Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Phase transformations”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 811 records · Page 45

Effect of nickel on the kinematic stability of retained austenite in carburized bearing steels – In-situ neutron diffraction and crystal plasticity modeling of uniaxial tension tests in AISI 8620, 4320 and 3310 steels

The presence of kinematically metastable retained austenite in the microstructure of bearing components can significantly affect the macro and micro-mechanical material response. In the present work, the influence of Ni on the stability of the retained austenite within three different grades of high carbon bearing steel using in-situ neutron diffraction is investigated. For the first time, the results show that presence of Ni increases the stability of the austenite in the elastic regime whereas the transformation rate remains unaffected. Crystal plasticity finite element (CPFE) modeling was used to study the deformation in these three steels and shows that the predominant factor causing the difference in mechanical behavior of these steels is the austenite stability. Finally, the elastic and plastic response of the matrix martensite was found to be identical among all specimens while the austenite demonstrates similar elastic behavior but remarkably different stabilities under monotonic loading.

36 MATERIALS SCIENCE↗

Femtosecond diffraction studies of the sodium chloride phase diagram under laser shock compression

The phase diagram of sodium chloride (NaCl) under laser shock compression has been studied at Linac Coherent Light Source (LCLS) at the x-ray free-electron laser facility. Both solid–solid (B1 → B2) and solid–liquid (B2 → liquid) transitions have been observed along the Hugoniot over nanosecond time scales. By combining structural measurements through in situ x-ray diffraction, pressure determination through velocimetry, and a thermal equation-of-state, the shock-compressed data are used to constrain the phase diagram of NaCl. Transformation into the B2 phase is found to occur at 28(2) GPa, and B2–liquid coexistence is observed between 54(4) and 66(6) GPa, with near full melt at 66(6) GPa. Late-time pressure release from an initial shocked B2-state results in a B2 → B1 back transformation. Our results show agreement with previous static compression data, suggesting that the time scale for melting is very rapid and that equilibrium states in NaCl are being accessed over nanosecond time scales. Finally, a multiphase equation-of-state description of NaCl incorporated into a one-dimensional hydrocode is used to interpret pressure and temperature evolution over these rapid time scales.

36 MATERIALS SCIENCE↗

Transformation-induced fracture toughening in CuAlBe shape memory alloys: A phase-field study

Stress-induced transformation ahead of a crack tip can relax the stress concentration and produce fracture toughness in shape memory alloys (SMAs). In this manuscript, we utilize a nonisothermal phase-field model (PFM) to study the martensitic transformation induced crack tip toughening in CuAlBe SMA. The force-displacement curve, transformation zone and high stress zone in single crystalline samples show high dependency on the grain orientation with respect to the crack alignment. Comparison between isothermal and non-isothermal simulations reveals that the transformation-induced self-heating decreases the toughening capability by increasing the critical transformation stress. Investigating the high stress zones in CuAlBe and the nontransforming CuAl alloy shows that the toughening is obtained by redistributing the stress concentration far from the crack tip, as the high stress zone follows the tip of the transformation zone. Increasing the acuity of the crack tip is found to generate more symmetric martensite wings on both side of the crack axis and a more localized high stress zone. The polycrystal specimen displays higher toughening due to the internal constraints related to the presence of various grains with difference orientations. Depending on the orientation of the grain inclosing the crack tip, the toughening can be lower or higher. Finally, coincidence of the crack tip with a triple junction is found to improve the toughening behavior.

42 ENGINEERING↗

Lead-Free Cs 4 CuSb 2 Cl 12 Layered Double Perovskite Nanocrystals

Concerns about the toxicity of lead-based perovskites have aroused great interest for the development of alternative lead-free perovskite-type materials. Recently, theoretical calculations predict that Pb 2+ cations can be substituted by a combination of Cu 2+ and Sb 3+ cations to form a vacancy-ordered layered double perovskite structure with superior optoelectronic properties. However, accessibilities to this class of perovskite-type materials remain inadequate, hindering their practical implementations in various applications. Here, we report the first colloidal synthesis of Cs 4 CuSb 2 Cl 12 perovskite-type nanocrystals (NCs). The resulting NCs exhibit a layered double perovskite structure with ordered vacancies and a direct bandgap of 1.79 eV. A composition-structure-property relationship has been established by investigating a series of Cs 4 Cu x Ag 2-2x Sb 2 Cl 12 perovskite-type NCs (0 ≤ x ≤ 1). The composition-induced crystal structure transformation, thus the electronic bandgap evolution has been explored by experimental observations and further confirmed by theoretical calculations. Taking advantages of both the unique electronic structure and solution processability, we demonstrate that the Cs 4 CuSb 2 Cl 12 NCs can be solution-processed as high-speed photodetectors with ultrafast photo-response and narrow bandwidth. We anticipate that our study will prompt future research to design and fabricate novel and high-performance lead-free perovskite-type NCs for a range of applications.

