At least 811 records · Page 45

Role of niobium in the high-temperature oxidation of titanium

Here, we compared the oxidation of Ti and Ti-2 at.% Nb at 800°C in Ar-20% O 2 and in sequential 16 O 2 - 18 O 2 atmospheres to clarify the role of niobium in the high-temperature oxidation of titanium. Niobium had no effect on the amount of oxygen dissolved in the metal or on oxygen diffusion in the metal. Instead, niobium enhanced oxidation resistance by segregating to TiO 2 grain boundaries, where it likely slowed outward Ti diffusion. These findings spotlight doping of TiO 2 grain boundaries as a strategy for improving the oxidation resistance of Ti alloys and, more generally, TiO 2 -forming alloys.

36 MATERIALS SCIENCE↗

Role of nitrogen in the high-temperature oxidation of titanium alloys

Here, we characterized the oxidation of pure Ti, Ti-0.8Si, and Ti-2Nb at 800 °C in N 2 -20% O 2 and in sequential isotopically labeled N 2 -20% O 2 atmospheres to clarify how nitrogen influences the high-temperature oxidation mechanisms of titanium alloys. The alloys always exhibited a nitride layer beneath a compact oxide scale with localized nitrogen concentrations in the underlying metal. Nitrogen is found to limit the oxygen concentrations in the metal. The synergy between alloying and nitrogen helps maintain compact oxide scales, preventing the formation of the lamellar scales observed during oxidation in nitrogen-free atmosphere and the oxidation of pure Ti regardless of the atmosphere.

36 MATERIALS SCIENCE↗

Characterization of a hybrid target multi-keV x-ray source by a multi-parameter statistical analysis of titanium K-shell emission

We studied the titanium K-shell emission spectra from multi-keV x-ray source experiments with hybrid targets on the OMEGA laser facility. Using the collisional-radiative TRANSPEC code, dedicated to K-shell spectroscopy, we reproduced the main features of the detailed spectra measured with the time-resolved MSPEC spectrometer. We developed a general method to infer the N e , T e and T i characteristics of the target plasma from the spectral analysis (ratio of integrated Lyman-α to Helium-α in-band emission and the peak amplitude of individual line ratios) of the multi-keV x-ray emission. Finally, these thermodynamic conditions are compared to those calculated independently by the radiation-hydrodynamics transport code FCI2.

42 ENGINEERING↗

Characterization and modeling of mechanical behavior of single crystal titanium deformed by split-Hopkinson pressure bar

Single crystal titanium samples were dynamically loaded using split-Hopkinson pressure bar (SHPB) and the resulting microstructures were examined. Characterization of the twins and dislocations present in the microstructure was conducted to understand the pathway for observed mechanical behavior. Electron backscatter diffraction (EBSD) was used to measure textures and quantify twinning. Microstructures were profusely twinned after loading, and twin variants and corresponding textures were different as a function of initial orientation. Focused ion beam (FIB) foils were created to analyze dislocation content using transmission electron microscopy (TEM). Large amounts of dislocations were present, indicating that plasticity was achieved through slip and twinning together. Viscoplastic self-consistent (VPSC) modeling was used to confirm the complex order of operations during deformation. The activation of different mechanisms was highly dependent upon crystal orientation. For [0001] and View the MathML source[101¯1]-oriented crystals, compressive twinning was observed, followed by secondary tensile twinning. Furthermore, dislocations though prevalent in the microstructure, contributed to final texture far less than twinning.

36 MATERIALS SCIENCE↗

Dynamic recrystallization in adiabatic shear banding: Effective-temperature model and comparison to experiments in ultrafine-grained titanium

Dynamic recrystallization (DRX) is often observed in conjunction with adiabatic shear banding (ASB) in polycrystalline materials. The recrystallized nanograins in the shear band have few dislocations compared to the material outside of the shear band. In this work, we reformulate the recently-developed Langer-Bouchbinder-Lookman (LBL) continuum theory of polycrystalline plasticity and include the creation of grain boundaries. While the shear-banding instability emerges because thermal heating is faster than heat dissipation, recrystallization is interpreted as an entropic effect arising from the competition between dislocation creation and grain boundary formation. We show that our theory closely matches recent results in sheared ultrafine-grained titanium. The theory thus provides a thermodynamically consistent way to systematically describe the formation of shear bands and recrystallized grains therein.

