Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ADDITIVES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 865 records · Page 48

The effect of additives on the speed of the crystallization front of xylitol with various degrees of supercooling

Some liquids can be kept in a supercooled or supersaturated metastable state for substantially long periods. Such liquids can be applied as long-term heat storage where the latent heat can be released when needed. As xylitol possesses a relatively high value of latent heat and as it can be easily supercooled, it has promising properties for this application. However, the speed of the crystallization of xylitol is low, leading to a low release rate of latent heat. Several additives have been experimentally tested for the purpose of accelerating the crystallization speed. The effect of the additives on the latent heat, on the melting temperatures, and on the long-term durability of the supercooled state was also measured. The highest speeds of the crystallization front, at a temperature of 22 C, were achieved with methanol as an additive leading to speeds 33 times higher in vertical experiments and in 170 times higher in horizontal ones than with pure xylitol. The improved speed of the crystallization front is mostly caused by the methanol flow currents generated as a result of the separation of methanol during crystallization, and to a lesser extent, as a result of the increase in the speed of the growth of the crystals. (author)

25 ENERGY STORAGE↗

Binder jet additive manufacturing method to fabricate near net shape crack-free highly dense Fe-6.5 wt.% Si soft magnets

High silicon (Si) electrical steel has the potential for efficient use in applications such as electrical motors and generators with cost-effective in processing, but it is difficult to manufacture. Increasing the Si content beyond 3 wt.% improves magnetic and electrical properties, with 6.5 wt.% being achievable. The main goal of this research is to design, develop, and implement a scalable additive manufacturing process to fabricate Fe with 6.5 wt.% Si (Fe–6Si) steel with high magnetic permeability, high electrical resistivity, low coercivity, and low residual induction that other methods cannot achieve because of manufacturing limitations. Binder jet additive manufacturing was used to deposit near net shape components that were subsequently sintered via solid-state sintering to achieve near full densification. Here, it is shown that the use of solid-state sintering mitigates cracking since no rapid solidification occurs unlike fusion-based additive technologies. The Fe–6Si samples demonstrated an ultimate tensile strength of 434 MPa, electrical resistivity of 98 μΩ cm, and saturation magnetization of 1.83 T with low coercivity and high permeability. The results strongly supports to replace the only available 0.1 mm thick chemical vapor deposition (CVD) produced Si steel using the cost effective AM method with good mechanical and magnetic properties for motor ap

36 MATERIALS SCIENCE↗

Convective heat transfer enhancement through additively built multiscale micro-tetrahedron features

Use of Additive Manufacturing (AM) to improve the heat transfer characteristics of tip shrouds in high-pressure turbines is being considered by industries. Existing designs of these components integrate micro-cooling channels to reduce the bulk temperature for improved life. In this research, closely packed micro tetrahedron features in addition to AM roughness has been considered. Further, this multiscale surface characteristics increased surface area per unit volume available for heat exchange. Micro-tet features were designed, manufactured, characterized, and evaluated systematically while increasing their height. An enormous increase in the overall wetted surface area by 200 % was measured. The convective heat transfer enhancement was ~3.72 times EDM rough coupon, and friction factor enhancement was ~5.5 times EDM rough coupon. Furthermore, the proposed design offers 2.5 times enhanced heat transfer for a given 2 W pumping power compared to our EDM rough coupon. Heat transfer enhancement was observed to not vary strongly with increased Reynolds number. Such complex designs are only possible through additive manufacturing for increased heat transfer with little pressure penalty. Finally, increasing the micro-tet height for increased surface area and improved heat exchange beyond an upper limit might not be a significant benefit as it gets compensated by increasing skin friction.

