Dual-Mode Adhesive Pad

Tool helps worker grip and move along large, smooth structure with no handgrips or footholds. Adheres to surface but easily released by actuating simple mechanism. Includes handle and segmented contact-adhesive pad. Bulk of pad made of soft plastic foam conforming to surface of structure. Each segment reinforced with rib. In sticking mode, ribs braced by side catches. In peeling mode, side catches retracted, and segmented adhesive pad loses its stiffness. Modified versions useful in inspecting hulls of ships and scaling walls in rescue operations.

Hartz, Leslie↗

Micro-measurements of mechanical properties for adhesives and composites using digital imaging technology

The need for a constituent based durability or accelerated life prediction procedure to be used for the engineering design of polymer matrix composites is discussed in the light of current plans for the High Speed Civil Transport (HSCT) concerns about the U.S. infrastructure (bridges, pipelines, etc.) and other technological considerations of national concern. It is pointed out that good measurement procedures for insitu resin properties are needed for both adhesives and composites. A double cantilever beam (DCB) specimen which shows promise for the easy determination of adhesive shear properties is presented and compared with measurements of strains within the bondline using a new optical digital imaging micro-measurement system (DIMMS). The DCB specimen is also used to assess damage in a bonded joint using a dynamic mechanical thermal analysis system (DMTA). The possible utilization of the same DIMMS and DMTA procedures to determine the insitu properties of the resin in a composite specimen are discussed as well as the use of the procedures to evaluate long term mechanical and physical aging. Finally, a discussion on the state-of-the art of the measurement of strains in micron and sub-micron domains is given.

Brinson, Hal F.↗

Permeability testing of composite material and adhesive bonds for the DC-XA composite feedline program

Hercules IM7/8552 carbon/epoxy and Hysol EA 9394 epoxy adhesive bonded between composite/titanium were tested for permeability after various numbers of thermal cycles between 100 C and liquid nitrogen (-196 C). The specimens were quenched from the 100 C temperature into liquid nitrogen to induce thermal shock into the material. Results showed that the carbon/epoxy system was practically impermeable even after 12 thermal cycles. The EA 9394 adhesive bondline was more permeable than the carbon/epoxy, but vacuum mixing minimized the permeability and kept it within allowable limits. Thermal cycling had little effect on the permeability values of the bondline specimens.

Nettles, A. T.↗

Verification of surface preparation for adhesive bonding

A survey of solid rocket booster (SRB) production operations identified potential contaminants which might adversely affect bonding operations. Lap shear tests quantified these contaminants' effects on adhesive strength. The most potent contaminants were selected for additional studies on SRB thermal protection system (TPS) bonding processes. Test panels were prepared with predetermined levels of contamination, visually inspected using white and black light, then bonded with three different TPS materials over the unremoved contamination. Bond test data showed that white and black light inspections are adequate inspection methods for TPS bonding operations. Extreme levels of contamination (higher than expected on flight hardware) had an insignificant effect on TPS bond strengths because of the apparent insensitivity of the adhesive system to contamination effects, and the comparatively weak cohesive strength of the TPS materials.

Myers, Rodney S.↗

Replacing Chlorinated-Solvent-Based Cleaners And Adhesives

Brief report describes tests conducted to assess feasibility of using selected chemicals as replacements for selected cleaners, primers, and adhesives containing chlorinated solvents. Cleaners, primers, and adhesives in question used in bonding insulating material in steel cases of solid-fuel rocket motors. Necessary to phase out use of chlorinated solvents because of concerns over toxicity and adverse effects on ozone layer in upper atmosphere.

Heaton, Harley↗

Solid Lubrication Fundamentals and Applications. Properties of Clean Surfaces: Adhesion, Friction, and Wear

This chapter presents the adhesion, friction, and wear behaviors of smooth, atomically clean surfaces of solid-solid couples, such as metal-ceramic couples, in a clean environment. Surface and bulk properties, which determine the adhesion, friction, and wear behaviors of solid-solid couples, are described. The primary emphasis is on the nature and character of the metal, especially its surface energy and ductility. Also, the mechanisms of friction and wear for clean, smooth surfaces are stated.

