Microstructural Constraints on the Formation History of Hibonite in Refractory Inclusions

Hibonite is a primary refractory phase occurring in many Ca-Al-rich inclusions (CAIs), typically with spinel and perovskite [1]. Previous mi-crostructural studies of hibonite in CAIs revealed the presence of numerous stacking defects along the (001) plane and correlated non-stoichiometry in hibonite [2,3]. These features are interpreted as complex inter-growths of stoichiometric and Ca-deficient hibonites, as shown by experimental studies of reaction-sintered CaO-Al2O3 compounds [4]. Here, we extend our transmission electron microscope (TEM) studies to hibonite-bearing CAIs in CM chondrites that have been well characterized isotopically [5-7]. In addition, we have undertaken a series of anneal-ing experiments to explore the effect of minor elements (Mg and Ti) on the microstucure of hibonite [8,9,this study]. The results of these experiments are being applied to hibonite in CAIs in order to better understand its formation conditions.

Han, J.↗

Oxidation of Alumina-Forming MAX Phases in Turbine Environments

Protective coatings for high temperature turbine components are based on YSZ thermal barriers and oxidation resistant, alumina-forming NiAl or NiCoCrAlY bond coats. Ti2AlC and Cr2AlC MAX phases are thus of special interest because of good oxidation resistance and CTE that can match Al2O3 and YSZ. Their alumina scales grow according to cubic kinetics due to grain growth in the scale, with initial heating dominated by fast TiO2 growth. Protective cubic kinetics are also found in high pressure burner rig tests of MAXthal 211 Ti2AlC, but with reduced rates due to volatile TiO(OH)2 formation in water vapor. YSZ-coatings on bulk Ti2AlC exhibit remarkable durability up to 1300C in furnace tests and at least a 25x life advantage compared to superalloys. At another extreme, Cr2AlC is resistant to low temperature Na2SO4 hot corrosion and exhibits thermal cycling stability bonded to a superalloy disk material. Accordingly, sputtered Cr2AlC coatings on disk specimens prevented hot corrosion detriments on LCF. Breakaway oxidation (Ti2AlC), scale spallation (Cr2AlC), interdiffusion, and processing as coatings still present serious challenges. However the basic properties of MAX phases provide some unusual opportunities for use in high temperature turbines.

ceramics↗

Rhombohedral Super Hetero Epitaxy of Cubic SiGe on Trigonal c-plane Sapphire

New rhombohedral super-hetero-epitaxy technology was developed at NASA. This epitaxy technology enables the growth of unprecedented cubic-trigonal hybrid single crystal structures with lattice match on sapphire (Al2O3) substrates, hence with little strain and very few defects at the interface.

Choi, Sang H.↗

Single Crystal Rhombohedral Epitaxy of Sige on Sapphire at 450.Degree. C.-500.Degree. C. Substrate Temperatures

Various embodiments may provide a low temperature (i.e., less than 850° C.) method of Silicon-Germanium (SiGe) on sapphire (Al2O3) (SiGe/sapphire) growth that may produce a single crystal film with less thermal loading effort to the substrate than conventional high temperature (i.e., temperatures above 850° C.) methods. The various embodiments may alleviate the thermal loading requirement of the substrate, which in conventional high temperature (i.e., temperatures above 850° C.) methods had surface temperatures within the range of 850° C.-900° C. The various embodiments may provide a new thermal loading requirement of the sapphire substrate for growing single crystal SiGe on the sapphire substrate in the range of about 450° C. to about 500° C.

Choi, Sang Hyouk↗

Reworking and Diagenesis of Martian Soil: Pathway to Murray Formation Sediments?

