Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Microstructure”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 829 records · Page 46

Manufacturing Li 2 TiO 3 -based tritium breeder materials by volume-controlled spark plasma sintering with an optimized microstructure

Multifunctional ceramic breeder materials are highly desirable for the deuterium-tritium fusion to achieve high efficiency in breeding tritium through neutron irradiation of lithium-containing blankets. Li 2 TiO 3 displays unique attributes as a potential ceramic breeder material. An optimized microstructure with three-dimensional interconnected pore structure is required for rapid transport of the tritium for effective fuel cycle, which however enviably results in the degradation of the thermal-mechanical properties of the breeding materials. In this work, nanocrystalline porous Li 2 TiO 3 ceramic pellets with controlled porosities of 14% and 20% are manufactured by volume-controlled spark plasma sintering. An optimized 3D interconnected pore structure is achieved consisting of both micro-sized pores and nano-sized pores embedded in nanocrystalline matrix, which could be beneficial to facilitate easy removal of bred T and He. Further, the 3D interconnected porous structure is well maintained upon isothermal annealing of the SPS-fabricated pellets at relevant operation temperature of the solid breeding materials. Single-phasic porous pellets also display enhanced thermal-mechanical properties, superior to current state-of-the-art materials which establish their potential as a promising tritium breeder material for nuclear fusion applications.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Metallic Technetium Sequestration in Nickel Core/Shell Microstructure during Fe(OH)2 Transformation with Ni doping

This study investigates the impacts of Ni doping on technetium-99 (Tc) sequestration in aqueous solutions through transformation of Fe(OH)2(s) to iron spinel (magnetite) under alkaline conditions. Extensive solid characterization was performed for the mineral phases produced, as well as the Tc/Ni speciation and distribution within these phases. X-ray diffraction results show that iron spinel was the dominant mineral product without detectable Ni incorporation. The doped Ni ions mainly precipitated as fine Fe/Ni oxide/hydroxide particles, including strongly reduced nanometer?sized spheroidal Ni-rich and metallic Ni phases. High-resolution analytical scanning transmission electron microscopy using energy dispersive X-ray spectroscopy and electron energy loss spectroscopy on the produced solid samples (focused ion beam-prepared specimens) revealed three Tc distribution domains dominated by nanocrystals and, especially, a Tc-rich metallic phase. Instances of metallic Tc were specifically found in spheroidal, Ni-rich and metallic nanoparticles exhibiting a core/shell microstructure that suggests strong reduction and sequential precipitation of Ni-Tc-Ni. Mass balance analysis showed nearly 100% Tc removal from the 4.8 × 10-4 M Tc solutions. The finding of the metallic Tc encapsulation indicates that Tc sequestration through Ni-doped Fe(OH)2(s)?to?iron spinel transformation process likely provides an alternative treatment pathway for Tc removal and could be combined into further waste treatment approaches.

Wang, Guohui↗

Microstructure and mechanical properties of ultrasonic spot welding of AA7075-T6 and A380 casting aluminum alloy

Ultrasonic spot welding (USW) was employed to join AA7075-T6 and casting Al alloy A380. Under a constant welding power, the influence of the welding time duration (from 1 s to 3 s) on peak temperature, microstructure, hardness, and mechanical strength of the joints were studied. It was found that the peak temperature increased with welding time. A sound solid-state metallurgical bonding was obtained at the joint interface. The cracks occurred at the edge of the joints were eventually eliminated as the welding time increased. A layer of refined grains formed in A380 adjacent to the bonding line. Further, hardness reduction occurred in AA7075 at the joint interface and the degree of hardness reduction and the volume increased with the peak temperature. By increasing welding time, lap shear tensile tests show that the peak load increased from 5.3 kN to 6.55 kN. The corresponding interfacial shear strength ranged from 96.29 MPa to 99.72 MPa, lower than the shear strength of both base materials (331 MPa for AA7075 and 185 MPa for A380). All joint samples exhibited interfacial fracture after lap shear tensile testing, with a thin layer of A380 remnant attached to AA7075 at the center of the fractured surface.