Miyoshi, Kazuhisa↗

Flexible polyacrylamide substrata for the analysis of mechanical interactions at cell-substratum adhesions

We have described a powerful tool for the study of mechanical interactions between cells and their physical environment. Although the approach has already been used in a variety of ways to measure traction forces and to characterize active and passive responses of cultured cells to mechanical stimulation, it can be extended easily and combined with other microscopic approaches, including fluorescent analog imaging (Beningo et al., 2001), photobleaching, calcium imaging, micromanipulation, and electrophysiology. This method will be particularly useful for studying the functions of various components at focal adhesions, and the effects of mechanical forces on focal adhesion-mediated signal transduction. In addition, the method can be extended to a 3D setting, e.g., by sandwiching cultured cells between two layers of polyacrylamide to create an environment mimicking that in the tissue of a multicellular organism. Whereas chemical interactions between cells and the environment have been investigated extensively, many important questions remain as to the role of physical forces in cellular functions and the interplay between chemical and physical mechanisms of communication. The present approach, as well as other approaches capable of probing physical interactions, should fill in this important gap in the near future.

NASA Discipline Cell Biology↗

Selected Contribution: Skeletal muscle focal adhesion kinase, paxillin, and serum response factor are loading dependent

This investigation examined the effect of mechanical loading state on focal adhesion kinase (FAK), paxillin, and serum response factor (SRF) in rat skeletal muscle. We found that FAK concentration and tyrosine phosphorylation, paxillin concentration, and SRF concentration are all lower in the lesser load-bearing fast-twitch plantaris and gastrocnemius muscles compared with the greater load-bearing slow-twitch soleus muscle. Of these three muscles, 7 days of mechanical unloading via tail suspension elicited a decrease in FAK tyrosine phosphorylation only in the soleus muscle and decreases in FAK and paxillin concentrations only in the plantaris and gastrocnemius muscles. Unloading decreased SRF concentration in all three muscles. Mechanical overloading (via bilateral gastrocnemius ablation) for 1 or 8 days increased FAK and paxillin concentrations in the soleus and plantaris muscles. Additionally, whereas FAK tyrosine phosphorylation and SRF concentration were increased by < or =1 day of overloading in the soleus muscle, these increases did not occur until somewhere between 1 and 8 days of overloading in the plantaris muscle. These data indicate that, in the skeletal muscles of rats, the focal adhesion complex proteins FAK and paxillin and the transcription factor SRF are generally modulated in association with the mechanical loading state of the muscle. However, the somewhat different patterns of adaptation of these proteins to altered loading in slow- vs. fast-twitch skeletal muscles indicate that the mechanisms and time course of adaptation may partly depend on the prior loading state of the muscle.

NASA Discipline Musculoskeletal↗

Integrin binding and mechanical tension induce movement of mRNA and ribosomes to focal adhesions

The extracellular matrix (ECM) activates signalling pathways that control cell behaviour by binding to cell-surface integrin receptors and inducing the formation of focal adhesion complexes (FACs). In addition to clustered integrins, FACs contain proteins that mechanically couple the integrins to the cytoskeleton and to immobilized signal-transducing molecules. Cell adhesion to the ECM also induces a rapid increase in the translation of preexisting messenger RNAs. Gene expression can be controlled locally by targeting mRNAs to specialized cytoskeletal domains. Here we investigate whether cell binding to the ECM promotes formation of a cytoskeletal microcompartment specialized for translational control at the site of integrin binding. High-resolution in situ hybridization revealed that mRNA and ribosomes rapidly and specifically localized to FACs that form when cells bind to ECM-coated microbeads. Relocation of these protein synthesis components to the FAC depended on the ability of integrins to mechanically couple the ECM to the contractile cytoskeleton and on associated tension-moulding of the actin lattice. Our results suggest a new type of gene regulation by integrins and by mechanical stress which may involve translation of mRNAs into proteins near the sites of signal reception.