In Gale crater, the Curiosity Mars rover has climbed over 300 meters of the Murray formation from the base of the Pahrump Hills to the crest of Vera Rubin Ridge. We discuss the possibility that fine-grained mudstone of the Murray formation is a diagenetic product of sediments with a chemical and mineralogical composition similar to present-day martian soil. Typical (low Ca-sulfate) Murray samples have Na2O, Al2O3, SiO2, SO3, TiO2 and FeOT concentrations within 10% (relative) of average martian soil. These oxides constitute ~85% of each sample. The Al/Si and Ti/Si ratios of Murray samples are comparable to average martian soil but distinct from other martian geologic units. Percentage difference in P2O5, Cl, K2O, Cr2O3, MnO, Ni, Zn, Br, and Ge between soil and Murray samples generally exceed 10%, but these elements and oxides amount to less than 4% of the samples. These constituents are highly variable in Murray mudstone and may reflect mobility in fluid interactions. Large discrepancies in MgO and CaO with ~50% lower concentrations in the Murray samples (~2% absolute differences) are indicative of open-system alteration if the Murray mudstone originated from soil-like material. Mineralogically, martian soil is dominated by plagioclase feldspar, pyroxenes, and olivine with minor hematite, magnetite, and Ca-sulfate. In comparison, Murray samples generally have less feldspar and pyroxene, little to no olivine, more iron oxides and Ca-sulfates, and Fe-containing phyllosilicates. If Murray mudstone originated from a Mars soil composition, aqueous alteration could have converted olivine and pyroxenes to iron oxides and phyllosilicates. Intermixed or zoned plagioclase feldspars could have lost a larger portion of calcic constituents, consistent with susceptibility to weathering, resulting in a change from ~An55 (soil) to ~An40 (Murray). This alteration could be consistent with the major element chemistry, including the small decrease in MgO and CaO. A subsequent influx of minor/trace elements and Ca-sulfate, e.g. from groundwater, would be required. In this diagenetic scenario, the bulk of the alteration would have been nearly isochemical, suggesting limited mineral segregation and aqueous alteration during transport from the drainage basin or a significant direct aeolian contribution to the Murray sediments.

Yen, Albert S.↗

Atomic Layer Deposition Josephson Junctions for Cryogenic Circuit Applications

Superconducting-insulating-superconducting (SIS) trilayers have been produced for Josephson Junction fabrication by thermal atomic layer deposition (ALD) processes. The trilayers are composed of alternating layers of Ti0.4N0.6/Al2O3/ Ti0.4N0.6, deposited at 450°C, in a thermal ALD reactor on Al2O3-coated silicon. The conformal nature of the ALD process provides excellent step coverage of superconducting and insulating films. The film thickness of a single ALD cycle being one mono-layer, allows us to precisely control the tunnel-barrier insulator thickness by counting the number of ALD cycles during the insulator deposition step. Tunnel-junctions with critical current 500 A/cm2 are reported. Fabrication of Josephson Junctions and progress toward development of a single-element ALD Superconducting Quantum Interference Device (SQUID) will be discussed

Atomic Layer Definition↗

Distribution of Fe3+ and H in Minerals During Partial Melting and Metasomatism of Spinel Peridotite

Oxygen fugacity and water content are crucial parameters for many chemical and physical properties of the Earth's mantle, for example bearing on fluid type, melting initiation, and deformation. However, the exact behaviour of Fe3+ and H during melting and metasomatism is still under debate. Here, the Fe3+/ΣFe ratio (Mössbauer and EMP) and water content (FTIR) of peridotite minerals are examined in mantle xenoliths from Kilbourne Hole (KH), NM, and Dish Hill (DH), CA (USA). These spinel peridotites have compositions consistent with partial melting with variable degrees of metasomatism (undetectable to cryptic to modal). Pyroxenites also allow to examine melt-rock reactions. Bulk-rock Fe2O3 content of the KH peridotites correlates with indices of melting (positive with bulk-rock Al2O3 and Cpx Yb contents, and negative with spinel Cr#) confirming that Fe3+ behaves as an incompatible element during melting. Correlations of the Fe3+/ΣFe ratio of minerals with these indices, however, indicates that Fe3+ is incompatible in Cpx but compatible in Opx and spinel during melting. Water contents in olivine, Cpx and Opx from most KH peridotites can be explained by partial melting and correlate negatively with the Fe3+/ΣFe ratio of spinel and Opx but positively with that of Cpx. This indicates partial control of Fe3+ on the incorporation of H in pyroxene, but not related to a redox equilibrium in Cpx. The higher Fe3+/ΣFe ratio of spinel in the metasomatized KH and DH peridotites, and in the pyroxenites confirms that oxidation characterizes modal metasomatism. Metasomatism, however, is not necessarily accompanied by water addition.

