experimentally observed hot-tearing resistance for all but one alloy. The poorly resistant hot-tearing alloys exhibited mainly coarse columnar grains while the most hot-tearing resistant alloys exhibited a much more refined grain microstructure. This is the first study in which good hot-tear resistance is demonstrated for multicomponent Al-Cu alloys with nominal Cu content greater than 7 wt pct.

36 MATERIALS SCIENCE↗

Structural evolution and atomic dynamics in Ni–Nb metallic glasses: A molecular dynamics study

In this work, the composition and temperature dependence of static and dynamic structures in Ni x Nb 1– x ( x = 50–70 at. %) were systematically studied using molecular dynamics with a new-released semi-empirical embedded atom method potential by Mendelev. The calculated pair correlation functions and the structure factor match well with the experimental data, demonstrating the reliability of the potential within relatively wide composition and temperature ranges. The local atomic structures were then characterized by bond angle distributions and Voronoi tessellation methods, demonstrating that the icosahedral $\langle$0,0,12,0$\rangle$ is only a small fraction in the liquid state but increases significantly during cooling and becomes dominant at 300 K. The most abundant clusters are identified as $\langle$0,0,12,0$\rangle$ and distorted icosahedron$\langle$0,2,8,2$\rangle$. The large fraction of these two clusters hints that the relatively good glass forming ability is near the eutectic point. Unlike Cu–Zr alloys, both the self-diffusion coefficient and shear viscosity are insensitive to compositions upon cooling in Ni–Nb alloys. The breakdown of the Stokes-Einstein relation happens at around 1.6 T g ( T g : glass transition temperature). In the amorphous state, the solid and liquid-like atoms can be distinguished based on the Debye-Waller factor $\langle$ u 2 $\rangle$. The insensitivity of the dynamic properties of Ni–Nb alloys to compositions may result from the relatively simple solidification process in the phase diagram, in which only one eutectic point exists in the studied composition range.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrical conductivity in directionally solidified lead-9 and -20 wt pct copper alloys

Composites consisting of aligned copper dendrites in a lead matrix have been produced by directional solidification processing for potential application as grids in lead-acid batteries. To promote a uniform composite of aligned copper dendrites in a protective lead matrix, two alloy compositions, Pb-9 and -20 wt pct Cu, have been directionally solidified through a temperature gradient of 4.5 K/mm at constant growth velocities which ranged from 1 to 100 micron/s. With slow growth rates (below about 10 microns/s), the copper dendrites were generally columnar and continuous along the sample length; at higher velocities (above 60 microns/s), they assumed an intricate and equiaxed morphology. In accordance with copper content and growth rate, the electrical conductivity of the directionally solidified composites was found to be as much as a 2.5 times that of pure lead. The results are compared with that predicted by a model based on a geometrical dendrite.

Kim, Shinwoo↗

Design of novel refractory equiatomic multi-principal elemental alloys based on Mo-Nb-Ti system for Gen IV reactor applications

Excellent irradiation damage resistance demonstrated by multi-principal elemental alloys (MPEAs) has sparked significant interest among researchers, prompting exploration into their vast compositional space, to validate their suitability for nuclear applications. A combined approach of thermodynamic and empirical parameters calculations alongside CALPHAD (CALculation of PHAse Diagrams) for phase formation predictions enable high-throughput material selection for sophisticated applications like nuclear, overcoming laborious and time-consuming experiments. Key thermodynamic and empirical parameters for eight novel equiatomic MPEAs, based on seven low thermal neutron cross section refractory elements, for predicting phase formation were calculated, and equilibrium and non-equilibrium simulations in CALPHAD were employed to comprehensively model the systems. Pseudo binary phase diagram simulations showed that Zr, V or equiatomic CrV additions to the base MoNbTi alloy (MoNbTi-Zr, MoNbTi-V and MoNbTi-CrV alloys) favor the formation of isomorphous body-centered cubic (BCC) phase at high temperatures, while Cr, Al, equiatomic ZrV, or equiatomic CrAl additions (MoNbTi-Cr, MoNbTi-Al, MoNbTi-ZrV or MoNbTi-CrAl alloys) limit the solubility of them. Equilibrium CALPHAD simulations at 750 oC were consistent with XRD results on MoNbTi, MoNbTiZr and MoNbTiCr alloys, and partially for others. Notably, elemental segregation observed in the backscattered electron (BSE) scanning electron microscopy (SEM) images of the alloys was accurately simulated through non-equilibrium Scheil solidification calculations in CALPHAD, further verified by experiments. The precipitation of TiCr2 Laves phase in Cr containing MoNbTiCr and MoNbTiCrAl was accurately predicted while discrepancies were noted in MoNbTiCrV. The equilibrium simulations also provided insights into phase compositions at specific temperatures offering a pathway for tailoring the desired microstructure and properties of these systems. Empirical parameters calculations successfully predicted random solid solution in the base MoNbTi alloy, and with an exception in MoNbTiV and MoNbTiAl, predicted intermetallic precipitation in the rest, especially, Laves phase precipitation in Cr containing alloys.

