BEND-TEST PROPERTIES OF 43XX-VANADIUM MODIFIED AND 5 PERCENT CHROMIUM SHEET STEELS
Bend-test properties of 43xx-vanadium modified and 5 percent chromium sheet steels
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Bend-test properties of 43xx-vanadium modified and 5 percent chromium sheet steels
The reaction between solid NaCl and air containing 1 pct SO2 has been studied between 500 and 700 C. The reaction product, Na2SO4, forms not only on the surface of the NaCl but also on surrounding areas of the substrate due to the volatility of the NaCl at these temperatures. At the higher temperatures, the vapor pressure of NaCl is so high that the majority of the reaction product is distributed on the substrate. Above 625 C, the reaction product is a liquid solution of NaCl and Na2SO4 that exists only so long as NaCl is supplied from the original crystal source. Eventually, the liquid solidifies by constitutional solidification as the NaCl is converted to Na2SO4. While it exists, the liquid NaCl-Na2SO4 solution is shown to be highly corrosive to Al2O3 and, on a scale of Al2O3 growing on alloy HOS 875, particularly attacks the grain boundaries of the scale at preferred sites where chromium and iron oxides and sulfides rapidly develop. This is proposed as one mechanism by which NaCl deposition contributes to the initiation of low temperature hot corrosion.
The dependence of the lifetimes of small quantities of a Multiply Alkylated Cyclopentane (MAC) lubricant oil, Pennzane (Registered Trademark) 2001A (Nye Lubricants, Inc.), in rolling and sliding contact with different metals was evaluated with a vacuum spiral orbit tribometer. The metals were the bearing alloys 52100 steel, 440C steel, 17-4 PH steel and Nitinol 60 and the elements chromium, vanadium and titanium. The lifetimes of the lubricant oil on different metals fell into distinct groups with 52100 greater than 440C approx. Nitinol 60 greater than 17-4 PH for the order of the lifetimes of the steels and chromium greater than vanadium greater than titanium for the order of the lifetimes for the elements. The limited life of the small quantities of oil is assumed to be due to its consumption by the tribochemical reaction of the oil with the different metal bearing materials. The lifetimes are then inversely related to the reaction rates of the oil molecules with the various metals: the longest life of 52100 steel having the lowest reaction rate and the shortest life of titanium having the highest reaction rate. Mechanisms for the tribochemical reactions are discussed.
The wideband laser has shown great potential in metal–ceramic coatings deposition due to the high efficiency and low dilution rate. However, the effects of wideband laser process on microstructure evolution and bonding mechanism at the coatings/substrate interface are still a critical problem and need further investigation. In this work, nickel composite coatings are fabricated on the surface high-strength low-alloy steel. The effects of laser fluence on microstructure evolution, shear strength and fracture mechanism are studied. Results indicated the added WC particles were partly dissolved due to the high-power laser irradiation. Many block precipitates and dense eutectic were synthesized in composite coatings. Reinforced phases mainly consist of Cr{sub 5}B{sub 3}, Cr{sub 23}C{sub 6}, W{sub 2}C and Cr{sub 3}Ni{sub 2}. The dilution of Q550 steel contributed to the formation of nickel dendrites and facilitated a dense metallurgical bonding at coating/substrate interface when laser fluence was high. Shear strength tests indicated the laser fluence and shear strength had a positive correlation. For Ni60/WC composite coatings designed in these experiments, the recommend laser fluence should be higher than 55 J/mm{sup 2}, above which the shear strength could be greater than 200 MPa. Fracture surfaces indicated the failure mechanism of composite coatings was quasi-cleavage fracture.
A survey was made of portions of the chromium-cobalt-nickel-molybdenum quaternary system at 1,200 degrees c by means of microscopic and x-ray diffraction studies. Since the face-centered cubic (alpha) solid solutions form the matrix of almost all practically useful high-temperature alloys, the solid solubility limits of the quaternary alpha phase were determined up to 20 percent molybdenum. The component cobalt-nickel-molybdenum, chromium-cobalt-molybdenum, and chromium-nickel-molybdenum ternary systems were also studied. The survey of these systems was confined to the determination of the boundaries of the face-centered cubic (alpha) solid solutions and of the phases coexisting with alpha at 1,200 degrees c.
