Prediction of good glass forming ability in amorphous soft magnetic alloys by thermocalc simulation with experimental validation
Alloys in a (Fe 70 Ni 30 ) 80 (BeSieNb) 20 system, with good glass forming ability (GFA), were identified using Thermocalc software to simulate liquidus temperatures (T's) and solidification ranges (areas between the liquidus and solidus in a binary phase diagram,a line at fixed T). Here, a region with excellent GFA was identified at 14-18% B and 0-7% Si with the balance Nb, showing minima in liquidus and solidification range. A region with a solidification range minimum, but no corresponding liquidus minimum was identified at 3-8% B and 5-10% Si but had lower GFA. A shallow liquidus minimum, with no minimum in solidification range, at 3-5% B and 1-3% Si had the lowest GFA and did not produce amorphous material. Measured GFA was ranked using parameters T rg , DT xg , and γ m , defined herein. Only the reduced glass transition temperature, T rg , was predictive for the alloys. Differential Scanning Calorimetry (DSC) data showed liquidus T's to agree. Curie temperatures, T c 's were observed to increase with B/Nb ratio. Simulations of liquidus and solidification range for alloys with 18 and 15% glass formers do not show regions with minima in both, indicating good GFA is not expected.