Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STRESS CORROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 811 records · Page 45

Structural Materials for Fission and Fusion Energy

Structural materials represent the key for containment of nuclear fuel and fission products as well as reliable and thermodynamically efficient production of electrical energy from nuclear reactors. Similarly, high-performance structural materials will be critical for the future success of proposed fusion energy reactors, which will subject the structures to unprecedented fluxes of high-energy neutrons along with intense thermomechanical stresses. Advanced materials can enable improved reactor performance via increased safety margins and design flexibility, in particular by providing increased strength, thermal creep resistance and superior corrosion and neutron radiation damage resistance. In many cases, a key strategy for designing highperformance radiation-resistant materials is based on the introduction of a high, uniform density of nanoscale particles that simultaneously provide good high temperature strength and neutron radiation damage resistance.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Oxidation of Superalloys in Extreme Environments

Superalloys like 718 and its derivatives primarily rely on the formation of an external Cr-rich oxide layer or scale for environmental protection at high temperatures. Operating conditions where environmental resistance is more of a concern generally involve higher temperatures or more corrosive environments, especially where S is present, usually due to fuel impurities. With clean fuels, the presence of water vapor and oxygen, such as a combustion environment in a natural gas-fired turbine, chromia forms a volatile oxy-hydroxide leading to accelerated Cr loss. In laboratory experiments, mass losses are measured due to this volatilization. For sulfidizing or hot corrosion environments, the role of alloy and coating composition on corrosion resistance will be reviewed. An increasing area of interest is the interaction between environmental degradation and the stress-induced deformation of the superalloy including the influence of oxidation-resistant coatings on mechanical properties. Strategies to study this interaction will be discussed.

36 MATERIALS SCIENCE↗

Characterization of texture and grain boundary character distributions of selective laser melted Inconel 625 alloy

Highlights: • <110> texture along layer build direction was generated in as-SLMed Inconel 625. • The stress relief process dominates texture and GBCD evolution. • SLMed IN 625 alloy can be GBEed via suitable post annealing. - Abstract: Select laser melting (SLM) is one of the practical metal additive manufacturing processes to fabricate complex structures. The inhomogeneous microstructure and high residual stress are typically resulted from a non-uniform melting and rapid solidification during a SLM process, which has the significant impact on part dimensional instability, corrosion resistance, and mechanical properties. The bulk of current research is limited to the general characterization of grain size, texture, and mechanical properties. However, grain boundary character distribution (GBCD) and its relationship with texture are yet to be understood. This study has shown that the preferred <110> along building direction and <100> along laser scanning direction were produced. The high density of low angle grain boundary (LAGB) can be an indicator of residual stress levels in the as-SLMed samples. The newly-developed ∑3, ∑9 and ∑27 grain boundaries were heavily populated, and the cluster of grains interfaced by ∑3{sup n} (n = 0, 1, 2…) was introduced at the expense of LAGB only at high recrystallization annealing (1150°C or over). The research results suggest that GBCD optimization be possible in the SLMed Inconel 625 alloy via suitable post annealing, which allows improving intergranular corrosion resistance and enhancing mechanical properties.

36 MATERIALS SCIENCE↗

Dose and dose rate effects on the microstructural and mechanical stability of long-range ordered precipitates in Inconel 718

Nickel-based alloys offer exceptional mechanical properties and corrosion resistance for various applications in extreme environments such as high neutron flux, temperature, and stress. Precipitates, resulting from thermal treatments, increase the strength and creep resistance of these alloys. Here, heavy ion irradiation is shown to destabilize the γ' and γ" precipitates in Inconel 718 nickel-based alloy by disordering and dissolution processes. Transmission electron microscopy and atom probe tomography reveal that the disordering and dissolution rates of the precipitates are proportional to both irradiation dose and dose rate. Irradiation induced disordering occurs at a higher rate than the dissolution. From analyzing the hardening contributions, microscale mechanical results suggest radiation-induced disordering is responsible for the majority of the softening response at low dose. In addition, low dose radiation-induced disordering results in strain localization and is believed to be the primary cause for the drastic degradation of uniform elongation and toughness in irradiated Inconel 718.

