Whistler Mode Wave‐Driven Electron Scattering Properties From ELFIN Measurements of the Precipitation Ratio
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Evidence is presented for a close association betwen individual whistler ducts and conjugate ionospheric disturbances sensed by the perturbation of subionospheric VLF, LF, and MF signals. It is found that even the weakest whistlers can be associated with ionospheric disturbances in both hemispheres. A case study has shown that slow-onset and 'overshoot' perturbation signatures to be consistent with multiple ionospheric disturbances that are associated with individual components of multipath-ducted whistlers.
Aspects of convection dominated electrons in the auroral zone are considered, giving attention to the plasma sheet as the source of auroral electrons, the convection electron spatial distribution, the observed electron spatial distribution, and the coupling of convection and precipitation. Questions regarding geomagnetically trapped electrons are also investigated, taking into account the source of Van Allen electrons, the inward radial diffuse transport, the spatial structure of Van Allen electrons, electron slot formation, and the rapid loss of outer zone MeV electrons.
Ternary uranium molybdenum alloys are currently being investigated for use as dispersion and monolithic nuclear fuels in research reactors. In this study, two such ternary alloys, with compositions U-8Mo-3Nb and U-7Mo-3Ti in wt.%, were examined using scanning electron microscopy (SEM), X-ray diffraction (XRD), and transmission electron microscopy (TEM) with high angle annular dark field (HAADF) imaging via scanning transmission electron microscopy (STEM) to identify phase constituents. These alloys were homogenized at 950°C for 96 hours and were expected to be single-phase bcc-!-U. However, upon examination, it was determined that despite homogenization, each of the alloys contained a small volume fraction precipitate phase. Through SEM and XRD, it was confirmed that the matrix retained the bcc-!-U phase, but the precipitate phases could not be identified using these methods. TEM specimens were prepared using site-specific focused ion beam (FIB) in situ lift out (INLO) technique to include at least one precipitate from each alloy. By electron diffraction, the precipitate phases for the U- 8Mo-3Nb and U-7Mo-3Ti alloys were identified as bcc-(Mo,Nb) solid solution and bcc- (Mo,Ti) solid solution, respectively.
An experimental campaign designed to study high-latitude auroral arcs was conducted in Sondre Stromfjord, Greenland, on February 26, 1987. The Polar Acceleration Regions and Convection Study (Polar ARCS) consisted of a coordinated set of ground-based, airborne, and sounding rocket measurements of a weak, sun-aligned arc system within the duskside polar cap. A rocket-borne barium release experiment, two DMSP satellite overflights, all-sky photography, and incoherent scatter radar measurements provided information on the large-scale plasma convection over the polar cap region while a second rocket instrumented with a DC magnetometer, Langmuir and electric field probes, and an electron spectrometer provided measurements of small-scale electrodynamics. The large-scale data indicate that small, sun-aligned precipitation events formed within a region of antisunward convection between the duskside auroral oval and a large sun-aligned arc further poleward. This convection signature, used to assess the relationship of the sun-aligned arc to the large-scale magnetospheric configuration, is found to be consistent with either a model in which the arc formed on open field lines on the dusk side of a bifurcated polar cap or on closed field lines threading an expanded low-latitude boundary layer, but not a model in which the polar cap arc field lines map to an expanded plasma sheet. The antisunward convection signature may also be explained by a model in which the polar cap arc formed on long field lines recently reconnected through a highly skewed plasma sheet. The small-scale measurements indicate the rocket passed through three narrow (less than 20 km) regions of low-energy (less than 100 eV) electron precipitation in which the electric and magnetic field perturbations were well correlated. These precipitation events are shown to be associated with regions of downward Poynting flux and small-scale upward and downward field-aligned currents of 1-2 micro-A/sq m. The paired field-aligned currents are associated with velocity shears (higher and lower speed streams) embedded in the region of antisunward flow.