36 MATERIALS SCIENCE↗

Creep performance and microstructure of grade 91 steel weldments with integrated welding and thermal processing

Ferritic-Martensitic steel welds typically require post weld heat treatment (PWHT) to restore toughness and high temperature performance. This off-line thermal process reduces disparities between weld and base metal, but can cause distortion, cracking, or simply be impractical due to assembly size and joint non-uniformity. Here we show integrated welding and thermal processing applied to modified 9Cr-1Mo (Grade 91) steel, favored for advanced power generation applications, performed in real time through the addition of a secondary heat source near the primary weld head. Optimal integrated processing reduces weld fusion and heat affected zone hardness by 125 HV, approaching performance of conventional 730 °C, 60 min PWHT processing. Microstructures and mechanical performance are compared for mechanized GTAW welds, with equivalent lifetimes noted in cross-weld creep rupture tests up to 234 MPa at 550 °C, and up to 104 MPa at 650 °C. The integrated process was validated on a Grade 91 pressure vessel with multipass cold wire feed GTAW. After 550 °C, 71.4 bar thermomechanical cyclic testing, the maximum weld hardness is <350 HV.

36 MATERIALS SCIENCE↗

Correlation between microstructure and residual stress formation in friction stir welded armor steels characterized by neutron diffraction

Friction stir welding (FSW) is a solid-state joining process that minimizes the heat-affected zone (HAZ) compared with fusion-based arc welding, making it well suited for joining martensitic armor steels where hardness and ballistic resistance are critical. This study investigates residual stress formation in three defect-free FSW butt-joint configurations relevant to armored-vehicle fabrication: similar rolled homogeneous armor (RHA–RHA, Case 1), similar high-hardness armor (HHA–HHA, Case 2), and dissimilar HHA–RHA (Case 3) joints produced under temperature-controlled conditions (770 °C). Neutron diffraction was employed to quantify the magnitude and spatial distribution of residual stresses in the longitudinal, transverse, and normal directions and to correlate them with weld microstructure and hardness. Tensile residual stresses were concentrated in the softened HAZ, reaching approximately 300 MPa for Case 2 and 400 MPa for Case 1 (≈50–70 % of the base-metal yield strength; ∼581 MPa for RHA and ∼566 MPa for HHA), while compressive residual stresses dominated the stir zone. The spatial extent of tensile stresses scaled with the width of the softened HAZ, which was largest in the dissimilar HHA–RHA joint and smallest in the HHA–HHA joint. Full-width-at-half-maximum (FWHM) analysis revealed low microstrain in overtempered HAZ regions and high microstrain in the stir zone associated with severe plastic deformation and fresh martensite formation. This work demonstrates that residual stress evolution in FSW of martensitic armor steels is governed not primarily by peak temperature or thermal contraction, as inferred from fusion-welding analogies, but by the competition between transformation-induced volumetric expansion and tempering-induced stress relaxation. The relative dominance of these mechanisms is shown to depend on alloy hardenability and local thermal history, leading to more extensive HAZ softening and broader tensile stress regions in the lower-hardenability RHA steel. These findings establish a transferable mechanistic framework for optimizing solid-state joining strategies in high-strength steels and other transformation-hardening alloys beyond armor applications.

Friction stir welding↗

Effect of post-weld heat treatment on microstructure and mechanical properties of rotary inertia friction welded dissimilar 422-4140 martensitic steel piston joints

The study investigated how post‐weld heat treatment (PWHT) temperature affects the microstructure and localized deformation/fracture during bend testing of rotary inertia friction welds (RIFW) between AISI 422 stainless steel and AISI 4140 steel. RIFW produced a fully martensitic interface with approximately 550 HV hardness in both the thermo-mechanically affected (TMAZ) and heat‐affected zones (HAZ). Due to differences in temper resistance, the 4140 TMAZ/HAZ softened progressively under PWHT temperatures from 525 °C to 700 °C, while the 422 TMAZ unexpectedly maintained about 550 HV up to 600 °C before significantly softening at temperatures ≥625 °C. This asymmetric softening generated steep hardness gradients across the interface at temperatures ≤600 °C. Furthermore, carbon migration across the interface was minimal up to 600 °C, moderate at 625 °C, and by 700 °C produced a carbide‐rich eutectoid layer in the 422 TMAZ alongside a carbon‐depleted soft ferrite layer in the 4140 TMAZ. Strain during bending was PWHT‐dependent, concentrating on the 4140 side; in as-welded joints, the high hardness led to deformation and crack initiation in the base metals, whereas in PWHT samples, cracking initiated in the softened 4140 TMAZ near the interface. The intermediate PWHT temperature of 625 °C offered the best balance of limited carbon diffusion across the interface, relatively low peak weld hardness and minimized hardness gradients across the interface, more homogenous deformation, and good bend test performance.

