Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CORROSION PROTECTION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 829 records · Page 46

Engineering Glass Passivation Layers -Model Results

The immobilization of radioactive waste into glass waste forms is a baseline process of nuclear waste management not only in the United States, but worldwide. The rate of radionuclide release from these glasses is a critical measure of the quality of the waste form. Over long-term tests and using extrapolations of ancient analogues, it has been shown that well designed glasses exhibit a dissolution rate that quickly decreases to a slow residual rate for the lifetime of the glass. The mechanistic cause of this decreased corrosion rate is a subject of debate, with one of the major theories suggesting that the decrease is caused by the formation of corrosion products in such a manner as to present a diffusion barrier on the surface of the glass. Although there is much evidence of this type of mechanism, there has been no attempt to engineer the effect to maximize the passivating qualities of the corrosion products. This study represents the first attempt to engineer the creation of passivating phases on the surface of glasses. Our approach utilizes interactions between the dissolving glass and elements from the disposal environment to create impermeable capping layers. By drawing from other corrosion studies in areas where passivation layers have been successfully engineered to protect the bulk material, we present here a report on mineral phases that are likely have a morphological tendency to encrust the surface of the glass. Our modeling has focused on using the AFCI glass system in a carbonate, sulfate, and phosphate rich environment. We evaluate the minerals predicted to form to determine the likelihood of the formation of a protective layer on the surface of the glass. We have also modeled individual ions in solutions vs. pH and the addition of aluminum and silicon. These results allow us to understand the pH and ion concentration dependence of mineral formation. We have determined that iron minerals are likely to form a complete incrustation layer and we plan to look more closely at Vivianite [Fe3(PO4)2-8(H2O)] and Siderite [FeCO3] in the next stage of the project.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of Different Zirconium Contents on the Corrosion Resistance of ZrO{sub 2}-TiO{sub 2} Film-Coated Stainless Steel

This work discusses the corrosion resistance of x%zirconia (ZrO{sub 2})–x%titania (TiO{sub 2}) nanocomposite films with different percentages of ZrO{sub 2} prepared on stainless steel by dipping the substrates in sol–gel solutions. The phase compositions and microstructures of the films were investigated by x-ray diffraction (XRD) and scanning electron microscopy (SEM). Tafel polarization curves and electrochemical impedance spectroscopy (EIS) were employed to investigate the corrosion resistance of the coated steel substrates during immersion in a 5% NaCl solution at room temperature. The results showed that when the percentage of ZrO{sub 2} in the sol–gel was relatively low, the film contained cracks, leading to a poor corrosion resistance. When the percentage of ZrO{sub 2} was higher, the corrosion resistance of the film was also affected by the sintering temperature; a sintering temperature of 650 °C gave the best protection of the metal surface, and the protection efficiency was 95%.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Hot corrosion of the B2 nickel aluminides

The hot corrosion behavior of the B2 nickel aluminides was studied to determine the inherent hot corrosion resistance of the beta nickel aluminides and to develop a mechanism for the hot corrosion of the beta nickel aluminides. The effects of the prior processing of the material, small additions of zirconium, stoichiometry of the materials, and preoxidation of the samples were also examined. Additions of 2, 5, and 15 w/o chromium were used to determine the effect of chromium on the hot corrosion of the beta nickel aluminides and the minimum amount of chromium necessary for good hot corrosion resistance. The results indicate that the beta nickel aluminides have inferior inherent hot corrosion resistance despite their excellent oxidation resistance. Prior processing and zirconium additions had no discernible effect on the hot corrosion resistance of the alloys. Preoxidation extended the incubation period of the alloys only a few hours and was not considered to be an effective means of stopping hot corrosion. Stoichiometry was a major factor in determining the hot corrosion resistance of the alloys with the higher aluminum alloys having a definitely superior hot corrosion resistance. The addition of chromium to the alloys stopped the hot corrosion attack in the alloys tested. From a variety of experimental results, a complex hot corrosion mechanism was proposed. During the early stages of the hot corrosion of these alloys the corrosion is dominated by a local sulphidation/oxidation form of attack. During the intermediate stages of the hot corrosion, the aluminum depletion at the surface leads to a change in the oxidation mechanism from a protective external alumina layer to a mixed nickel-aluminum spinel and nickel oxide that can occur both externally and internally. The material undergoes extensive cracking during the later portions of the hot corrosion.

