Oxygen Effects and Selective Oxidation of Group IV Alloying Additions in Group V-Based Refractory Multi-principal Element Alloys

Refractory multi-principal element alloys (RMPEAs) hold significant potential for advancing ultra-high-temperature technologies due to their remarkable strength retention under these conditions. However, the beneficial effects of alloying on microstructural evolution and mechanical properties are often obscured by the presence of interstitial alloying elements. The intricate interactions between substitutional alloying elements of Groups IV, V, and VI and interstitial content, whether intentional or incidental, remain poorly understood. In this study, we investigate the impact of dissolved oxygen on the microstructural evolution and stability of RMPEAs primarily composed of Group V elements, Nb and V, along with Group IV elements Ti, Zr, and Hf. We show that the strong affinity of oxygen for Group IV elements Zr and Hf leads to the internal precipitation of oxides during heat treatment, which competes with the homogenization of the as-cast dendritic microstructure. Here, we demonstrate that careful control and design of oxygen content and Group IV alloying additions are essential to minimize micro-segregation and prevent the detrimental precipitation of internal oxides. To address these challenges, we propose employing non-equilibrium solidification calculations to predict and optimize as-cast solidification structures, thereby reducing the reliance on homogenization processes.

Alloy design↗

A Successful Synthesis of the CoCrFeNiAl0.3 Single-Crystal, High-Entropy Alloy by Bridgman Solidification

For the first time, a face-centered-cubic, single-crystal CoCrFeNiAl{sub 0.3} (designated as Al0.3), high-entropy alloy (HEA) was successfully synthesized by the Bridgman solidification (BS) method, at an extremely low withdrawal velocity through a constant temperature gradient, for which it underwent two BS steps. Specially, at the first BS step, the alloy sample underwent several morphological transitions accompanying the crystal growth from the melt. This microstructure evolves from as-cast dendrites, to equiaxed grains, and then to columnar crystals, and last to the single crystal. In particular, at the equiaxed-grain region, some visible annealing twins were observed, which indicates a low stacking fault energy of the Al0.3 alloy. Although a body-centered- cubic CoCrFeNiAl (Al1) HEA was also prepared under the same conditions, only a single columnar-crystal structure with instinctively preferential crystallographic orientations was obtained by the same procedure. A similar morphological transition from dendrites to equiaxed grains occurred at the equiaxed-grain region in Al1 alloy, but the annealing twins were not observed probably because a higher Al addition leads to a higher stacking fault energy for this alloy.

36 MATERIALS SCIENCE↗

Formation mechanisms of Sn-rich δ phase and its role in strengthening Cu-10Sn manufactured by laser powder bed fusion

Cu-Sn alloys produced via laser powder bed fusion (L-PBF) additive manufacturing (AM) have gained significant attention because they combine the advantages of AM relevant to intricate component design with outstanding combinations of strength, ductility, and resistance to wear and corrosion. However, a detailed understanding of the microstructure that contributes to the enhancement of the mechanical properties of L-PBF Cu-10Sn alloys remains unclear. In particular, there is a lack of understanding of the formation mechanisms of the Sn-rich δ phase commonly observed in Cu-10Sn. This study reveals two distinct variants of the δ phase possessing unique morphological characteristics. These characteristics are attributed to the local solidification conditions inherent to the melt pool boundaries versus those at the interiors of melt pools. A phase transformation pathway that elucidates the origin of the morphological variants of the δ phase from the Sn-rich metastable phases during the cyclic heating of the AM process is proposed. We report superior mechanical properties in L-PBF Cu-10Sn compared to those of conventionally manufactured counterparts due to the synergistic contributions from grain boundaries, dislocations, and the δ phase. Notably, the δ phase alone contributes approximately 22 % to the overall strength observed in the L-PBF Cu-10Sn alloy. The discovery of two types of distinct Sn-rich δ phase offers key insights into precise microstructural control in AM Cu-Sn alloys to enhance mechanical properties, providing practical strategies for improving material performance for diverse applications in automotive, aerospace, and machinery industries.