42 ENGINEERING↗

Fatigue behavior and modeling for additive manufactured 304L stainless steel: The effect of surface roughness

The fatigue strength of additively manufactured metallic parts in their as-built surface condition is mainly dominated by the surface roughness. Post-processing is often inevitable to reduce surface roughness effects even though post-processing diminishes the main advantage of additive manufacturing, which is net-shaped direct-to-service production. This work investigates the underlying mechanisms responsible for fatigue failure of additively manufactured 304L stainless steel parts in as-built and machined/polished surface conditions. Both strain- and force-controlled, fully reversed fatigue tests were conducted to gain a comprehensive understanding of surface roughness effects on fatigue behavior. The sensitivity to surface roughness is shown to be dependent on the control mode, with stress-based fatigue tests showing greater sensitivity than strain-based fatigue tests. Moreover, the fatigue life estimation for as-built specimens was performed based on surface roughness parameters as well as the fatigue properties of the specimens in machined/polished surface condition of the material without using any fatigue data of specimens in as-built surface condition. Accordingly, the effect of surface roughness on the fatigue behavior could be estimated reasonably well in both strain-life and stress-life approaches.

36 MATERIALS SCIENCE↗

Gradient process parameter optimization in additive friction stir deposition of aluminum alloys

As one of the most novel additive manufacturing methods, currently selection and optimization of processing parameters in additive friction stir deposition (AFSD) have mainly relied on experiments and subsequent characterization of microstructural and mechanical properties. Such approaches are both time- and resource-consuming. Therefore, an ultrasound elastography enhanced gradient process parameter optimization method was applied in the present work to obtain a window of optimized processing parameters for AFSD processing of aluminum alloy by varying both rotational and linear deposition speeds. Further, the quality of AFSD processed layer was investigated for physical nature of surface, dynamic elastic modulus, and microstructural aspects in cross-sections of the deposited layer. The efficiency in exploring process parameters was significantly enhanced by implementing a high-throughput screening experimental design based on application of gradient process parameters and continuous ultrasound elastographs. In addition, the applied ultrasonic elastography technique assisted in evaluating the homogeneity in microstructure and mechanical properties of AFSD sample over the entire gradients of the process parameters. The techniques adopted in current work can be further extended to identify suitable parameters for AFSD fabrication of components with desired mechanical properties such as hardness, fatigue, etc.

36 MATERIALS SCIENCE↗

Microstructure and high temperature properties of tungsten processed via electron beam melting additive manufacturing

There is considerable interest in the adoption of additive manufacturing for processing refractory metals. The layer-wise fabrication approach enables opportunities for producing complex geometries which cannot be otherwise be achieved via powder metallurgy. However, the processing science is still in its nascent stages and structure–property relations are relatively unexplored. Fundamental research is needed to further develop the technology and enable the fabrication of refractory metals for high temperature applications. Here we focus on the processing of pure tungsten using electron beam melting additive manufacturing. Experimentally we develop a suitable processing window for achieving high density crack free material. Microstructural analysis reveals that the microstructure generally consists of a columnar structure with a (111) build direction fiber preference, although, fiber switching was observed. Process induced deformation is believed to drive the formation of subgrains whose boundaries exhibit a high dislocation density. Additionally, high temperature tensile testing reveals that the material exhibits excellent properties closer to that of annealed tungsten. Significant mechanical anisotropy was observed to be present which is likely driven by strong crystallographic texture.

36 MATERIALS SCIENCE↗

In situ synchrotron X-ray imaging and mechanical properties characterization of additively manufactured high-entropy alloy composites

Laser beam directed energy deposition has become an increasingly popular advanced manufacturing technique for materials discovery as a result of the in situ alloying capability. In this study, we leverage an additive manufacturing enabled high throughput materials discovery approach to explore the composition space of a graded W x (CoCrFeMnNi) 100–x sample spanning 0 ≤ x ≤ 21 at%. In addition to microstructural and mechanical characterization, synchrotron high speed x-ray computer aided tomography was conducted on a W 20 (CoCrFeMnNi) 80 composition to visualize melting dynamics, powder-laser interactions, and remelting effects of previously consolidated material. Results reveal the formation of the Fe 7 W 6 intermetallic phase at W concentrations> 6 at%, despite the high configurational entropy. Unincorporated W particles also occurred at W concentrations> 10 at% accompanied by a dissolution band of Fe 7 W 6 at the W/matrix interface and hardness values greater than 400 HV. In this work, the primary strengthening mechanism is attributed to the reinforcement of the Fe 7 W 6 and W phases as a metal matrix composite. The in situ high speed x-ray imaging during remelting showed that an additional laser pass did not promote further mixing of the Fe 7 W 6 or W phases suggesting that, despite the dissolution of the W into the Fe 7 W 6 phase being thermodynamically favored, it is kinetically limited by the thickness/diffusivity of the intermetallic phase, and the rapid solidification of the laser-based process.