4140 low-alloy steel↗

Effect of Ni content in Cu 1-x Ni x coating on microstructure evolution and mechanical properties of W/Mo joint via low-temperature diffusion bonding

The 93W and Mo1 refractory metals were bonded with different Cu 1- x Ni x coating interlayers of various Ni content using plasma-activated sintering at 700 °C. The effects of the Ni content in the Cu 1- x Ni x coating interlayer on the interfacial microstructure evolution and mechanical properties of the W/Mo joints were studied. The maximum average shear strength of the W/Mo joint was 316.5 MPa when the Ni content of the Cu 1- x Ni x coating interlayer was 25 %. When the Ni content of the Cu 1- x Ni x coating interlayer was below 50 %, the atomic diffusion at the W/Mo joint interface was adequate without the formation of intermetallic compounds, as demonstrated by the High Resolution Transmission Electron Microscope analyses of the joints. The presence of Ni in Cu 1- x Ni x promoted diffusion bonding at the interface, which contributed to the high mechanical properties of the W/Mo joint. With an increase in the Ni content of the Cu 1- x Ni x coating interlayer, the MoNi intermetallic compound (IMC) nucleated and grew at the Cu 1- x Ni x coating/Mo1 interface. When the Ni content of the Cu 1- x Ni x coating interlayer was above 50 %, the generation of a brittle MoNi IMC weakened the shear strength of the W/Mo joint dramatically.

36 MATERIALS SCIENCE↗

Microstructural evolution of a silicon carbide-carbon coated nanostructured ferritic alloy composite during in-situ Kr ion irradiation at 300°C 450°C

This work focuses on irradiation behaviors of a novel silicon carbide and carbon coated nanostructured ferritic alloy (SiC-C@NFA) composite for potential applications as a cladding and structural material for next generation nuclear reactors. The SiC-C@NFA samples were irradiated with 1 MeV Kr ions up to 10 dpa at 300 and 450 °C. Microstructures and defect evolution were studied in-situ at the IVEM-Tandem facility at Argonne National Laboratory. The effects of ion irradiation on various phases such as α-ferrite matrix, (Fe,Cr) 7 C 3 , and (Ti,W)C precipitates were evaluated. The α-ferrite matrix showed a continuous increase in dislocation density along with spatial ordering of dislocation loops (or loop strings) at >5 dpa. The size of the dislocation loops at 450 °C was larger than that at 300 °C. The nucleation and growth of new (Ti,W)C precipitates in α-ferrite grains were enhanced with the ion dose at 450 °C. This study provides new insight into the irradiation resistance of the SiC-C@NFA system.

(FeCr)(7)C-3↗

Microstructure and diffusion behavior of uranium fuel with minor additives

Fission product lanthanides in metallic fuels are known to cause adverse fuel-cladding chemical interaction (FCCI). Tin (Sn) and palladium (Pd) are being explored as the potential additives to reduce or mitigate lanthanide-induced FCCI by forming stable Sn-Ln and Pd-Ln compounds. The current study is an investigation of the fuel alloys, U–4Sn, U–4Sn-4Ln, U–4Pd, and U–4Pd-4Ln (wt. %), and their diffusion behaviors with Fe. Microstructural analysis was performed using scanning electron microscopy (SEM). Further, the binary phases in the UPd and USn alloys are identified as UPd 3 and suspected U 2 Sn, where U 2 Sn is unknown in the literature. The binary phases in the UPdLn alloy are identified as PdLn and Pd-rich Pd-Ln (Pd 4 Ln 3 and Pd 3 Ln 2 ), and in the USnLn alloy is SnLn. Diffusion of Fe with these binary phases is insignificant compared to the diffusion with U. The Ln-induced FCCI can be mitigated by the additives.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Tensile behavior and microstructural evolution of a Fe-25Ni-20Cr austenitic stainless steel (alloy 709) from room to elevated temperatures through in-situ synchrotron X-ray diffraction characterization and transmission electron microscopy

Uniaxial tensile tests were done on Fe-25Ni-20Cr Austenitic Stainless Steel (Alloy 709) along with in-situ synchrotron measurement at different temperatures (25 degrees C, 500 degrees C, 700 degrees C and 900 degrees C). The X-Ray diffraction data was collected in-situ in order to follow the phases present as well as to derive the dislocation density as a function of strain through peak broadening analysis based on the modified Williamson-Hall method and see how trends are affected as a function of temperature. The XRD data were complemented by TEM and STEM-EDX characterization done on the post-experiment samples to observe the deformed microstructures. Finally, the paper presents a depiction of the tensile behavior of this advanced steel by interpreting the stress-strain curves and the effect of temperature through the information gained by in-situ XRD and TEM observations as well as fractography done ex-situ on the samples tested to rupture.