Peslier, A. H.↗

Durability of YSZ Coated Ti2AlC in 1300°C Mach 0.3 Burner Rig Tests

A thermal barrier coating system survived burner rig testing at 1300°C for 500 h. A 160 µm thick YSZ coating was applied to a Ti2AlC MAX phase sample by PS-PVD and tested face-on in an atmospheric Mach 0.3 jet fuel burner, using 5-h thermal cycles. No TBC spallation or recession was observed, only a 2.4 mg/sq. cm mass gain. The modest weight gain precluded severe volatility losses under high velocity burner conditions. The coating surface exhibited colonies of (111) flourite fiber-textured columns separated by craze patterns, with no visible moisture attack. The metastable tetragonal t' YSZ phase was obtained initially, transitioning to teq and cubic YSZ, but with little detrimental monoclinic. The thickness of the alumina TGO was ~21-23 m under the heated YSZ face and ~13-15 m on the uncoated, cooler backside. The backside exhibited removal of initial transient TiO2 nodules and etching of the underlying Al2O3 scale by volatile hydroxides in high temperature, high velocity water vapor. Aerodynamic forces produced some bending of the cantilevered sample due to creep. The test indicated exceptional stability of YSZ coatings on Ti2AlC under turbine conditions.

Smialek, J.↗

Thermochemistry of Protective Coatings and Molten Silicate Debris

The durability of gas-turbine engine components can be significantly affected by the ingestion of siliceous particles, which can melt at high temperature and corrode protective coatings that are essential for long life requirements. The silicate debris consists mainly of CaO-MgO-Al2O3-SiO2 (CMAS) and is usually ingested by aircraft engines during and after take-off, sticking to their hot surfaces and resulting in the formation of calcium rare-earth silicate oxyapatites. The thermochemistry of coatings and their reaction products with molten silicate debris are crucial to understand in order to improve the durability of gas-turbine engines. Here we discuss results of high temperature drop solution calorimetry, drop-and-catch calorimetry (DnC) and differential thermal analysis (DTA) techniques for the thermodynamic properties of both thermal barrier coatings (TBCs) and environmental barrier coatings (EBCs) and their reaction with CMAS compositions. The enthalpies of solution of Y2Si2O7, Yb2Si2O7, 31YSZ, and 16RESZ based coatings and the oxyapatite are moderately positive. However, oxyapatite formation is only favorable over coating dissolution in terms of enthalpy for 7YSZ. The enthalpies of mixing between the coatings and the molten silicate are less exothermic for Yb2Si2O7 and CaYb4Si3O13 than for 7YSZ, indicating lower energetic stability of the latter against molten silicate corrosion. We also report for the first time the calorimetric measurements of the enthalpies of formation of rare-earth silicate based EBC coatings and oxyapatites (rare-earth, RE = Y, Yb, Gd, Dy, Er, Nd and Sm).

Costa, Gustavo↗

Calorimetric Measurements of the Thermodynamic Properties of RE-Silicate Coating Materials

Thermodynamic quantities of coatings materials and siliceous debris-induced corrosion products are crucial to understand in order to develop mitigation strategies necessary to improve the durability of gas-turbine engines. Siliceous induced corrosion can occur when debris consisting mainly of CaO-MgO-Al2O3-SiO2 (CMAS) is ingested by aircraft engines during and after take-off, which sticks to hot surfaces and forms calcium rare-earth silicate oxyapatites. In this work, high-temperature oxide melt drop solution calorimetry (HT drop solution calorimetry) was used to obtain the enthalpies of formation for RE silicate (RE2Si2O7, RE2SiO5 where RE = Yb, Er, Y, Dy, Nd, Lu and Gd) environmental barrier coatings (EBCs) and the calcium RE silicate oxyapatite Ca2RE8(SiO4)6O2 (RE = Yb, Er, Y, Dy, Nd, Gd and Sm) corrosion products. Trends in the enthalpy of formation as a function of the ionic potential of the rare-earth cations in their related crystallographic sites are discussed.