25 ENERGY STORAGE↗

Clinkerless ultra-high strength concrete based on alkali-activated slag at high temperatures

This work investigates the degradation mechanisms of clinkerless alkali-activated slag based ultra-high strength concrete (AAS-UHSC) upon exposure to high temperatures up to 800 °C. The heat-induced mechanical, mineralogical, molecular, microstructural, and pore structure alterations of AAS-UHSC prepared with various activator types, water-to-powder ratios, and fiber incorporation are studied. The results demonstrate the beneficial roles of potassium incorporation on improving the thermal stability and integrity of AAS-UHSC, via suppressing deleterious crystallization and transformation of aluminosilicate phases at high temperature. In contrast to Portland cement clinker-based UHSC, no sign of explosive spalling is observed in AAS-UHSC, likely due to the presence of microcracks that enhance the pore network connectivity. The mechanical degradation of AAS-UHSC at high temperature below 600 °C is resulted from dehydration and decomposition of phases and consecutive thermal cracking, together with enlarged porosity and coarsened pore structure. As the temperature rising to 800 °C, crystallization and transformation of phases, as well as formation of porous microstructure, considerably aggravate the mechanical degradation of AAS-UHSC. In contrast to the thermal damage mitigation by polymeric fibers in conventional UHSC, the fiber incorporation has little positive impact on the thermal resistance of AAS-UHSC.

36 MATERIALS SCIENCE↗

Decoding Li + /Na + Exchange Route Toward High-Performance Mn-Based Layered Cathodes for Li-Ion Batteries

Li + /Na + exchange has been extensively explored as an effective method to prepare high-performance Mn-based layered cathodes for Li-ion batteries, since the first report in 1996 by P. G. Bruce (Nature, 1996. 381, 499–500). Understanding the detailed structural changes during the ion-exchange process is crucial to implement the synthetic control of high-performance layered Mn-based cathodes, but less studied. Herein, in situ synchrotron X-ray diffraction, density functional theory calculations, and electrochemical tests are combined to conduct the systemic studies into the structural changes during the ion-exchange process of an Mn-only layered cathode O3-type Li 0.67 [Li 0.22 Mn 0.78 ]O 2 (LLMO) from the corresponding counterpart P3-type Na 0.67 [Li 0.22 Mn 0.78 ]O 2 (NLMO). The temperature-resolved observations combined with theoretical calculations reveal that the Li + /Na + exchange is favorable thermodynamically and composited with two tandem topotactic phase transitions: 1) from NLMO to a layered intermediate through ≈60% of Li + /Na + exchange. 2) then to the final layered product LLMO through further Li insertion. Moreover, the intermediate-dominate composite is obtained by slowing down the exchange kinetics below room temperature, showing better electrochemical performance than LLMO obtained by the traditional molten-salt method. Finally, the findings provide guides for the synthetic control of high-performance Mn-based cathodes under mild conditions.

25 ENERGY STORAGE↗

Processing and properties of hafnium-doped tin-modified lead zirconate titanate 95/5 ceramics

Niobium (Nb)-doped lead-tin-zirconate-titanate (PSZT) ceramics near the lead-zirconate-titanate 95/5 orthorhombic AFE-rhombohedral FE morphotropic phase boundary (PSZT 13.5/81/5.5 -1.6Nb) were prepared with up to 10 mol.% of hafnium (Hf) substituted for zirconium. The ceramics were prepared by a traditional solid-state synthesis route and sintered to near full density at 1150°C for 6 h in sealed alumina crucibles with self-same material as the lead vapor source. All compositions were ~98% dense with no detectable secondary phases by X-ray diffraction. The grain size was ~3 μm for all compositions, consisting of equiaxed grains with intergranular porosity. The compositions exhibited remnant polarization values of ~32 μC/cm 2 . Depolarization by the hydrostatic pressure-induced FE-AFE phase transition occurred at 310 MPa for all compositions, resulting in a total depolarization output of 32.4 μC/cm 2 for the PSZT ceramics. Evaluation of the R3c-R3m and R3m-Pm $\bar{3}$ m phase transition temperatures by impedance spectroscopy showed temperatures on heating ranging from 86 to 92°C and 186 to 182°C, respectively, for increasing nominal Hf content. Thermal hysteresis of the phase transitions was also observed in the ceramics, with the transition temperature on cooling being 1–4°C lower. The study demonstrated that the PSZT ceramics are relatively insensitive to variations in Hf content in the range of 0 to 10 mol.%.

