Some characteristics of polymers in composite materials and as electrical conductors

The characteristics of carbon fibers (CF) made from polyacrylonitrile (PAN) materials are discussed, together with research on conducting polymers. CF materials have better mechanical properties, chemical inertness, and higher stiffness than metallic materials but are subject to environmental instability, flammability, and delamination fatigue. Polymerization procedures for the monopolymer PAN are described, noting the use of SEM and X-ray diffraction techniques for studying the fiber structure. High modulus and strength of CF are caused by covalent sp(2) bonds in hexagonal carbon rings, which are stronger than the same links in diamonds. Details of the molecular chain structures and macroformations, stress-strain as a function of temperature, and thermosetting and glass transition temperatures of polymers are provided. Computational quantum chemistry techniques are being applied to studying electrical conductance in polymers, mainly to discover ways to stabilize the materials. Doped CH(x) has exhibited photovoltaic properties and other polymers have become superconductors at cryogenic temperatures.

Hansen, C. F.↗

An improved process for preparing Tris(N-methylamino)methylsilane monomer for use in producing silicon carbide-silicon nitride fibers

A technique is described for the preparation of tris(N-methylamino)methylsilane by a process which may be used for large-scale production. The steps include synthesis, filtration to remove the salt byproduct, and distillation to remove the product from the reaction mixture under anhydrous conditions. Tris(N-methylamino)methylsilane is a precursor used to prepare silicon carbide-silicon nitride fibers that have been shown to have high tensile modulus (29 x 10 to the 6th psi for 0.4 mil diameter), high tensile strength (10.5 x 10 to the 4th psi), and high electrical resistivity (7 x 10 to the 8th ohm-cm).

Penn, B. G.↗

Off-axis tensile properties and fracture in a unidirectional graphite/polyimide composite (Celion 6000/PMR 15)

Tensile properties of unidirectional Celion 6000 graphite/PMR 15 polyimide composites prepared by hot molding and cold molding processes were measured at room temperature and 316 C, the upper use temperature of the polyimide resin, at both 45 and 90 deg to the fiber axis. The resulting fractures were characterized by scanning electron microscopy and materialographic techniques. Variation in tensile properties with processing history occurred in the elastic modulus and strain to failure for specimens loaded at 90 deg at 316 C, and in the fracture stress, and hence the in-plane shear stress, for those loaded at 45 deg at room temperature. Significant plastic deformation was observed in the 45 deg orientation at 316 C for material produced by both processing methods. In general, fracture occurred by both failure within the matrix and at the fiber-matrix interface; the degree of interfacial failure increased with temperature. Secondary cracking below the primary fracture surface was also observed.

Harper, J.↗

Modification of epoxy-reinforced glass-cloth composites with a perfluorinated alkyl ether elastomer

A perfluorinated alkyl ether diacyl fluoride prepolymer (molecular weight about 1500) was coreacted with Epon 828 epoxy resin and diamino diphenyl sulfone to obtain an elastomer-toughened, glass-cloth composite. Improvements in flexural toughness, impact resistance, and water resistance, without loss of strength, modulus of elasticity or a lowering of the glass-transition temperature, were realized over those of the unmodified composite. Factors concerning optimization of the process are discussed. Results suggest that a simultaneously interpenetrating polymer network may be formed which gives rise to a measured improvement in composite mechanical properties.

Rosser, R. W.↗

Development of new and improved polymer matrix resin systems, phase 1

Vinystilbazole (vinylstryrylpyridine) and vinylpolystyrulpyridine were prepared for the purpose of modifying bismaleimide composite resins. Cure studies of resins systems were investigated by differential scanning calorimetry. The vinylstyrylpyridine-modified bismaleimide composite resins were found to have lower cure and gel temperatures, and shorter cure times than the corresponding unmodified composite resins. The resin systems were reinforced with commercially avialable satin-weave carbon cloth. Prepregs were fabricated by solvent or hot melt techniques. Thermal stability, flammability, moisture absorption, and mechanical properties of the composites (such as flexural strength, modulus, tensile and short beam shear strength) were determined. Composite laminates showed substantial improvements in both processability and mechanical properties compared to he bismaleimide control systems. The vinylstyrylpyridine modified bismaleimide resins can be used as advanced matrix resins for graphite secondary structures where ease of processing, fireworthiness, and high temperature stability are required for aerospace applications.

