Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CHROMIUM ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 811 records · Page 45

Adsorption of Chlorine on Zr(0001) Surface: First-Principles Predictions

The adsorption of atomic and gaseous chlorine on Zr (0001) surface has been investigated using state-of-the-art density functional theory calculations as part of an effort to gain fundamental understanding of chlorination processes occurring in fuel cladding materials. Zirconium alloys, including Zircaloy-4, Zircaloy-2 and Zr-Nb alloys (Zirlo{sup TM} and Zr-2.5Nb) are the most common fuel cladding materials in nuclear light water reactors (LWRs) due to their favorable mechanical properties, corrosion resistance, low thermal-neutron capture cross section and criticality. The United States produces a large amount of cladding material from used nuclear fuel, which could approach 1,000 MT/year in the next 50 years. In nuclear fuel recycling, spent nuclear fuel assemblies are disassembled and the cladding hulls are separated from the U oxide spent fuel. Zr can be recovered from Zr cladding using the chlorination method. However the presence of impurities in the recovered ZrCl{sub 4} was reported, including Sn, Cr and Fe. Thus, further efforts are necessary to improve the purification process significantly. This requires fundamental understanding of chlorination processes in cladding materials. Most of the material properties are expected to be similar between the pure zirconium and its alloys due to the fact that the alloy composition consists of more than 95 weight-percent zirconium and less than 2% of tin, niobium, iron, chromium, nickel and other metals. Therefore, while the overarching goal is to understand the chlorination process occurring in complex fuel cladding materials, chlorination of pure zirconium was used as an initial system for the modeling and simulation efforts in this study.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Development of a Thin Film Primary Surface Heat Exchanger for Advanced Power Cycles

This project objective is to develop a high-temperature design upgrade for an existing primary surface heat exchanger so that the redesigned hardware is capable of operation in CO 2 at temperatures up to 1,510°F (821°C) and pressure differentials up to 130 psi (9 bar). The heat exchanger is proposed for use as a recuperator in an advanced low-pressure oxy-fuel Brayton cycle that is predicted to achieve over 50% thermodynamic efficiency, although the heat exchanger could also be used in other high-temperature, low-differential pressure cycles. This report describes the progress to date, which includes continuing work performed to select and test new candidate materials for the recuperator redesign, final mechanical and thermal performance analysis results of various redesign concepts, and the preliminary design of a test loop for the redesigned recuperator including a budgetary estimate for detailed test loop design, procurement, and test operation. A materials search was performed in order to investigate high-temperature properties of many candidate materials, including high-temperature strength and nickel content. These properties were used to rank the candidate materials, resulting in a reduced list of nine materials for corrosion testing. Multiple test rigs were considered and analyzed for short-term corrosion testing and Thermal Gravimetric Analysis (TGA) was selected as the most cost-effective option for evaluating corrosion resistance of the candidate materials. In addition, tantalum, niobium, and chromium coatings were identified as potential options for increased corrosion resistance. The test results show that many materials exhibit relatively low weight gain rates, and that niobium and tantalum coatings may improve corrosion resistance for many materials, while chromium coatings appear to oxidize and debond quickly. Metallurgical analysis of alloys was also performed, showing evidence of intergranular attack in 282 that may cause long-term reliability problems in CO 2 service at these temperatures. However, long-term testing in a flowing environment is recommended in order to understand accurately the severity of the attack. Detailed economic modeling of the existing air cycle recuperator and CO 2 cycle recuperator options was also completed, including costs for material, fabrication, fuel, maintenance, and operation. The analysis results show that the increased capital cost for high-temperature materials may be offset by higher cycle efficiencies, decreasing the overall lifetime cost of the system. The economic analysis also examines costs associated with increased pressure drop and material changes for two redesign options. These results show that, even with slightly reduced performance and/or higher material costs, the lifetime cost per energy production may still be reduced by over 12%. The existing recuperator design information was provided by Solar Turbines, Inc. via several models, drawings, and design handoff meetings. Multiple fluid/thermal and structural models were created in order to analyze critical recuperator performance and mechanical strength in critical areas throughout the redesign process. These models were analyzed for a baseline condition (consistent with current Mercury 50 operation) for validation purposes. Results are presented for heat transfer coefficients and pressure drops, matching well with the existing operational data. Simulation of higher-temperature CO 2 conditions was also performed, showing a slight expected increase in both heat transfer and pressure drop. Mechanical analysis results for critical areas on the cross-flow and counter-flow sheets have also been obtained for air and CO 2 cases. These results show similar stresses in both cases but significantly reduced safety factors for the CO 2 case due to reduced yield and creep rupture strengths of alloy 625 at the higher temperatures. A concept brainstorm session and initial down-selection were completed in order to identify promising redesign options for further analysis. Detailed analysis of all promising redesign options was performed via finite element and computational fluid dynamic simulations in order to characterize mechanical and thermal-fluid performance of each option. These options included material change, various sheet thickness configurations, pitch and phasing of cross-flow and counter-flow sheets, and separator sheets. The analysis results have identified two viable redesign options that maintain existing safety margins optimally through a material change to Haynes 282 and (A) sheet thickness increases of 40% on the counter-flow sheet and 75% on the hot side cross-flow corrugation sheet or (B) addition of a separator sheet in the counter-flow section while maintaining the original counter-flow sheet thickness and increasing the cross-flow corrugation sheet thickness by 90% to account for the increase in cell height. While both options satisfy mechanical stress constraints, the separator sheet design has a higher part count, slightly reduced heat transfer, and slightly higher pressure drop than the first option and is not preferred. Finally, several test loop concepts have been developed for different full-scale and reduced-scale recuperator testing options. For each option, various loop components, such as heat exchangers, valves, heaters, and compressors, were evaluated in an effort to maximize utilization of existing resources. All concepts utilize an existing 3-MW CO 2 compressor, heater, and loop coolers, but the concepts vary by incorporating different amounts of new equipment for achieving various flow rates (all concepts operate at design pressure and temperature). The third concept achieves a 1 kg/s test without purchasing any costly equipment (coolers, heaters, blowers, etc.). Since the stacked cell design of the recuperator results in the same flow conditions at each core cell (even for a reduced-scale test). Thus, test loop Concept #3 was selected for the preliminary design. This loop design is detailed within the report, culminating in a budgetary estimate of $1,013,000.00 for the detailed design, construction, commissioning, and operation of a high-temperature recuperator test loop.

