Strength of biaxially prestressed ceramic plates after nonuniform heating.
Biaxial prestressing in ceramic plates under nonuniform thermal stress for damage reduction study
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Biaxial prestressing in ceramic plates under nonuniform thermal stress for damage reduction study
Development of the plasma sprayed graded, layered ZRO2/CoCrAlY seal system for gas turbine engine blade tip seal applications up to 1589 K (2400 F) surface temperature was continued. The effect of changing ZRO2/CoCrAlY ratios in the intermediate layers on thermal stresses was evaluated analytically with the goal of identifying the materials combinations which would minimize thermal stresses in the seal system. Three methods of inducing compressive residual stresses in the sprayed seal materials to offset tensile thermal stresses were analyzed. The most promising method, thermal prestraining, was selected based upon potential, feasibility and complexity considerations. The plasma spray equipment was modified to heat, control and monitor the substrate temperature during spraying. Specimens were fabricated and experimentally evaluated to: (1) substantiate the capability of the thermal prestrain method to develop compressive residual stresses in the sprayed structure and (2) define the effect of spraying on a heated substate on abradability, erosion and thermal shock characteristics of the seal system. Thermal stress analysis, including residual stresses and material properties variations, was performed and correlated with thermal shock test results. Seal system performance was assessed and recommendations for further development were made.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Low alloy SA508 bainitic steel is often welded to 300 series austenitic stainless steel in nuclear power plants. These dissimilar metal weldments use 309L butter applied to the low alloy steel and 308L groove filler material to join the 309L to austenite. High alloy steels (such as the 308L and 309L material used here) have been identified as having greater susceptibility to irradiation-assisted stress corrosion cracking (IASCC). Evidence is presented here of cracking under tensile loads in 309L weldment butter in LWR hydrothermal conditions that correlates irradiation induced changes at δ ferrite–γ austenite phase boundaries and γ–γ grain boundaries; specifically intergranular Cr 23 C 6 precipitates. Cracking is not observed in irradiated 308L groove filler under the same conditions. Both the 309L butter and 308L filler material have a duplex or mixed δ–γ phase microstructure due to solidification during the welding procedure. We have performed constant extension rate autoclave immersion tests in BWR normal water chemistry hot water (288 °C, 10 MPa, 2000 wt. ppb dissolved oxygen, <100 nS/cm conductivity, neutral pH) of proton irradiated (2 MeV, approximately 3 displacements per atom at a depth of 10 μm) tensile specimens. Proton irradiation to the dpa levels used here induced Cr 23 C 6 carbide precipitation at γ–γ grain boundaries and δ–γ phase boundaries in the 309L butter but not the 308L filler. Cracking was observed in the proton-irradiated volume of 309L at these interfaces in the vicinity of the Cr 23 C 6 precipitates. We hypothesis the SA508 is the source of carbon in the 309L butter. Cr depletion at γ–γ grain boundaries was also observed and may also be a root cause of cracking. Furthermore, the 309L butter is under significant tensile residual stress in the weldment that adds to applied tensile loads and this too may be a contributing factor.
The influence of orientation on the tensile and stress rupture behavior of 52 Mar-M247 single crystals was studied. Tensile tests were performed at temperatures between 23 and 1093 C; stress rupture behavior was examined between 760 and 1038 C. The mechanical behavior of the single crystals was rationalized on the basis of the Schmid factor contours for the operative slip systems and the lattice rotations which the crystals underwent during deformation. The tensile properties correlated well with the appropriate Schmid factor contours. The stress rupture lives at lower testing temperatures were greatly influenced by the lattice rotations required to produce cross slip. A unified analysis was attained for the stress rupture life data generated for the Mar-M247 single crystals at 760 and 774 C under a stress of 724 MPa and the data reported for Mar-M200 single crystals tested at 760 C under a stress of 689 MPa. Based on this analysis, the stereographic triangle was divided into several regions which were rank ordered according to stress rupture life for this temperature regime.
Cu/Ag nanostructured multilayered films (NMFs) with different stacking sequences were investigated by synchrotron X-ray diffraction during the tensile deformations for interface stress study. The lattice strains were carefully traced and the stress partition, which usually occurs in the multiphase bulk metallic materials during plastic deformations, was first quantitatively analyzed in the NMFs here. The interface stress of the Cu/Ag NMFs was carefully analyzed during the tensile deformation and the results revealed that the interface stress was along the loading direction and exhibited three-stage evolution. This tensile interface stress has a detrimental effect on the deformation, leading to the early fracture of the NMFs.