36 MATERIALS SCIENCE↗

Photothermal Atomic Force Microscopy Coupled with Infrared Spectroscopy (AFM-IR) Analysis of High Extinction Coefficient Materials: A Case Study with Silica and Silicate Glasses

Photothermal atomic force microscopy coupled with infrared spectroscopy (AFM-IR) brings significant value as a spatially resolved surface analysis technique for disordered oxide materials such as glasses, but additional development and fundamental understanding of governing principles is needed to interpret AFM-IR spectra, since the existing theory described for organic materials does not work for materials with high extinction coefficients for infrared (IR) absorption. This paper describes theoretical calculation of a transient temperature profile inside the IR-absorbing material considering IR refraction at the interface as well as IR adsorption and heat transfer inside the sample. Furthermore, this calculation explains the differences in peak positions and amplitudes of AFM-IR spectra from those of specular reflectance and extinction coefficient spectra. It also addresses the information depth of the AFM-IR characterization of bulk materials. AFM-IR applied to silica and silicate glass surfaces has demonstrated novel capability of characterizing subsurface structural changes and surface heterogeneity due to mechanical stresses from physical contacts, as well as chemical alterations manifested in surface layers through aqueous corrosion.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

THE NEED FOR A NEW JOINING TECHNOLOGY FOR THE CLOSURE WELDING OF RADIOACTIVE MATERIALS CONTAINERS

One of the activities associated with cleanup throughout the Department of Energy (DOE) complex is packaging radioactive materials into storage containers. Much of this work will be performed in high-radiation environments requiring fully remote operations, for which existing, proven systems do not currently exist. These conditions demand a process that is capable of producing acceptable (defect-free) welds on a consistent basis; the need to perform weld repair, under fully-remote operations, can be extremely costly and time consuming. Current closure welding technology (fusion welding) is not well suited for this application and will present risk to cleanup cost and schedule. To address this risk, Fluor and the Pacific Northwest National Laboratory (PNNL), are proposing that a new and emerging joining technology, Friction Stir Welding (FSW), be considered for this work. FSW technology has been demonstrated in other industries (aerospace and marine) to produce near flaw-free welds on a consistent basis. FSW is judged capable of providing the needed performance for fully-remote closure welding of containers for radioactive materials for the following reasons: FSW is a solid-state process; material is not melted. As such, FSW does not produce the type of defects associated with fusion welding, e.g., solidification-induced porosity, cracking, distortion due to weld shrinkage, and residual stress. In addition, because FSW is a low-heat input process, material properties (mechanical, corrosion and environmental) are preserved and not degraded as can occur with 'high-heat' fusion welding processes. When compared to fusion processes, FSW produces extremely high weld quality. FSW is performed using machine-tool technology. The equipment is simple and robust and well-suited for high radiation, fully-remote operations compared to the relatively complex equipment associated with the fusion-welding processes. Additionally, for standard wall thicknesses of radioactive materials containers, the FSW process can perform final closure welding in a single pass (GTAW requires multiple passes) resulting in increased productivity. Together, the performance characteristics associated with FSW, i.e., high weld quality, simple machine-tool equipment and increased welding efficiency, are expected to reduce risk to upcoming DOE radioactive materials packaging campaigns. FSW technology requires some development/adaptation for this application, along with approval from the governing code of construction prior to production operations. This paper addresses the need for a new joining technology, a description of the FSW process and why it is well-suited for this application, and several activities required for commercialization.

42 ENGINEERING↗

Polarization Losses under Accelerated Stress Test Using Multiwalled Carbon Nanotube Supported Pt Catalyst in PEM Fuel Cells

The electrochemical behavior for Pt catalysts supported on multiwalled carbon nanotubes and Vulcan XC-72 in proton exchange membrane fuel cells under accelerated stress test was examined by cyclic voltammetry, electrochemical impedance spectroscopy, and polarization technique. Pt catalyst supported on multiwalled carbon nanotubes exhibited highly stable electrochemical surface area, oxygen reduction kinetics, and fuel cell performance at a highly oxidizing condition, indicating multiwalled carbon nanotubes show high corrosion resistance and strong interaction with Pt nanoparticles. The Tafel slope, ohmic resistances, and limiting current density determined were used to differentiate kinetic, ohmic, mass-transfer polarization losses from the actual polarization curve. Kinetic contribution to the total overpotential was larger throughout the stress test. However, the fraction of kinetic overpotential decreased and mass-transfer overpotential portion remained quite constant during accelerated stress test, whereas the fraction of ohmic overpotential primarily originating from severe proton transport limitation in the catalyst layer increased under the anodic potential hold.

30 DIRECT ENERGY CONVERSION↗

Influence of surface modifications on pitting corrosion behavior of nickel-base alloy 718. Part 1: Effect of machine hammer peening

The effect of surface modifications induced by machine hammer peening on pitting corrosion behavior of nickel-base alloy 718 in a 3.5 wt.% NaCl solution is investigated. Severe work hardening and high compressive residual stress are generated with surface smoothing and microstructure evolution in terms of formation of nano-grains and nano-twins in the near surface region after machine hammer peening. Electrochemical tests results show that machine hammer peening has a beneficial influence on the corrosion resistance, indicated by a significant increase of the critical pitting potential (+134 mV) accompanied with lower corrosion current density and higher polarization resistance.