Sn–Bi solders may be applied for electronic applications where low-temperature soldering is required, i.e., sensitive components, step soldering and soldering LEDs. In spite of their potential to cover such applications, the mechanical response of soldered joints of Sn–Bi alloys in some cases does not meet the strength requirements due to inappropriate resulting microstructures. Hence, careful examination and control of as-soldered microstructures become necessary with a view to pre-programming reliable final properties. The present study aims to investigate the effects of solidification thermal parameters (growth rate — V{sub L} and cooling rate — T-dot{sub L}) on the microstructure of the Sn–52 wt.%Bi solder solidified under unsteady-state conditions. Samples were obtained by upward directional solidification (DS), followed by characterization through metallography and scanning electron microscopy (SEM). The microstructures are shown to be formed by Sn-rich dendrites decorated with Bi precipitates surrounded by a complex regular eutectic mixture, with alternated Bi-rich and Sn-rich phases. Experimental correlations of primary (λ{sub 1}), secondary (λ{sub 2}), tertiary (λ{sub 3}) dendritic and eutectic spacings (λ{sub coarse} and λ{sub fine}) with cooling rate and growth rate are established. Two ranges of lamellar eutectic sizes were determined, described by two experimental equations λ = 1.1 V{sub L}{sup −1/2} and λ = 0.67 V{sub L}{sup −1/2}. The onset of tertiary branches within the dendritic array along the Sn–52 wt.%Bi alloy DS casting is shown to occur for cooling rates lower than 1.5 °C/s. - Highlights: • The Sn–52 wt.%Bi solder was shown to have two eutectic sizes. • The fishbone eutectic is preferably located adjacent to the Bi-rich lamellar phases. • The onset of tertiary dendritic branches in Sn–Bi is associated with T-dot{sub L} < 1.5 °C/s. • Higher eutectic fraction and λ{sub 3} provoked a reverse increase in σ{sub u} and σ{sub y}.
Ferritic stainless steel is used as a coating for equipment in the petroleum refining industry. Welding is the main manufacturing and maintenance process used. However, little information on the metallurgical alterations caused by welding of these steels is found in the literature, prompting this study. In this study the authors evaluated the HAZ microstructure of AISI 444 ferritic stainless steel welded plates, by scanning electron microscopy (SEM) and X-ray diffraction (XRD). The results indicated that a weld thermal cycle caused microphase precipitation in the HAZ of the ferritic stainless steel. Also needle-like Laves phase precipitation occurred in the HAZ, near the partially-melted zone. Other secondary phases such as chi and sigma were observed, as well as nitride, carbide and carbonitride precipitates.
Energetic precipitating particles (EPPs) can cause significant direct constituent changes in the mesosphere and stratosphere (middle atmosphere) during certain periods. Both protons and electrons can influence the polar middle atmosphere through ionization and dissociation processes. EPPs can enhance HOx (H, OH, HO2) through the formation of positive ions followed by complex ion chemistry and NOx (N, NO, NO2) through the dissociation of molecular nitrogen. The HOx increases result in direct ozone destruction in the mesosphere and upper stratosphere via several catalytic loss cycles. Such middle atmospheric HOx-caused ozone loss is rather short-lived due to the relatively short lifetime (hours) of the HOx constituents. The NOx family has a considerably longer lifetime than the HOx family and can also lead to catalytic ozone destruction. EPP-caused enhancements of the NOx family can affect ozone directly, if produced in the stratosphere. Ozone decreases from the EPPs lead to a reduction in atmospheric heating and, subsequent atmospheric cooling. Conversely, EPPs can cause direct atmospheric heating through Joule heating. Measured HOx constituents OH and HO2 showed increases due to solar protons. Observed NOx constituents NO and NO2 were enhanced due to both solar protons and precipitating electrons. Other hydrogen- and nitrogen-ocntaining constituents were also measured to be directly influenced by EPPs, including N2O, HNO3, HO2NO2, N2OS, H2O2, ClONO2, HCl, and HOCl. Observed constituents ClO and CO were directly affected by EPPs as well. Many measurements indicated significant direct ozone decreases. A significant number of satellites housed instruments, which observed direct EPP-caused atmospheric effects, including Nimbus 4 (BUV), Nimbus 7 (SBUV), several NOAA platforms (SBUV/2), SME, UARS (HALOE, CLAES), SCISAT-1 (ACE-FTS), Odin (OSIRIS), Envisat-l (GOMOS, MIPAS, SCIAMACHY), and Aura (MLS). Measurements by rockets and ground-based radar also indicated EPP direct impacts. Atmospheric models have been used with some success in predicting the direct EPP impacts on the mesosphere and stratosphere. A review of the observed direct effects of EPP on the middle atmosphere will be given in this presentation.