36 MATERIALS SCIENCE↗

On the existence of orthorhombic martensite in a near-α titanium base alloy used for additive manufacturing

Additive manufacturing is a state-of-the-art production technology to produce tailor-made and highly complex parts. Among various other alloys, Ti base alloys are frequently used in this manufacturing technique due to their well-balanced properties and their wide range of applications. Allotropic phases and the occurrence of athermal phase transformations are the main reasons why these alloys hold a great development potential and are the basis of extensive use. High cooling rates during manufacturing lead to martensitic phases and the formation of nanometer-sized microstructures resulting in extraordinary strength. Simultaneously, such high cooling rates cause a high amount of lattice defects and the occurrence of residual stresses, which finally may result in delamination effects and cracks. Usually, a common approach to reduce residual stresses during additive manufacturing is to decrease thermal gradients by increasing the heat input or preheating the building platform. Instead of applying the typical approaches to lower thermal gradients, this study deals with the origin of the ‘softer’ orthorhombic martensite by accelerating the solidification process. The implementation of the orthorhombic phase in bulk components was inspired by a new phase transformation herein reported for the first time in the powder material, which also validates the possible occurrence of two martensitic phases in the same alloy. Various sophisticated characterization techniques like high energy and high-temperature X-ray diffraction, high-resolution transmission electron microscopy as well as atom probe tomography were applied to characterize this softer orthorhombic martensitic phase in detail aiming to highlight the opportunities accompanied by this new approach for additive manufacturing of titanium alloys.

36 MATERIALS SCIENCE↗

Phase stability in cast and additively manufactured Al-rich Al-Cu-Ce alloys

Additively manufactured (AM) eutectic Al alloy systems have been studied extensively for advantageous thermal stability and mechanical properties due to their refined microstructures. Al-Cu-Ce alloys are one subset of these AM eutectic alloys. Here we studied phase stability in AM Al-Cu-Ce alloys and compared it to that of conventionally cast ones. A new phase, Al 8 Cu 3 Ce, was identified in the microstructures of both AM and cast Al-Cu-Ce alloys. This Al 8 Cu 3 Ce phase was not previously included on experimental or thermodynamically calculated phase diagrams of the Al-Cu-Ce system. Therefore, we performed additional thermodynamic modeling of the system. These models were experimentally validated with cast and subsequently heat-treated Al-Cu-Ce alloys. We found that despite the refined microstructure of the AM alloys, the phases formed were consistent with the cast alloys, suggesting that AM processing did not significantly alter the formation and stability of phases from that in the conventional alloys. In conclusion, this work has resolved inconsistent previous descriptions of the Al-Cu-Ce ternary phase diagram in the Al-rich region and resulted in the addition of the Al 8 Cu 3 Ce as an equilibrium phase above 500 °C.

36 MATERIALS SCIENCE↗

Heterogeneous phase transformation pathways in additively manufactured Al-Ce-Mn alloys