03 NATURAL GAS↗

Process development for Ni-Cr-ThO2 and Ni-Cr-Al-ThO2 sheet

A process was developed for the production of thin gauge Ni-Cr-ThO2 sheet. The process was based on the elevated temperature deposition of chromium onto a wrought Ni-2%ThO2 sheet and subsequent high temperature diffusion heat treatments to minimize chromium concentration gradients within the sheet. The mechanical properties of the alloy were found to be critically dependent on those of the Ni-2%ThO2 sheet. A similar process for the production of a Ni-Cr-Al-ThO2 alloy having improved oxidation resistance was investigated but the non-reproducible deposition of aluminum from duplex Cr/Al packs precluded successful scale-up. The mechanical properties of the Ni-Cr-Al-ThO2 alloys were generally equivalent to the best Ni-Cr-ThO2 alloy produced in the programme.

Cook, R. C.↗

Research experiences on materials science in space aboard Salyut and Mir

From 1980 through 1991 approximately 500 materials processing experiments were performed aboard the space stations Salyut 6, Salyut 7 and Mir. This includes work on catalysts, polymers, metals and alloys, optical materials, superconductors, electronic crystals, thin film semiconductors, super ionic crystals, ceramics, and protein crystals. Often the resulting materials were surprisingly superior to those prepared on earth. The Soviets were the first to fabricate a laser (CdS) from a crystal grown in space, the first to grow a heterostructure in space, the first super ionic crystal in space, the first crystals of CdTe and its alloys, the first zeolite crystals, the first protein crystals, the first chromium disilicide glass, etc. The results were used to optimize terrestrial materials processing operations in Soviet industry. The characteristics of these three space stations are reviewed, along with the advantages of a space station for materials research, and the problems encountered by the materials scientists who used them. For example, the stations and the materials processing equipment were designed without significant input from the scientific community that would be using them. It is pointed out that successful results have been achieved also by materials processing at high gravity in large centrifuges. This research is also continuing around the world, including at Clarkson University. It is recommended that experiments be conducted in centrifuges in space, in order to investigate the acceleration regime between earth's gravity and the microgravity achieved in orbiting space stations. One cannot expect to understand the influence of gravity on materials processing from only two data points, earth's gravity and microgravity. One must also understand the influence of fluctuations in acceleration on board space stations, the so-called 'g-jitter.' This paper is presented in outline and graphical form.