Hsu, M. S.↗

Fracture toughness of fibrous composite materials

Laminates with various proportions of 0 deg, 45 deg, and 90 deg plies were fabricated from T300/5208 and T300/BP-907 graphite/epoxy prepreg tape material. The fracture toughness of each laminate orientation or lay-up was determined by testing center-cracked specimens, and it was also predicted with the general fracture-toughness parameter. The predictions were good except when crack-tip splitting was large, at which time the toughness and strengths tended to be underpredicted. By using predictions, a parametric study was also made of factors that influence fracture toughness. Fiber and matrix properties as well as lay-up were investigated. Without crack-tip splitting, fracture toughness increases in proportion to fiber strength and fiber volume fraction, increases linearly with E(22)/E(11), is largest when the modulus for non-0 deg fibers is greater than that of 0 deg fibers, and is smallest for 0(m)/90(p)(s) lay-ups. (The E(11) and E(22) are Young's moduli of the lamina parallel to and normal to the direction of the fibers, respectively). For a given proportion of 0 deg plies, the most notch-sensitive lay-ups are 0(m)/90(p)(s) and the least sensitive are 0(m)/45(n)(s) and alpha(s). Notch sensitivity increases with the proportion of 0 deg plies and decreases with alpha. Strong, tough matrix materials, which inhibit crack-tip splitting, generally lead to minimum fracture toughness.

Poe, C. C., Jr.↗

The Chemical Nature of the Fiber/resin Interface in Composite Materials

Carbon fiber/epoxy resin composites are considered. The nature of the fiber structure and the interaction that occurs at the interface between fiber and matrix are emphasized. Composite toughness can be improved by increased axial tensile and compressive strengths in the fibers. The structure of carbon fibers indicates that the fiber itself can fail transversely, and different transverse microstructures could provide better transverse strengths. The higher surface roughness of lower modulus and surface-treated carbon fibers provides better mechanical interlocking between the fiber and matrix. The chemical nature of the fiber surface was determined, and adsorption of species on this surface can be used to promote wetting and adhesion. Finally, the magnitude of the interfacial bond strength should be controlled such that a range of composites can be made with properties varying from relatively brittle and high interlaminar shear strength to tougher but lower interlaminar shear strength.

Diefendorf, R. J.↗

Composite Structural Materials

The development and application of filamentary composite materials, is considered. Such interest is based on the possibility of using relatively brittle materials with high modulus, high strength, but low density in composites with good durability and high tolerance to damage. Fiber reinforced composite materials of this kind offer substantially improved performance and potentially lower costs for aerospace hardware. Much progress has been made since the initial developments in the mid 1960's. There were only limited applied to the primary structure of operational vehicles, mainly as aircrafts.

Ansell, G. S.↗

Creep of chemically vapor deposited SiC fibers

The creep, thermal expansion, and elastic modulus properties for chemically vapor deposited SiC fibers were measured between 1000 and 1500 C. Creep strain was observed to increase logarithmically with time, monotonically with temperature, and linearly with tensile stress up to 600 MPa. The controlling activation energy was 480 + or - 20 kJ/mole. Thermal pretreatments near 1200 and 1450 C were found to significantly reduce fiber creep. These results coupled with creep recovery observations indicate that below 1400 C fiber creep is anelastic with neglible plastic component. This allowed a simple predictive method to be developed for describing fiber total deformation as a function of time, temperature, and stress. Mechanistic analysis of the property data suggests that fiber creep is the result of beta-SiC grain boundary sliding controlled by a small percent of free silicon in the grain boundaries.