36 MATERIALS SCIENCE↗

Deformation Behavior of Pure Copper Castings with As-Cast Surfaces for Electrical Parts

Herein, the tensile deformation behavior of pure copper castings with as-cast surfaces was investigated. It was found that small and sufficiently large uniform elongation types corresponded, respectively, to the presence or absence of a Cu-Cu{sub 2}O eutectic phase in the microstructure. Fissure defects were observed near the as-cast surfaces when the eutectic phase was present, probably leading to stress concentration. On the other hand, surface pinholes were observed when the eutectic phase was absent, and these were not prevented by directional solidification. Although the as-cast specimens (non-directionally solidified) exhibited a slightly reduced uniform elongation compared to the machined specimens in the absence of the eutectic phase, the directionally solidified as-cast samples exhibited a uniform elongation that was similar to that of the machined specimens. In addition, micropore arrays were formed along the grain boundaries inside the castings when the eutectic phase was absent, whereas almost no micropores were observed inside the directionally solidified as-cast specimens because the solidification process involved a faster cooling rate and/or higher temperature gradient. These results do not only suggest the existence of surface pinholes but also indicate that microporosity can reduce the cross-sectional area of the specimens, thus, affecting their uniform elongation.

36 MATERIALS SCIENCE↗

Effect of melt spinning on grain size and texture in Ni-Mo alloys

Chill-block melt-spun ribbons of Ni-Mo alloys with Mo contents of 8 to 41.8 wt pct have been examined for microstructure and texture dependence on processing conditions. Linear features observed in grains solidified with a planar liquid-solid interface at the quench side of the ribbons have been identified to be due to the twins on the (111)gamma plane formed during solidification. Grain size variation with the wheel surface speed and the alloy composition has been studied. The crystallographic texture on the quench side and the free surface side of the ribbons has been investigated.

Tewari, S. N.↗

Establishing model credibility for process-microstructure-property relationships in additive manufacturing using exascale computing

Additive Manufacturing (AM) of alloys holds significant promise as a disruptive technology in various industries, yet its adoption is often hindered by challenges in achieving consistent part quality. These issues are primarily due to the complex process-microstructure-property (PSP) relationships inherent to AM. Computational models can greatly aid in understanding these relationships, but their widespread impact and adoption has been limited by a lack of validated, open-source, and computationally efficient PSP modeling frameworks and hardware limitations. Here, this study leverages the ExaAM software suite and data from the AMBench-2018 series of laser powder bed fusion (LPBF) benchmark experiments to perform a comprehensive model assessment, including verification, validation, sensitivity analysis, and uncertainty quantification. The RADICAL-EnTK workflow manager was used to perform an ensemble of heat transport, solidification, and mechanical response simulations on the exascale computer Frontier, considering uncertainties in critical model inputs such as laser spot size and nucleation parameters, and consisting of 125 explicit grain structure simulations and 7875 crystal plasticity simulations. For a selected location within the Inconel 625 AMBench-2018 test artifact, sensitivity analysis and uncertainty quantification were performed using the predicted distributions of grain structure and mechanical properties. Qualitative agreement was found between the predicted grain size and texture and the observed AMBench-2018 microstructure, the mean predicted yield stress was within 5% of the experimental measurement mean, and the mean predicted engineering stress at 5% strain was within 10% of the experimental measurement mean. The insights gained from development and validation of the ExaAM PSP modeling framework will help guide future directions for enhancing the credibility and reliability of PSP models in AM, thereby accelerating the adoption of AM technologies in various industries.

Additive manufacturing↗

Microstructures of niobium-germanium alloys processed in inert gas in the 100 meter drop tube

The 100 meter drop tube at NASA's Marshall Space Flight Center has been used for a series of experiments with niobium-germanium alloys. These experiments were conducted with electromagnetic levitation melting in a 200 torr helium environment. Liquid alloys experienced large degrees of undercooling prior to solidification in the drop tube. Several interesting metastable structures were observed. However, the recalescence event prevented extended solid solubility of germanium in the A-15 beta phase. Liquids of eutectic composition were found to undercool in the presence of solid alpha and solid Nb5Ge3.