The effects of two coatings, Codep B-1 and CoCrAlY, with and without simulated engine exposures at 982 C (1800 F) and 1093 C (2000 F), were evaluated on cast sections of Rene 80. Section thicknesses were from 0.075 cm (0.030 inch) to 0.15 cm (0.060 inch). Tensile and stress rupture properties, mechanical fatigue, thermal fatigue, ballistic impact and hot corrosion at R. T. and elevated temperatures were investigated. Thin sections generally had poorer tensile strengths and lower stress rupture lives than standard 1/4 inch round gage bars. The coatings, as-applied, had little effect on tensile strengths, rupture lives and mechanical fatigue and they increased thermal fatigue, ballistic impact and hot corrosion resistance. By providing considerable exposure protection to the Rene 80, the coatings improved all properties compared to exposed bare specimens.
Fatigue cracks often initiate from the surface extrusion/intrusions formed due to the operation of persistent slip bands (PSBs). Suppression of these surface topographical features by hard surface coatings can significantly extend fatigue lives under lower stress amplitudes (i.e., high cycle fatigue), while cracks initiate early in the coating or in the coating–substrate interface under higher stress amplitudes (i.e., low cycle fatigue), deteriorating the fatigue performance. However, both beneficial and detrimental effects of the coatings appear to be affected by the coating–substrate material combination and coating thickness. A quantitative understanding of the role of these factors in the fatigue performance of materials is still lacking. In this study, crystal plasticity simulations were employed to elucidate the dependence of the coating’s effects on two factors—i.e., the coating thickness and loading amplitudes. The results revealed that the thicker coatings more effectively suppress the operation of the PSBs, but generate higher tensile and shear stresses, normal and parallel to the interfaces, respectively, promoting interfacial delamination. The tensile stresses parallel to the interface within the coating, which favors coating fracture, are not sensitive to the coating thickness.
We report on an overlooked factor affecting stability: the residual stresses in perovskite films, which are tensile and can exceed 50 MPa in magnitude, a value high enough to deform copper. These stresses provide a significant driving force for fracture. Films are demonstrated to be more unstable under tensile stress—and conversely more stable under compressive stress— when exposed to heat or humidity. Increasing the formation temperature of perovskite films directly correlates with larger residual stresses, a result of the high thermal expansion coefficient of perovskites. Specifically, this tensile stress forms upon cooling to room temperature, as the substrate constrains the perovskite from shrinking. No evidence of stress relaxation is observed, with the purely elastic film stress attributed to the thermal expansion mismatch between the perovskite and substrate. Additionally, the authors demonstrate that using a bath conversion method to form the perovskite film at room temperature leads to low stress values that are unaffected by further annealing, indicating complete perovskite formation prior to annealing. It is concluded that reducing the film stress is a novel approach for improving perovskite stability, which can be accomplished by lower formation temperatures, flexible substrates with high thermal expansion coefficients, and externally applied compressive stress after fabrication.
The effect of aqua blasting and laser engraving on surface microstructure development, residual stress and corrosion resistance of type 316L stainless steel has been investigated. Aqua blasting resulted in a deformed near-surface microstructure containing compressive residual stresses. Subsequent laser engraving produced a surface layer with tensile residual stresses reaching to a depth of 200 microns. Changes of surface roughness topography were accompanied by the development of a thick oxide/hydroxide film after laser engraving. The atmospheric corrosion behavior of all surfaces with MgCl{sub 2}-laden droplets was compared to their electrochemical response in 1M NaCl and 0.7 M HCl aqueous solutions. The measured total volume loss after atmospheric corrosion testing was similar for all investigated surface conditions. Laser-engraved surface exhibited the smallest number of corrosion sites, but the largest mean corrosion depth.
Models for grain size dependence of flow stress typically ignore contributions from geometrically necessary dislocations (GNDs) in the grain boundary regions. Ashby had proposed the following equation for flow stress (τ) as a function of grain size (d) and effective plastic strain ($\bar{ε}$): $τ = τ_{0} + C'G\sqrt{^{b\bar{ε}}_{d}}$ using an unknown empirical coefficient, C’, In this study, the coefficient, C’, and equation for the grain size dependence of flow stress were investigated in Mg-4Al using nanoindentation. C’ ranges from 1.4 to 7.11 that is related to the hardness difference (∆H0) between the adjacent grains as $C' + 0.62\sqrt{ΔH_{0}}$. Ashby equation was used to predict uniaxial stress-strain curves in grain sizes of 55 µm, 187 µm, and 333 µm. The results showed lower flow stress and lower hardening rate compared to experimentally measured tensile stress-strain response. The discrepancy seems to be a result of hardening effect of SSDs. Here, we propose a modified Ashby equation that takes into account the hardening effect of SSDs and GNDs separately, resulting in a better agreement between calculated and experimentally measured values. This analysis demonstrates estimation of uniaxial stress-strain response using nanoindentation measurements that captures effects of grain size, and strain hardening from SSDs and GNDs. The combination of the revised equation and nanoindentation method will enable rapid exploration of stress-strain response of a diverse range of single-phase polycrystalline alloys.
