Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INTERMETALLICS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 865 records · Page 48

Improving Joint Formation and Tensile Properties of Dissimilar Friction Stir Welding of Aluminum and Magnesium Alloys by Solving the Pin Adhesion Problem

Friction stir welding (FSW), as a solid-state welding technology invented by TWI in 1991, has potential to join dissimilar Al/Mg alloys. In this study, the pin adhesion phenomenon affecting joint quality during FSW of 6061-T6 aluminum and AZ31B magnesium alloys was investigated. The adhesion phenomenon induced by higher heat input easily transformed the tapered-and-screwed pin into a tapered pin, which greatly reduced the tool’s ability to drive the plasticized materials and further deteriorated joint formation. Under the condition without the pin adhesion, the complex intercalated interlayer at the bottom of stir zone was beneficial to mechanical interlocking of Al/Mg alloys, improving tensile properties. However, the formation of intermetallic compounds was still the main reason of the joint fracture, significantly deteriorating tensile properties. Under the welding speed of 60 mm/min without the pin adhesion phenomenon, the maximum tensile strength of 107 MPa and elongation of 1.2% were achieved.

36 MATERIALS SCIENCE↗

In Situ SEM Observations of Fracture Behavior of Laser Welded–Brazed Al/Steel Dissimilar Joint

Laser welding–brazing of 6061-T6 aluminum alloy to DP590 dual-phase steel with Al-Si12 flux-cored filler wire was performed. The microstructure at the brazing interface was characterized. Fracture behavior was observed and analyzed by in situ scanning electron microscope. The microstructure of the brazing interface showed that inhomogeneous intermetallic compounds formed along the thickness direction, which had a great influence on the crack initiation and propagation. In the top region, the reaction layer at the interface consisted of scattered needle-like Fe(Al,Si){sub 3} and serration-shaped Fe{sub 1.8}Al{sub 7.2}Si. In the middle region, the compound at the interface was only serration-shaped Fe{sub 1.8}Al{sub 7.2}Si. In the bottom region, the interface was composed of lamellar-shaped Fe{sub 1.8}Al{sub 7.2}Si. The cracks were first detected in the bottom region and propagated from bottom to top along the interface. At the bottom region, the crack initiated and propagated along the Fe{sub 1.8}Al{sub 7.2}Si/weld seam interface during the in situ tensile test. When the crack propagated into the middle region, a deflection of crack propagation appeared. The crack first propagated along the steel/Fe{sub 1.8}Al{sub 7.2}Si interface and then moved along the weld seam until the failure of the joint. The tensile strength of the joint was 146.5 MPa. Some micro-cracks were detected at Fe(Al,Si){sub 3} and the interface between the steel substrate and Fe(Al,Si){sub 3} in the top region while the interface was still connected.

36 MATERIALS SCIENCE↗

Effect of Localized Corrosion on Fatigue–Crack Growth in 2524-T3 and 2198-T851 Aluminum Alloys Used as Aircraft Materials

Corrosion and fatigue of aluminum alloys are major issues for the in-service life assessment of aircraft structures and for the management of aging air fleets. The aim of this work was to evaluate the effect of localized corrosion on fatigue crack growth (FCG) resistance of the AA2198-T851 Al-Li alloy (Solution Heat Treated, Cold Worked, and Artificially Aged), comparing it with the FCG resistance of AA2524-T3 (Solution Heat Treated and Cold Worked), considering the effect of seawater fog environment. Before fatigue tests, the corrosion behavior of 2198-T851 and 2524-T3 aluminum alloys was verified using open circuit potential and potentiodynamic polarization techniques. Fatigue in air and corrosion fatigue tests were performed applying a stress ratio (R) of 0.1, 15 Hz (air) and 0.1 Hz (seawater fog) frequencies, using a sinusoidal waveform in all cases. The results showed that the localized characteristics of the 2198-T851 and 2524-T3 aluminum alloys are essentially related to the existence of intermetallic compounds, which, due to their different nature, may be cathodic or anodic in relation to the aluminum matrix. The corrosive medium has affected the FCG rate of both aluminum alloys, in a quite similar way. Graphical Abstract: .