Highlights: • The microstructure evolution of Ti-47Al-2Cr-2Nb alolly was investigated in detail. • The foramtion of B{sub 2} phase can be adjusted in Ti-47Al-2Cr-2Nb alloy. • A new mechanism of B{sub 2} phase on room temperature mechanical properties of Ti-47Al-2Cr-2Nb alloy was proposed. - Abstract: The formation of B{sub 2} phase was adjusted via various hot isostatic pressing processes in Ti-47Al-2Cr-2Nb alloy. The microstructure evolution and a new mechanism of B{sub 2} phase on room temperature mechanical properties was investigated by BSE, EBSD and TEM in detail. The result shows that the formation of B{sub 2} phase leads to Cr element content decrease in γ matrix phase, which results in lattice parameter increase, namely the c/a ratio of γ matrix phase. Finally, at room temperature the mechanical properties of Ti-47Al-2Cr-2Nb alloy deteriorates.
The infrastructure for transportation in the United States allows for a high level of mobility and freight activity for the current population of 300 million residents, and several million business establishments. According to a Department of Transportation study, more than 230 million motor vehicles, ships, airplanes, and railroads cars were used on 6.4 million kilometers (4 million miles) of highways, railroads, airports, and waterways in 1998. Pipelines and storage tanks were considered to be part of this deteriorating infrastructure. The annual direct cost of corrosion in the infrastructure category was estimated to be approximately $22.6 billion in 1998. There were 583,000 bridges in the United States in 1998. Of this total, 200,000 bridges were steel, 235,000 were conventional reinforced concrete, 108,000 bridges were constructed using pre-stressed concrete, and the balance was made using other materials of construction. Approximately 15 percent of the bridges accounted for at this point in time were structurally deficient, primarily due to corrosion of steel and steel reinforcement. Iron-based amorphous metals, including SAM2X5 (Fe{sub 49.7}Cr{sub 17.7}Mn{sub 1.9}Mo{sub 7.4}W{sub 1.6}B{sub 15.2}C{sub 3.8}Si{sub 2.4}) and SAM1651 (Fe{sub 48}Mo{sub 14}Cr{sub 15}Y{sub 2}C{sub 15}B{sub 6}) have been developed, and have very good corrosion resistance. These materials have been prepared as a melt-spun ribbons, as well as gas atomized powders and thermal-spray coatings. During electrochemical testing in several environments, including seawater at 90 C, the passive film stabilities of these materials were found to be comparable to that of more expensive high-performance alloys, based on electrochemical measurements of the passive film breakdown potential and general corrosion rates. These materials also performed very well in standard salt fog tests. Chromium (Cr), molybdenum (Mo) and tungsten (W) provided corrosion resistance, and boron (B) enabled glass formation. The high boron content of this particular amorphous metal made it an effective neutron absorber, and suitable for criticality control applications. These amorphous alloys appear to maintain their corrosion resistance up to the glass transition temperature. Visionary research is proposed to extend the application of corrosion-resistant iron-based amorphous metal coatings, and variants of these coatings, to protection of the Nation's transportation infrastructure. Specific objectives of the proposed work are: (1) fabrication of appropriate test samples for evaluation of concept; (2) collection of production and test data for coated steel reinforcement bars, enabling systematic comparison of various coating options, based upon performance and economic considerations; and (3) construction and testing of concrete structures with coated steel reinforcement bars, thereby demonstrating the value of amorphous-metal coatings. The benefits of ceramic coatings as thermal barriers will also be addressed.
The upper operating temperature of tubes in heat exchangers/steam generators is strongly influenced by the degradation that can occur because of the reaction of the exchanger/generator tubing with the deposits that accumulate on the surface of the tubes. In fact, severe corrosion has been observed in some biomass fired systems, particularly with elevated potassium and chlorine concentrations in the deposits. Wood gasifiers have recently been and are currently being constructed at several sites in North America. In these systems, the syngas is burned to produce steam and the performance of the heat exchanger tubes under ash deposits is of great concern. As temperatures of the heat exchangers are increased in an effort to increase their operating efficiency, the performance of the tubes is of greater interest. The corrosion behavior of alloy steel tubes as a function of temperature has been investigated by exposing samples of selected alloys to ash collected from the steam generator fired by syngas produced in wood gasifiers. This study compares corrosion rates from laboratory exposures of synthesis gas and ash at 500 C and 600 C. This study investigated the material performance of four ferritic steels and one austenitic steel exposed to conditions expected on the fireside of a wood gasifier. The purpose of this study was to identify an effective method for determining material performance for samples exposed to both the process gas and the fly ash that is typically observed within the steam generator for times up to 1000 hours. Mass changes were measured for all of the samples, but this information can be misleading concerning material performance due to the difficulty in sufficiently cleaning the samples after exposure in the ash. Therefore, small cross sections of the samples were collected and imaged using optical microscopy. Oxide thicknesses were measured along with metal losses. The metal loss information provides a clear indication of material performance. The metal loss rates for the ferritic steels at 500 C were almost half of those observed at 600 C and the rates decreased with increasing exposure time. It was also reported that the metal loss rates generally decrease with increasing chromium concentration.
