Conversion of near-ultraviolet radiation into visible and infrared emissions through energy transfer in Yb{sub 2}O{sub 3} doped SrO-TiO{sub 2}-SiO{sub 2} glasses
We demonstrated the conversion of near-ultraviolet radiation of 250-350 nm into visible emission of 450-600 nm and near-infrared emission of 970-1100 nm in the Yb{sub 2}O{sub 3} doped transparent 40SrO-20TiO{sub 2}-40SiO{sub 2} glasses. The observed broad visible emission band centered at 510 nm is associated with silicon-oxygen-related defects in the glassy matrix, and the near-infrared emission originated from the Yb{sup 3+} {sup 2}F{sub 5/2}{yields}{sup 2}F{sub 7/2} transition is due to the energy transfer from silicon-oxygen-related defects to Yb{sup 3+}. The energy transfer process was studied by both the steady state spectra and the time-resolved spectra of Yb{sup 3+} at 15 K. The temperature dependent energy transfer rate was calculated. The Yb{sub 2}O{sub 3} concentration dependent energy transfer efficiency has also been evaluated, and the maximum value is 56% for 12 mol % Yb{sub 2}O{sub 3} doped glass.