36 MATERIALS SCIENCE↗

Effect of the Combined Addition of Y and Ti on the Second Phase and Mechanical Properties of China Low-Activation Martensitic Steel

In this study, approximately 0.35% Ti and two different Y contents were added to China low-activation martensitic (CLAM) steel during melting in a vacuum induction melting furnace. Scanning electron microscopy, transmission electron microscopy, x-ray diffraction, tensile tests, and Charpy impact tests were used to investigate the effects of the combined addition of Y and Ti on the second phase and mechanical properties. The results indicated that Y and Fe formed the large intermetallic compound Fe-Y; the compound easily aggregated in the grain boundaries and exhibited the strength of CLAM steel. Ti did not combine with Y to form the Y-Ti-O phase; however, it could combine with Ta and W to form MC precipitates, which were generally in the 20-50 nm size range. The CLAM steel with a higher Y content exhibited lower yield and tensile strengths at room temperature, with both steels yielding almost identical strengths at 600 °C.

36 MATERIALS SCIENCE↗

The Effect of Mo Particles Addition in Ag-Cu-Ti Filler Alloy on Ti(C,N)-Based Cermet/45 Steel-Brazed Joints

Reliable brazing of Ti(C,N)-based cermet and 45 steel was successfully achieved by using the Mo-particle-reinforced Ag-Cu-Ti composite filler. The effects of Mo content on the interfacial microstructure and mechanical properties of Ti(C,N)-based cermet/45 steel joints were analyzed. The results showed that the joint microstructure was primarily composed of Ni{sub 3}Ti+Cu{sub 3}Ti{sub 2}, Ag(s,s)+Cu(s.s), CuTi+Mo, Ti-based solid solution, and FeTi+Fe{sub 2}Ti. With the increase in Mo content in filler, the thickness of the Ni{sub 3}Ti+Cu{sub 3}Ti{sub 2} layer adjacent to the Ti(C,N)-based cermet decreases, while more blocky Ti-Cu intermetallic were observed in the brazing seam. The shear strength of the joint could be significantly improved by adding suitable amounts of Mo into the Ag-Cu-Ti filler, and the peak value of 263 MPa was achieved when the alloys were brazed with Ag-Cu-Ti+8wt.%Mo composite filler at 920 °C for 20 min.

36 MATERIALS SCIENCE↗

Effect of Al on Grain Refinement and Mechanical Properties of Mg-3Nd Casting Alloy

The effect of Al on the grain refinement and mechanical properties of as-cast Mg-3Nd alloy was investigated systematically by a series of microstructural analysis, solidification analysis and tensile tests. The results show that Al has an obvious refining effect on the as-cast Mg-3Nd alloy. With increasing Al content, the grain size of the as-cast Mg-3Nd alloy decreases firstly, then increases slightly after the Al content reaching 3 wt.%, and the minimum grain size of the Mg-3Nd alloy is 48 ± 4.0 μm. The refining mechanism can be attributed to the formation of Al{sub 2}Nd particles, which play an important role in the heterogeneous nucleation. The strength and elongation of the Mg-3Nd alloy refined by Al also increase with increasing Al content and slightly decrease when the Al content is more than 3 wt.%, and the strengthening mechanism is attributed to the grain refinement as well as dispersed intermetallic particles. Furthermore, the microstructural thermal stability of the Mg-3Nd-3Al alloy is higher than that of the Mg-3Nd-0.5Zr alloy. Overall, the Mg-3Nd alloy with Al addition is a novel alloy with wide and potential application prospects.