Costa, Gustavo↗

Carbonatite metasomatism and water systematics of peridotite xenoliths from Lanzarote, Canaries

Water in Earth’s mantle, present as structural hydrogen in minerals, influences large scale processes like mantle deformation, plate tectonics, and melting. To better understand the processes controlling water concentrations in the Earth’s upper mantle, we analyzed hydrogen (calculated as ppm wt. H2O), major, and trace element concentrations in minerals from harzburgite xenoliths of Lanzarote, Canaries. Previous studies have shown evidence for carbonatite metasomatism in Lanzarote peridotites and carbonatite magmas have erupted in the Canaries. Thus, the Canaries offer a rare opportunity to examine the role of metasomatism and carbonatitic magmas in rehydrating the oceanic lithosphere during plume-lithosphere interaction. Major element data (obtained by electron microprobe) show that these peridotites are highly depleted compared to the primitive mantle, with a high average olivine Mg# (91.1 ± 0.5), low bulk rock Al2O3 (0.4 to 1.4 wt.%), high spinel Cr# (40 to 72) from which high degrees of melting were estimated (15 to 21%). There is no evidence of hydrous phases (e.g., amphibole and phlogopite), thus water in these peridotites is thought to be stored only in nominally anhydrous minerals and melt inclusions. Water concentrations (determined by polarized FTIR spectroscopy), in the peridotite silicate minerals range from 2.7 to 13 ppm in olivine, 42 to 265 ppm in orthopyroxene (Opx), and 76 to 470 ppm in clinopyroxene (Cpx). Reconstructed bulk rock water concentrations range from 5 to 115 ppm, generally lower than estimates for the depleted mantle (DM, 50-200 ppm). Trace element data in Opx, Cpx, and bulk rock frequently show high La/Yb ratios (up to 12.2, 71.5, 45.2; respectively) and strong negative Zr, Hf, and Ti anomalies relative to REE, consistent with carbonatite metasomatism. With decreasing Ti/Eucpx ratios, a proxy for carbonatite metasomatism, the bulk water increases. The calculated trace element compositions of melts in equilibrium with Cpx strongly resemble those of carbonatites. However, the bulk rock water concentrations are two magnitudes lower than what is expected by equilibrium with a carbonatite melt. Evidently, carbonatitic metasomatism did rehydrate of the Lanzarote mantle lithosphere but less so than expected, implying lower partitioning of H in the presence of CO2than a silicate melt.

S. Patterson↗

Durability of YSZ coated Ti2AlC in 1300°C high velocity burner rig tests

A thermal barrier coating system survived 500 h in cyclic burner rig tests at 1300°C, exceeding the life of all previous systems. An yttria stabilized zirconia (7YSZ) thermal barrier coating (TBC) was plasma sprayed on the oxidation resistant Ti2AlC MAX phase and tested in a jet fuel burner. No coating spallation or recession was observed, only a 2.4 mg/sq.cm mass gain due to typical cubic Al2O3 oxidation kinetics. The modest weight gain contrasted with large TBC spallation or oxide volatility losses that might occur under cyclic, high velocity (~100 m/s) burner conditions. The coating surface exhibited colonies of [111]flourite fiber-textured columns separated by craze crack patterns, but with no visible moisture attack. The thickness of the alumina scale under the YSZ face was >20 μm, more than twice that formed on TBC/superalloy systems at failure. TiO2 nodules, initially formed on the uncoated backside, were then removed as volatile hydroxides formed in high temperature, high velocity water vapor (~10%). Overall, the test indicated the exceptional stability of the YSZ/Ti2AlC system under turbine conditions, due in large part to good thermal expansion matching.