36 MATERIALS SCIENCE↗

Diagnosis of PV Cell Antireflective Coating Degradation Resulting From Hot-Humid High-Voltage Potential Aging

Corrosion of the antireflective coating on a photovoltaic cell ("ARc corrosion") has previously been observed in studies using hot-humid test conditions with external high-voltage (HV) bias. This study primarily focuses on known vulnerable legacy aluminum back surface field cells in mini-modules (MiMos) put through comparative stepped stress tests. Each cell type had MiMos at +1500 V, -1500 V, or unbiased ("Voc") potential, which were sequentially subjected to test conditions of 60 degrees C/60% relative humidity (RH) for 96 h, as in International Electrotechnical Commission Technical Specification 62804-1; 70 degrees C/70% RH for 200 h; and 85 degrees C/85% RH for 200 h. Characterizations at each step included visual camera and electroluminescence (EL) imaging, colorimetry, and current-voltage curve tracing. Final characterizations included: Suns-Voc, spatial mapping of external quantum efficiency, high-resolution photoluminescence, EL, and dark lock-in thermography imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy, and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos from previous studies that underwent stepped HV aging and separate outdoor aged full-sized modules. ARc corrosion was specifically seen for the glass/encapsulant/cell side of the +1500 V (HV+) stressed MiMos and modules. Appearance, color, and reflectance were the most distinguishing characteristics relative to glass corrosion, gridline corrosion and delamination, and other concurrent degradation modes. SEM/EDS and SAM identified the conversion of silicon nitride to hydrated silica, hydrous silica, or hydrated amorphous silica, which preferentially occurred at the edges and tips of the pyramidal textured cell surface.

14 SOLAR ENERGY↗

Damp Heat Induced Degradation of Silicon Heterojunction Solar Cells With Cu-Plated Contacts

Damp heat exposure is one of the most stringent environments for testing the durability of solar cells in packaged modules. Damp heat stresses and induces a variety of degradation modes in solar cells and modules: for example, moisture-induced corrosion of electrodes and interconnections, deterioration of polymeric materials, and/or thermally activated diffusion processes. To screen for these and other potential degradation modes, we subject one-cell modules containing silicon heterojunction (SHJ) solar cells with Cu-plated contacts to extended damp heat tests at 85 °C/85% relative humidity. SHJ cells were laminated with two common encapsulants: ethylene vinyl acetate (EVA) and polyolefin elastomer (POE), and two constructions: glass-backsheet and glass-glass. We observe degradation in all components of solar cell maximum power (PMP): current, voltage, and fill factor, and find evidence of increased carrier recombination and nonideal diode behavior with increasing stress. For glass-backsheet constructions, EVA samples generally degrade more than POE by a factor of approximately 1.5x PMP, and the different encapsulants produce different degradation patterns. Similar trends are observed in glass-glass modules, but to a lesser degree. In a different experiment, we observe a decrease in effective minority carrier lifetime of nonmetallized SHJ precursors measured after damp heat. This implies that some degradation unrelated to the contacts is to be expected and confirms the observation of increasing recombination.

14 SOLAR ENERGY↗

Diagnosis of PV Cell Antireflective Coating Degradation Resulting from Hot-Humid, High Voltage Potential Aging

Corrosion of the antireflective coating on a photovoltaic cell ("ARc corrosion") has previously been observed in studies using hot-humid test conditions with external high-voltage (HV) bias. This study primarily focuses on known vulnerable, legacy aluminum back surface field (Al-BSF) cells in mini-modules (MiMos) put through comparative stepped stress tests. Each cell type had MiMos at +1500 V, -1500 V, or unbiased ("Voc") potential, which were sequentially subjected to test conditions of 60deg C/60% relative humidity (RH) for 96 h, as in International Electrotechnical Commission (IEC) Technical Specification 62804-1; 70 deg C/70% RH for 200 h; and 85 deg C/85% RH for 200 h. Characterizations at each step included visual camera and electroluminescence (EL) imaging, colorimetry, and current-voltage (I-V) curve tracing. Final characterizations included: Suns-Voc; spatial mapping of external quantum efficiency (EQE); high-resolution photoluminescence (PL), EL, and dark lock-in thermography (DLIT) imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS), and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos from previous studies that underwent stepped HV aging and separate outdoor aged full-sized modules. ARc corrosion was specifically seen for the glass/encapsulant/cell side of the +1500V (HV+) stressed MiMos and modules. Appearance, color, and reflectance were the most distinguishing characteristics relative to glass corrosion, gridline-corrosion and -delamination as well as other concurrent degradation modes. SEM/EDS and SAM identified conversion of silicon nitride to hydrated silica, hydrous silica, or hydrated amorphous silica, which preferentially occurred at the edges and tips of the pyramidal textured cell surface.