Bayuzick, R. J.↗

Amorphous and nanocrystalline phase formation in highly-driven Al-based binary alloys

Remarkable advances have been made since rapid solidification was first introduced to the field of materials science and technology. New types of materials such as amorphous alloys and nanostructure materials have been developed as a result of rapid solidification techniques. While these advances are, in many respects, ground breaking, much remains to be discerned concerning the fundamental relationships that exist between a liquid and a rapidly solidified solid. The scope of the current dissertation involves an extensive set of experimental, analytical, and computational studies designed to increase the overall understanding of morphological selection, phase competition, and structural hierarchy that occurs under far-from equilibrium conditions. High pressure gas atomization and Cu-block melt-spinning are the two different rapid solidification techniques applied in this study. The research is mainly focused on Al-Si and Al-Sm alloy systems. Silicon and samarium produce different, yet favorable, systems for exploration when alloyed with aluminum under far-from equilibrium conditions. One of the main differences comes from the positions of their respective T 0 curves, which makes Al-Si a good candidate for solubility extension while the plunging T 0 line in Al-Sm promotes glass formation. The rapidly solidified gas-atomized Al-Si powders within a composition range of 15 to 50 wt% Si are examined using scanning and transmission electron microscopy. The non-equilibrium partitioning and morphological selection observed by examining powders at different size classes are described via a microstructure map. The interface velocities and the amount of undercooling present in the powders are estimated from measured eutectic spacings based on Jackson-Hunt (JH) and Trivedi-Magnin-Kurz (TMK) models, which permit a direct comparison of theoretical predictions. For an average particle size of 10 {micro}m with a Peclet number of ~0.2, JH and TMK deviate from each other. This deviation indicates an adiabatic type solidification path where heat of fusion is reabsorbed. It is interesting that this particle size range is also consistent with the appearance of a microcellular growth. While no glass formation is observed within this system, the smallest size powders appear to consist of a mixture of nanocrystalline Si and Al. Al-Sm alloys have been investigated within a composition range of 34 to 42 wt% Sm. Gas atomized powders of Al-Sm are investigated to explore the morphological and structural hierarchy that correlates with different degrees of departure from full equilibrium conditions. The resultant powders show a variety of structural selection with respect to amount of undercooling, with an amorphous structure appearing at the highest cooling rates. Because of the chaotic nature of gas atomization, Cu-block melt-spinning is used to produce a homogeneous amorphous structure. The as-quenched structure within Al-34 to 42 wt% Sm consists of nanocrystalline fcc-Al (on the order of 5 nm) embedded in an amorphous matrix. The nucleation density of fcc-Al after initial crystallization is on the order of 10 22 -10 23 m -3 , which is 10 5 -10 6 orders of magnitude higher than what classical nucleation theory predicts. Detailed analysis of liquid and as-quenched structures using high energy synchrotron X-ray diffraction, high energy transmission electron microscopy, and atom probe tomography techniques revealed an Al-Sm network similar in appearance to a medium range order (MRO) structure. A model whereby these MRO clusters promote the observed high nucleation density of fcc-Al nanocrystals is proposed. The devitrification path was identified using high temperature, in-situ, high energy synchrotron X-ray diffraction techniques and the crystallization kinetics were described using an analytical Johnson-Mehl-Avrami (JMA) approach.