36 MATERIALS SCIENCE↗

Cross-slip and easy-glide CRSS in titanium: Theoretical predictions and in-situ TEM measurements

This study investigates the mechanics of prismatic and first-order pyramidal $\langle$a$\rangle$ slip in titanium (Ti), elucidating the physics of easy-glide and cross-slip through a combination of theory and experiments. Screw-character prismatic (Pr) dislocations in Ti are of particular interest because their complex cores can be stable or unstable, leading to activation by either cross-slip or planar glide. To investigate these mechanisms, site-specific micro tensile samples were prepared using focused ion beam (FIB) milling and mounted on a push-to-pull (PTP) device for in-situ transmission electron microscopy (TEM) tensile testing. The in-situ experiments provide direct observations of the onset of dislocation motion and the precise determination of the critical resolved shear stress (CRSS) for the activated mechanisms, and its evolution with load cycling. A comprehensive theory has been developed to predict the CRSS values for easy glide, cross-slip, and multiplication of dislocations. Predicted critical stresses for pyramidal (π)-to-Pr and reverse cross-slip agree closely with the experimental measurements. The latter cross-slip stress is a factor of two higher than that of unobstructed planar slip. The model accounts for overlapping dislocation cores and employs a Wigner-Seitz based cell to evaluate misfit energies. By combining ab initio density functional theory (DFT) with anisotropic elasticity, the framework identifies minimum energy pathways for dislocation glide, which can be intermittent and zig-zag. A simplified expression utilizing (π) and Pr Schmid factor ratios is proposed for critical stress corresponding to (π)-to-Pr cross-slip transition. The results are strongly dependent on crystal orientation, underscoring non-Schmid behavior. Overall, this study explores key critical stress parameters essential for informing higher-scale simulations of plasticity in Ti.

Critical stress↗

Tumor Bed Delineation for Partial Breast and Breast Boost Radiotherapy Planned in the Prone Position: What Does MRI Add to X-ray CT Localization of Titanium Clips Placed in the Excision Cavity Wall?

Purpose: To compare tumor bed (TB) volumes delineated using magnetic resonance imaging plus computed tomography and clips (MRCT) with those delineated using CT and clips (CT/clips) alone in postlumpectomy breast cancer patients positioned prone and to determine the value of MRCT for planning partial breast irradiation (PBI). Methods and Materials: Thirty women with breast cancer each had 6 to 12 titanium clips secured in the excision cavity walls at lumpectomy. Patients underwent CT imaging in the prone position, followed by MRI (T{sub 1}-weighted [standard and fat-suppressed] and T{sub 2}-weighted sequences) in the prone position. TB volumes were delineated separately on CT and on fused MRCT datasets. Clinical target volumes (CTV) (where CTV = TB + 15 mm) and planning target volumes (PTV) (where PTV = CTV + 10 mm) were generated. Conformity indices between CT- and MRCT-defined target volumes were calculated (ratio of the volume of agreement to total delineated volume). Discordance was expressed as a geographical miss index (GMI) (where the GMI = the fraction of total delineated volume not defined by CT) and a normal tissue index (the fraction of total delineated volume designated as normal tissue on MRCT). PBI dose distributions were generated to cover CT-defined CTV (CTV{sub CT}) with {>=}95% of the reference dose. The percentage of MRCT-defined CTV (CTV{sub MRCT}) receiving {>=}95% of the reference dose was measured. Results: Mean conformity indices were 0.54 (TB), 0.84 (CTV), and 0.89 (PTV). For TB volumes, the GMI was 0.37, and the NTI was 0.09. Median percentage volume coverage of CTV{sub CT} was 97.1% (range, 95.3%-100.0%) and of CTV{sub MRCT} was 96.5% (range, 89.0%-100.0%). Conclusions: Addition of MR to CT/clip data generated TB volumes that were discordant with those based on CT/clips alone. However, clinically satisfactory coverage of CTV{sub MRCT} by CTV{sub CT}-based tangential PBI fields provides support for CT/clip-based TB delineation remaining the method of choice for PBI/breast boost radiotherapy planned using tangential fields.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