36 MATERIALS SCIENCE↗

Effect of Sm-Rich Phase on Corrosion Behavior of Hot-Extruded AZ31-1.5Sm Magnesium Alloy

The effects of Sm on the corrosion and microstructure behavior of hot-extruded AZ31 magnesium alloy were investigated by SEM, TEM, weight loss analysis, and electrochemical measurements. The results indicated that granular Al{sub 2}Sm phase ~ 4 μm in size in the hot-extruded AZ31 magnesium alloy modified with 1.5 wt.% Sm leads to significant grain refinement. The corrosion rate decreased from 15.98 × 10{sup −4} to 11.19 × 10{sup −4} g cm{sup −2} h{sup −1} in the transverse section and from 8.57 × 10{sup −4} to 6.20 × 10{sup −4} g cm{sup −2} h{sup −1} in the longitudinal section. Compared to the unmodified alloy, the corrosion potential of the Sm-modified alloy in the transverse and longitudinal sections increased by 98 and 62 mV, respectively, and the R{sub ct} value (charge transfer resistance) in the transverse and longitudinal sections of the modified alloy increased from 1764 and 1756 to 2928 and 2408 Ω cm{sup 2}, respectively. The results showed that the corrosion resistance of hot-extruded AZ31 magnesium alloy was significantly improved by Sm addition due to the grain refinement, the decreased dislocation density, and the suppression of micro-galvanic corrosion caused by Al-Sm-(Mn) intermetallic compounds.

36 MATERIALS SCIENCE↗

The Effect of Boron and Zirconium on the Structure and Tensile Properties of the Cast Nickel-Based Superalloy ATI 718Plus

The effects of boron and zirconium on cast structure, hardness, and tensile properties of the nickel-based superalloy 718Plus were investigated. For this purpose, five alloys with different contents of boron and zirconium were cast via vacuum induction melting and then purified via vacuum arc remelting. Microstructural analysis by light-optical microscope and scanning electron microscope equipped with energy-dispersive x-ray spectroscopy and phase studies by x-ray diffraction analysis were performed. The results showed that boron and zirconium tend to significantly reduce dendritic arm spacing and increase the amount of Laves, Laves/gamma eutectic, and carbide phases. It was also found that boron led to the formation of B{sub 4}C and (Cr, Fe, Mo, Ni, Ti){sub 3}B{sub 2} phases and zirconium led to the formation of intermetallic phases and ZrC carbide. In the presence of boron and zirconium, the hardness and its difference between dendritic branches and inter-dendritic spaces increased by concentrating such phases as Laves in the inter-dendritic spaces. These elements had a negative effect on tensile properties of the alloy, including ductility and strength, mainly because of the increase in the Laves phase. It should be noted that the largest degradation of the tensile properties occurred in the alloys containing the maximum amount of zirconium.

36 MATERIALS SCIENCE↗

Analysis of Microstructure and Sliding Wear Behavior of Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} High-Entropy Alloy

Α Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} high-entropy alloy (HEA) of the well-known family of CoCrFeNiTi has been designed using empirical parameters. The aim of this design was the production of a HEA with fcc structure that gives ductile behavior and also high strength because of the solid solution effect. The VEC calculations (8.1) supported the fcc structure while the δ factor calculations (4.97) not being out of the limit values, advised a significant lattice distortion. From the other hand, the ΔΗ{sub mix} calculations (− 9.64 kJ/mol) gave strong indications that no intermetallic would be formed. In order to investigate its potential application, the Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} HEA was prepared by vacuum arc melting and a primary assessment of its surface degradation response was conducted by means of sliding wear testing using different counterbody systems for a total sliding distance of 1000 m. An effort to correlate the alloy’s wear response with the microstructural characteristics was attempted. Finally, the wear behavior of the Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} HEA was compared with that of two commercially used wear-resistant alloys. The results obtained provided some first signs of the high-entropy alloys’ better wear performance when tested under sliding conditions against a steel ball.