36 MATERIALS SCIENCE↗

An additively manufactured AlCuMnZr alloy microstructure and tensile mechanical properties

In this study, selective laser melting (SLM) was used to fabricate an AlCuMnZr alloy. The microstructural features that resulted from additive manufacturing (AM) were significantly refined compared to the corresponding cast alloy features. A combination of fine equiaxed and columnar grains along with in-situ formation of θ' precipitates during AM leads to enhanced yield strength (up to 300°C) in the as-fabricated AM alloy. The refinement of brittle intermetallics and a bimodal grain size distribution leads to improved tensile elongation in the AM alloy. The results illustrate the microstructural advantages that can result from additive processing over conventionally processed microstructures.

36 MATERIALS SCIENCE↗

Directional solidification of alloys in systems containing a liquid miscibility gap

The problem considered is the unidirectional growth of alloys close to monotectic composition and within the miscibility gap when the direction of gravity is down the temperature gradient (solidification upwards) or up the temperature gradient (solidification downwards). The systems Al-In and Al-Bi are taken as examples. With solidification upwards it is shown that bulk liquid composition adjusts to that of the monotectic while in the reverse situation, the bulk liquid gradually rises. In the former case it is possible to grow aligned fibrous structures of monotectic composition but in the latter the microstructures are irregular and globular.

Grugel, R. N.↗

Effect of processing parameters and strut dimensions on the microstructures and hardness of stainless steel 316L lattice-emulating structures made by powder bed fusion

In this study, we present the effects of input processing parameters and strut thickness (in square struts) on microstructure and properties in laser powder bed fusion additively manufactured stainless steel 316L lattice-emulating structures. Lattice-emulating X-structures with square cross-sections of 1.5, 1.0, and 0.5 mm were fabricated using three different parameter sets with varying power, speed, and therefore, linear energy density. Grain size and morphology were shown to be dictated by epitaxial growth, which was dependent on weld pool morphology. Additionally, grain size and morphology were shown to change across the thickness direction of the struts (from the bottom inclined surface to the top inclined surface). The spatial variation in grain size was reflected by changes in hardness through the thickness of each strut. The 0.5 mm struts exhibited more significant grain elongation in the strut direction and larger sub-grain solidification cell diameters than their thicker counterparts. The larger sub-grain solidification cell diameters in the 0.5 mm samples resulted in correspondingly lower hardness values when compared to samples of higher thicknesses.

36 MATERIALS SCIENCE↗

Carbon nanotube (CNT) reinforced 316L stainless steel composites made by laser powder bed fusion: Microstructure and wear response

Carbon nanotube (CNT) reinforced 316L stainless steel (SS) composites were fabricated by laser powder bed fusion (LPBF) additive manufacturing (AM). This study focuses on microstructure evolution, hardness, and wear behavior. The wear behavior for AM 316L SS and 1 wt% CNT/316L SS was studied by a dry sliding test under normal loads of 10, 15, and 25 N. The addition of CNT to 316L SS led to the change of solidification mode from cellular/columnar to dendritic growth, producing grain refinement. Nanoscale dendrites were observed. Although TEM characterization confirmed the existence of CNT in cell interior, most CNT were damaged, resulting in carbon material segregation along cellular/dendritic boundaries. The wear rate was found dramatically decreased due to the improved hardness. Compared to the adhesive and abrasive wear in AM 316L SS, the wear mechanism of CNT/316L composite was adhesion and oxidative wear. Furthermore, enhanced cellular/dendritic boundary strengthening by carbon segregation was the main strengthening mechanism of CNT/316L composite.

36 MATERIALS SCIENCE↗

Numerical investigation of electromagnetic pulse welded interfaces between dissimilar metals

The quality of an electromagnetic pulse weld is strongly affected by a variety of interacting physical phenomena including large plastic deformation, materials mixing, localised heating and rapid cooling, and possible localised melting and interfacial cracks and void. In the present study, a thermomechanically coupled dynamic model has been developed to quantitatively resolve the high speed impact joining interface characteristics as well as the process induced interface temperature evolution, defect formation and possible microstructural composition variations. Reasonably good agreement has been obtained between the predicted results and the experimental measurements in terms of interfacial morphology characteristics. The modelling framework is expected to provide further understanding of the hierarchical interfacial features of the non-equilibrium material joining process and the weld formation mechanisms.