36 - MATERIALS SCIENCE↗

Analyzing the microstructural evolution and hardening response of an Al-Si-Mg casting alloy with Cr addition

Highlights: • The formation of β-Al{sub 5}FeSi intermetallics was suppressed since impurity Fe has been consumed by Al{sub 13}Cr{sub 4}Si{sub 4} intermetallics; • A large number of Al{sub 13}Cr{sub 4}Si{sub 4} dispersoids were observed in Al dendrites in the as-quenched and aged alloy; • The precipitation of Cr-bearing dispersoids harden the as-quenched alloy by over 10HV; • The current thermodynamic database underestimate the solubility of Fe in Al{sub 13}Cr{sub 4}Si{sub 4} intermetallics during solidification simulation. - Abstract: Chromium is added to Al-Si based casting alloys for the mitigation of die soldering. In the present work, EBSD, EDS and TEM characterizations are combined with thermodynamic simulations to study the microstructural evolution and hardening response of an Al-Si-Mg-Cr casting alloy during heat treatments. It is shown that the Fe-containing intermetallic compounds formed in the inter-dendritic region were acicular π-Al{sub 8}(Fe, Cr)Mg{sub 3}Si{sub 6} phase and polyhedral Al-(Cr, Fe)-Si phase which is structurally similar to face-centered cubic Al{sub 13}Cr{sub 4}Si{sub 4}. The polyhedral Al-(Cr, Fe)-Si intermetallics that crystallized prior to β-Al{sub 5}FeSi consumed impurity Fe, suppressing the formation of β phase during gravity die casting process. Also, Cr-addition enables the precipitation of nano-scale Cr-bearing dispersoids in Al dendrite during solution treatment at 813 K. Hardness increment of over 10 HV can be induced by the Cr-bearing dispersoids for as-quenched alloy. Though the dispersoids have a moderate hardening effect on the as-quenched alloy, they may impair the ageing hardening response by acting as heterogeneous nucleation sites for coarse Mg-Si rods and Si particles when quenching into water at 338 K.

36 MATERIALS SCIENCE↗

Thermodynamics and Kinetics of Refractory Multi-principal Element Alloys: An Experimental and Modeling Comparison

Here, the search for structural alloys capable of ultrahigh temperature performance has led to the exploration of refractory multi-principal element alloys (RMPEAs). In this work, experimental results for solidification segregation and homogenization of two RMPEAs, NbTaTiW and MoNbTaTi, are compared to simulations using the Scheil and DICTRA modules in Thermo-Calc®. Scheil calculations accurately predict the observed solidification segregation, while DICTRA predicts general trends and can provide a minimum time to achieve homogenization at a given temperature.

36 MATERIALS SCIENCE↗

Investigation of structural and magnetic properties of rapidly-solidified iron-silicon alloys at ambient and elevated temperatures