36 MATERIALS SCIENCE↗

Processing and properties of PSZT 95/5 ceramics with varying Ti and Nb substitution

Niobium doped lead-tin-zirconate-titanate ceramics near the PZT 95/5 orthorhombic AFE – rhombohedral FE morphotropic phase boundary Pb 1-0.5y (Zr 0.865-x Ti x Sn 0.135 ) 1-y Nb y O 3 were prepared according to a 2 2+1 factorial design with x = 0.05, 0.07 and y = 0.0155, 0.0195. The ceramics were prepared by a traditional solid-state synthesis route and sintered to near full density at 1250°C for 6 hours. All compositions were ~98% dense with no detectable secondary phases by XRD. The ceramics exhibited equiaxed grains with intergranular porosity and grain size was ~5 μm, decreasing with niobium substitution. Compositions exhibited remnant polarization values of ~32 μC/cm 2 , increasing with Ti substitution. Depolarization by the hydrostatic pressure induced FE-AFE phase transition was drastically affected by variation of the Ti and Nb substitution, increasing at a rate of 113 MPa / 1% Ti and 21 MPa / 1% Nb. Total depolarization output was insensitive to the change in Ti and Nb substitution, ~32.8 μC/cm 2 for the PSZT ceramics. The R3c-R3m and R3m-Pm3m phase transition temperatures on heating ranged from 90 to 105°C and 183 to 191°C, respectively. Ti substitution stabilized the R3c and R3m phases to higher temperatures, while Nb substitution stabilized the Pm3m phase to lower temperatures. Thermal hysteresis of the phase transitions was also observed in the ceramics, with transition temperature on cooling being as much as 10°C lower.

36 MATERIALS SCIENCE↗

Iron Oxide Reduction Rate Affects Iron Product Morphology

Magnetite concentrates from different parts of the Mesabi Range, exhibiting varying tendencies to encapsulate, were reduced using thermogravimetric analysis (TGA) and a high-temperature confocal scanning laser microscope (CSLM). Gas-phase mass-transfer conditions were intentionally varied by employing two reactors with different geometries: the TGA produced significantly slower reduction, whereas the CSLM setup yielded reduction rates up to 20 times faster under mass-transfer-controlled conditions. A preliminary mechanism is proposed to explain the transition from a porous iron product to a dense encapsulating layer. Encapsulation is interpreted as the outcome of competition between pore creation, driven by the reduction rate, and pore elimination, driven by surface diffusion. When pore formation is insufficient to counteract pore coarsening, a dense iron layer develops and restricts further reduction.

encapsulation↗

Non-compact oxide-island growth induced by surface phase transition of the intermetallic NiAl during vacuum annealing

Crystal structure and composition are inter-dependent and decoupling their effects on surface reactivity is challenging. Using low-energy electron microscopy to spatially and temporally resolve the oxide film growth during the oxidation of NiAl(100), we differentiate such coupled effects by monitoring oxide growth while simultaneously fine-tuning the surface structure and composition during oxidation. We demonstrate that the oxidation of chemically ordered surfaces results in compact oxide island growth whereas non-compact oxide growth during the surface phase transition. By incorporating the surface phase transition induced chemical disordering into kinetic Monte Carlo simulations, we illustrate that the non-compact oxide growth is induced by the composition effect on the surface diffusion of oxygen, which can be described by the concept of “ant in the labyrinth”.