Regel, Liya L.↗

Calculation of Reactive-evaporation Rates of Chromia

A methodology is developed to calculate Cr-evaporation rates from Cr2O3 with a flat planar geometry. Variables include temperature, total pressure, gas velocity, and gas composition. The methodology was applied to solid-oxide, fuel cell conditions for metallic interconnects and to advanced-steam turbines conditions. The high velocities and pressures of the advanced steam turbine led to evaporation predictions as high as 5.18 9 10-8 kg/m2/s of CrO2(OH)2(g) at 760 °C and 34.5 MPa. This is equivalent to 0.080 mm per year of solid Cr loss. Chromium evaporation is expected to be an important oxidation mechanism with the types of nickel-base alloys proposed for use above 650 °C in advanced-steam boilers and turbines. It is shown that laboratory experiments, with much lower steam velocities and usually much lower total pressure than found in advanced steam turbines, would best reproduce chromium-evaporation behavior with atmospheres that approach either O2 + H2O or air + H2O with 57% H2O.

ADSORPTION HEAT↗

COSAM program overview

The COSAM program for reduction of the use of strategic alloying elements in nickel-based superalloys for gas turbine engines was reviewed. Sources, consumption, and pricing of cobalt, tantalum, columbium, and chromium are surveyed. Research projects in strategic element substitution, advanced processing concepts, and the development of alternate materials (intermetallics and iron-base alloys) are listed and research plans for FY 1983 and FY 1984 summarized.

Stephens, J. R.↗

A study of microstructural evolution of Fe-18Cr-8Ni, Fe-17Cr-12Ni, and Fe-20Cr-25Ni stainless steels after mechanical alloying and annealing

In this study, high-energy mechanical alloying technique was used to produce nanocrystalline stainless steels of three different compositions from elemental powders. The microstructural evolution (grain growth and phase transformation) as a function of alloy compositions and annealing temperatures were investigated by room and high temperature x-ray diffraction experiments, transmission electron microscopy and focused ion beam microscopy. The results revealed that stainless steels with low nickel content (i.e., Fe-18Cr-8Ni) underwent a deformation-induced martensitic transformation during room temperature mechanical alloying. Deformation-induced martensitic transformation with increasing nickel content (i.e., Fe-17Cr-12Ni and Fe-20Cr-25Ni) would not be possible by room temperature milling but was created by high strain rate cryogenic processing, the degree to which was compositional dependent. Post process annealing induced the reverse transformation from martensite-to-austenite the ratio of which was found to be a factor of alloy composition and annealing temperature. The real time in-situ x-ray studies showed that the martensite-to-austenite reverse transformation was completed at around 600 °C and 800 °C for Fe-18Cr-8Ni and Fe-20Cr-25Ni steels, respectively. Microscopy studies revealed a significant enhancement in the resistance to grain growth for Fe-17Cr-12Ni steel over other compositions at elevated temperatures as high as 1200 °C. As such, cryogenic processing following by reverse martensitic transformation of high Ni containing alloys provides a pathway for developing higher heat resistant stainless steel alloys.