In this work, we investigated the ambient temperature structural properties (~300 K) and the ambient and high temperature (up to 900 K) direct current (DC) magnetic properties of melt-spun Fe-x wt.% Si (x = 3, 5, & 8) alloys. The wheel surface speeds selected for the study were 30 m/s and 40 m/s. The thickness, width, lattice parameter, saturation magnetization (MS), and intrinsic coercivity (HCI) of the melt spun ribbons are presented and compared with data in the literature. The ribbons produced at the lower wheel surface speed (30 m/s) were continuous having relatively uniform edges compared to the ribbons produced at the higher wheel surface speed. The thickness and the width of the melt-spun ribbons ranged between ~15-60 μm and 500-800 μm, respectively. The x-ray diffraction spectra of the melt-spun ribbons indicated the presence of disordered α-phase, irrespective of the composition, and the wheel-surface speed. The lattice parameter decreased gradually as a function of increasing silicon content from ~0.2862 nm (Fe-3 wt.% Si) to ~0.2847 nm (Fe-8 wt.% Si). Wheel surface speed was not shown to have a significant effect on the magnetization, but primarily impacted the ribbon structure. A decreasing trend in the saturation magnetization was observed as a function of increased silicon content. The intrinsic coercivity of the melt-spun alloys ranged between ~50 to 200 A/m. Elevated temperature evaluation of the magnetization in the case of Fe-3 & 5 wt.% Si alloy ribbons was distinctly different from the Fe-8 wt.% Si alloy ribbons. The curves of the as-prepared Fe-3 wt.% Si and Fe-5 wt.% Si alloy ribbons were irreversible while that of Fe-8 wt.% Si was reversible. The MS for any of the combinations of wheel surface speed and composition decreased monotonically with the increase in temperature (from 300 – 900 K). The percentage decrease in MS from 300 K to 900 K for the Fe-3 wt.% Si and Fe-5 wt.% Si alloys was ~19-22 %, while the percentage decrease in the same temperature range for Fe-8 wt.% Si alloy was ~26-30 %. It appears that Fe-3 wt.% Si and Fe-5 wt.% Si alloys ribbons are primarily comprised of the α phase (disordered phase) with any minor constituents being beyond the detection limits of the studies performed, while the Fe-8 wt.% Si alloy ribbons are comprised of disordered and regions of short-range ordering.

Elevated Temperature↗

Microstructural heterogeneities in additively manufactured refractory alloy C103 and their implications for room and elevated temperature mechanical behavior

Considering the vast component design space enabled by fusion-based additive manufacturing (F-BAM) processes, e.g., directed energy deposition (DED), the scale-up manufacturing of Nb-alloys with F-BAM is advantageous for structural applications. However, varying thermokinetic parameters-induced microstructural heterogeneities are prevalent within the F-BAM processed alloys. Such microstructural heterogeneities can have significant implications for the room and elevated temperature mechanical behavior. While a few studies investigating F-BAM processed alloy C103 are available, none of these studies investigate the microstructural heterogeneities – including those associated with solidification growth modes and second phase particles – and the effect thereof on the mechanical behavior. To this end, we investigate the microstructurally heterogeneous regions with varying solidification growth morphologies, segregation behavior, and second phase particle attributes within the laser-DED processed alloy C103. The implications of such heterogeneous regions for room- and elevated-temperature tensile behavior and damage mechanisms are revealed. Particularly, the interface between the cellular and planar region is identified as susceptible to deformation localization. The implications of hot isostatic pressing (HIP) for the consolidation behavior, microstructural evolution, and resulting mechanical behavior are also discussed. Although the recrystallization and grain growth led to a reduced yield strength in the HIPed condition, the homogenization of microstructure alleviated the deformation localization sites, such as the planar/cellular interface within the melt pool. The homogenized microstructure alongside the enhanced consolidation upon HIP led to an enhanced elongation to failure. Findings establish microstructural design considerations in F-BAM processed Nb alloys and also facilitate design of post-processing heat treatments for achieving improved mechanical properties.

36 MATERIALS SCIENCE↗

A compact and flexible induction furnace for in situ X-ray microradiograhy and computed microtomography at Elettra: design, characterization and first tests

A compact and versatile induction furnace for in situ high-resolution synchrotron and laboratory hard X-ray microradiography and computed microtomography is described. The furnace can operate from 773 to 1723 K. Its programmable controller enables the user to specify multiple heating and cooling ramp rates as well as variable dwell times at fixed temperatures allowing precise control of heating and cooling rates to within 5 K. The instrument can work under a controlled atmosphere. Thanks to the circular geometry of the induction coils, the heat is homogeneously distributed in the internal volume of the graphite cell ( ca . 150 mm 3 ) where the sample holder is located. The thermal gradient within the furnace is less than 5 K over a height of ca . 5 mm. This new furnace design is well suited to the study of melting and solidification processes in geomaterials, ceramics and several metallic alloys, allowing fast heating (tested up to 6.5 K s -1 ) and quenching (up to 21 K s -1 ) in order to freeze the sample microstructure and chemistry under high-temperature conditions. The sample can be held at high temperatures for several hours, which is essential to follow phenomena with relatively slow dynamics, such as crystallization processes in geomaterials. The utility of the furnace is demonstrated through a few examples of experimental applications performed at the Elettra synchrotron laboratory (Trieste, Italy).