Ellis, David L.↗

The Weathering of Aluminum Alloy Sheet Materials Used in Aircraft

This report presents the results of an investigation of the corrosion of aluminum alloy sheet materials used in aircraft. It has for its purpose to study the causes of corrosion embrittlement in duralumin-type alloys and the development of methods for its elimination. The report contains results, obtained in an extensive series of weather-exposure tests, which reveal the extent to which the resistance of the materials to corrosion was affected by variable factors in their heat treatment and by the application of various surface protective coatings. The results indicate that the sheet materials are to be regarded as thoroughly reliable, from the standpoint of their permanence in service, provided proper precautions are taken to render them corrosion-resistant.

Mutchler, Willard↗

Feasibility Study for Cathodic Protection of Waste Tanks at Hanford

The Hanford Nuclear Reservation site contains approximately 211 million liters of radioactive and chemically hazardous waste arising from nuclear weapons production, beginning with World War II, and continuing through the Cold War. The waste is stored in 177 carbon-steel underground storage tanks, of which 149 are single-shell tanks (SSTs) and the remaining are double-shell tanks (DSTs). The mission of an ongoing River Protection Project is to retrieve the waste from the underground storage tanks and then treat and immobilize (i.e., vitrify) it for disposal. Waste from the older SSTs is being progressively retrieved into the newer DSTs for storage pending treatment, immobilization, and disposal. Waste chemistry controls are in place to mitigate general corrosion, pitting corrosion, and stress corrosion cracking (SCC) and minimize corrosion risks to the carbon steel tank liners of DST at the Hanford Site. The chemistry control program focuses on preserving liner integrity while balancing the need for caustic/nitrite additions that have large downstream impacts on vitrification. Some of the DSTs store salt cake or sludge waste layers contain out-of-specification interstitial liquids that contact the primary tank bottom or sidewall. Remediation of such layers through chemical additions is not practical. At the present time, the most significant leak integrity concern at Hanford is for corrosion of the tank bottoms of DSTs where the solids layer is out of specification because of hydroxide ion depletion and consequently, pH values that are less than 12. Cathodic protection (CP) has been proposed as a possible way to protect the liners of such tanks against corrosion. The objective of this project was to investigate the feasibility of applying CP to Hanford DSTs to mitigate internal corrosion of the carbon steel tank primary liners. The scope of the project included (1) a literature review on the application of CP to storage tank systems, in general, and to waste tanks at the Savannah River Site (SRS) and Hanford, (2) a review of the finite element analysis (FEA) model recently developed to evaluate potentials for a DST, and (3) the development of a boundary element analysis (BEA) model for CP for a DST. Tank AN-107, one of the Hanford DSTs, was selected for this work because (1) the bottommost waste layer in the tank is out-of-specification, and (2) electrochemical and resistivity data, based on recent waste sampling and testing, are available for this tank. The overarching conclusion of this study is that, based on the available information, it is feasible to apply CP to mitigate internal corrosion of the primary liners of the Hanford DSTs. However, significant additional information and work are required before a CP system can be designed. Recommendations for next steps in the design of the CP system will be presented.

WIERSMA, BRUCE↗

Understanding the high-temperature behavior and corrosion resistance of Cr-Nb coated cladding for BWRs

While Cr-coated Accident Tolerant Fuel has proven successful in Pressurized Water Reactors, its dissolution in high dissolved oxygen Boiling Water Reactor environments represents a major technological barrier. Here, this study presents a comprehensive evaluation of novel Cr-Nb alloys as a coating breakthrough solution for Accident Tolerant Fuel cladding in Boiling Water Reactors. We systematically investigated Physical Vapor Deposited Cr-Nb coatings with 13% and 24 at% Nb content on commercial Zr-based cladding through rigorous testing under both normal and accident conditions. Our results demonstrate Cr-Nb coatings remained completely intact during extended Boiling Water Reactor autoclave testing, while pure Cr coatings failed catastrophically due to oxide dissolution. Under Loss-of-Coolant Accident conditions at 1100°C, Cr-Nb coatings maintained protective capability for 45 min. At 800°C, the alloy coatings matched pure Cr's excellent corrosion resistance. Despite microstructural changes during prolonged high-temperature exposure, no coating delamination occurred, ensuring continued protection of the underlying Zr substrate. These findings establish Cr-Nb coatings as a viable Accident Tolerant Fuel solution for Boiling Water Reactors.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of neutron and ion irradiation on the metal matrix and oxide corrosion layer on Zr-1.0Nb cladding alloys