On the existence of orthorhombic martensite in a near-α titanium base alloy used for additive manufacturing

Additive manufacturing is a state-of-the-art production technology to produce tailor-made and highly complex parts. Among various other alloys, Ti base alloys are frequently used in this manufacturing technique due to their well-balanced properties and their wide range of applications. Allotropic phases and the occurrence of athermal phase transformations are the main reasons why these alloys hold a great development potential and are the basis of extensive use. High cooling rates during manufacturing lead to martensitic phases and the formation of nanometer-sized microstructures resulting in extraordinary strength. Simultaneously, such high cooling rates cause a high amount of lattice defects and the occurrence of residual stresses, which finally may result in delamination effects and cracks. Usually, a common approach to reduce residual stresses during additive manufacturing is to decrease thermal gradients by increasing the heat input or preheating the building platform. Instead of applying the typical approaches to lower thermal gradients, this study deals with the origin of the ‘softer’ orthorhombic martensite by accelerating the solidification process. The implementation of the orthorhombic phase in bulk components was inspired by a new phase transformation herein reported for the first time in the powder material, which also validates the possible occurrence of two martensitic phases in the same alloy. Various sophisticated characterization techniques like high energy and high-temperature X-ray diffraction, high-resolution transmission electron microscopy as well as atom probe tomography were applied to characterize this softer orthorhombic martensitic phase in detail aiming to highlight the opportunities accompanied by this new approach for additive manufacturing of titanium alloys.

36 MATERIALS SCIENCE↗

Synergetic effect of carbon and AlF 3 coatings on the lithium titanium oxide anode material for high power lithium-ion batteries

A carbon coated commercial lithium titanium oxide (Li 4 Ti 5 O 12 ; LTO) was acoustically mixed with nano-sized AlF 3 and heat treated to form a simultaneous coating layer of carbon and AlF 3 on LTO particles. The surface modified LTO samples were characterized by a variety of means such as X-ray diffraction, Fourier transform infrared spectrometer, high-resolution transmission electron microscope, and inductively coupled plasma mass spectrometry. The results indicate that both carbon and AlF 3 layers exist on the surface of LTO particles and that the distribution of the carbon and AlF 3 differs depending on post heat treatment temperature. The carbon and AlF 3 coating layers formed by optimal post heat treatment at 350 °C significantly improves electrochemical performance, which increases charge capacity by 30% over the pristine LTO after 50 cycles at a high current density of 5C. Thus, LTO with a simultaneous coating layer of carbon and AlF 3 formed by acoustic mixing and post heat treatment shows a potential to further improve commercially-optimized carbon-coated LTO by alleviating its inherently low conductivity. In conclusion, this is an effective way to stabilize the interface between LTO particles and electrolyte, and is a practical approach to promote the wide usage of LTO, one of the most potent anode materials

25 ENERGY STORAGE↗

Thermophysical property and electrical conductivity of titanium isopropoxide – polysiloxane derived ceramics

In this work, high temperature resistant Si-O-C-Ti has been successfully prepared based on the pyrolysis of polysiloxane (PSO) and titanium (IV) isopropoxide (TTIP) at 1200–1400 °C. PSO can homogeneously mix with TTIP to enhance its conversion to TiC. The carbothermal reactions between TiO 2 (product of thermal decomposition of TTIP) and carbon result in the formation of TiC. All the Si-O-C-Ti composites pyrolyzed at 1200–1300 °C are stable up to 1000 °C in an oxidizing air atmosphere. TiC leads to high electrical conductivity at elevated temperatures; the maximum conductivity is 1176.55 S/m at 950 °C, which is the first reported value of >1000 S/m conductivity for Si-O-C-Ti ceramics. However, too high a pyrolysis temperature, such as 1400 °C, can potentially ‘destabilize’ the Si-O-C-Ti system by consuming the free carbon and result in lower conductivities.