14 SOLAR ENERGY↗

Enhancement of Hot Corrosion Resistance of Modified 9Cr-1Mo Steel Through Surface Nanostructuring and Pre-oxidation

Nanosize grains of ~ 65 nm were developed with large misorientation angles of grain boundaries in surface region of normalized and tempered modified 9Cr-1Mo steel by ultrasonic shot peening (USSP) with hard steel balls of 3 mm diameter. The surface roughness and the depth of nanostructured surface region were found to increase with the duration of USSP from 0.5 to 5 min. Hot corrosion tests were performed for the Un-USSP and the samples USSPed for the durations of 0.25 and 1.5 min and also for the samples subjected to USSP and subsequently pre-oxidation at 600 °C for 4 h. The hot corrosion resistance at 600 °C under 100% NaCl coating was significantly improved by USSP for 1.5 min and subsequent pre-oxidation at 600 °C for 4 h. The results are discussed in terms of the formation of more uniform and effective protective iron–chromium oxide layer on the USSPed surface from the subsequent pre-oxidation treatment, prior to hot corrosion of the specimens under 100% NaCl coating at 600 °C.

36 MATERIALS SCIENCE↗

Review of SiC material development for nuclear fusion applications: Cross-cutting research and emerging opportunities

The SiC-based materials, particularly SiC-fiber-reinforced SiC matrix (SiC/SiC) composites, show strong potential for structural and functional applications in future fusion power plants because they can operate at high temperatures with a range of coolants and breeders, thereby enabling higher energy conversion efficiency. Here, this paper presents recent advancements in the development of SiC-based materials, focusing on processing techniques and material performance and resistance under fusion-relevant environments. The processing activities have emphasized near-net-shape fabrication and the joining of SiC subcomponents, with processing methods and material compositions informed by previous irradiation experiments on various grades of SiC. Research on irradiation effects has remained focused on degradation mechanisms and the microstructural optimization of SiC/SiC composites irradiated to high neutron damage levels. Analysis of irradiation defects in SiC has advanced via the application of cutting-edge characterization methods, among which Raman spectroscopy is becoming a common tool to assess atomic-scale chemical disorder. Fusion–fission crosscutting irradiation research has explored combined effects in SiC/SiC composites with application-relevant geometries, including bowing of SiC/SiC composite channels under neutron flux gradients, stress evolution in SiC/SiC composite tubes under through-thickness temperature gradients, and irradiation-enhanced corrosion in SiC. Finally, research opportunities for component testing and assessment under fusion-relevant conditions, in support of emerging concepts from the private fusion sector, are discussed.

Advanced manufacturing↗

The performance of NSF in BWR operating conditions - 2016-0062

NSF is a zirconium alloy in the zirconium-tin-niobium-iron family. The nominal alloy content is 1 % tin, 1 % niobium, and 0.4 % iron. The initial targeted component for NSF in boiling water reactors (BWRs) is the fuel assembly channel. A BWR fuel channel encases the fuel bundle such that boiling is confined within the channel while the water remains solid outside the channel. The BWR fuel channel also defines the gap between the bundles where the cruciform control blade inserts and withdraws to control the criticality of the core. The key performance requirements of the BWR fuel channel are dimensional stability (including both shape and thickness) and adequate mechanical properties to withstand the applied stresses. The distortion mechanisms that affect dimensional stability are fluence gradient-induced bow, shadow corrosion-induced bow, and elastic and creep bulge. Although NSF is known to have improved irradiation growth characteristics compared with both Zircaloy-2 and Zircaloy-4 that translates to increased dimensional stability in fuel channels, the BWR corrosion performance, tensile properties, and irradiation creep performance are less well known. This paper reports on the physical metallurgy of NSF, oxide thickness and hydrogen content after in-reactor operation, mechanical properties (both irradiated and unirradiated), in-reactor creep response, and irradiation growth and bow of NSF channels. (authors)

36 MATERIALS SCIENCE↗

Vacancy-mediated transport and segregation tendencies of solutes in FCC Ni under diffusional creep

Nickel-based alloys are known for their excellent corrosion resistance and high-temperature strength. However, at high temperatures, polycrystals experience grain boundary-stress-driven vacancy diffusion leading to diffusion-driven creep. Understanding the fundamentals of defect migration is essential to predict diffusion creep behavior. In this talk, we explore the Nabarro-Herring diffusion creep and the associated solute segregation that is likely to result from the different diffusivities of the solute and solvent elements. Density functional theory calculations are performed to determine the formation, migration and binding energies of the solute and vacancy defects in stress-free and stressed states. The dilute-limit transport coefficients are then calculated using the self-consistent mean field theory as implemented in the Kinetic Cluster Expansion (KineCluE) code. Predictions of diffusion creep strain rates and solute segregation are then presented for various solutes, stress and temperatures. This work opens research avenues for exploration of diffusion creep via characterization of elemental segregation to grain boundaries.