When alloys are strained to a certain limit under the plastic deformation, ductile fracture occurs. Whether the required deformation can be put into effect before fracture appears has become a serious concern. A combination of compression tests, ductile fracture criteria as well as finite element simulation (FEM) were employed in this study to establish the fracture initiation prediction model of Ti-47Al-2Nb-2Cr alloy. To obtain the critical fracture strain, a technique was proposed to calculate the data for deformed cylindrical samples through isothermal compression tests in the temperature range between 1223 and 1423 K with strain rates ranging from 0.001 to 1 s{sup −1}. Five commonly used ductile fracture criteria were compared by FE simulation of compressing tests. It was found that the Brozzo criterion was found to be suitable and accordingly a failure criterion, considering temperature and strain ratio was established. Hot working parameters (critical fracture value and critical strain) in deformation could be obtained through the finite element simulation, revealing that this newly established failure criterion could accurately predict cracking initiation in compressing deformation of Ti-47Al-2Nb-2Cr alloy ingot.
Widmannstätten laths in Ti48Al2Cr2Nb alloy were obtained by containerless electromagnetic levitation during undercooled solidification rather than heat treatments in most cases. The nucleation of γ{sub Widmannstätten} is confirmed by the thermal history of the second recalescence behaviour. High dislocation density, stacking faults and dislocation slip are observed by transmission electron microscopy. By quantitative analysis of the transformation energy, the driving force for γ{sub Widmannstätten} in the solid state phase transformation is calculated, compared with that of heat treatments. Meanwhile, the proper undercoolings (ΔT = 257–300 K), post-solidification cooling rates (11.1–29.1 K/s), the fine lamellar colony sizes (306–467 μm) and proper undercoolings in the solid state phase transformation are in favour of promoting the formation of Widmannstätten laths at moderate undercoolings. - Graphical abstract: Display Omitted - Highlights: • Widmannstätten laths were observed in undercooled TiAl alloy. • The influencing factors were discussed in undercooled TiAl alloy. • An analysis of the nucleation of γ{sub Widmannstätten} is carried out.
Debris generated from total hip arthroplasty (THA) components made from metal alloys can cause, in some cases, inflammatory cell (e.g., macrophages) responses that lead to adverse local tissue reactions (ALTR) and implant failure. The lack of information on intracellular chemical alterations of metal debris has hindered the understanding of the pathogenesis of ALTR. The goal of this study was to characterize intracellular debris within macrophages using Synchrotron imaging and spectroscopy. We studied periprosthetic tissues of two retrieved THAs with (1) a metal-on-metal (MoM) articulation and (2) a metal-on-polyethylene (MoP) articulation exhibiting corrosion of the metal femoral head. The MoM-THA exhibited different valence states of chromium- and cobalt-containing debris, suggesting three different moieties: Cr 2 O 3 , CrPO 4 , and an alloy-oxide mixture. The findings further suggest that Cr 2 O 3 formed in the tribological interfaces of the implant, while CrPO 4 is a by-product of the phagocytosis process of cobalt alloy-containing debris. Titanium debris appeared to occur in a mixed crystalline/amorphous oxide state. It remains unclear if this chemical state results from the tribochemical processes at the implant surface or intracellular alterations. The MoP-THA specimen exhibited no intracellular particulate debris associated with macrohpages, indicating that the ALTR may be entirely triggered by metal ionic species in this case. A better understanding of in vivo chemical alteration of implant debris will aid in assessing the risk for ALTR during implant design and material choice. However, various techniques are needed to accurately determine the interaction between metal particles and the inta- and extra-cellular environment.
This paper reports on the processing of Fe{sub 48}Cr{sub 15}Mo{sub 14}Y{sub 2}C{sub 15}B{sub 6} amorphous alloy coatings on Cu-10%Ni (wt.%) alloy using spark plasma sintering. The amorphous alloy coatings were sintered at temperatures ranging from 575 to 675 °C at a pressure of 50 MPa. The development of microstructure, phases, and wear properties with sintering temperature of the coatings is investigated. The sintered coatings were found to be near fully dense with hardness close to that of the sintered bulk amorphous alloy. X-ray analysis indicated increasing degree of devitrification of the amorphous coatings with increasing sintering temperature. The wear behavior of the coatings is significantly influenced by the sintering temperature with volume wear rate first decreasing in the temperature range of 575-650 °C and then increasing above 650 °C. The variation in wear behavior is explained based on relative stability of the protective surface layer and embrittlement of the surface with the sintering temperature.