alumina, MAX phases, thermal barrier coatings (TBC↗

Secondary eclipses of WASP-18b – near-infrared observations with the Anglo-Australian Telescope, the Magellan Clay Telescope and the LCOGT network

We present new eclipse observations for one of the hottest ‘hot Jupiters', WASP-18b, for which previously published data from HST WFC3 and Spitzer have led to radically conflicting conclusions about the composition of this planet’s atmosphere. We measure eclipse depths of 0.15 ± 0.02 per cent at Ks and 0.07 ± 0.01 per cent at z′ bands. Using the VSTAR line-by-line radiative transfer code and both these new observations with previously published data, we derive a new model of the planetary atmosphere. We have varied both the metallicity and C/O ratio in our modelling, and find no need for the extreme metallicity suggested by Sheppard et al. Our best-fitting models slightly underestimate the emission at z′ band and overestimate the observed flux at Ks-band. To explain these discrepancies, we examine the impact on the planetary emission spectrum of the presence of several types of hazes which could form on the night side of the planet. Our Ks-band eclipse flux measurement is lower than expected from clear atmosphere models and this could be explained by haze particles larger than 0.2 μm with the optical properties of Al2O3, CaTiO3 or MgSiO3. We find that z′-band measurements are important for understanding the contribution of photochemical hazes with particles smaller than 0.1 μm at the top of the atmosphere.

L. Kedziora-Chudczer↗

Petrology, Geochemistry, and Pairing of Lunar Meteorites from the Dominion Range

Introduction: During the 2018-2019 Antarctic Search for Meteorites (ANSMET) field season in the Dominion Range (DOM), 7 lunar meteorite stones were collected: DOM 18242 (15.1 g), DOM 18244 (25.1 g), DOM 18262 (6.8 g), DOM 18509 (16.5 g), DOM 18543 (13.6 g), DOM 18666 (45.9 g), and DOM 18678 (11.6 g). Here we present the initial results of electron microprobe and X-ray computed tomography (XCT) studies of these stones and look at the details of their petrography and mineral chemistry, as well as investigate possible pairing relationships, both with each other and with previously described lunar meteorites. Most of the work presented here is on the DOM 18509, 18543, and 18678 stones; subsamples of the other stones are in hand and similar measurements will be made on them by the time of the meeting. Methods: Textures in DOM 18509, DOM 18543, and DOM 18678 were characterized in 2D by optical microscopy, backscattered electron (BSE) imaging and elemental X-ray images on thin sections, as well as in 3D by X-ray computed tomography (XCT) on sample chips. Mineral compositions were assessed through a combination of wavelength dispersive spectroscopy EPMA (electron probe microanalysis) and x-ray mapping on the JEOL 8530 at NASA JSC. The bulk composition of all three meteorites was determined based on analyses of the fusion crust glass. XCT analyses were done on the Nikon XTH 320 at NASA JSC. ICP-MS data on bulk rock subsamples for each meteorite will be carried out in the near future. Results: The stones are all similar in macroscopic appearance with a dark aphanitic matrix hosting a variety of small- to medium-sized angular mineral and lithic fragments (often light colored in nature) [1,2]. Based on EPMA and XCT results, the three meteorites are polymict regolith breccias comprised of mineral, glass, and lithic clasts ranging up to several mm in length. Melt veins run through all three meteorite samples. Mineral clasts in all 3 stones are dominated by pyroxene and plagioclase (An82-96), with minor amounts of SiO2, olivine (Fo1-52), and FeTi-oxides. Pyroxene grains are mostly Fe-rich pigeonite and augite, and larger clasts are normally zoned and have fine exsolution lamellae. The lithic clasts in all stones consists of: (1) basalt clasts that contain zoned pyroxene, plagioclase laths, and ilmenite, with minor silica and Fe-rich olivine; (2) granulitic clasts; (3) anorthosite clasts; (4) Si-rich clasts that also contain ilmenite, troilite, high-Ca pyroxene, fayalite, and K-feldspar likely mesostasis from late stage basalts). All three meteorites contain glassy fusion crust that is highly vesicular, high in FeO and Al2O3 (15-17 wt% each), ferroan (Mg# of 23-24), and moderately rich in TiO2 (1.4-1.8 wt%). The composition of the fusion crust can serve as a proxy for the bulk meteorite composition and is identical within error for all three meteorites. Implications: The lithic and mineral clasts in all three stones are similar in clast population and assemblages as well as mineral chemistry. In addition, the fusion crust composition, a proxy for bulk composition, is within error of each other for all three stones. Thus DOM 18509, DOM 18543, and DOM 18678 are almost certainly paired. Based on similarities in macroscopic description as well as preliminary classification data [1,2], all 7 lunar stones from DOM are likely paired, though additional quantitative analyses are needed to confirm this. The presence of spherules and vesicular fusion crusts indicates that the DOM pairing group is a regolith breccia. The presence of basaltic and gabbroic clasts as well as more feldspathic materials, suggest that the regolith from which these meteorites formed contained a mixture of feldspathic highland material and mare material, suggesting a possible provenance near a marehighlands boundary. No evidence of KREEPy lithologies have been observed so far in these meteorites, however, future ICP-MS data on bulk rock chips for the stones will reveal any KREEP component if present. The DOM pairing group has many similarities to previously described lunar breccia meteorite MET 01210, however more detailed compositional data will be needed to make a definitive comparison.