36 MATERIALS SCIENCE↗

Identifying multiple synergistic factors on the susceptibility to stress relaxation cracking in variously heat-treated weldments

The 347H austenitic stainless steel has been widely used for pressure vessels and pipeline (PVP) applications due to its excellent creep and corrosion resistance, which fit ideally to the harsh conditions in petrochemical industries, fossil fuel or nuclear power plants, and modern energy storages. However, a failure mode has been commonly observed with cracks emerging at the heat affected zone (HAZ) of weldments during post-weld heat treatment (PWHT) or under intermediate to high temperature service conditions. This phenomenon is termed as Stress Relaxation Cracking (SRC) since the purpose of PWHT is to relieve the welding-induced residual stress fields, or as Stress Age Cracking (SAC) if failure happens during service. A leading literature explanation of this failure suggests that the residual stress relaxation and the precipitation dissolution and/or re-precipitation occur in the same temperature range, which can lead to locally high strains and thus to crack at the grain boundaries. Since in situ spatial measurements of residual stress fields, microstructural evolution, and failure processes are nearly infeasible, this work recourses to a micromechanical finite element framework that models the high temperature failure as the nucleation and growth of grain boundary cavities, whereas various parameters such as thermomechanical loading history and its evolution, the competition of grain-interior dislocation creep and grain-boundary diffusion in failure lifetime, and microstructural heterogeneities (such as the precipitate free zone near grain boundaries) can be quantitatively incorporated. It can be concluded from these microstructure-explicit simulations that an accurate knowledge of residual stress evolution and a carefully calibrated set of material constitutive parameters are the essential prerequisites for lifetime predictions. The understanding of individual governing factors also leads to a mechanistic interpretation of the observed SRC susceptibility C-curves. In conclusion, these results suggest that the criticality of residual stress evolution, but not the precipitation-induced local strains, be the leading factor for SRC.

347H stainless steel weldments↗

Spectral changes in Si–O–Si stretching band of porous glass network upon ingress of water

Water ingress into porous glass can induce internal stress, resulting in strains in chemical bonds of the network. For silica and silicate glasses, the position of Si–O–Si stretching mode in infrared spectroscopy is known to vary with the degree of strain in the Si–O network. Then, one could hypothesize that the stress due to water ingress could be probed with infrared spectroscopy. We tested this hypothesis using porous layers formed through aqueous corrosion on a model nuclear waste glass. The porosity and thickness of the porous layer were determined using ellipsometry. The humidity-dependent infrared spectra of the samples showed red-shifts of the Si–O–Si stretching band; however, it was difficult to deconvolute the spectral change due to variation of effective refractive index of the sample upon water ingress. Thus, it was infeasible to unambiguously determine the internal stress of porous glass network upon water ingress using the infrared spectroscopy alone.

36 MATERIALS SCIENCE↗

Microstructure and in-service degradation of baffle former bolts – in-core components of light water reactors

This report presents a microstructure evaluation of the baffle former bolt, a commercial pressurized water reactor component. Using SEM, EDS, and EBSD analysis the material was identified as AISI 316 steel with an annealed austenite microstructure. Findings include abnormal grain growth in a fraction of the grains and the absence of retained ferrite. Notable observations include an overlapping of pre- and post-irradiation deformation, including defect-free channel formation as an active deformation mechanism in the near-surface layer of BFB. Specimen surfaces, exposed to high-temperature, high-pressure water, exhibited signs of in-service corrosion degradation. EBSD and EDS analyses highlighted intergranular corrosion, possible grain boundary oxidation with depths less than 3 µm, and, unexpectedly, short cracks filled with Cr-rich oxides measuring around 5-6 µm. The presence of defect-free channels from EBSD data suggests episodes of high mechanical stresses during service. The specimens provide a potentially unique insight into the in-service degradation of NPP components, strain localization, and crack initiation processes. An intact corrosion layer reveals a complex component's in-service history. Further research is underway for a detailed analysis.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