Xu, W.↗

Directionally Solidified Ceramics Produced

Produced Multiphase, interpenetrating structures are an alternative route to obtaining structural ceramic materials with adequate strength, toughness, and stability for high-temperature aerospace applications. The eutectic architecture, a continuous-reinforcing phase within a higher volume phase or matrix, can be described as a naturally occurring, in situ composite. The phases of a eutectic are thermodynamically compatible at high homologous temperatures. Strong and stable materials have been produced. Toughness, however, remains a technical obstacle. The potential for producing materials with enhanced toughness along with adequate strength and stability was demonstrated using the laser-heated float zone (LHFZ) growth method at the NASA Glenn Research Center at Lewis Field. LHFZ growth at Glenn provides a means to efficiently produce and record the underlying growth phenomena associated with two-phase structures. To initiate directional solidification, a seed of single-crystal sapphire (<0001> direction) was lowered onto the molten liquid until wetting occurred and then withdrawn at a constant rate. Neither the crystal nor the source rod was rotated. The materials produced were tested mechanically in tension, and the resulting microstructure was examined with a scanning electron microscope. Both the inherent properties of the constituent phases and the properties of the interface between them affect the mechanical behavior and the fracture surfaces. The following scanning electron micrographs show the microstructures of two different materials that were tested to failure in tension. In the left micrograph, the flat fracture surface is typical of a material that is strong but has low toughness. In the right micrograph, the crack is effectively deflected at the interface between the two phases, achieving higher toughness at moderately lower strength levels. Conducting mechanical tests to determine the high temperature properties of these materials is the next step in determining their eventual suitability.

Farmer, Serene C.↗

Microstructural and mechanical characterization of Al–Zn–Si nanocomposites

In this paper the addition of silicon nanoparticles into Al–Zn alloys to form metallic matrix nanocomposites by mechanical alloying process was investigated. The influence of various process parameters such as milling time and Si concentration in the Al–Zn matrix has an interesting effect on the microstructure and mechanical properties of the synthesized nanocomposites. The microstructural characterization of the nanocomposites was evaluated by transmission electron microscopy and energy dispersive X-ray spectroscopy (TEM–EDXS) and the mechanical properties were measured by nanoindentation and micro-hardness tests. The results showed that during mechanical milling Si is added to the Al–Zn matrix achieving a uniform and homogeneous dispersion. After solidification, it forms small particles of AlZnSi with blocky morphology in interdendritic regions. The nanoindentation profiles showed that the elastic modulus and hardness properties increase with increasing milling time. However, a high concentration of Si (> 1.2 wt.%) results in a saturation of Si in the Al–Zn matrix, which adversely affects the mechanical properties. Thus, it is important to tune the milling time and concentration of Si added to the Al–Zn alloys to control the growth of brittle phases that result in reduction of the mechanical properties of the material. - Highlights: • A novel technique for addition of Si nanocomposites into Al–Zn liquid alloy is reported. • Good dispersion and homogeneity of Si in the Al–Zn matrix are obtained. • Increasing Si content above 1.2 wt.% decreases the mechanical properties of Al–Zn alloy. • The saturation point of Si in 1.2 wt.% differs from Galvalume® composition. • The Al–Zn–1.5Si alloy with addition of nanocomposite shows 5.7 GPa of hardness.

36 MATERIALS SCIENCE↗

Rapid solidification of highly undercooled liquids

Melt undercooling is considered as a fundamental processing parameter for powders and for melt-spun and surface-melted samples. With reference to experimental results for Mn, Al, Al-Be, Al-Fe, and InSb-Sb powders, it is shown that the undercooling behavior in droplets is influenced by powder size, coating, melt superheat, and cooling rate. Droplet sample microstructures can be compared directly with those of rapidly quenched powders to establish the application of laboratory-scale studies to large-scale processing.

Perepezko, J. H.↗