R.A. Zeigler↗

Ceramic Heat Pipe for Thermal Management of a High Frequency Inductor

As the power density of electric machines and power electronics continues to increase to meet the demands of more electric aircraft, the thermal management of these devices becomes increasingly important. Ideally, the thermal management solution of the device should have high thermal conductivity and be electrically insulating so that it can be directly integrated with the device in question. Technical ceramics are a class of materials that meet these two requirements. Direct liquid cooling by submerging electric components in a dielectric fluid is an alternate option, but adds system complexity and may incur pumping loss. In this work, the thermal management solution for a high frequency inductor is presented. A conventional wicked heat pipe is designed that is made from a solid ceramic case with a sintered ceramic wick. This heat pipe can provide structural support for the core and windings and is electrically insulating, so it does not incur any additional eddy current losses from the high frequency magnetic fields. It does not require additional pumping power, because conventional wicked heat pipes are passive devices. In this paper, the manufacturing process of the ceramic heat pipe is also presented. It is shown that the sintering of large diameter spherical ceramic particles is difficult due to their high specific surface area and low surface free energy. To overcome this difficulty, a flux material was used to initiate liquid phase sintering. The results of the sintering trials show that for the 120 μm diameter α-Al2O3 powder selected for the wick, the combination of 1650°C sintering temperature and the addition of 5 wt% talc sintered the porous matrix together sufficiently for use as a heat pipe wick.

High frequency inductor↗

Apollo Sample 64455: Petrologic and Geochemical Characterization of a Glass-Coated Impact Melt Rock