We present observations from the Defense Meteorological Satellite Program and Reimei satellites, where common-volume high-resolution ground-based auroral imaging data are available. These satellite overpasses of ground-based all-sky imagers reveal the specific features of the electron populations responsible for different types of pulsating aurora modulations. The energies causing the pulsating aurora mostly range from 3 keV to 20 keV but can at times extend up to 30 keV. The secondary, low-energy electrons (<1 keV) are diminished from the precipitating distribution when there are strong temporal variations in auroral intensity. There are often persistent spatial structures present inside regions of pulsating aurora, and in these regions there are secondary electrons in the precipitating populations. The reduction of secondary electrons is consistent with the strongly temporally varying pulsating aurora being associated with field-aligned currents and hence parallel potential drops of up to 1 kV.
This report discusses work conducted at Idaho National Laboratory in fiscal year 2022 associated with the precipitates in Alloy 709 (A709). The purpose of this work is to support the development of the A709 Code Cases to qualify A709 in Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code. This would permit the use of A709 for elevated-temperature nuclear construction. This work encompassed two broad goals. The first goal was to understand the microstructure of the second commercial heat of plate A709 purchased through the Advanced Reactors Technologies Program in both the solution-annealed and precipitation-treated conditions. Transmission electron microscopy was utilized to characterize these microstructures. Direct comparisons were then made between the solution-annealed and precipitation-treated conditions as well as between the first and second commercial heats of plate A709. The second goal was to understand the impact of variations in the time and temperature of the precipitation treatment on the properties of A709. The precipitation treatment temperature was varied from 750°C to 800°C for times ranging from 3 hours to 30 hours. The hardness of each precipitation treatment variation was measured. All of the precipitation treatment variations investigated besides a specimen from the second commercial heat of plate A709 precipitation treated at 800? for 9 hours met the room-temperature hardness requirement specified in ASTM A213 and SA-213 for UNS S31025. The hardness measured for the specimen from the second commercial heat of plate A709 that was precipitation treated at 800? for 9 hours is considered an outlier. The next step is to look at the extremes of the precipitation treatment variations investigated and conduct elevated-temperature mechanical testing. The purpose of this testing would be to assess if these time and temperature variations have any impact on the mechanical performance.
In this study, the microstructural features of 7A52 heat-treatable aluminum alloys welded by variable polarity plasma arc (VPPA) combined with gas metal arc welding (GMAW) (VPPA–GMAW) were investigated and compared with those of 7A52 aluminum alloys welded by GMAW. The grain structures and modification of the precipitates were analyzed by optical microscopy and transmission electron microscopy. Complementary to modification of the precipitates, the precipitation evolution in the heat-affected zone and magnesium loss in the fusion zone were measured by differential scanning calorimetry and inductively coupled plasma spectroscopy. In VPPA–GMAW, the weld only needs one pass by depositing on one side of the 10-mm-thick aluminum alloy plates because of the large penetration capability of VPPA and good fluidity of the molten metal in the weld pool. Accordingly, the effect of excessive heat input on the microstructure can be minimized. The results show that the grain growth is not obvious and the magnesium loss is small in the fusion zone of VPPA–GMAW compared with that of GMAW under the condition of equal heat input to the workpiece. Small precipitates inside the grains remain homogeneously distributed, and a large volume fraction of the η′ phase exists. The VPPA–GMAW weld exhibits less tendency to soften; thus, VPPA–GMAW is appropriate for welding thick-plate aluminum alloys with a high production rate.