36 MATERIALS SCIENCE↗

Electrochemical Behavior Assessment of As-Cast Mg-Y-RE-Zr Alloy in Phosphate Buffer Solutions (X Na{sub 3}PO{sub 4} + Y Na{sub 2}HPO{sub 4}) Using Electrochemical Impedance Spectroscopy and Mott–Schottky Techniques

In the present study, electrochemical behavior of as-cast Mg-Y-RE-Zr alloy (RE: rare-earth alloying elements) was investigated using electrochemical tests in phosphate buffer solutions (X Na{sub 3}PO{sub 4} + Y Na{sub 2}HPO{sub 4}). X-ray diffraction techniques and Scanning electron microscopy equipped with energy dispersive x-ray spectroscopy were used to investigate the microstructure and phases of the experimental alloy. Different electrochemical tests such as potentiodynamic polarization (PDP), electrochemical impedance spectroscopy (EIS) and Mott–Schottky (M–S) analysis were carried out in order to study the electrochemical behavior of the experimental alloy in phosphate buffer solutions. The PDP curves and EIS measurements indicated that the passive behavior of the as-cast Mg-Y-RE-Zr alloy in phosphate buffer solutions was weakened by an increase in the pH, which is related to formation of an imperfect and less protective passive layer on the alloy surface. The presence of the insoluble zirconium particles along with high number of intermetallic phases of RE elements mainly Mg{sub 24}Y{sub 5} in the magnesium matrix can deteriorate the corrosion performance of the alloy by disrupting the protective passive layer that is formed at pH values over 11. These insoluble zirconium particles embedded in the matrix can detrimentally influence the passivation. The M–S analysis revealed that the formed passive layers on Mg-Y-RE-Zr alloy behaved as an n-type semiconductor. An increase in donor concentration accompanying solutions of higher alkalinity is thought to result in the formation of a less resistive passive layer.

36 MATERIALS SCIENCE↗

Investigation of the Tribological Properties of AlxSi-1.2Fe(Mn) (x = 5-13 wt.%) Alloys

The effect of Fe-impurity and Mn modification on the sliding wear behavior of Al-xSi-1.2Fe(Mn) (x = 5-13 wt.%) alloys was investigated in dry sliding against AISI 52100 steel. According to the results, in the Si range of 5-9 wt.%, Fe-impurity promotes the formation of finely distributed β-Al{sub 5}FeSi intermetallics in the matrix increasing its hardness and potential to support the tribolayer leading to the improved wear characteristics. The presence of Fe in the composition of Al-(9-13)Si alloys, however, leads to the formation of primary β-platelets that their sizes and volume fractions increase with Si concentration. The formation of primary compounds increases the hardness, but makes the alloys less ductile and more vulnerable to microcracking and wear. Manganese modification converts the β-Fe platelets to the α-Al{sub 15}(Fe,Mn){sub 3}Si{sub 2} compounds with different morphologies. The substitution of fine β-platelets by α-Chinese scripts in Al-(5-9)Si-1.2FeMn alloys reduces the wear resistance, but the formation of primary α-compounds with star-like or polyhedral morphologies in Al-(9-13)Si-1.2FeMn alloys improves their wear characteristics. Moreover, it was found that the formation of Fe(Mn)-rich compounds affects the friction coefficient which is likely due to the fracture of particles in the subsurface region, their interaction with contacting surfaces, and their effect on the stability of the tribolayer.

36 MATERIALS SCIENCE↗

Mechanical Properties and Interface Evaluation of Al/AZ31 Multilayer Composites Produced by ARB at Different Rolling Temperatures

Many researchers have studied the microstructure and mechanical properties of Al/Mg composites rolled at a unique temperature; however, the effect of rolling temperature, which is one of the more decisive accumulative roll bonding (ARB) parameters, has not been investigated. In this work, laminated Al/Mg composites were fabricated by ARB at different temperatures using AZ31 magnesium alloy and commercially pure aluminum sheets. The microstructure of the layers and the mechanical properties of the rolled Al/AZ31 composites were investigated. Tensile and bending properties of the multilayer materials were examined by tensile and three-point bending tests. The results showed that mechanical bonding of the layers was improved with increasing rolling temperature. As a result, the intermediate rolling temperature (300 °C) indicated the best mechanical properties. Moreover, hot rolling caused an accelerated formation of intermetallic compounds.