In the course of studies on the iron-rich multicomponent system Fe-Mn-Cr-Mo-Nb-Al-Si-C, work was concentrated on pertinent quinary and six-component combinations namely Fe-Mn-Al-Si-C, Fe-Cr-Al-Si-C and Fe-Mn-Cr-Al-Si-C which had been elaborated at 65, 72, and 80 wt pct Fe. Manganese acts as a strong stabilizer for the cementite carbide. Chromium seems to stabilize the iron aluminide Fe2Al5 which forms in a considerable amount within an alloy of nominal composition Fe(65)Mn(15)Cr(12)Al(5)Si(2)C(1) (percent by weight). Although the Mn3AlC carbide is, like Fe3AlC, a perovskite carbide, manganese does not appear to favor the formation of the perovskite carbide. Because of the relatively low sintering temperature (700 C), for al large portion of the samples equilibria conditions are not always reached.
Heat-resistant piston rings and linings increase engine efficiency. Report discusses research on materials for piston rings and cylinder coatings in automotive Stirling engines. Data from tests show cobalt-based alloy, Stellite 6B, good choice for piston rings and PS200, plasma-sprayed metal-bonded chromium carbide matrix with dispersed solid lubricants, functions well as cylinder coating. Materials make it possible to place piston rings at tops of pistons ("hot" piston rings) instead of at cooler bottoms.
One or more embodiments relates to a method of casting a creep-resistant Ni-based superalloy and a homogenization heat treatment for the alloy. The method includes forming a feed stock having Nickel (Ni) and at least one of Chromium (Cr), Cobalt (Co), Aluminum (Al), Titanium (Ti), Niobium (Nb), Iron (Fe), Carbon (C), Manganese (Mn), Molybdenum (Mo), Silicon (Si), Copper (Cu), Phosphorus (P), Sulfur (S) and Boron (B). The method further includes fabricating the creep-resistant Ni-based superalloy in a predetermined shape using the feed stock and at least one process such as vacuum induction melting (VIM), electroslag remelting (ESR) and/or vacuum arc remelting (VAR).
Positron annihilation lifetime studies were carried out on cold worked pure Fe and Fe-9Cr alloy subjected to isochronal annealing in the temperature range from 300 to 1323 K. The measured lifetimes of Fe-9Cr alloy showed three distinct annealing stages as compared to pure Fe viz., initial annealing of defects, a plateau between 623 K and 873 K and noticeable increase beyond 1123 K. The second annealing stage is likely due to the formation of chromium rich nanoclusters. Third annealing stage beyond 1123 K is attributed to highly defected martensitic phase formation during cooling from y-phase.
Creep strength enhanced ferritic (CSEF) steels containing 9-12wt% chromium have been extensively used in fossil-fuel-fired power plants. Despite their excellent creep resistance at high temperatures, premature failures (especially Type IV cracking) are often found in the fine-grained heat affected zone (HAZ) or intercritical HAZ of the welded components. This failure mode is preceded by the strain localization in the HAZ, as measured by the Digital Image Correlation (DIC) technique. The present work aims to develop a finite-element based computational method to determine the micromechanical and microstructural origin of the strain localization phenomenon. We construct a two-dimensional digital microstructure based on the actual microstructure of ferritic steel weldments by using the Voronoi-tessellation method, to account for the effects of its large grain-size gradients. A mechanism-based finite element method is developed for modeling the high temperature deformation resulting from a synergy of thermally activated dislocation movements, diffusional flow and grain boundary sliding. The numerical results agree well with the strain measurements by our DIC technique, particularly revealing the effect of pre-welding tempering on the evolution of strain localization in HAZ of creep resistant steel weldments. It is found that the diffusional creep with dependence on grain sizes, dislocation creep with dependence on material strength, and more importantly, grain boundary sliding, contribute synergistically to the creep strain accumulation in the HAZ, and their relative degree of significance is quantified. The creep rupture life will be investigated in the companion paper.
The relationship between stress and strain, and between stress and permanent set, for 18:8 alloy as affected by prior plastic deformation is discussed. Hysteresis and creep and their effects on the stress-strain and stress-set curves are also considered, as well as the influence of duration of the rest interval after cold work and the influence of plastic deformation on proof stresses, on the modulus of elasticity at zero stress, and on the curvature of the stress-strain line. A constant (c sub 1) is suggested to represent the variation of the modulus of elasticity with stress.