Kudrna Prašek, Marko↗

Fundamental Aspects of Selective Melting Additive Manufacturing Processes

Certain details of the additive manufacturing process known as selective laser melting (SLM) affect the performance of the final metal part. To unleash the full potential of SLM it is crucial that the process engineer in the field receives guidance about how to select values for a multitude of process variables employed in the building process. These include, for example, the type of powder (e.g., size distribution, shape, type of alloy), orientation of the build axis, the beam scan rate, the beam power density, the scan pattern and scan rate. The science-based selection of these settings con- stitutes an intrinsically challenging multi-physics problem involving heating and melting a metal alloy, reactive, dynamic wetting followed by re-solidification. In addition, inherent to the process is its considerable variability that stems from the powder packing. Each time a limited number of powder particles are placed, the stacking is intrinsically different from the previous, possessing a different geometry, and having a different set of contact areas with the surrounding particles. As a result, even if all other process parameters (scan rate, etc) are exactly the same, the shape and contact geometry and area of the final melt pool will be unique to that particular configuration. This report identifies the most important issues facing SLM, discusses the fundamental physics associated with it and points out how modeling can support the additive manufacturing efforts.

36 MATERIALS SCIENCE↗

High-gradient continuous-casting furnace

High gradient allows rapid growth rates in directionally-solidified eutectic alloys. Furnace design permits cost reductions in directional solidification process through its increased solidification rates, which reduces melt/mold interaction. It produces structural engineering materials for any application requiring properties directionally-solidified eutectic materials.

Scheuermann, C. M.↗

Metal shell technology

Metallic shells are fabricated for a size range from several millimeters down to less than 500 microns in diameter. The technology, developed at JPL, is based on the hollow-jet instability for the large-shell formation, and in addition, on the Bernoulli's force for the microbubble generation. Various materials were processed into hollow spheres, such as AL1100, tin, lead, and a metallic glass-forming alloy, AuPbSb. They exhibited a range of contrasting solidification behaviors and surface characteristics. Some of their potential applications will be explored in this paper.

Lee, M. C.↗

Observations of a monotectic solidification interface morphology

For detailed studies of the region around a solidification interface on a microscopic scale, a very thin (essentially two-dimensional) test cell may be translated across two temperature-controlled heating/cooling blocks and viewed with a microscope. Such a device is sometimes referred to as a temperature gradient microscope stage (TGS). Of particular interest in this study is the behavior of a monotectic type solution during solidification. Succinonitrile based model systems for metallic monotectic alloys, when solidified on a TGS, form an unusual 'worm-like' micromorphology. These interfaces are observable in situ under high optical magnification during growth.

Kaukler, W. F.↗

Microstructures of niobium-germanium alloys processed in inert gas in the 100 meter drop tube

The 100 meter drop tube at NASA's Marshall Space Flight Center has been used for a series of experiments with niobium-germanium alloys. These experiments were conducted with electromagnetic levitation melting in a 200 torr helium environment. Liquid alloys experienced large degrees of undercooling prior to solidification in the drop tube. Several interesting metastable structures were observed. However, the recalescence event prevented extended solid solubility of germanium in the A-15 beta phase. Liquids of eutectic composition were found to undercool in the presence of solid alpha and solid Nb5Ge3.

Bayuzick, R. J.↗

Arc Casting Intermetallic Alloy (Materials Preparation Center)

Arc casting of intermetallic (La-Ni-Sn) AB5 alloy used for metal hydride hydrogen storage. Upon solidification the Sn is partially rejected and increases in concentration in the remaining liquid. Upon completing solidification there is a great deal of internal stress in the ingot. As the ingot cools further the stress is relieved. This material was cast at the Ames Laboratorys Materials Preparation Center http://www.mpc.ameslab.gov

36 MATERIALS SCIENCE↗