A detailed study has been carried out on recrystallised Zr-1.0Nb alloys corroded and irradiated under different conditions, including ex-autoclave and ex-reactor samples. After 540 days in reactor and damage around 5 dpa, the neutron irradiated sample shows no serious evidence for radiation enhanced corrosion and is still in pre-transition stage. The good corrosion resistance of the neutron irradiated Zr-1.0Nb can be related to the higher volume fraction of tetragonal phase and fewer interconnected nano porosity/cracks in the oxide. This indicates less tetragonal to monoclinic transition, leads to more protective oxide in the neutron irradiated sample, containing little evidence for short circuit paths for the penetration of oxygen or water towards the metal-oxide interface. These observations on a sample with a slow overall oxidation rate are consistent with the hypothesis that interconnected porosity can lead to early transitions and rapid oxidation. Tetragonal oxide can be either stabilised by irradiation, or stabilised by local release of impurity species from SPPs such as dissolution of Fe from Zr-Nb-Fe precipitates or radiation introduced precipitates (RIPs) which is likely to be small β-Nb clusters. The oxide consists of well-aligned columnar-equiaxed microstructure in the autoclave sample while a more complex oxide grain structure was observed in the neutron-irradiated sample. As oxide continues to grow, there are more < a > and < c > loops, dissolved Fe and RIPs in the metal matrix, however, the corrosion rate is low enough for the tetragonal oxide to stabilise and suboxide + Zr(Osat) phases exist for protectiveness, so there is no enhanced corrosion after radiation. In situ ion irradiation in the TEM revealed no visible defect clusters or voids in the oxide, suggesting that radiation damage to the metal matrix rather than oxide may have a stronger effect on corrosion mechanisms after neutron irradiation, however, cascade damages are not visible in this case. Neutron irradiation also seems to have little effect on promoting fast oxidation or dissolution of β-Nb precipitates into the surrounding oxide or metal during irradiation. Furthermore, these results are discussed in the light of the current mechanisms for corrosion of nuclear fuel cladding alloys.

(S)TEM↗

Capabilities to improve corrosion resistance of fuel claddings by using powerful laser and plasma sources

The treatment conditions of fuel claddings of the E110 alloy by using powerful UV or IR laser radiation, which lead to the increase in the corrosion resistance at the high-temperature (T = 1100°C) oxidation simulating a loss-of-coolant accident, are determined. The possibility of the complete suppression of corrosion under these conditions by using pulsed laser deposition of a Cr layer is demonstrated. The behavior of protective coatings of Al, Al{sub 2}O{sub 3}, and Cr planted on steel EP823 by pulsed laser deposition, which is planned to be used in the BREST-OD-300, is studied. The methods of the almost complete suppression of corrosion in liquid lead to the temperature of 720°C are shown.

36 MATERIALS SCIENCE↗

A Combined Density Functional Theory and Monte Carlo Investigation of the Competitive Adsorption of Atomic Oxygen and Chlorine to the Ni (111) Surface