36 MATERIALS SCIENCE↗

Effects of carbonitrides and carbides on microstructure and properties of castable nanostructured alloys

In this work, to develop advanced reduced-activation ferritic-martensitic (RAFM) steels for fusion reactor structural applications, both carbonitride- and carbide-strengthened castable nanostructured alloys (CNAs) were explored for higher densities of MX (M = Ti/Ta/V/etc. and X = C/N) nanoprecipitates. Additionally, systematic comparisons between the two types of CNAs indicated generally similar microstructures and comparable tensile properties and creep resistance. However, the carbide-CNAs did show some advantages over the carbonitride-CNAs in terms of the uniformly distributed higher density of MC nanoprecipitates, greater Charpy impact upper shelf energies, less deuterium retention and swelling, and potentially less transmutation-induced composition changes and consequently thermodynamically more stable carbides. The carbide-CNAs showed the best-balanced high performance in the examined properties, in contrast to the significantly varied performance of oxide-dispersion-strengthened alloys and the generally lower performance of current RAFM steels.

36 MATERIALS SCIENCE↗

Microstructure Evolution of U–Zr System in A Thermal Cycling Neutron Diffraction Experiment: Extruded U–10Zr (wt. %)

Microstructure evolution of 1073 K extruded U–10Zr (wt. %) fuel during thermal cycling (303–1073 K with a ~9 hour hold at 873 K during cooling) was investigated using in situ neutron diffraction. Analysis was performed using Rietveld texture and crystal structure refinements from time–of–flight neutron diffraction data, with a focus on the evolution of textures and lattice parameters as a function of temperature. The α–U phase exhibits lattice contraction with increasing temperature along the b lattice direction and lattice expansion in the other directions while the other phases exhibit lattice expansion with temperature in all directions. Contrary to the established phase diagram, the β–U phase is absent at the temperatures of the thermal cycling. (001) α and (110) γ plane normals are observed with a strong preferred orientation along the extrusion direction. Finally, the variant selection of (001) α ||(110) γ is observed for the first time.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Modified microstructures in proton irradiated dual phase 308L weldment filler material

In this study, the effect of proton irradiation on the microstructure of δ ferrite—γ austenite mixed phase 308L filler material in a 508–304 dissimilar metal weldment was investigated over a depth of 0 to 10 µm. Ni–Si–Mn G-phase precipitates were observed with SEM and TEM in δ ferrite but not in γ austenite. Our density functional theory based calculations show that the G/Fe interface energy in δ-Fe is significantly lower than that in γ-Fe (0.35 versus 1.25 J/m 2 ), which provides a thermodynamics-based explanation for our experimental observations of preferential formation of G-phase in δ ferrite. STEM-EDS, TEM dark field imaging, and diffraction patterns confirmed the Ni–Si–Mn enriched precipitates were G-phase precipitates with a stoichiometry of Mn 6 Ni 16 Si 7 . Intragranular voids and Ni–Si enriched clusters were observed in irradiated γ austenite. Additionally, Ni and Si segregation was observed along the void interfaces. In both cases, Ni–Si clusters and segregation to voids, selected area diffraction patterns did not reveal the existence of a second phase. Proton irradiation induced Cr depletion and Si and Ni enrichment at γ-γ austenite grain boundaries that was characterized with STEM/EDS.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Temperature and time effects of post-weld heat treatments on tensile properties and microstructure of Zircaloy-4

Opportunities exist to expand the application of Zircaloy-4 (Zry-4) into lower-temperature (<100°C) applications. Welded areas within these structures are potential failure points and post-weld heat treatments (PWHTs) are not yet standardized for application in this temperature range. Zry-4 tungsten inert gas (TIG) welds were given PWHTs from 450-900°C with hold times from 0.5-48 hours to investigate changes to tensile properties and microstructure. Treatment of 800°C for 1 hour was found to produce the most ductile material, measured by total elongation of the tensile bar (16.5%). Furthermore, both PWHT time and temperature were observed to increase total elongation, except in extreme (>800°C or >18hours) cases, but the effect of temperature was stronger. The second order cumulative annealing parameter shows a trend with tensile properties. Average grain sizes in the fusion zone and heat affected zone did not change under any of the PWHTs until the development of an undesirable blocky-alpha phase, which was only observed to form in the heat affected zones for hold times greater than 18hr at 800°C.