Heat treatment of additively manufactured Al-Ce based multicomponent alloys leads to complex microstructure evolution. In this research, the ability to extend the phase transformation theories involving nucleation of a product phase from a heterogeneous multi-phase microstructure typical to that of additively manufactured samples is explored. The Al-10Ce-8Mn (wt%) was used as a model alloy system. Under additive manufacturing conditions different solidification microstructures were obtained due to spatial and temporal variations of thermal gradients (G) and liquid-solid interface velocities (R) within a given melt pool. Near the melt pool boundary (high G and low R, referred as MPB region), initially, Al 20 Mn 2 Ce forms from the liquid followed by a eutectic of FCC Al and Al 11 Ce 3 . In the melt pool interiors (low G and high R referred as ES region) a eutectic structure between FCC Al and Al 20 Mn 2 Ce is observed. During subsequent heat treatments, the MPB and ES regions transform into different sets of microstructures. In the MPB region, a fine globular microstructure containing FCC Al, Al 11 Ce 3 , Al 6 Mn, and Al 12 Mn results from the decomposition of Al 20 Mn 2 Ce. In the ES region a faceted Al 51 Mn 7 Ce 4 plate phase results from the decomposition of Al 20 Mn 2 Ce. The formation of the Al 51 Mn 7 Ce 4 phase within the eutectic microstructure at the boundaries of FCC Al and Al 20 Mn 2 Ce has not been reported in the literature. Further, these two distinct phase transformation pathways are rationalized based on the role of driving force on the nucleation of (Al 6 Mn) and/or metastable intermetallic (Al 51 Mn 7 Ce 4 ) phases at the interface of aluminum (FCC) and the non-equilibrium intermetallic (Al 20 Mn 2 Ce) phases.

36 MATERIALS SCIENCE↗

Multi-material additive manufacturing of aluminum 6061-T6 alloy with stainless steel 304: Suppression of intermetallic compounds and interface growth mechanism

Fabricating integrated aluminum-steel structures is difficult because of metallurgical incompatibilities that promote intermetallic compound (IMC) formation at their interfaces. This work introduces a practical route for additively manufacturing 6061-T6 aluminum alloy (AA6061-T6) directly onto 304 stainless steel (SS304) using a high shear strain rate-assisted interfacial bonding mechanism. Through the friction extrusion deposition-based additive manufacturing method, both single- and multi-layer deposits of AA6061-T6 were successfully fabricated on SS304, yielding a robust hybrid multi-material structure. Comprehensive analyses of deposition quality, interface porosity, and bonding performance showed that the interface achieved a tensile strength exceeding 154 MPa under quasi-static loading. Microstructural observations revealed that the deposited aluminum layers experienced severe plastic deformation, resulting in pronounced grain refinement. Importantly, the interfacial zone was found to be free of brittle IMCs, instead containing a thin amorphous layer that evolved through a non-linear reaction-zone growth law. This solid-state additive strategy establishes a promising pathway for lightweight structural systems, nuclear energy component cladding, and multifunctional engineering components, redefining how dissimilar metals can be integrated for advanced applications.

Aluminum alloy↗

Observation of keyhole-mode laser melting in laser powder-bed fusion additive manufacturing

Laser powder-bed fusion additive manufacturing of metals employs high-power focused laser beams. Typically, the depth of the molten pool is controlled by conduction of heat in the underlying solid material. But, under certain conditions, the mechanism of melting can change from conduction to so-called “keyhole-mode” laser melting. In this mode, the depth of the molten pool is controlled by evaporation of the metal. Keyhole-mode laser melting results in melt pool depths that can be much deeper than observed in conduction mode. In addition, the collapse of the vapor cavity that is formed by the evaporation of the metal can result in a trail of voids in the wake of the laser beam. In this paper, the experimental observation of keyhole-mode laser melting in a laser powder-bed fusion additive manufacturing setting for 316L stainless steel is presented. Finally, the conditions required to transition from conduction controlled melting to keyhole-mode melting are identified.