The effect of surface processing by laser IR radiation on strength and Portevin–Le Chatelier serrated deformation of AlMg6 aluminum–magnesium alloy is experimentally studied. Laser processing consists in local “shots” on the surface at the nodes of a square grid in the gauge part of a flat sample. The conditions under which such laser processing causes an increase in the surface microhardness, ultimate tensile strength, and the critical strain of the first stress drop in the stress–strain curve; decreases the probability of deformation band formation; suppresses necking at the prefracture stage; and changes the main crack morphology. The possible mechanism of the effect of laser processing on band formation, serrated deformation, and alloy strength are discussed.
The intent of this testing was to evaluate the residual stresses that occur in and around the attachment details of a case stiffener segment that has been subjected to flight/recovery followed by proof loading. Not measured in this test were stresses relieved at joint disassembly due to out-of-round and interference effects, and those released by cutting the specimens out of the case segment. The test article was lightweight case stiffener segment 1U50715, S/N L023 which was flown in the forward stiffener position on flight SRM 14A and in the aft position on flight SRM24A. Both of these flights were flown with the 3 stiffener ring configuration. Stiffener L023 had a stiffener ring installed only on the aft stub in its first flight, and it had both rings installed on its second flight. No significant post flight damage was found on either flight. Finally, the segment was used on the DM-8 static test motor in the forward position. No stiffener rings were installed. It had only one proof pressurization prior to assignment to its first use, and it was cleaned and proof tested after each flight. Thus, the segment had seen 3 proof tests, two flight pressurizations, and two low intensity water impacts prior to manufacturing for use on DM-8. On DM-8 it received one static firing pressurization in the horizontal configuration. Residual stresses at the surface and in depth were evaluated by both the x-ray diffraction and neutron beam diffraction methods. The x-ray diffraction evaluations were conducted by Technology for Energy Corporation (TEC) at their facilities in Knoxville, TN. The neutron beam evaluations were done by Atomic Energy of Canada Limited (AECL) at the Chalk River Nuclear Laboratories in Ontario. The results showed general agreement with relatively high compressive residual stresses on the surface and moderate to low subsurface tensile residual stresses.
Tensile stress-rupture experiments were performed on woven Hi-Nicalon reinforced SiC matrix composites with BN interphases in air. Modal acoustic emission (AE) was used to monitor the damage accumulation in the composites during the tests and microstructural analysis was performed to determine the amount of matrix cracking that occurred for each sample. Fiber fractograph), was also performed for individual fiber failures at the specimen fracture surface to determine the strengths at which fibers failed. The rupture strengths were significantly worse than what would have been expected front the inherent degradation of the fibers themselves when subjected to similar rupture conditions. At higher applied stresses the rate of rupture "?as larger than at lower applied stresses. It was observed that the change in rupture rate corresponded to the onset of through-thickness cracking in the composites themselves. The primary cause of the sen,ere degradation was the ease with which fibers would bond to one another at their closest separation distances, less than 100 nanometers, when exposed to the environment. The near fiber-to-fiber contact in the woven tows enabled premature fiber failure over large areas of matrix cracks due to the stress-concentrations created b), fibers bonded to one another after one or a few fibers fail. i.e. the loss of global load sharing. An@, improvement in fiber-to-fiber separation of this composite system should result in improved stress- rupture properties. A model was den,eloped in order to predict the rupture life-time for these composites based on the probabilistic nature of indin,idual fiber failure at temperature. the matrix cracking state during the rupture test, and the rate of oxidation into a matrix crack. Also incorporated into the model were estimates of the stress-concentration that would occur between the outer rim of fibers in a load-bearing bundle and the unbridged region of a matrix crack after Xia et al. For the lower stresses, this source of stress-concentration was the likely cause for initial fiber failure that would trigger catastrophic failure of the composite.
High temperature mechanical measurements were conducted to study the effect of the dynamic precipitation process of PH 13-8 Mo maraging steel. Yield stress, ultimate tensile strength, total elongation, hardness, strain rate sensitivity and activation volume were evaluated as a function of the temperature. The dynamic changes in the mechanical properties at different temperatures were evaluated and a balance between precipitation hardening and annealed softening is discussed. A comparison between hardness and yield stress and ultimate tensile strength over a temperature range from 300 to 600 °C is made. The behavior of the strain rate sensitivity was correlated with the intermetallic precipitates formed during the experiments.
High temperature mechanical measurements were conducted to study the effect of the dynamic precipitation process of PH 13-8 Mo maraging steel. Yield stress, ultimate tensile strength, total elongation, hardness, strain rate sensitivity and activation volume were evaluated as a function of the temperature. The dynamic changes in the mechanical properties at different temperatures were evaluated and a balance between precipitation hardening and annealed softening is discussed. A comparison between hardness and yield stress and ultimate tensile strength over a temperature range from 300 to 600 °C is made. The behavior of the strain rate sensitivity was correlated with the intermetallic precipitates formed during the experiments.