In this work the effect of electron irradiation on the mechanical properties of Bi2Sr2CaCu2O8 (Bi-2212) superconductor was studied by exposing the Bi-2212 superconductor with different doses of electron irradiation. Bi-2212 samples were prepared by using co-precipitation method. Irradiation was performed with irradiation dose of 100 kGray and 200 kGray, respectively. Characterization of the samples was performed by using X-Ray Diffraction (XRD) and Scanning Electron Microscopy (SEM). Instron Universal Testing machine was used to measure the strength of the samples. The XRD patterns for the non-irradiated and irradiated samples show well-defined peaks of which could be indexed on the basis of a Bi-2212 phase structure. XRD patterns also indicate that electron irradiation did not affect the Bi-2212 superconducting phase. SEM micrographs show disorientation in the texture of the microstructure for irradiated samples. Sample exposed to 200 kGray electron irradiation dose shows enhancement of grain size. Their grain growth and texture improved slightly compared to other sample. The results also show that enlargement of grain size resulted in higher mechanical strength.
The effect of the microstructure heterogeneity on the tensile plastic deformation characteristic of friction stir welded (FSW) 2024 aluminum alloy was investigated for the potential applications on light weight design of vehicles. The microstructure characteristics of the FSW joints, such as the grain structure, dislocation density and the distribution of precipitation, were studied by electron backscattered diffraction (EBSD) and transmission electron microscopy (TEM). The tensile deformation characteristic of the FSW joints was examined using the automatic strain measuring system (ASAME) by mapping the global and local strain distribution, and then was analyzed by mechanics calculation. It is found that the tensile deformation of the FSW joints is highly heterogeneous leading to a significant decrease in global ductility. The FSW joints mainly contain two typical deformation zones, which show great effect on the regional inhomogeneous deformation. One is the nugget zone (NZ) with a region of 8 mm in width, and the other is part of the BM with a region of 10 mm in width. The BM of the joints is the weakest region where the strain localizes early and this localization extends until fracture with a strain over 30%, while the strain in the NZ is only 4%. Differences in regional strain of FSW joints, which are essentially controlled by grain structure, the distribution of precipitation and dislocation density, result in decrease on the overall mechanical properties. - Highlights: Black-Right-Pointing-Pointer Microstructure heterogeneity of welds on tensile deformation behavior is studied. Black-Right-Pointing-Pointer The welds contain two typical deformation zones, affecting the global ductility. Black-Right-Pointing-Pointer Regional strain of welds is controlled by grain structure and dislocation density. Black-Right-Pointing-Pointer Theoretical calculation is in good agreement with experimental result.
We have studied the effect of sintering temperature on the structural and phase transformations of alloys produced by the spark plasma sintering of Ti + 23.5 at % Al + 21 at % Nb powder mixtures at temperatures in the range 1100–1550°C. The sintered alloys have been characterized by X-ray diffraction, scanning electron microscopy, and energy dispersive X-ray spectroscopy (elemental X-ray mapping). The alloys sintered at temperatures of 1100 and 1200°C have been shown to have a nonuniform microstructure. According to electron microscopy results, the alloys consist of grains of the α{sub 2} and Nb{sub 2}Al phases and small precipitates of the O-phase (intermetallic compound Ti{sub 2}AlNb). In addition, there are particles of unreacted niobium and titanium. The alloys sintered at a temperature of 1300°C have a uniform lamellar structure.