36 MATERIALS SCIENCE↗

Damage evolution and ductile fracture of commercially-pure titanium sheets subjected to simple tension and cyclic bending under tension

This paper describes a study into the evolution of damage in commercial-purity titanium (CP–Ti) sheets subjected to cyclic bending under tension (CBT) and uniaxial tension (simple tension, ST). Sections were taken from sheets that were strained to various levels under both methods and were imaged using X-ray computed tomography (XCT) to reveal insights into the size, density, and distribution of microvoids in the sheets. Digital image correlation (DIC) was also used to observe the surface strain of CBT and ST sheets during testing. These results showed that elongation to failure (ETF) for CBT deformation is about 2.5× higher than for ST, local longitudinal strains in the bulk of the CBT sample are around 1.3× higher than the peak strain in the ST necked region, and 1.7× higher in the localized region of CBT failure. It was found that the volume-density of voids in both sheets followed a similar exponential increase with strain, reaching nearly 45× higher in the CBT than the ST sheets before the onset of failure, mainly due to the higher strain levels achieved. A higher volume density of voids developed in the center of sheets at high levels of strain, for both processes, with the density in the sheet center becoming approximately double that found near the edges. Scanning electron microscopy (SEM) was used to examine the fracture surface of CBT and ST sheets after failure. The observations are presented and discussed highlighting the CBT process as effective to delay ductile fracture of the CP-Ti sheets.

Commercially pure titanium↗

Oxygen stoichiometry control of nanometric oxide compounds: The case of titanium ferrites

Three techniques have been coupled with an original device, based on H{sub 2}/H{sub 2}O equilibrium, controlling oxygen partial pressure: XRD, TGA and DC conductivity in order to characterize very reactive compounds such as nanometric powders. From XRD, both the structure and the oxygen stoichiometry (thanks to their lattice parameter) were investigated in situ. From TGA, it was the oxygen stoichiometry (thanks to mass gain or loss) which was determined. From DC conductivity, it was both the structure and the oxygen stoichiometry (thanks to the activation energy) which were obtained. The advantages were to determine very rapidly and with a small amount of powder the equilibrium conditions (T, pO{sub 2}) necessary to obtain the desired phase and stoichiometry. These methods have been evaluated for nanometric titanium ferrites. Two phenomena have been observed during the reducing process: the precipitation of a rhombohedral phase and a significant grain growth linked together. - Graphical abstract: XRD patterns of Fe{sub 3(1-{delta})}O{sub 4} nanometric powders obtained in situ during a reducing treatment. The stoichiometric compound was obtained by a thermal annealing at 460 deg. C under pO{sub 2}=3x10{sup -26} Pa ({Phi}{sub DRX}=100 nm). In inset, data of the experimental lattice parameter compared to the theoretical one. {alpha} represents the rhomboedrical phase which precipitates during this thermal treatment, then disappeared. Highlights: > The control of the deviation from oxygen stoichiometry is rarely consider in literature. > At the nanometric scale, it is necessary to develop synthesis routes under appropriate atmosphere. > These synthesis must be coupled with in situ characterization tools. > It opens the door to fast and precise studies concerning the evolution of nanometric materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Enhanced visible light activity of nano-titanium dioxide doped with multiple ions: Effect of crystal defects

Titanium dioxide photocatalysts co-doped with iron(III) and lanthanum(III) have been prepared through a modified sol-gel method. Doping with Fe{sup 3+} resulted in a relatively lower anatase to rutile phase transformation temperature, while La{sup 3+} addition reduced the crystal growth and thus retarded the phase transformation of titania nanoparticles. The presence of Fe{sup 3+} ions shifted the absorption profile of titania to the longer wavelength side of the spectrum and enhanced the visible light activity. On the other hand, La{sup 3+} addition improved the optical absorption of titania nanoparticles. Both the dopants improved the life time of excitons by proper transferring and trapping of photoexcited charges. In the present work, considerable enhancement in photocatalytic activity under visible light was achieved through synergistic effect of optimum concentrations of the two dopants and associated crystal defects. - Graphical abstract: Photocatalytic activity studies indicate a synergistic effect of dopants and crystal defects leading to an enhanced photochemical activity. Highlights: Black-Right-Pointing-Pointer An aqueous sol-gel synthesis of Fe{sup 3+} and La{sup 3+} co-doped TiO{sub 2} is being reported. Black-Right-Pointing-Pointer Optical and microstructural properties of titania were modified by co-doping. Black-Right-Pointing-Pointer Enhanced activity of titania by the crystal defects is being reported.