Dicarlo, J. A.↗

Fatigue behavior of continuous fiber silicon-carbide-aluminum composites

Four lay-ups of continuous fiber silicon carbide (SCS2) fiber/aluminum matrix composites were tested to assess fatigue mechanisms including stiffness loss when cycled below their respective fatigue limits. The lay-ups were 0 (sub 8), 0(sub 2)/ + or - 45 (sub 2s), 0/90 (sub 2s),and 0/ + or 45/90 (subs). The data were compared with predictions from the author's previously published shakedown model which predicts fatigue-induced stiffness loss in metal matrix composites. A fifth lay-up, + or - 45 (sub 2s), was tested to compare shakedown and fatigue limits. The particular batch of silicon-carbide fibers tested in this program had a somewhat lower modulus (340 GPa) than expected and displayed poor bonding to the aluminum matrix. Good agreement was obtained between the stiffness loss model and the test data. The fatigue damage below the fatigue limit was primarily in the form of matrix cracking. The fatigue limit corresponded to the laminate shakedown for the + or - 45 (sub 2s) laminate.

Johnson, W. S.↗

Transformation toughened ceramics for the heavy duty diesel engine technology program

The objective of this program is to develop an advanced high temperature oxide structural ceramic for application to the heavy duty diesel engine. The approach is to employ transformation toughening by additions of ZrO.5HfO.5O2 solid solution to the oxide ceramics, mullite (2Al2O3S2SiO2) and alumina (Al2O3). The study is planned for three phases, each 12 months in duration. This report covers Phase 1. During this period, processing techniques were developed to incorporate the ZrO.5HfO.5O2 solid solution in the matrices while retaining the necessary metastable tetragonal phase. Modulus of rupture and of elasticity, coefficient of thermal expansion, fracture toughness by indent technique and thermal diffusivity of representative specimens were measured. In Phase 2, the process will be improved to provide higher mechanical strength and to define the techniques for scale up to component size. In Phase 3, full scale component prototypes will be fabri-]cated.

Musikant, S.↗

Interaction between a crack and a soft inclusion

With the application to weld defects in mind, the interaction problem between a planar-crack and a flat inclusion in an elastic solid is considered. The elastic inclusion is assumed to be sufficiently thin so that the thickness distribution of the stresses in the inclusion may be neglected. The problem is reduced to a system of four integral equations having Cauchy-type dominant kernels. The stress intensity factors are calculated and tabulated for various crack-inclusion geometries and the inclusion to matrix modulus ratios, and for general homogeneous loadiong conditions away from the crack-inclusion region.

Xue-Hui, L.↗

Pultrusion Process for Fabrication of Tethers (preliminary Concepts)

Three composite materials were manufactured by the pultrusion process, coiled on 24 inch diameter spools for a period of two months, uncoiled and evaluated for memory recall. These materials were pultruded to lengths of approximately 150 feet and cross section profiles were maintained at 0.143 inch in thickness by 0.566 inch in width. Mechanical properties were studied and results compared. The reinforcement material volume percent of each was identical. Of the three systems, the Kevlar reinforced composite had the highest specific strength, the lowest flexural modulus, and the lowest memory recall. Further evaluations of materials and fabrication technology of pultrusion should be conducted to address some problem areas encountered in this preliminary concept. Areas for further study are suggested.

Macconochie, I. O.↗

Exploratory development of foams from liquid crystal polymers

Two types of liquid crystal polymer (LCP) compositions were studied and evaluated as structural foam materials. One is a copolymer of 6-hydroxy-2-naphthoic acid, terephthalic acid, and p-acetoxyacetanilide (designed HNA/TA/AAA), and the other is a copolymer of p-hydroxybenzoic acid and 6-hydroxy-2-naphthoic acid (designated HBA/HNA). Experimental results showed that the extruded HNA/TA/AA foams have better mechanical quality and appearance than HBA/HNA foams. Heat treatment improved foam tensile strength and break elongation, but reduced their modulus. The injection molding results indicated that nitrogen foaming agents with a low-pressure process gave better void distribution in the injection molded LCP foams than those made by the conventional injection-molding machine and chemical blowing agents. However, in comparing LCP foams with other conventional plastic foams, HBA/HNA foams have better mechanical properties than foamed ABS and PS, but are comparable to PBT and inferior to polycarbonate foams, especially in heat-deflection temperature and impact resistance energy. These deficiencies are due to LCP molecules not having been fully oriented during the Union-Carbide low-pressure foaming process.