36 MATERIALS SCIENCE↗

Mechanisms of Ti 3 Al precipitation in hcp α -Ti

Here, nucleation and growth of Ti3Al α( 2 ) ordered domains in alpha-Ti-Al-X alloys were characterised using a combination of transmission electron microscopy, atom probe tomography and small angle X-ray scattering. Model alloys based on Ti-7Al (wt.%) and containing O, V and Mo were aged at 550 °C for times up to 120d and the resulting precipitate dispersions were observed at intermediate points. Precipitates grew to around 30nm in size, with a volume fraction of 6-10% depending on tertiary solutes. Interstitial O was found to increase the equilibrium volume fraction of α 2 , while V and Mo showed relatively little influence. Addition of any of the solutes in this study, but most prominently Mo, was found to increase nucleation density and decrease precipitate size and possibly coarsening rate. Coarsening can be described by the Lifshitz-Slyozov-Wagner model, suggesting a matrix diffusion-controlled coarsening mechanism (rather than control by interfacial coherency). Solutionising temperature was found to affect nucleation number density with an activation energy of E f = 1.5 +/- 0.4 eV, supporting the hypothesis that vacancy concentration affects α 2 nucleation. The observation that all solutes increase nucleation number density is also consistent with a vacancy-controlled nucleation mechanism.

36 MATERIALS SCIENCE↗

Local ordering in disordered Nd x Zr 1-x O 2-0.5x pyrochlore as observed using neutron total scattering

Pyrochlore complex oxides (A 2 B 2 O 7 ) are an important class of fluorite-derivative ceramics with exceptional chemical and structural versatility which make them ideal model systems for studying disordering mechanisms over a range of spatial scales. Here, neutron total scattering methods were used to analyze the structural behavior in the non-stoichiometric series Nd x Zr 1-x O 2-0.5x (0.5 ≤ x ≤ 0.23) as a function of Nd content, x. Characterization of the structure functions using Rietveld refinement and the pair distribution functions with small-box refinement reveal complex disordering pathways; the average, long-range phase changes over a very narrow compositional range from pyrochlore ($Fd\bar{3}m$) to defect fluorite ($Fm\bar{3}m$) through full randomization of the cation and anion sublattices at x ~ 0.31, while the local, short-range structure continuously adopts a weberite-type atomic arrangement (C222 1 ). Comparison to a previously studied Ho 2 Ti 2-x Zr x O 7 solid solution series reveals how changes in chemical composition and stoichiometry modify defect formation and determine how disordering progresses across different length scales in pyrochlore oxides.

36 MATERIALS SCIENCE↗

Strain-tuning of transport gaps and semiconductor-to-conductor phase transition in twinned graphene

We show, through the use of the Landauer-Büttiker (LB) formalism and a tight-binding (TB) model, that the transport gap of twinned graphene can be tuned through the application of a uniaxial strain in the direction normal to the twin band. Remarkably, we find that the transport gap E gap bears a square-root dependence on the control parameter ϵ x – ϵ c , where ϵ x is the applied uniaxial strain and ϵ c ~ 19% is a critical strain. We interpret this dependence as evidence of criticality underlying a continuous phase transition, with ϵ x – ϵ c playing the role of control parameter and the transport gap E gap playing the role of order parameter. For ϵ x < ϵ c , the transport gap is non-zero and the material is semiconductor, whereas for ϵ x < ϵ c the transport gap closes to zero and the material becomes conductor, which evinces a semiconductor-to-conductor phase transition. The computed critical exponent of 1/2 places the transition in the meanfield universality class, which enables far-reaching analogies with other systems in the same class.

36 MATERIALS SCIENCE↗

Theory of strain phase equilibria and diagrams

Chemical phase equilibria and phase diagrams are well established and have served as indispensable guides for designing materials through chemical tuning. However, a general thermodynamic theory for strain phase equilibria remains elusive despite extensive studies which have revealed dramatic impacts of mechanical strain on the stability of phases and domain states in solid-state materials. Here, we establish the thermodynamic theory of strain equilibria and a general framework for efficiently constructing multidomain and multiphase diagrams of arbitrarily strained solids under incoherent conditions. As examples, we obtain temperature-strain phase diagrams of ferroelectric PbTiO 3 , strongly correlated VO 2 , and unconventional ferroelectric Hf 0.5 Zr 0.5 O 2 . We reveal the analogs of the Gibbs phase rules, multiple- and multi-critical points, common-tangent construction, and level rule in strain equilibria to those in the familiar chemical phase equilibria. Finally, our strain equilibria theory offers a powerful framework for predicting the thermodynamic stability of structural phases and domains in strained solids and for guiding the strain engineering of their functional properties.