36 MATERIALS SCIENCE↗

Exfoliation of titanium oxide powder into nanosheets using hydrothermal reaction and its reassembly into flexible papers for thin-film capacitors

We have discovered a methodology to realize the fabrication of flexible metal oxide film using two-dimensional (2D) nanosheets. Atomic scale titanium oxide (TiO{sub x}) nanosheets were exfoliated from bulk TiO{sub x} powder that had a layered structure via the modified Sasaki’s method. The vacuum-assisted filtration generates films with laterally aligned TiO{sub x} nanosheets. The 2D sheet-like structure and hydrophilic nature of TiO{sub x} nanosheets enables the film consisting of TiO{sub x} nanosheets to be bendable. Also, we demonstrate the fabrication of electrochemical capacitors using this film. The mechanically flexible metal oxide film is expected to open up the possibility of fabricating flexible energy storage devices from 2D metal oxide nanosheets. - Graphical abstract: The modified Sasaki’s method, combined process of hydrothermal reaction and bulky ion exchange, enables to obtain TiO{sub x} monolayer nanosheets. The vacuum-assisted filtration generates bendable films with laterally aligned TiO{sub x} nanosheets. Also, we demonstrate the fabrication of electrochemical capacitors using this film. - Highlights: • TiO{sub x} single sheets, a novel 2-dimensional material, were exfoliated from bulk powders via the modified Sasaki’s method. • In our method, the acid treatment of TiO{sub x} bulk powders was simply modified by applying the hydrothermal reaction. • Then, the delamination procedures of large cation exchange were conducted following the method proposed by Sasaki et al. • Reassembly of TiO{sub x} sheets into flexible free-standing films was simply achieved via vacuum assisted filtration method. • TiO{sub x} films were used as a flexible supercapaictor electrode material.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mechanism and kinetics of carbide dissolution in near alpha Ti-5.6Al-4.8Sn-2Zr-1Mo-0.35Si-0.7Nd titanium alloy

The present work evaluates the influence of bulk carbon content and aging temperature on the stability of carbide in near alpha Ti-5.6Al-4.8Sn-2Zr-1Mo-0.35Si-0.7Nd titanium alloy. The carbide particles were formed during heat treatment in the {beta} phase field and preserved by water quenching. Subsequent aging treatments at 750-850 Degree-Sign C caused partial dissolution of these precipitates, as a result of the peritectoid reaction between the {beta} phase and carbide. The models based on interface reaction controlled dissolution, via uniform atomic detachment, dislocation mechanism or vacancy flow, yielded experimental predictions comparable to the observed dissolution kinetics. Furnace cooling after heat treatment in the {beta} phase field dissolved carbide particles completely, and the microstructure changed from acicular-like or block {alpha} to equiaxed {alpha} with increase of carbon content. - Highlights: Black-Right-Pointing-Pointer Carbide dissolution occurs at precipitate/matrix interfaces, forming {beta}-depleted zone. Black-Right-Pointing-Pointer Peritectoid reaction is responsible for drastic reduction of carbide volume fraction. Black-Right-Pointing-Pointer Slower dissolution rate is accounted by dislocation, vacancy flow, and curvature. Black-Right-Pointing-Pointer Lamellar changed to equiaxed {alpha} with increasing carbon from {beta} furnace cooling.

36 MATERIALS SCIENCE↗

Interfacial characterization of alumina-to-alumina joints fabricated using silver–copper–titanium interlayers

Two Ag–Cu–Ti interlayers with different compositions (Ag–35.3Cu–1.75Ti and Ag–26.7Cu–4.5Ti) were used to join sintered polycrystalline Al{sub 2}O{sub 3} having different amounts of porosity to investigate the effect of titanium and porosity contents on evolution of interfacial chemistry and microstructures. X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and energy dispersive spectroscopy (EDS) were used to characterize the interfacial microstructure. Two reaction layers, Ti{sub 2}O and Cu{sub 3}Ti{sub 3}O, were found at the interface of Ag–Cu–Ti interlayers and Al{sub 2}O{sub 3} using a series of simulated and experimental selected area diffraction patterns (SADP) of TEM and EDS. The total thickness of Ti{sub 2}O and Cu{sub 3}Ti{sub 3}O reaction layers at the interfaces increases with increasing amounts of Ti in the Ag–Cu–Ti interlayers but is independent of the porosity content in the Al{sub 2}O{sub 3}. Two possible formation mechanisms of Ti{sub 2}O and Cu{sub 3}Ti{sub 3}O reaction layers at the interface of Ag–Cu–Ti interlayers and Al{sub 2}O{sub 3} have been proposed based on the interfacial characterization performed in the present study. - Highlights: • Effect of alumina porosity and % Ti in interlayer on interface structure delineated • SEM, EDS, XRD, TEM with SADP used to delineate phases, compositions, crystallography • Ti{sub 2}O and Cu{sub 3}Ti{sub 3}O reaction layers identified and their formation mechanisms proposed.

