At least 811 records · Page 45

Microstructure and Mechanical Properties of Three-Layer TIG-Welded 2219 Aluminum Alloys with Dissimilar Heat Treatments

2219-C10S and 2219-CYS aluminum alloys are 2219 aluminum alloys with different heat treatment processes, and they have been widely used in the aerospace industry. In the present study, 2219-C10S and 2219-CYS aluminum alloys were butt-welded by three-layer tungsten inert gas arc welding (with the welding center of the third layer shifted toward the CYS side), and the microstructure characteristics and mechanical properties of the welded joint were investigated. The lamellar θ′ phases, the bulk or rod θ phases, and the coarse rod-shaped or pancake-shaped Al-Cu-Fe-Mn phases coexisted in the two aluminum alloys. The Cu content of the α-Al matrix and the distribution of eutectic structures of different welding layers in the weld zone (WZ) were varied, implying that the segregation degrees of the Cu element were different due to the different welding thermal cycles in different welding layers. The microhardness values of the CYS side were much higher than those of the C10S side in each region on both sides of the joint. The tensile test deformation was concentrated mainly in the regions of WZ and the over aged zone (OAZ), where the microhardness values were relatively low. The main deformation concentrated region was transferred from the CYS side to the C10S side with the increase in the tensile load during the tensile test. The fracture behavior of the tensile test showed that the macroscopic crack initiated near the front weld toe had gone through the crack blunt region, the shear fracture region of the partially melted zone (PMZ), and the shear fracture region of OAZ. Meanwhile, the fracture characteristics gradually evolved from brittle to ductile. The concentrated stress and the dense eutectic structure in the region near the front weld toe of the C10S side contributed to the fracture of the joint. The shift of the welding center of the third layer to the CYS side resulted in two effects: (i) the microhardness values from the middle layer to the top layer in the PMZ of the CYS side were the most significantly increased and (ii) the distance between the front weld toe and the fusion line of the CYS side was significantly larger.

36 MATERIALS SCIENCE↗

Studies on Enhancement of Silt Erosion Resistance of 13/4 Martensitic Stainless Steel by Low-Temperature Salt Bath Nitriding

Low-temperature salt bath nitriding of heat treated and tempered 13/4 Martensitic stainless steel (13/4HTT) was carried at 450 °C (N450) and 500 °C (N500) for 10 h each. The nitrided samples were characterized by using x-ray diffractometer, field emission scanning electron microscope and optical microscope. The nanohardness and elastic modulus of the cross section of nitrided specimen were measured by nanoindentation test using Hysitron TI950 triboindenter. The nitrided 13/4HTT (N450 and N500) and 13/4HTT specimens were subjected to slurry erosion test in a slurry pot tester. The test was conducted for 48 h, and weight loss was measured after every 6 h. The relative speed of slurry with respect to specimen was 4.55 m/s. It was found that the weight loss due to erosion of the N450 is 83% less than that of 13/4HTT and that of N500 was 92% more than that of 13/4HTT. The erosion mechanism is correlated to the phases present in the specimens. The improvement in the slurry erosion resistance of N450 is due to presence of expanded martensite (α{sub N}-Fe). Increasing the temperature of nitriding to 500 °C led to the decrease in the slurry erosion resistance of N500 due to the formation of brittle CrN phase.

36 MATERIALS SCIENCE↗

Notch Sensitivity and Failure Behavior of TiAl and K418 Alloys

The notch sensitivity of tensile specimens of TiAl and K418 alloys has been investigated, and the notch strength has been quantitatively analyzed. The fracture surface of the specimens has also been observed and analyzed by scanning electron microscopy (JEOL-6700F). By comparing notch rod tensile specimens and special notch rod tensile specimens, it was found that the basic nature, fracture driving force, and fracture criteria of the brittle TiAl alloy and the ductile K418 alloy are different. The final fracture of the K418 alloy is controlled by strain and not by stress, and the specimens do not exhibit notch sensitivity. However, the final fracture of the TiAl alloy is controlled by stress, and the specimens exhibit small notch sensitivity. For the special notch rod tensile specimens, the K418 specimens do not exhibit notch sensitivity. However, for the TiAl alloy, when the notch depth reaches 10% of the specimen diameter, the tensile strength decreases, and when the notch depth reaches 20% of the specimen diameters, the tensile strength sharply decreases.