Non-NASA Center↗

Multiwalled Carbon Nanotube/nanofiber Arrays as Conductive and Dry Adhesive Interface Materials

We demonstrate the possibility of making conductive and dry adhesive interfaces between multiwalled carbon nanotube (MWNT) and nanofiber (MWNF) arrays grown by chemical vapor deposition with transition-metal as catalyst on highly Boron doped silicon substrates. The maximum observed adhesion force between MWNT and MWNF surfaces is 3.5 mN for an apparent contact area of 2 mm by 4 mm. The minimum contact resistance measured at the same time is approx.20 Omega. Contact resistances of MWNT-MWNT and MWNT-gold interfaces were also measured as pressure forces around several mN were applied at the interface. The resulting minimum contact resistances are on the same order but with considerable variation from sample to sample. For MWNT-MWNT contacts, a minimum contact resistance of approx.1 Omega is observed for a contact area of 2 mm by 1 mm. The relatively high contact resistances, considering the area density of the nanotubes, might be explained by the high cross-tube resistances at the contact interfaces.

Tong, Tao↗

Adhesive Bonding of Titanium to Carbon-Carbon Composites for Heat Rejection Systems

High temperature adhesives with good thermal conductivity, mechanical performance, and long term durability are crucial for the assembly of heat rejection system components for space exploration missions. In the present study, commercially available adhesives were used to bond high conductivity carbon-carbon composites to titanium sheets. Bonded pieces were also exposed to high (530 to 600 Kelvin for 24 hours) and low (liquid nitrogen 77K for 15 minutes) temperatures to evaluate the integrity of the bonds. Results of the microstructural characterization and tensile shear strengths of bonded specimens will be reported. The effect of titanium surface roughness on the interface microstructure will also be discussed.

Cerny, Jennifer↗

Composites with improved fiber-resin interfacial adhesion

The adhesion of fiber reinforcement such as high modulus graphite to a matrix resin such as polycarbonate is greatly enhanced by applying a very thin layer, suitably from 50 Angstroms to below 1000 Angstroms, to the surface of the fiber such as by immersing the fiber in a dilute solution of the matrix resin in a volatile solvent followed by draining to remove excess solution and air drying to remove the solvent. The thin layer wets the fiber surface. The very dilute solution of matrix resin is able to impregnate multifilament fibers and the solution evenly flows onto the surface of the fibers. A thin uniform layer is formed on the surface of the fiber after removal of the solvent. The matrix resin coated fiber is completely wetted by the matrix resin during formation of the composite. Increased adhesion of the resin to the fibers is observed at fracture. At least 65 percent of the surface of the graphite fiber is covered with polycarbonate resin at fracture whereas uncoated fibers have very little matrix resin adhering to their surfaces at fracture and epoxy sized graphite fibers exhibit only slightly higher coverage with matrix resin at fracture. Flexural modulus of the composite containing matrix resin coated fibers is increased by 50 percent and flexural strength by 37 percent as compared to composites made with unsized fibers.

Cizmecioglu, Muzaffer↗

Light-Curing Adhesive Repair Tapes

Adhesive tapes, the adhesive resins of which can be cured (and thereby rigidized) by exposure to ultraviolet and/or visible light, are being developed as repair patch materials. The tapes, including their resin components, consist entirely of solid, low-outgassing, nonhazardous or minimally hazardous materials. They can be used in air or in vacuum and can be cured rapidly, even at temperatures as low as -20 C. Although these tapes were originally intended for use in repairing structures in outer space, they can also be used on Earth for quickly repairing a wide variety of structures. They can be expected to be especially useful in situations in which it is necessary to rigidize tapes after wrapping them around or pressing them onto the parts to be repaired.