36 MATERIALS SCIENCE↗

Microstructure characterization and nano & micro hardness of tri-modal microstructure of titanium alloy under different hot working conditions

Highlights: • The contents and sizes of α{sub p} and α{sub l} are determined by the processing parameters of first and second step. • The morphology of α{sub s} embedded in β phase is determined by the accumulated distortional strain energy and dislocations. • α{sub p} becomes harder as the strain rate of the first step increases due to the constantly enhanced work hardening effect. • β{sub t} is always harder than α{sub p} and α{sub l} due to the interfacial-strengthening effect. • The hardness of α{sub l} makes the greatest contribution in the integrated hardness of tri-modal microstructure. - Abstract: In this work, the dependences of tri-modal microstructure parameters and corresponding nano & micro hardness on through-process processing parameters were quantitatively studied during the three-step thermo-mechanical processing of TA15 titanium alloy. It is found that the processing parameters of first step, especially for the deformation temperature and strain rate, mainly affect primary equiaxed α (α{sub p}) through the α → β phase transformation and the competition between dynamic recovery and dynamic recrystallization. The second processing step primarily affects the content and thickness of lamellar α (α{sub l}). In the third processing step, compared with low-temperature aging, normal annealing provides sufficient driving force for α{sub l} and secondary lamellar α (α{sub s}) growing, which leads to thicker α{sub l} and α{sub s}. As for the nano & micro hardness, in one sample undergoing different process, transformed β matrix (β{sub t}) is always harder than α{sub l} and α{sub s} due to the interfacial-strengthening effect. In addition, with increasing strain rate of the first step, α{sub p} becomes harder due to the constantly enhanced work hardening effect while the hardness of β{sub t} varies little because of the competition between interfacial strengthening and distribution disorder degree. However, the nano hardness of α{sub l} decreases firstly and then increases with strain rate, which presents the same trend with the micro hardness of integrated hardness at different processing conditions.

36 MATERIALS SCIENCE↗

High-temperature deformation behavior and microstructural characterization of high-Mn bearing titanium-based alloy

Highlights: • The hot deformation behavior of a biomedical low-cost Ti-10Mn alloys was studied. • The flow curves of the alloy display periodic serrations attributed to dynamic strain aging. • Mn alloying increases the activation energy to 243 kJ/mol compared to pure Ti. • The dynamic recovery is more effective than dynamic recrystallization at hot deformation. - Abstract: Ti-Mn alloys exhibit an excellent potential for biomedical applications as well as structural engineering applications, especially in the aerospace industry. In order to control and enhance grain structure during the manufacturing of Ti-Mn alloys and thereby help to enhance mechanical properties such as strength and toughness, we studied the hot-deformation behavior of βTi-10Mn alloys. Isothermal compression tests were conducted in the strain rate range of 0.01–10 s{sup −1} and temperatures in the range of 850–1000 °C using a Gleeble thermomechanical simulator. High-temperature flow stress curves exhibited discontinuous yielding and pronounced periodic serrations without any strain hardening during compression straining of these alloys. Such peculiar behavior of this alloy is due to active dynamic strain aging in its β-bcc structure. Metallographic observations by electron-backscattered diffraction (EBSD) analysis revealed that dynamic recovery (DRV) is more active than continuous dynamic recrystallization (CDRX) when the alloy is deformed at high strain rates, i.e. higher than 1 s{sup −1}. Furthermore, the constitutive behavior of the alloy was modeled and the apparent hot-deformation activation energy of the alloy was estimated to be 243 kJ/mol, which is ~60% higher than the self-diffusion energy in pure titanium.

36 MATERIALS SCIENCE↗