36 MATERIALS SCIENCE↗

Development of LWR fuels with enhanced accident tolerance. Final report

After a tsunami triggered plant black out at the Fukushima Daiichi site, followed by hydrogen explosions, the US Department of Energy partnered with fuel vendors to study safer alternatives to the current UO2 – zirconium alloy fuel system. This accident tolerant fuel (ATF) alternative should better tolerate a loss of cooling in the core for a considerably longer time while maintaining or improving the fuel performance during normal operation conditions. General Electric, Oak Ridge National Laboratory, and their partners are proposing to replace zirconium alloy cladding in current commercial light water power reactors with an iron-chromium-aluminum (FeCrAl) cladding such as APMT, C26M or FeCrAl ODS, which has been named IronClad by GE. Extensive testing and evaluation has been conducted to determine the suitability of FeCrAl for the entire fuel cycle from rod fabrication to used fuel disposition. Most of the environmental characterization was conducted to evaluate the behavior of IronClad under normal operation conditions and under severe accident conditions. Results show that FeCrAl has excellent corrosion resistance under normal operation conditions and FeCrAl is several orders of magnitude more resistant than zirconium alloys to degradation by superheated steam under accident conditions, generating less heat of oxidation and lower amount of combustible hydrogen gas. Higher parasitic neutron absorption and potential tritium release into the coolant effects can be minimized by design and operational measures. IronClad material can be manufactured using traditional melting and forging (C26M) or powder metallurgy processes (APMT & FeCrAl ODS). Tubes can be made to full length of 5 m with a wall thickness of 0.4 mm by pilgering or drawing. The fuel rods can be readily hermetically sealed in an industrial production setting by welding end caps to the thin wall tubing using either TIG or resistance welding. The implementation of FeCrAl IronClad cladding is a near term solution to enhance the safety of the current fleet of commercial light water power reactors.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Development of a Corrosion Monitoring System for Advanced Molten Salt Reactors

Molten salt reactors (MSRs) have been identified as one of several possible next-generation advanced reactor designs that could replace the aging fleet. There are many inherent advantages to MSRs, including higher power density, lower pressure, low stored energy, and prompt negative temperature reactivity coefficient Ezell et al. [2018]. However, there are challenges related to the operating temperatures, as well as, the corrosive salts attacking the structural materials. During the Molten Salt Reactor Experiment (MSRE), which was operated at Oak Ridge National Laboratory (ORNL) (Ignatiev et al. [2014], Forsberg et al. [2007], Forsberg et al. [2008], Delpech et al. [2009], Serp et al. [2014], Ignatiev and Surenkov [2017]) corrosion was monitored by sampling the salt for chromium. However, this type of monitoring does not identify the location of corrosion. In FY18, ORNL developed a novel in-situ corrosion sensor that could be placed on the outside of the structure to monitor changes in magnetic susceptibility of salt-wetted alloys as corrosion occurs Holcomb et al. [2019]. Initial testing with this novel sensor demonstrated a correlation between the change in signal output from the sensor to the various levels of pre-corroded test specimens. However, all initial testing was performed at room temperatures, which is not realistic for the harsh MSR environment. Based on this research, FY19 funding allowed for development of a high-temperature version of the sensor to be installed at various locations on the reactor infrastructure. The high-temperature sensor can operate at up to 750°C and can monitor development of corrosion inside the pipe. This sensor measures the increase in magnetic susceptibility that occurs as chromium dissolves from the inner surface of the pipe, when paramagnetic structural alloys become ferromagnetic with the loss of chromium. This report will discuss the development of corrosion monitoring sensor and the testing with results of corroded specimens at increasing temperatures.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Heat and corrosion resistant cast CF8C stainless steel with improved high temperature strength and ductility

A CF8C type stainless steel alloy and articles formed therefrom containing about 18.0 weight percent to about 22.0 weight percent chromium and 11.0 weight percent to about 14.0 weight percent nickel; from about 0.05 weight percent to about 0.15 weight percent carbon; from about 2.0 weight percent to about 10.0 weight percent manganese; and from about 0.3 weight percent to about 1.5 weight percent niobium. The present alloys further include less than 0.15 weight percent sulfur which provides high temperature strength both in the matrix and at the grain boundaries without reducing ductility due to cracking along boundaries with continuous or nearly-continuous carbides. The disclosed alloys also have increased nitrogen solubility thereby enhancing strength at all temperatures because nitride precipitates or nitrogen porosity during casting are not observed. The solubility of nitrogen is dramatically enhanced by the presence of manganese, which also retains or improves the solubility of carbon thereby providing additional solid solution strengthening due to the presence of manganese and nitrogen, and combined carbon.

36 MATERIALS SCIENCE↗

Fretting of Secondary-Seal-Ring Candidate Materials in Air at Temperatures to 816 C

Superalloys containing chromium showed decreasing fretting damage with increasing temperature of 816 C. This trend was related to the ability of the alloys to generate self-protecting oxide films. The damage at 816 C was one-third to one-tenth of that at 23 C. Osmium, chromium, and chromium carbide platings were fretted at 23 and 450 C. Osmium was extremely protective at 23 C but oxidized excessively at 450 C. Chromium and chromium carbide gave about the same protection at 450 C as the oxide films that formed on the superalloys. High graphite and low graphite carbons were fretted at 23 and 327 C. High graphite carbon was superior at 327 C, but low graphite carbon was the best material examined at 23 C.