36 MATERIALS SCIENCE↗

Mechanical Properties and Microstructural Evolution of Yb-Modified Al-20%Si Alloy

In the study, the mechanical properties and microstructural evolution of hypereutectic Al-20%Si-xYb alloys (x = 0, 0.1, 0.3, 0.5 and 0.7 wt.%) were studied. The as-prepared samples were characterized by scanning electron microscopy, optical microscope, x-ray diffraction (XRD) and electron probe microanalysis. The characterization results showed with the addition amount of Yb increasing to 0.5%, the eutectic Si structure was gradually modified from coarse needle-like/platelet-like structure into fine coral-like fibrous structure and the primary Si phases were gradually converted from coarse platelet-like/star-like/polygonal shape into fine blocky shape. In particular, according to the results of WDS and XRD analyses, the Yb-rich intermetallic phase in the Al-20%Si alloy is Al{sub 3}Yb. Tensile test was carried out to study the mechanical properties of Al-20%Si-x%Yb alloys, and results showed that the elongation and ultimate tensile strength increased by 73.6% and 64.5%, respectively.

36 MATERIALS SCIENCE↗

The Sliding Wear and Frictional Behavior of M50-10 wt.%(Sn-Ag-Cu) Self-Lubricating Materials at Elevated Temperatures

As the main steel used in the aero-engine main shaft bearings, the tribological properties of M50 can directly affect the performance of aero-engine. The purpose of this study is to design the reasonable composition of Sn-Ag-Cu alloy and investigate the wear mechanisms of M50-10 wt.%(Sn-Ag-Cu) composites (MSACC) prepared by SPS sliding against Si{sub 3}N{sub 4} ball from 25 to 550 °C at 12 N-0.25 m/s. XRD, EPMA, FESEM and EDS mappings are conducted to understand the major mechanisms leading to the improvement in the sliding behavior of MSACC. The results indicate that MSACC with different specifications of Sn-Ag-Cu alloy shows excellent friction and wear properties from 25 to 550 °C compared to M50. M50-10 wt.%(50Sn40Ag10Cu) (MSACC-2) shows the distinguished tribological performance for the lower friction coefficients of 0.22-0.61 and less wear rates of 1.7-4.1 × 10{sup −6} mm{sup 3} N{sup −1} m{sup −1}, which is attributed to the formed excellent lubricating structure consisting of the lubricating film with massive Sn-Ag-Cu alloy and intermetallic compounds formed during the friction process, as well as the underneath mixed layer who can well support the lubricating film due to the good intersolubility between the designed Sn-Ag-Cu alloy and M50 (Fe).

36 MATERIALS SCIENCE↗

Role of Centrifugal Casting on Electrochemical Corrosion Behavior of A356-SiCp Composite in 3.5 wt.% NaCl

Role of graded microstructure in a centrifugally cast A356-SiC particle (SiCp) composite alloy disk on passivity and localized corrosion behavior in 3.5 wt.% NaCl environment has been investigated. The area fraction of SiCp has been found to decrease from the outer periphery to the core of the disk, while the apparent size and area fraction of the intermetallics and Mg-rich phase increase from the periphery to the core. As a consequence, the corrosion resistance of the as-cast disk varies with the distance from the periphery in the order 45 < 65 < 25 < 5 mm. The corrosion resistance of the centrifugally cast disk can be significantly improved through solution annealing at 540 °C for 2 h and solution annealing + aging at 175 °C for 2 h. However, between the two, the former has shown a better corrosion resistance and passivity than the latter. In the latter case, the aging treatment resulted in the precipitation of Mg{sub 2}Si phase which is prone to the corrosion attack.