36 MATERIALS SCIENCE↗

Wetting and Brazing of Chromium Film-Deposited Alumina Using AgCu Filler Metal

Wetting behavior of AgCu filler on chromium film-deposited Al{sub 2}O{sub 3} ceramics was studied by sessile drop method under vacuum, and brazing of chromium-deposited alumina using AgCu was carried out. Cr film can improve the wettability of AgCu filler on alumina ceramics, and the contact angle decreased dramatically. However, with further increase in temperature and extension of wetting time, Cr atom might diffuse excessively to molten alloy or substrate leading to thinned or disappeared Cr film on alumina; thus, the contact angle of AgCu on alumina increased. The reliable alumina joint was obtained via chromium deposition using AgCu filler brazed at 900 °C for 10 min, and no hard or brittle intermetallic compounds formed in the brazed joint. The maximum shear strength of 16.8 MPa was achieved when the thickness of deposited chromium film was 2 μm.

36 MATERIALS SCIENCE↗

Effect of Boron Content on Microstructure, Mechanical Properties, and Oxidation Resistance of Mo-Si-B Composites

Mo-Si-B composites with boron content from 0 to 8 wt.% were prepared by spark plasma sintering using Mo, Si, and B elemental powders. The effects of boron content on the phase composition, mechanical properties, and high-temperature oxidation resistance of the Mo-Si-B composites were investigated. The results show the evolution of the major phase constitution of the composites with increasing boron content is in the following sequence: (MoSi{sub 2}, Mo{sub 5}Si{sub 3}) → (MoSi{sub 2}, Mo{sub 5}Si{sub 3}, Mo{sub 5}SiB{sub 2}) → (MoSi{sub 2}, MoB) → (MoSi{sub 2}, MoB, MoB{sub 2}). As the boron content increases, both the hardness and flexural strength of the composites increases, but the fracture toughness of the composites gradually decreases. The strengthening mechanisms for the composites are second-phase strengthening and grain refinement strengthening. However, the formation of brittle phases, i.e., Mo{sub 5}SiB{sub 2}, MoB, and MoB{sub 2}, reduces the toughness of the composites. In addition, since a dense barrier layer of SiO{sub 2}-B{sub 2}O{sub 3} formed on the surface of the composites inhibits the inward diffusion of oxygen, B-doped Mo-Si-B exhibits better oxidation resistance compared with non-doped composites.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Cast Al-5Zn-2Mg Alloy Subjected to Equal-Channel Angular Pressing

In the present work, cast Al-5Zn-2Mg alloy was processed through equal-channel angular pressing (ECAP) in route B{sub C} up to four number of passes. Microstructure and mechanical properties were investigated on processed and unprocessed materials. In cast condition, the material was composed of dendritic structure. After homogenization treatment, large-sized grains were observed. After ECAP processing, significant grain refinement was observed. After ECAP processing, high-density dislocations and high degree of misorientation between the grains were observed. In cast material, rod-shaped precipitates were observed, while, after ECAP processing, spherical-shaped precipitates were observed. ECAP processing leads to a noticeable improvement in the mechanical properties of the material. After four passes, 122% improvement in the microhardness and 135% improvement in the ultimate tensile strength of the material were observed. After three passes, a slight decrease in the mechanical properties was observed. This is attributed to the dissolution of the metastable η′ phase, annihilation of dislocations, dynamic recrystallization and texturing during ECAP processing. Brittle fracture mode was observed in tensile testing cast and homogenized samples. After ECAP processing, fracture mode was changed into shear fracture mode.

36 MATERIALS SCIENCE↗

Effect of Ni Addition to Sn0.7Cu Solder Alloy on Thermal Behavior, Microstructure, and Mechanical Properties