Bill, R. C.↗

Tunnel magnetoresistance effect in magnetic tunnel junctions using Fermi-level-tuned epitaxial Fe{sub 2}Cr{sub 1−x}Co{sub x}Si Heusler alloy

This paper reports a systematic investigation on the structural and magnetic properties of Fe{sub 2}Cr{sub 1−x}Co{sub x}Si Heusler alloys with various compositions of x by co-sputtering Fe{sub 2}CrSi and Fe{sub 2}CoSi targets and their applications in magnetic tunnel junctions (MTJs). Fe{sub 2}Cr{sub 1−x}Co{sub x}Si films of high crystalline quality have been epitaxially grown on MgO substrate using Cr as a buffer layer. The L2{sub 1} phase can be obtained at x = 0.3 and 0.5, while B2 phase for the rest compositions. A tunnel magnetoresistance (TMR) ratio of 19.3% at room temperature is achieved for MTJs using Fe{sub 2}Cr{sub 0.3}Co{sub 0.7}Si as the bottom electrode with 350 °C post-annealing. This suggests that the Fermi level in Fe{sub 2}Cr{sub 1−x}Co{sub x}Si has been successfully tuned close to the center of band gap of minority spin with x = 0.7 and therefore better thermal stability and higher spin polarization are achieved in Fe{sub 2}Cr{sub 0.3}Co{sub 0.7}Si. The post-annealing effect for MTJs is also studied in details. The removal of the oxidized Fe{sub 2}Cr{sub 0.3}Co{sub 0.7}Si at the interface with MgO barrier is found to be the key to improve the TMR ratio. When the thickness of the inserted Mg layer increases from 0.3 to 0.4 nm, the TMR ratio is greatly enhanced from 19.3% to 28%.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Parameters affecting the stability of the digestate from a two-stage anaerobic process treating the organic fraction of municipal solid waste

This paper focused on the factors affecting the respiration rate of the digestate taken from a continuous anaerobic two-stage process treating the organic fraction of municipal solid waste (OFMSW). The process involved a hydrolytic reactor (HR) that produced a leachate fed to a submerged anaerobic membrane bioreactor (SAMBR). It was found that a volatile solids (VS) removal in the range 40-75% and an operating temperature in the HR between 21 and 35 {sup o}C resulted in digestates with similar respiration rates, with all digestates requiring 17 days of aeration before satisfying the British Standard Institution stability threshold of 16 mg CO{sub 2} g VS{sup -1} day{sup -1}. Sanitization of the digestate at 65 {sup o}C for 7 days allowed a mature digestate to be obtained. At 4 g VS L{sup -1} d{sup -1} and Solid Retention Times (SRT) greater than 70 days, all the digestates emitted CO{sub 2} at a rate lower than 25 mg CO{sub 2} g VS{sup -1} d{sup -1} after 3 days of aeration, while at SRT lower than 20 days all the digestates displayed a respiration rate greater than 25 mg CO{sub 2} g VS{sup -1} d{sup -1}. The compliance criteria for Class I digestate set by the European Commission (EC) and British Standard Institution (BSI) could not be met because of nickel and chromium contamination, which was probably due to attrition of the stainless steel stirrer in the HR.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Thermal effects on transducer material for heat assisted magnetic recording application

Heat Assisted Magnetic Recording (HAMR) is a promising technology for next generation hard disk drives with significantly increased data recording capacities. In HAMR, an optical near-field transducer (NFT) is used to concentrate laser energy on a magnetic recording medium to fulfill the heat assist function. The key components of a NFT are transducer material, cladding material, and adhesion material between the cladding and the transducer materials. Since transducer materials and cladding materials have been widely reported, this paper focuses on the adhesion materials between the Au transducer and the Al{sub 2}O{sub 3} cladding material. A comparative study for two kinds of adhesion material, Ta and Cr, has been conducted. We found that Ta provides better thermal stability to the whole transducer than Cr. This is because after thermal annealing, chromium forms oxide material at interfaces and chromium atoms diffuse remarkably into the Au layer and react with Au to form Au alloy. This study also provides insights on the selection of adhesion material for HAMR transducer.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Ceramic Rolling and Annealing on Mechanical Properties of AlCoCrFeNi{sub 2.1} Eutectic High-Entropy Alloys