Designing the next generation of corrosion resistant alloys will rely, in part, on developing a better understanding of how to favor the formation of protective surface oxide films in chemically aggressive environments. In this work, we examined the early stages of oxygen adsorption on Ni (111) in the presence of chloride, a known corrosive agent. The analysis was accomplished from first principles via the construction of a database of density functional theory (DFT) calculations which was then used to fit a cluster expansion model Hamiltonian. DFT calculations showed that the face centered cubic (fcc) sites were most stable for adsorption of both chloride and oxygen in agreement with the literature. Hence, only adsorption to the fcc sites was considered in the cluster expansion and the DFT database. The potential function was constructed with the aid of a genetic algorithm (GA) which helped with the selection of appropriate clusters from a candidate pool of figures. The potential function that was developed contained a total of 50 coupled (i.e. Cl-O) and non-coupled (i.e. Cl-Cl and O-O) clusters and was reasonably good at predicting DFT results with a leave-one-out cross validation score of 28.6 meV/site. The potential function was then used to perform a systematic and efficient calculation of the adsorption isotherms of oxygen and chloride at 300 K. It was observed that relatively large chloride chemical potentials were required to displace adsorbed oxygen. Furthermore, the chloride adsorption isotherms indicated a rapid shift between 0.6 ML and 1 ML. Here, this transition was explained by the need for a large chloride chemical potential to overcome the repulsive forces between the chloride adatoms.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrochemical Corrosion Behavior of Plasma-Sprayed FeCrNiMoCBSi Amorphous/Nanocrystalline Coatings in Simulated Seawater Medium

A novel FeCrNiMoCBSi coating was fabricated on F22 marine steel by plasma spraying. The coating microstructure and composition were characterized by scanning electron microscope, transmission electron microscope, x-ray diffraction, differential scanning calorimetry, and x-ray photoelectron spectroscopy. The results showed that the coating consisted of amorphous and nanocrystalline phases. Additionally, the corrosion resistance in simulated seawater was evaluated by electrochemical corrosion methods. It was found that the coating exhibited an excellent resistance to pitting corrosion. For long-time immersion tests, the corrosion resistance was gradually decreased with the increasing through-porosity due to the permeation of the corrosive solution into the coating. The coating lost its efficacy through three stages, namely the protection stage, the permeation stage, and the failure stage.

36 MATERIALS SCIENCE↗

Influence of native oxide film on corrosion behavior of additively manufactured stainless steel 316L

The influence of the native oxide film on passive film properties and localized corrosion of additively manufactured SS 316L was studied in 1 wt% HCl by XPS characterization, electrochemical polarization curves, and post-test morphology analysis by SEM. Increased Cr oxidation kinetics was observed in the as-polished sample with the native oxide film resulting in formation of an overall more protective and compact film compared to the cathodically-activated sample. Electrochemical analysis showed that corrosive attack varied between dislocation cell boundaries to cell interiors depending on the initial surface state and polarization conditions. In conclusion, a corrosion mechanism is proposed to explain this variation.

36 MATERIALS SCIENCE↗

Carburization effects on the corrosion of Cr, Fe, Ni, W, and Mo in fluoride-salt cooled high temperature reactor (FHR) coolant

Corrosion of structural alloys in fluoride salt cooled high temperature reactors (FHRs) is affected by the presence of carbon. The stability of the carbides of alloying elements augments their corrosion, however the same property can be useful if these stable carbides are used to protect materials. Exposure tests of pure elements Cr, Fe, Ni, W, and Mo in graphite crucibles at 700 °C were conducted in molten FLiNaK salt for 100 h. Carbide particles were detected on the surfaces of Cr, Mo, and W samples after exposure. The ranking of these elements, from least to greatest corrosion resistance by mass loss per unit area was Cr < Fe < W < Mo < Ni. The stability of chromium carbides was further investigated using chromium samples which were pre-carburized in a reducing hydrocarbon environment at 800 °C prior to exposure tests in molten FLiNaK. In conclusion, the chromium carbide layer produced by pre-carburization was resistant to attack by molten fluoride and slowed corrosion of the underlying chromium metal.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Superheater Corrosion In Biomass Boilers: Today's Science and Technology