Chung, T. S.↗

Finite Element Prediction of Loss Factors for Structures with Frequency-dependent Damping Treatments

A finite element procedure is described for calculating the loss factors for elastic structures to which frequency-dependent viscoelastic damping treatments were applied. The frequency dependence of the viscoelastic damping material is treated by approximating its shear modulus with a second-order polynomial so that the stiffnesses associated with the constant, linear, and quadratic terms can be combined, respectively, with the stiffness, damping, and mass matrices assembled for the rest of the structure. A single complex eigenvalue analysis is then performed in which the eigenvalues are purely imaginary. The loss factor is computed by the modal strain energy (MSE) approach. In the the MSE approach, the loss factor of a composite structure vibrating in one of its natural modes may be visualized as a weighted average of the loss factors of the component parts, with the relative stored energies as weighting constants. The finite element procedure, which can treat very general geometries, is illustrated for the case of a vibrating constrained-layer damped plate.

Everstine, G. C.↗

Formulation/cure technology for ultrahigh molecular weight silphenylene-siloxane polymers

Molecular weights above one million were achieved for methylvinylsilphenylene-siloxane terpolymers using a two-stage polymerization technique which was successfully scaled up to 200 grams. The resulting polymer was vulcanized by two different formulations and compared to an identically formulated commercial methylvinyl silicone on the basis of ultimate strength, Young's modulus, percent elongation at failure, and tear strength. Relative thermal/oxidative stabilities of the elastomers were assessed by gradient and isothermal thermogravimetric analyses performed in both air and nitrogen. The experimental elastomer exhibited enhanced thermal/oxidative stability and possed equivalent or superior mechanical properties. The effect of variations in prepolymer molecular weight on mechanical properties was also investigated.

Hundley, N. H.↗

Preparation of silicon carbide-silicon nitride fibers by the pyrolysis of polycarbosilazane precursors

The development of silicon carbide-silicon nitride fibers (SiC-Si3N4) by the pyrolysis of polycarbosilazane precursors is reviewed. Precursor resin, which was prepared by heating tris(N-methylamino)methylsilane or tris(N-methylamino)phenylsilane to about 520 C, was drawn into fibers from the melt and then made unmeltable by humidity conditioning at 100 C and 95 percent relative humidity. The humidity treated precursor fibers were pyrolyzed to ceramic fibers with good mechanical properties and electrical resistivity. For example, SiC-Si3N4 fibers derived from tris(N-methylamino)methylsilane had a tensile rupture modulus of 29 million psi and electrical resistivity of 6.9 x ten to the 8th power omega-cm, which is ten to the twelfth power times greater than that obtained for graphite fibers.

Penn, B. G.↗

The stress distribution in pin-loaded orthotropic plates

The performance of mechanically fastened composite joints was studied. Specially, a single-bolt connector was modeled as a pin-loaded, infinite plate. The model that was developed used two dimensional, complex variable, elasticity techniques combined with a boundary collocation procedure to produce solutions for the problem. Through iteration, the boundary conditions were satisfied and the stresses in the plate were calculated. Several graphite epoxy laminates were studied. In addition, parameters such as the pin modulus, coefficient of friction, and pin-plate clearance were varied. Conclusions drawn from this study indicate: (1) the material properties (i.e., laminate configuration) of the plate alter the stress state and, for highly orthotropic materials, the contact stress deviates greatly from the cosinusoidal distribution often assumed; (2) friction plays a major role in the distribution of stresses in the plate; (3) reversing the load direction also greatly effects the stress distribution in the plate; (4) clearance (or interference) fits change the contact angle and thus the location of the peak hoop stress; and (5) a rigid pin appears to be a good assumption for typical material systems.

Klang, E. C.↗