36 MATERIALS SCIENCE↗

Evolution of carbide precipitates in Haynes® 282 superalloy processed by wire arc additive manufacturing

Precipitation hardening regulated with heat treatments is a critical technique for tuning the mechanical properties of Ni-based superalloys fabricated with additive manufacturing, where mechanical deformation is no longer viable for microstructural refinement. As one of the key precipitates, carbides prevail in the additively manufactured alloys, whose precipitation kinetics remain largely vague. This work studies the influence of heat treatments on the evolution of MC- and M 23 C 6 -type carbides within a Haynes® 282 superalloy prepared by wire arc additive manufacturing (WAAM). SEM-EDS analysis was performed to identify the evolution pathways of the carbides, and TEM and XRD characterizations were carried out to track the crystallographic features. The MC-type carbides are originally present in the as-printed alloy, which distribute uniformly across the whole material and remain largely unchanged in size during the heat treatments. By contrast, the incipiently non-existent M 23 C 6 -type carbides precipitate during an aging treatment at 1010 °C, which majorly extend along the grain boundaries as kinetically feasible sites. Further experimental and computational analysis confirms the enhancing effect of the M 23 C 6 -type carbides on the Vickers hardness. For the first time, this work revealed the evolution pathways of carbides within a Haynes® 282 superalloy prepared by WAAM, providing critical information for tunning the microstructure and mechanical properties. Finally, the carbide evolution kinetics established in this work can be potentially extended to other alloys prepared with WAAM, providing critical information to prevent mechanical failures associated with carbide coarsening.

36 MATERIALS SCIENCE↗

Performance of discontinuity-free components produced by additive turning computer aided manufacturing strategy

Computer aided manufacturing (CAM) techniques for directed energy deposition (DED) affect the material properties of the manufactured component based on the scan strategy used. In this study, we investigate the material characteristics of turning-style toolpath strategies to generate axisymmetric components with additive manufacturing (AM), referred to in this research as additive turning. This novel approach leverages existing CAM technology for turning, where the component rotates around a stationary cutting tool, to generate toolpath trajectories for DED with varying wall-thicknesses and controlled deposition angles. This strategy allows for entire components to be deposited in one continuous deposition, resulting in reduced cycle-time and improved material usage efficiency compared to conventional AM strategies where the beam is switched off at the end of every layer. Results from this study show that the use of additive turning can produce over 99 % dense components with less variation and anisotropy in texture and hardness, as well as a lower variation in elongation to failure when compared to conventional strategies. This research highlights that various CAM strategies could be deployed for AM to improve process efficiency or enable localized control over part performance.

36 MATERIALS SCIENCE↗

Effect of electrolyte additives in improving the cycle and calendar life of graphite/Li{sub1.1}[Ni{sub1/3}Co{sub1/3}Mn{sub1/3}]{0.9}O{sub 2} Li-ion cells.

Lithium-rich layered metal oxide Li{sub 1.1}[Ni{sub 1/3}Co{sub 1/3}Mn{sub 1/3}]{sub 0.9}O{sub 2} was investigated as a potential positive electrode material for high-power batteries for hybrid electric vehicle (HEV) applications. In order to evaluate the power and life characteristics of the graphite/Li{sub 1.1}[Ni{sub 1/3}Co{sub 1/3}Mn{sub 1/3}]{sub 0.9}O{sub 2} cell chemistry, hybrid pulse power characterization (HPPC) and accelerated calendar life tests were conducted on several pouch cells containing electrolytes with and without additives. The data show that the cells containing 0.5 wt% lithium bis(oxalate)borate (LiBOB) or vinyl ethyl carbonate (VEC) additives, or the novel lithium difluoro(oxalato)borate (LiDFOB) additive, have much improved cycle and calendar life performance.

25 ENERGY STORAGE↗

Effect of phosphorus additions on the sintering and transport properties of proton conducting BaZr{sub 0.85}Y{sub 0.15}O{sub 3-{delta}}