36 MATERIALS SCIENCE↗

Driving rapid atomic order in MnAl via low-magnitude magnetic field annealing

Application of a mild (60 mT), uniform magnetic field during short-term thermal treatment of kinetically retained, atomically disordered (paramagnetic) ε-MnAl was found to deliver a significant ~50 % increase in the formation of L1 0 atomically ordered (ferromagnetic) τ-MnAl product phase, compared to that produced by conventional (i.e., zero-field) annealing under identical thermal conditions. The magnetic field, applied in a passive closed-circuit configuration during annealing, induced significant changes in the structural, magnetic, and phase evolution of the material. Computational results based on electronic structure calculations demonstrate that the effective magnetic susceptibility of τ-MnAl is sensitive to the orientation, rather than the magnitude, of an applied magnetic field in the vicinity of the Curie temperature. The uniaxial magnetocrystalline anisotropy of the L1 0 structure is proposed to act as a filter for selective propagation of the population of τ-MnAl variants that are favorably aligned with the applied field. In this manner, crystallographic “gridlock” is alleviated that would otherwise arise from the coexistence of multiple, energetically equivalent τ-phase variants within the parent ε-phase matrix. These results confirm that static, low-magnitude magnetic field annealing is able to accelerate L1 0 atomic ordering in the MnAl system and likely can exert similar influences in relevant magnetic systems, facilitating efficient tailoring of structure-sensitive magnetic properties for the manufacture of magnetic materials.

36 MATERIALS SCIENCE↗

Quantitative characterization of gradient microstructures: A study on friction stir spot processing of pure cobalt

Heterogeneous microstructures in polycrystalline metals can enhance the strength and ductility, outperforming homogeneous structures of similar composition. This study investigates deformed cobalt via friction stir spot processing with varying dwell times to uncover the effects of plastic deformation and heat generation on the formation of morphological, phase, and grain boundary character gradients. A new approach to quantify the morphological gradients in materials, which describes grain morphology in terms of density followed by parametric regression, enables direct quantification of processing depth and gradient sharpness. Results show that longer processing times increase the steepness of morphological gradients and reduce the deformation depth for friction stir spot processing with low plunge depths and high tool rotational speeds. The amount of retained FCC is increased in the shorter processing conditions, primarily due to refined grain size, increased defect content, and reduced heat generation. Crystallographic texture analysis of the HCP phase indicated a dominant B-fiber described by (0001) ∥ shear plane normal in the extreme processing conditions and the formation of a P-fiber, shear direction ∥ ⟨11$\bar2$0⟩ for intermediate dwell times. The texture of the FCC phase for low processing times was a C texture {100}⟨011⟩ where longer processing times were dominated by a [001] fiber texture with a main {110}⟨100⟩ orientation and emergence of a slight [111] fiber in the longest processing condition. The approaches outlined in this work give insight into quantifying gradients and improve the understanding of highly deformed cobalt.

36 MATERIALS SCIENCE↗

A unified system for Coleman–De Luccia transitions

Highlights: • Monotonicity controls whether radius of CDL bounce is negative mode direction. • Decays from de Sitter and Anti-de Sitter analyzed in single geometric framework. • de Sitter to Anti-de Sitter instantons come in two types, similar to type-A vs type-B. We show that the presence or absence of negative modes associated with the expansion or contraction of Coleman–De Luccia instantons is controlled by the monotonicity properties of a single function parameterized by the tension and two vacuum energies. This approach simplifies and unifies certain aspects of phase transitions between two de Sitter vacua, between two Anti-de Sitter, and between one of each. This strategy may serve as a guide for identifying negative modes in more complicated gravitational theories, for instance supergravity.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Distinguishing localization from chaos: Challenges in finite-size systems

Highlights: • Provides an overview of the current understanding of the many-body localization phase transition. • Discusses the subtleties of finite-size scaling near this transition • Assesses the implications of these subtleties for numerical studies of spin chains. • Explores scaling of diagnostics in models with known localization transitions. • Presents suggestions for future numerical work. We re-examine attempts to study the many-body localization transition using measures that are physically natural on the ergodic/quantum chaotic regime of the phase diagram. Using simple scaling arguments and an analysis of various models for which rigorous results are available, we find that these measures can be particularly adversely affected by the strong finite-size effects observed in nearly all numerical studies of many-body localization. This severely impacts their utility in probing the transition and the localized phase. In light of this analysis, we discuss a recent study (Šuntajs et al., 2020) of the behaviour of the Thouless energy and level repulsion in disordered spin chains, and its implications for the question of whether MBL is a true phase of matter.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