It was firstly proved that AlCoCrFeNi{sub 2.1} could optimize the strength-ductility combination by ceramic rolling at room temperature. The technique greatly enhanced the strength of the materials at the price of slight ductility, which is different from the previous studies. When the thickness reduction was 23.06%, the yield strength and compressive strength were 1611.42 and 2212.99 MPa, respectively, with the plastic strain of 28.36%. Such an excellent combination of strength and ductility was attributed to the distribution of the residual stress, the high hydrostatic stress and the shear bands in ceramic rolling process. The plastic strain of the material increased to 38.54%, and the strength reduced to 1900.73 MPa after annealing at 800 °C for 1 h. A lot of like-flower patterns of recrystallized ultrafine grain were observed after annealing at 800 °C due to the sluggish diffusion in HEAs and the effect of ceramic rolling. In addition, after annealing at 800 °C, the fracture mode changed to shearing fracture of microvoid aggregation from cleavage/quasi-cleavage fracture of as-rolled sample due to the deposition of the second phase in the tested sample.

36 MATERIALS SCIENCE↗

Control of Carbon Content in Ultrafine Cemented Carbide by Heat Treatment in Reducing Atmospheres Containing Carbon Oxides

In this work, the method of control of carbon content in the ultrafine-grained cemented carbide alloy was proposed. The treating of the WC-8Co-0.4VC-0.4Cr{sub 3}C{sub 2} compacts was made in a CO + CO{sub 2} gas mixture at CO concentrations from 0 to 80 vol.% during 50 min at the initial stage of the conventional sintering at a temperature of 700 °C. Conditions for increasing and decreasing the carbon content are CO concentrations of CO in gas mix more than 65 vol.% and less than 35 vol.%, respectively. It is shown that even a small deviation from the stoichiometric carbon content (0.3 wt.%) leads to an increase in porosity and a multiple decrease in the strength of the ultrafine-grained cemented carbide. A comparative analysis with literature data showed that the obtained ultrafine-grained solid alloy WC-8Co-0.4VC-0.4Cr{sub 3}C{sub 2} with stoichiometric composition is not inferior in hardness and toughness to the analogs obtained by hot pressing and electrospark sintering.

36 MATERIALS SCIENCE↗

Microband induced plasticity and the temperature dependence of the mechanical properties of a carbon-doped FeNiMnAlCr high entropy alloy

Highlights: • A superior fcc HEA with the strength of 1.5 GPa at the cryogenic condition is developed. • The strengthening mechanisms of HEAs at different temperatures are clarified. • The temperature dependence of MBIP effect is revealed. - Abstract: The uniaxial mechanical properties of the high entropy alloy (HEA) Fe{sub 40.4}Ni{sub 11.3}Mn{sub 34.8}Al{sub 7.5}Cr{sub 6} doped with 1.1 at.% C have been determined for both the as-cast and recrystallized states at temperatures from 77 to 973 K. Very high yield strengths were obtained at 77 K of 928 MPa for the as-cast HEA and 1037 MPa for the recrystallized HEA. The yield strength decreased sharply to 293 K and more slowly to 973 K, where it was ~200 MPa [11] in both conditions. The lattice friction stress, which results from the increase of the Peierls barrier, was the major contributor to the large yield strength at 77 K. On the other hand, the grain boundaries lose their strengthening ability at a high temperature, which largely accounts for the sharp drop in yield strength of the fine-grained (5 μm) recrystallized HEA at 973 K. The elongation to failure was highest at 293 K and 673 K with the lowest values at 77 K. Transmission electron microscopy was used to study the effects of temperature on the deformation mechanisms of the HEAs, especially the temperature dependence of the microband-induced plasticity effect. At temperatures ranging from 77 K to 673 K microbands form in the as-cast HEA, while dislocation clusters were observed in the recrystallized HEA over this temperature range. Only tangled dislocations were found at 973 K for both the as-cast and recrystallized HEA due to thermally-activated deformation.

36 MATERIALS SCIENCE↗