Introduction and Background: Impact melts are a key product of the impact cratering process. Impact melts can turbulently entrain pre-existing rock fragments, and melt part of those entrained materials until thermal equilibrium is achieved [1–3]. Lunar impact melt rocks are valuable for determining the precise ages of basin-forming and cratering events, which anchor the cratering chronology and dynamics of the entire solar system [4, and references therein]. Additionally, entrained clasts can inform on the petrology and age of crustal materials that predate the melt-forming impact. In lithologies where no pristine samples are available, entrained materials may hold the record of endogenous lunar volatiles, provided we can untangle their impact histories as high temperature impact melt can heat the clasts and may alter their native volatiles or isotopic signatures [5–6]. Here, we characterize an Apollo 16 sample, 64455,70B, in an effort to understand the physical, microstructural, and geochemical consequences of impact melt contact metamorphism. We acquired optical light and x-ray maps of the sample, as well as quantitative analyses via electron probe microanalysis (EPMA). These tasks allow us to better understand the interaction between impact melts and entrained clasts, ultimately closing knowledge gaps in high-temperature impact processing on planetary surfaces. Sample Description: Sample 64455 is an oblong crystalline rock encased in glass to form an egg-like shape [7–8]. The impact melt coating has altered the outer (1 to 2 mm) rind of the crystalline rock and has preserved schlieren. The interior crystalline rock is likely a crystalline impact melt rock based on its bulk Ir content of 2.25 parts per billion [9]. The composition of the impact melt glass rind cannot be solely derived from the crystalline interior, the glassy rind is more aluminous and less magnesian [10]. Neither the crystalline interior nor the glassy rind were radiometrically age dated, although several studies investigated its cosmogenic isotopes and exposure ages, which reveal the sample was exposed on the lunar surface for ~1–2 Ma [11–13]. Preliminary Results: The interior crystalline rock consists primarily of plagioclase with interstitial pyroxene and olivine. Plagioclase grains are zoned and compositions range from An97–89, while pyroxene compositions generally range from En68Fs19Wo13 to En82Fs15Wo3 and olivine are Fo77 to Fo85. Minor phases include Fe-Ni metal, Ca-phosphates, a K- and Si-rich phase, sulfides, and Fe-phosphides. The glass rind contains approximately 44 wt.% SiO2, 25 wt.% Al2O3, 6 wt.% FeO, 8 wt.% MgO, and 14 wt.% CaO, with other oxides at <1 wt.% each, although the composition of the glass becomes more variable closest to the crystalline rock. The rind consists of rounded plagioclase, pyroxene, and olivine crystals with interstitial melt. In some locations, the rounded crystals are surrounded by closely-packed, blade-like crystals, <5 µm in width. These results indicate that the crystalline interior has partially melted where in contact with the high-temperature impact melt and while further investigation is needed, pyroxene may have preferentially melted relative to olivine and plagioclase. Future Work: We plan to conduct electron backscatter diffraction (EBSD) mapping in order to determine crystallinity and crystal orientation. Next using transmission electron microscopy (TEM) data in conjunction with EBSD and EPMA information, we will model the diffusion of moderately volatile elements between the melt and remnant crystals.

A C Stadermann↗

Solid Particle Erosion of a Plasma Spray – Physical Vapor Deposition Environmental Barrier Coating in a Combustion Environment

Environmental barrier coatings (EBCs) were developed to reduce the susceptibility of SiC-based composites to the rapid volatilization and surface recession that occurs in the presence of water vapor. Extensive research and development has been performed on EBCs, and their corresponding failure mechanisms under different environmental conditions. However, one key failure mechanism, solid particle erosion (SPE), has not been thoroughly investigated. As a result, the present work investigates the SPE behavior of a ytterbium disilicate (Yb2Si2O7) environmental barrier coating (EBC) deposited via plasma spray-physical vapor deposition (PS-PVD). Erosion testing was performed at elevated temperature (1,200 °C) in a simulated combustion environment at the NASA Glenn Research Center Erosion Burner Rig Facility. Alumina (Al2O3) particles were used as the eroding media. A range of particle kinetic energies and impingement angles were investigated along with the effect of coating surface roughness. The post-erosion damage morphology was characterized using scanning electron microscopy (SEM). The SPE behavior of the PS-PVD EBC was shown to be comparable to other EBC systems reported in the literature.