36 MATERIALS SCIENCE↗

Microstructural Characterization, Mechanical Properties, and Corrosion Resistance of Dental Co-Cr-Mo-W Alloys Manufactured by Selective Laser Melting

In this paper, the microstructure, mechanical properties, and corrosion resistance of the dental Co-Cr-Mo-W alloys fabricated by selective laser melting (SLM) were systematically investigated and correlated. The microstructure of the SLM group (SG) specimens is composed of extremely fine columnar crystals, exhibiting supersaturated and homogeneous character. The matrix mainly consists of face-centered-cubic (FCC) cobalt solid solutions, and minimal hexagonal-close-packed (HCP) cobalt solid solutions. Mechanical test results showed that the 0.2% yield strength of SG was 775 ± 7 MPa, and the ultimate tensile strength was 1118 ± 25 MPa. The elongation of SG was 8.28 ± 0.4%, and the microhardness of SG was 476 ± 10 HV. All of these values largely exceeded the cast group (CG) specimens. The high strength is attributed to their fine columnar crystals and supersaturated matrices. The fewer content from the HCP phase and a lack of intermetallic compounds or eutectic contribute to the high ductility. Furthermore, a higher E{sub corr}, lower I{sub corr} were acquired for better corrosion resistance compared to cast specimens, due to even less composition segregation and more microstructural homogeneity.

36 MATERIALS SCIENCE↗

Influence of Oxygen Partial Pressure Variation on Oxidation Resistance of Ti-46.7Al-1.9W-0.5Si at 750, 850 and 950 °C

γ-TiAl intermetallic alloys can be potentially employed as structural materials for many industries where high temperature and access of atmosphere with variable oxygen partial pressures are often met. Different partial pressures of oxygen may influence oxidation behavior and induce different oxide scale phase constitutes. This study investigated the influences of oxygen partial pressures on the oxidation resistance of a γ-TiAl alloy, Ti-46.7Al-1.9W-0.5Si (at.%), in Ar-O{sub 2} environments (5%O{sub 2}, 20%O{sub 2} and 80%O{sub 2}) at 750, 850 and 950 °C, respectively. The oxidation products were characterized using scanning electron microscopy, energy-dispersive x-ray analysis, x-ray diffraction and transmission electron microscopy. The oxidation kinetic results achieved by a discontinuous gravimetric method revealed that the alloy oxidized following a parabolic rate law. The oxidation resistance of the alloy was enhanced with increasing the oxygen partial pressures at all three experimental temperatures. Multilayered oxide scales of TiO{sub 2}/Al{sub 2}O{sub 3} were developed during the oxidation process. The enhancement of oxidation resistance was resulted from preferential generation of Al{sub 2}O{sub 3} and the reduction in defects in TiO{sub 2} with increasing the oxygen partials pressures.

36 MATERIALS SCIENCE↗

The Influence of Galvanizing Parameters on the Structural Development of Zn-Al-Based Coatings

The evolution of some layers’ characteristics, deposited by galvanization, was monitored according to the technological parameters of the process. Two types of alloys from the Zn-Al and Zn-Al-Ti-B systems were used for deposition. The structure of the deposited layers was analyzed by optical and electron microscopy. The chemical composition, phases and compounds in the structures were identified. The mechanical properties of the structural constituents of the layers were determined by nanoindentation. These techniques highlighted the typical non-uniformities in terms of composition and properties in the layers, mainly due to the diffusion and distribution of iron from the steel substrate in the deposited layers. The evaluation of iron diffusion in the deposited layer was done by differential thermal analysis. The values of the critical temperatures (melting temperature, eutectic temperature and solidification temperature) were correlated with the parameters used during deposition. It was observed that the structure of the coatings is layered, with a specific order from the steel substrate to the edge. In these layers, the constituents are mixtures of soft solid solutions of Al in Zn (η and β) and hard intermetallic compounds. Moreover, increasing the immersion time in the galvanizing bath and the bath temperature leads to an increase in iron diffusion in the coating layer, which contributes to lower coating thickness, thus reducing its durability in operation.

36 MATERIALS SCIENCE↗