This report broadens a previous review of published literature on corrosion of recovery boiler superheater tube materials to consider the performance of candidate materials at temperatures near the deposit melting temperature in advanced boilers firing coal, wood-based fuels, and waste materials as well as in gas turbine environments. Discussions of corrosion mechanisms focus on the reactions in fly ash deposits and combustion gases that can give corrosive materials access to the surface of a superheater tube. Setting the steam temperature of a biomass boiler is a compromise between wasting fuel energy, risking pluggage that will shut the unit down, and creating conditions that will cause rapid corrosion on the superheater tubes and replacement expenses. The most important corrosive species in biomass superheater corrosion are chlorine compounds and the most corrosion resistant alloys are typically FeCrNi alloys containing 20-28% Cr. Although most of these materials contain many other additional additions, there is no coherent theory of the alloying required to resist the combination of high temperature salt deposits and flue gases that are found in biomass boiler superheaters that may cause degradation of superheater tubes. After depletion of chromium by chromate formation or chromic acid volatilization exceeds a critical amount, the protective scale gives way to a thick layer of Fe 2 O 3 over an unprotective (FeCrNi) 3 O 4 spinel. This oxide is not protective and can be penetrated by chlorine species that cause further acceleration of the corrosion rate by a mechanism called active oxidation. Active oxidation, cited as the cause of most biomass superheater corrosion under chloride ash deposits, does not occur in the absence of these alkali salts when the chloride is present as HCl gas. Although a deposit is more corrosive at temperatures where it is molten than at temperatures where it is frozen, increasing superheater tube temperatures through the measured first melting point of fly ash deposits does not necessarily produce a step increase in corrosion rate. Corrosion rate typically accelerates at temperatures below the first melting temperature and mixed deposits may have a broad melting temperature range. Although the environment at a superheater tube surface is initially that of the ash deposits, this chemistry typically changes as the deposits mature. The corrosion rate is controlled by the environment and temperature at the tube surface, which can only be measured indirectly. Some results are counter-intuitive. Two boiler manufacturers and a consortium have developed models to predict fouling and corrosion in biomass boilers in order to specify tube materials for particular operating conditions. It would be very useful to compare the predictions of these models regarding corrosion rates and recommended alloys in the boiler environments where field tests will be performed in the current program. Manufacturers of biomass boilers have concluded that it is more cost-effective to restrict steam temperatures, to co-fire biofuels with high sulfur fuels and/or to use fuel additives rather than try to increase fuel efficiency by operating with superheater tube temperatures above melting temperature of fly ash deposits. Similar strategies have been developed for coal fired and waste-fired boilers. Additives are primarily used to replace alkali metal chloride deposits with higher melting temperature and less corrosive alkali metal sulfate or alkali aluminum silicate deposits. Design modifications that have been shown to control superheater corrosion include adding a radiant pass (empty chamber) between the furnace and the superheater, installing cool tubes immediately upstream of the superheater to trap high chloride deposits, designing superheater banks for quick replacement, using an external superheater that burns a less corrosive biomass fuel, moving circulating fluidized bed (CFB) superheaters from the convective pass into the hot recirculated fluidizing medium and adding an insulating layer to superheater tubes to raise their surface temperature above the dew point temperature of alkali chlorides. These design changes offer advantages but introduce other challenges. For example, operating with superheater temperatures above the dew point of alkali chlorides could require the use of creep-resistant tube alloys and doesn't eliminate chloride corrosion. Improved test methods that can be applied within this project include automated dimensional metrology to make a statistical analysis of depth of penetration and corrosion product thickness, and simultaneous thermal analysis measurements to quantify the melting of complex ashes and avoid the unreliability of the standard ash fusion test. Other important developments in testing include the installation of individually-temperature-controlled superheater loops for corrosion testing in operating boilers and temperature gradient testing.

09 BIOMASS FUELS↗

Annual Report for SCC

The Advanced Combustion Project addresses fundamental issues of fire-side and steam-side corrosion and materials performance in oxy-fuel combustion environments and provides an integrated approach into understanding the environmental and mechanical behavior such that environmental degradation can be ameliorated and long-term microstructural stability, and thus mechanical performance, can lead to longer lasting components and extended power plant life.