Solid particle erosion; environmental barrier coat↗

Laboratory Investigation of the Effect of Venusian Weathering on Mineral Spectra

Introduction: The recent selection of two missions to Venus has renewed the importance of deter-mining weathering reactions between minerals and the Venusian atmosphere, and the spectral signatures of minerals before, during, and after these reactions. The rate at which weathering reactions progress also constrain show long unstable minerals will be present on the surface (e.g., [1]), and enables the use of mineralogy as a constraint on surface age(e.g., [2-3]).In order to gain an understanding of how mineral compositions and spectra change with weathering, we have begun conducting experiments in a 1 atm experimental setup at Wesleyan University. This setup exposes minerals to the temperature and most abundant gases of the Venus atmosphere (CO2, SO2, N2).We conducted initial experiments using biotite, calcite, and montmorillonite in order to test our methodology with minerals that may be relevant to recording the history of water on Venus. Methods: Experiments were conducted in Thermo Fisher Scientific Lindberg/Blue M Mini-Mite horizontal tube furnaces at Wesleyan University. Experiments used natural mineral chips and powders, and were conducted at 1 atmosphere and 460 °C under pre-mixed gases provided by Air Gas(Table 1). The furnaces are set up in a flow through configuration so that solid samples are exposed to a fixed gas composition, and quartz glass process tubes were used in all experiments (1/4” diameter for experiment V4, ½” diameter for all others). These conditions were maintained for the du-rations listed in Table 1, at which point the furnace was turned off with gas flowing until the sample was cool enough to extract under N2and be placed in a desiccator for storage. Run products were carbon coated and examined using a Hitachi SU5000 Field Emission Gun Scanning Electron Microscope (SEM) equipped with an EDAX Octane Pro EDS detector located at Wesley-an University. Visible-Near Infrared Spectroscopy (VNIR) analysis was performed on powdered samples under a nitrogen atmosphere using an ASD Fieldspec Proover the 350-2500 nm range. Powdered mineral samples were milled to a particle size of < 45μm and were spiked with an internal standard (Al2O3, corundum) to obtain quantitative mineralogy. Samples were analyzed using a Panalytical X’Pert pro X-ray Diffractometer (XRD), with an X’Celerator high speed detector and Co Kα radiation, with data collected at a step size of 0.02 ̊/minute step counting rate from 2 to 80 degrees 2θ at 45 mA/40kV in the X-ray Diffraction Laboratory located at NASA Johnson Space Center. Materials Data Inc (MDI) software suite, JadeTMv9 was used for Rietveld refinement to determine phase abundances and mineral identification by comparing XRD patterns to International Center for Diffraction Data (ICDD) database patterns. Table 1: Experimental matrix. Experiment Name Duration (Days)Gas Com-position (trace gas)MineralsV487SO2/N2(1.4%)Montmorillonite, biotiteV519SO2/N2(1.4%)CalciteV619CO2/SO2/N2(1.4% SO2, 2.1% N2)Montmorillonite, biotiteV828SO2/N2(1.4%)Biotite, calcite Results: Calcite. In both experiments, calcite was exposed to the SO2/N2gas mixture, and in both experimental run products, XRD analysis detected anhydrite, which is consistent with EDS measurements conducted in the SEM. The XRD analyses show greater amounts of anhydrite present after 28 days than 19, suggesting the calcite reaction progressed further given longer duration. Grain surface morphology as seen in the SEM also shows secondary mineral growth (Fig. 1). VNIR spectra show no change, as expected since anhydrite lacks spectral features in this wavelength range. Montmorillonite. Montmorillonite was exposed to two different gas mixtures, the SO2/N2mix and CO2/SO2/N2mix over different durations (87 and 19 days, respectively). VNIR analyses of both run products show a reduction in the 1441and1910 nm water features as well as a shift of the 1411 and 2011 nm features to shorter wavelengths that may indicate re-structuring in the crystal lattice and the production of amorphous phases [4]. XRD results are consistent with this, showing a shift of the 001 peak from 15Åto 10Åin both run products. The amount of X-ray amorphous material in the montmorillonite run products was greater than that present in the unreacted clay, being the greatest in the 87 day V4 experiment. No other secondary phases were detected in the run products, however sulfur was present in EDS analyses of powder samples.

A R Santos↗