Allred, Ronald↗

The Effects of Temperature, Humidity and Aircraft Fluid Exposure on T800H/3900-2 Composites Bonded with AF-555M Adhesive

Fiber reinforced resin matrix composites and structural adhesives have found increased usage on commercial and military aircraft in recent years. Due to the lack of service history of these relatively new material systems, their long-term aging performance has not been well established. In this study, single lap shear specimens (SLS) were fabricated by secondary bonding of Scotch-Weld(TradeMark) AF-555M between pre-cured adherends comprised of T800H/3900-2 uni-directional laminates. The adherends were co-cured with wet peel-ply for surface preparation. Each bond-line of the SLS specimen was measured to determine thickness and inspected visually using an optical microscope for voids. A three-year environmental aging plan for the SLS specimens at 82 C (180 F) and 85% relative humidity was initiated. SLS strengths were measured for both controls and aged specimens at room temperature and 82 C. The effect of this exposure on lap shear strength and failure modes to date is reported. In addition, the effects of water, saline water, deicing fluid, JP-5 jet fuel and hydraulic fluid on both the composite material and the adhesive bonds were investigated. The up to date results on the effects of these exposures will be discussed.

Miner, Gilda A.↗

Laser Surface Preparation for Adhesive Bonding of Ti-6Al-4V

Adhesively bonded structures are potentially lighter in weight than mechanically fastened ones, but existing surface treatments are often considered unreliable. Two main problems in achieving reproducible and durable adhesive bonds are surface contamination and variability in standard surface preparation techniques. In this work three surface pretreatments were compared: laser etching with and without grit blasting and conventional Pasa-Jell treatment. Ti-6Al-4V surfaces were characterized by contact angle goniometry, optical microscopy, and X-ray photoelectron spectroscopy (XPS). Laser -etching was found to produce clean surfaces with precisely controlled surface topographies and PETI-5 lap shear strengths and durabilities were equivalent to those produced with Pasa-Jell.

Belcher, Marcus A.↗

Comparison of Adhesion and Retention Forces for Two Candidate Docking Seal Elastomers

To successfully mate two pressurized vehicles or structures in space, advanced seals are required at the interface to prevent the loss of breathable air to the vacuum of space. A critical part of the development testing of candidate seal designs was a verification of the integrity of the retaining mechanism that holds the silicone seal component to the structure. Failure to retain the elastomer seal during flight could liberate seal material in the event of high adhesive loads during undocking. This work presents an investigation of the force required to separate the elastomer from its metal counter-face surface during simulated undocking as well as a comparison to that force which was necessary to destructively remove the elastomer from its retaining device. Two silicone elastomers, Wacker 007-49524 and Esterline ELASA-401, were evaluated. During the course of the investigation, modifications were made to the retaining devices to determine if the modifications improved the force needed to destructively remove the seal. The tests were completed at the expected operating temperatures of -50, +23, and +75 C. Under the conditions investigated, the comparison indicated that the adhesion between the elastomer and the metal counter-face was significantly less than the force needed to forcibly remove the elastomer seal from its retainer, and no failure would be expected.

Hartzler, Brad D.↗

Adhesive Wear of Rollers in Vacuum

This work was done to support NASA's James Webb Space Telescope that is equipped with a Near Infrared Camera and Spectrograph and Micro Shutter Assembly (MSA). A MSA mechanism's qualification test in cryogenic vacuum at 30deg K for 96K cycles resulted in roller wear and formation of some debris. Lab tests in vacuum were conducted at NASA Glenn Research Center (GRC) to understand the wear of Ti6Al4V mated with 440F steel rollers. Misalignment angle was found to have the most significant effect on debris formation. At misalignment angle of 1.4deg, significant amount of wear debris were formed within 50,000 cycles. Very few wear particles were found for a zero misalignment angle, and the total wear was small even after 367,000 cycles. The mode of wear in all the tests was attributed to adhesion, which was clearly evident from video records as well as the plate-like amalgamated debris material from both rollers. The adhesive wear rate was found to be approximately proportional to the misalignment angle. The wear is a two-way phenomenon, and the mixing of both roller materials in wear debris was confirmed by x-ray fluorescence (XRF) and EDX spectra. While there was a net loss of mass from the steel rollers, XRF and energy dispersive x-ray (EDX) spectra showed peaks of Ti on steel rollers, and peaks of Fe on Ti rollers. These results are useful for designers in terms of maintaining appropriate tolerances to avoid misalignment of rolling elements and the resulting severe wear

Shaeef, Iqbal↗