36 MATERIALS SCIENCE↗

Microstructural and crystallographic effects of sol-gel synthesized Ti-doped UO 2 sintered under reducing conditions

Titanium (Ti)-doped UO 2 microspheres of three different Ti concentrations (1000, 2000, and 4000 wppm) were synthesized using an internal gelation process. The microspheres were pressed into pellets, and a two-step heat treatment was applied to form monolithic cylindrical pellets with high densities (≥95%TD). Microstructure of these samples consisted of equiaxed grains with >300% increase in average grain size compared to the undoped UO 2 pellets. Secondary Ti-rich chemical phases corresponding to a liquid eutectic formed during sintering were observed at grain boundaries of UO 2 for samples doped with 4000 wppm Ti. Furthermore, these Ti-rich chemical phases were not observed in 1000 or 2000 wppm Ti samples at microscale using electron microscopy investigations. The 0.02–0.04% lower lattice parameter values for the Ti-doped UO 2 samples compared to the undoped UO 2 confirms the incorporation of Ti into the UO 2 lattice.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Emulation of neutron damage with proton irradiation and its effects on microstructure and microchemistry of Zircaloy-4

This work assesses the potential of proton irradiation to simulate the neutron damage to the matrix and laves phase Zr(Fe,Cr) 2 precipitates in Zircaloy-4. Isothermal proton irradiation has been performed on Zircaloy-4 samples at irradiation temperatures ranging from 250 to 350 °C. Two-step proton irradiation was also performed to enhance the amorphization of and iron loss from the laves phase Zr(Fe,Cr) 2 precipitates. The irradiated microstructures, including dislocation loops and rafts near SPPs, were observed in proton irradiated Zircaloy-4, which are consistent with neutron irradiated material at a similar damage level. The amount of irradiation-induced hardening after proton irradiation was similar to post neutron irradiated data. The significant amorphization of the SPPs and concurrent Fe redistribution observed on neutron irradiated materials can be effectively emulated using a two-step proton irradiation on Zircaloy-4. Hence, the neutron irradiation effect on Zircaloy-4 can be mostly captured using the two-step proton irradiation described in this study.

36 MATERIALS SCIENCE↗

Unveiling microstructure-property correlations in nuclear materials with high-energy synchrotron X-ray techniques

Understanding the microstructure-property correlation is critical for the performance evaluation of in-service materials and the development of advanced materials for nuclear reactor applications. Experimental studies are challenging for nuclear materials which are often hazardous. Recent developments in high-energy synchrotron X-ray (HEX) techniques offer the potential to address this challenge, by providing direct observations of internal responses to external stimuli in bulk-like materials, through in situ or 3D measurements. Here, in this review, developments in HEX techniques are introduced and recent applications in nuclear materials are presented. The results offer unprecedented insights into materials performance and provide unique input to computational models.

36 MATERIALS SCIENCE↗

Microstructure analysis of laser beam weldments performed on neutron-irradiated 304L steel containing 3 and 8 appm helium

We report that AISI 304 L austenitic stainless steel is one of the major structural materials used in light water reactors (LWRs). In the future, 304 L components may require repair, and several welding techniques have been proposed as candidates. In this study, laser beam welding using the low-energy contribution approach was performed in ~2016 on neutron-irradiated AISI 304 L steel with nominal values of 3 and 8 appm helium (He). The goal was to investigate the impact of helium on the irradiated material weldability and evaluate helium-associated damage. The weld and heat-affected zone (HAZ) microstructure was studied using scanning electron microscopy, electron backscatter diffraction, and transmission electron microscopy (TEM). Analysis of the weldment cross-sections did not reveal severe cracking. Still, evidence of incipient helium-associated damage was observed in the HAZ, manifesting as degraded grain boundaries (GBs) “decorated” by pore chains and mostly small (i.e., ≤ 25-30 µm) scattered cracks. The largest observed crack was ~50 µm in length. Helium-associated damage was localized within ~200-300 µm of the weld pool boundary, and the fraction of the compromised GBs, as a rule, was below ~9-11% of the total GB network. TEM analysis showed significant annealing of the radiation-induced defects at distances up to ~300 µm from the weld pool boundary. Inside the HAZ, the cavities (likely, helium bubbles) tended to form at GBs and inclusions, such as manganese sulfide precipitates in the grain interior. Crystallography analysis of the HAZ damage showed that random high-angle boundaries were most susceptible to helium-associated damage. In contrast, low-angle random boundaries and twin boundaries appeared to be strongly resistant to degradation from the combined effects of helium and welding.

36 MATERIALS SCIENCE↗