Dispersion strengthened nickel-yttria sheet alloy produced from comminuted powders
Report on initial efforts to dispersion-strengthen nickel with Y2O3 in an attempt to replace radioactive ThO2 as the strengthening phase in dispersion-strengthened alloys. Nickel-Y2O3 powders were processed by the NASA comminution and blending (NASCAB) method and subsequently thermomechanically worked. Experimental variables included volume per cent Y2O3 (2% and 4%), powder cleaning temperature (315, 371, and 426 C), a screening step in the process, and the number (up to 23) of cold-roll-anneal cycles. Tensile strengths, determined at 1093 C, as well as some stress-rupture life data, are presented.