The hot working characteristics of {delta} phase in the delta-processed Inconel 718 alloy during isothermal compression deformation at temperature of 950 deg. C and strain rate of 0.005 s{sup -1}, were studied by using optical microscope, scanning electron microscope and quantitative X-ray diffraction technique. The results showed that the dissolution of plate-like {delta} phase and the precipitation of spherical {delta} phase particles coexisted during the deformation, and the content of {delta} phase decreased from 7.05 wt.% to 5.14 wt.%. As a result of deformation breakage and dissolution breakage, the plate-like {delta} phase was spheroidized and transferred to spherical {delta} phase particles. In the center with largest strain, the plate-like {delta} phase disappeared and spherical {delta} phase appeared in the interior of grains and grain boundaries.
Observations of the plasma-wave spectra from the four major outer planets are examined with particular attention given to the instabilities related to the precipitation of energetic particles. Wave-particle interactions involving hiss, chorus, and electron-cyclotron harmonic emissions are studied. These interactions contribute about 10 exp 13 W into the Jovian atmosphere, and the electron-cyclotron emissions on Saturn are shown to contribute significantly to the precipitation of energetic electrons. Whistler-mode waves are shown to exist at Uranus with intensities that could put 3-40 keV electrons on strong diffusion, but the amplitudes of the emissions are not sufficient to make them a significant part of precipitation. Weak electron-cyclotron harmonic emissions and whistler modes are detected at Neptune, suggesting that the present dataset is based on regions of low wave intensities.
Highlights: • Novel thermal barrier coating (TBC) with YSZ and ZrO{sub 2} + SiO{sub 2} + Al{sub 2}O{sub 3} eutectic ceramic top coat • TBC deposited via atmospheric plasma spraying and a hybrid water stabilized plasma torch spraying • Effect of eutectic ceramic TBC on LCF behaviour at 900 °C • Damage mechanisms in cyclic loading of cast nickel-based superalloy coated with TBC • The dislocation structures of a Ni-base superalloy were observed. - Abstract: Thermal barrier coatings (TBCs) are widely applied to protect high-temperature components against high temperatures in harsh environments. Nineteen cylindrical specimens of Inconel 713LC were manufactured using the investment castings technique, and 10 specimens were subsequently coated with a novel complex thermal barrier coating (TBC) system. The TBC system comprises a metallic CoNiCrAlY bond coat (BC) and a complex ceramic top coat (TC). The TC is a mixture of a near eutectic nanocrystalline ceramic made of zirconia (ZrO{sub 2}), alumina (Al{sub 2}O{sub 3}), silica (SiO{sub 2}) and conventional yttria stabilized zirconia (YSZ) ceramic in the ratio of 50/50 in wt%. Low cycle fatigue (LCF) tests were carried out in a symmetrical push-pull cycle under strain control at 900 °C. Cyclic hardening/softening curves, cyclic stress-strain curves and fatigue life curves of the TBC-coated and uncoated material were assessed. Fatigue life curves in total strain representation showed transient behaviour. Fracture surfaces and polished sections parallel to the loading axis of the TBC-coated and uncoated specimens prior and after cyclic loading were observed by means of scanning electron microscopy (SEM) to study the degradation mechanisms during high-temperature LCF. TBC delamination was observed at the TC/BC interface, and rafting of precipitates occurred after high-temperature exposure. The microstructural investigations further the discussion of the differences in the stress-strain response and the fatigue life of the TBC-coated and uncoated superalloy.
A series of base metal and cross-weld creep-rupture tests were conducted on the advanced austenitic alloy, HR6W, to evaluate the material for use at advanced ultrasupercritical (A-USC) steam conditions. Creep deformation and rupture were evaluated by traditional methods and data were compared with other studies to evaluate the creep response of the material. Optical and scanning electron microscopy revealed changes in failure mode and precipitation behavior. Thermodynamic predictions of phase stability were conducted and the results were compared with the experimental data. This research confirmed the important role of W and the precipitation of laves phase in the alloy system, but a direct relationship between laves phase content and creep strength was not observed. Furthermore, Cr content was investigated as an additional factor which may be important in the microstructural stability of the alloy which had not been previously considered. Finally, when compared to commercially available stainless steels, this heat of HR6W showed no creep strength advantage for A-USC application.