20 FOSSIL-FUELED POWER PLANTS↗

Effects of CO 2 and H 2 S on Corrosion of Martensitic Steels in Brines at Low Temperature

Corrosion studies were conducted for martensitic carbon steels in 5 wt% NaCl brine solutions at 4°C and 10 MPa (1,450 psi). These studies simulated different subsurface environments relevant to Arctic drilling. Here, two high-strength martensitic carbon steels, S-135 and UD-165, were studied in three different environments: (1) a CO 2 -NaCl-H 2 O solution with a CO 2 :H 2 O molar ratio of 0.312 in the whole system, (2) an H 2 S-NaCl-H 2 O solution with an H 2 S:H 2 O molar ratio of 3.12 × 10 –4 , and (3) a CO 2 -H 2 S-NaCl-H 2 O solution with the same acid gas to water ratios as environments 1 and 2. Results from the CO 2 +H 2 S mixed environment indicated that sour corrosion mechanism was dominant when the CO 2 :H 2 S molar ratio was 1,000. This impact of a small amount of H 2 S on the corrosion mechanism could be attributed to the specific adsorption of H 2 S on the steel surface. Electrochemical and mass loss measurements showed a distinct drop in the corrosion rate (CR) by more than one order of magnitude when transitioning from sweet to sour corrosion. This inhibiting effect on CR was attributed to the formation of a protective sulfide thin film. Tafel analyses of the anodic reaction showed that the Bockris mechanism was unlikely in the conditions tested. As a result, when comparisons were made between modeled and experimental CRs, good agreement was found in the CO 2 -only and H 2 S-only environments, but not in the CO 2 +H 2 S environment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Superior Nanoscale Passive Oxide Layers Synthesized Under Photon Irradiation for Environmental Protection

We report on synthesis and functional properties of ultra-thin oxide layers synthesized on metal surfaces by room temperature photon irradiation. We show that the impedance of a passive aluminum oxide film synthesized under ultraviolet photon irradiation is an order of magnitude larger than that of native oxide in a 0.5 M NaCl solution. Further, the structure and impedance of existing native oxide layers can be dramatically improved by minutes-long exposure to photon-irradiation. Depth profiling studies with X-ray photoelectron spectroscopy shows that chlorine uptake in UV-synthesized oxides, compared to that of native oxides, is reduced which can contribute to the improvement in corrosion resistance. The results are of significance to synthesis of ultra-thin passive layers on metal and alloy structures for environmental protection.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

High temperature environmental effects on metals

The current status of knowledge and ability to predict high-temperature environmental attack of metals is reviewed with particular reference to the gas turbine engine. Environmental attack is caused by high temperatures, combustion products, and impurities. A schematic representation of life-limiting factors of turbine components shows that environmental attack can lead to very early failures. Attention is given to high-temperature oxidation with prevailing modes of oxidation attack, and to hot corrosion and other impurity effects. Erosion attack results from the direct mechanical removal of component material by impact of hard substances like ash, sand, or dirt. Solutions to hot-corrosion problems can be found semiempirically by using improved alloys or ceramics, protective surface coatings, additives to the engine environment, and air/fuel cleanup to eliminate detrimental impurities.

Grisaffe, S. J.↗

Application of Direct Assessment Approaches and Methodologies to Cathodically Protected Nuclear Waste Transfer Lines

The U.S. Department of Energy&#x27;s (DOE) Hanford Site is responsible for the safe storage, retrieval, treatment, and disposal of approximately 54 million gallons (204 million liters) of radioactive waste generated since the site&#x27;s inception in 1943. Today, the major structures involved in waste management at Hanford include 149 carbon steel single-shell tanks, 28 carbon-steel double-shell tanks, plus a network of buried metallic transfer lines and ancillary systems (pits, vaults, catch tanks, etc.) required to store, retrieve, and transfer waste within the tank farm system. Many of the waste management systems at Hanford are still in use today. In response to uncertainties regarding the structural integrity of these systems,&#x27; an independent, comprehensive integrity assessment of the Hanford Site piping system was performed. It was found that regulators do not require the cathodically protected pipelines located within the Hanford Site to be assessed by External Corrosion Direct Assessment (ECDA) or any other method used to ensure integrity. However, a case study is presented discussing the application of the direct assessment process on pipelines in such a nuclear environment. Assessment methodology and assessment results are contained herein. An approach is described for the monitoring, integration of outside data, and analysis of this information in order to identify whether coating deterioration accompanied by external corrosion is a threat for these waste transfer lines.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