The influence of phosphorous additions on the sintering and electrical transport properties of the proton-conducting perovskite BaZr{sub 0.85}Y{sub 0.15}O{sub 3-{delta}} (BZY) has been studied with a view to the use of phosphates as typical dispersants for the formation of stabilised solid suspensions or as possible sintering aids. P{sub 2}O{sub 5} additions, (1-x)BZY{center_dot}xP{sub 2}O{sub 5}, monotonously promote densification in the intermediate compositional range 0.04{<=}x{<=}0.08. Nonetheless, BZY reacts with phosphorous forming the phase Ba{sub 3}(PO{sub 4}){sub 2} at temperatures as low as 600 Degree-Sign C. The associated loss of Ba from the perovskite, leads to a decrease in the perovskite lattice parameter, the formation of yttria-based impurity phases and impaired grain growth. Such reaction has an extremely detrimental effect on bulk and grain boundary conductivities. It is, therefore, vital that the current results are taken into account by the protonics community when attempting to prepare the stabilised solid suspensions of BZY nanopowders required for thin ceramic applications. Alternative dispersants to phosphate esters must be found. - Graphical Abstract: Sintering experiments performed at 1500 Degree-Sign C for 5 h and at 1400 Degree-Sign C for 24 h of (1-x)BaZr{sub 0.85}Y{sub 0.15}O{sub 3-{delta}}{center_dot}xP{sub 2}O{sub 5} in the range x=0-0.10. Highlights: Black-Right-Pointing-Pointer P{sub 2}O{sub 5} additions, (1-x)BZY{center_dot}xP{sub 2}O{sub 5}, promote densification in the intermediate compositional range 0.04{<=}x{<=}0.08. Black-Right-Pointing-Pointer BZY reacts with phosphorous forming the phase Ba{sub 3}(PO{sub 4}){sub 2} at temperatures as low as 600 Degree-Sign C. Black-Right-Pointing-Pointer Detrimental effects on bulk and grain boundary conductivities are shown. Black-Right-Pointing-Pointer Alternative dispersants to phosphate esters must be found.

36 MATERIALS SCIENCE↗

Effect of silver addition on the creep parameters of Sn-7 wt.% Bi alloy during transformation

The strain-time relations of Sn-7 wt.% Bi and Sn-7 wt.% Bi-1 wt.% Ag alloys have been obtained under different constant stresses (8.7-19.1 MPa) in the temperature range (313-373 K). The results showed that the transient and the steady state creep parameters n, {beta} and {epsilon}{sub st} depend on both the deformation temperature and the applied stress. The temperature dependence of these parameters indicates a transition temperature at 343 K. The Ag-free samples are more hard than those with Ag addition. This is explained by precipitation of Bi atoms which segregate to form a non-coherent cubic {alpha}-phase Sn-7 wt.% Bi samples. While, Ag addition prevents precipitation segregate on the grain boundaries. The analysis of the X-ray diffraction patterns shows that, Ag addition increases the Sn crystallite size but decreases Bi crystallite size. The energy activating the steady state creep in the two alloys in the low and high temperature ranges (before and after transformation temperature) were found to be 51.2 {+-} 1.6 and 88.1 {+-} 1.4 kJ/mol for Sn-7 wt.% Bi alloy and 34.3 {+-} 1.9 and 57 {+-} 1.8 kJ/mol for Sn-7 wt.% Bi-1 wt.% Ag alloy, respectively.

36 MATERIALS SCIENCE↗

Depressing effect of 0.1 wt.% Cr addition into Sn-9Zn solder alloy on the intermetallic growth with Cu substrate during isothermal aging

In this paper, the effect of 0.1 wt.% Cr addition into Sn-9Zn lead-free solder alloys on the growth of intermetallic compound (IMC) with Cu substrate during soldering and subsequent isothermal aging was investigated. During soldering, it was found that 0.1 wt.% Cr addition did not contribute to forming the IMC, which was verified as the same phase structure as the IMC for Sn-9Zn/Cu. However, during solid-state isothermal aging, the IMC growth was remarkably depressed by 0.1 wt.% Cr addition in the Sn-9Zn solder, and this effect tended to be more prominent at higher aging temperature. The activation energy for IMC growth was determined as 21.2 kJ mol{sup -1} and 42.9 kJ mol{sup -1} for Sn-9Zn/Cu and Sn-9Zn-Cr/Cu, respectively. The reduced diffusion coefficient was confirmed for the 0.1Cr-containing solder/Cu. Energy-dispersive X-ray mapping and point analysis also showed ZnCr phase existing in solder matrix, which can reduce diffusion rate of Zn atoms.

36 MATERIALS SCIENCE↗