The addition of Ni on lead-free solder alloys Sn0.7Cu was tested in this study. A small amount of Ni was added to the solder alloys to evaluate the thermal behavior, microstructure, and mechanical properties of the composite solders after sintering and isothermal aging for 3 days and then compared with the results of the binary Sn0.7Cu solder. The results indicated that the ultimate tensile strength and yield tensile strength changed when adding 0.25 wt.% of Ni. The tested results of the differential scanning calorimeter showed that the addition of Ni (such as 0.5 and 1 wt.%) could obviously increase the solidification temperature of Sn0.7Cu alloys in the cooling process. When the Ni content was increased to 0.25 wt.% in the ternary condition, which includes the Sn0.7Cu-xNi (x = 0, 0.1, 0.25, 0.5, and 1 wt.%) solder alloys for the indentation creep test, the minimum creep rate reached the maximum; however, the trend was reversed as the Ni content was higher than this level. In addition, the microstructure of Sn-0.7Cu-xNi solder alloys was obviously different with the eutectic Sn-0.7Cu solder, such that the Ni gradually accumulated in the (Cu, Ni){sub 6}Sn{sub 5} IMCs within the Ni-containing solder alloys. Additionally, this process refined the microstructure of the Sn-0.7Cu solder. The fracture surface of the eutectic Sn-0.7Cu solder revealed ductile fracture modes; however, there was no mixed ductile–brittle fracture mode occurred when the Ni content was in the range of 0-1 wt.%.

36 MATERIALS SCIENCE↗

The Effects of Sc Addition on the Microstructure and Mechanical Properties of Be-Al Alloy Fabricated by Induction Melting

This study investigated the alloying effects of 0.4 wt.% Sc on the microstructure, mechanical properties, and fracture behavior of a cast Be-Al alloy prepared by vacuum induction melting. The micromechanics of Sc-containing secondary-phase particles (SPs) were characterized by nanoindentation, and the fracture behavior of the alloy was investigated via tensile fractography and optical metallography. The addition of 0.4 wt.% Sc significantly modified the alloy microstructure by decreasing the secondary dendritic arm spacing (SDAS), weakening the dendritic structure of Be, and producing an equiaxed/cellular alloy microstructure with refined Be grains. Sc alloying increased the Vickers hardness by 36%, elastic modulus by 28%, yield strength by 35%, ultimate strength by 52%, but decreased the elongation from 3.6 to 2.9%. Sc-containing SPs had a higher elastic modulus, yield strength, microhardness, and a lower plasticity index than the Be and Al matrices, resulting in interface separation during the fracture process. SPs located at the Be/Al interfaces did not act as microcrack sources for the matrices, whereas highly faceted SPs within the Be grains induced microcrack formation and decreased the elongation. The failure mode of the cast Be-Al-0.4Sc alloy still involved the brittle cleavage failure of Be regions and ductile dimple failure of Al regions, which was not the case with the cast Be-Al alloy.

36 MATERIALS SCIENCE↗

Tailoring Microstructure and Properties of a Superelastic Ti–Ta Alloy by Incorporating Spark Plasma Sintering with Thermomechanical Processing

A powder metallurgy Ti–35 at.% Ta alloy was produced using a spark plasma sintering process. The sintered alloy exhibited Ta-rich regions at a sintering temperature of 1100 °C. Complete diffusion of elemental powders was achieved via homogenization heat treatment at 1500 °C for 12 h, but the ductility declined drastically. The brittle behavior of the homogenized sample was due to the high-oxygen content, continuous grain boundary α-phase and high-angle grain boundaries. Excellent mechanical properties were achieved when hot forging was used along with preheating the homogenized specimen at 1100 °C. The mechanisms underlying this phenomenon were suppression of the solid grain boundary α-phase, high fraction of low-angle grain boundaries and dynamic recrystallization. Tensile strength improved to the maximum value of 868 MPa. The strain recovery ratio increased to 90% in the first cycle during a cyclic loading–unloading test. Incomplete strain recovery of the first cycle was due to the presence of the martensite phase (α″).

36 MATERIALS SCIENCE↗

Effect of Dual-Phase Heat Treatment on Microstructure and Mechanical Properties of S135 High-Strength Drill Pipe Steel

Effect of dual-phase heat treatment (DPHT) on microstructure and mechanical properties of S135 high-strength drill pipe steel was studied by means of optical microscope, scanning electron microscope and mechanical property testing. The results show that the ferrite–martensite dual-phase microstructures were obtained at 760-800 °C. With increase in DPHT temperature, the volume fraction of martensite increases and the ferrite decreases. When the DPHT temperature is low, martensite is distributed as an island on the ferrite matrix, and ferrite is distributed as an island on the martensite matrix when the DPHT temperature is high. The hardness and strength of the steel increase, the plasticity and toughness decrease, the steel changes from ductile fracture to brittle fracture and the micro-fracture morphology changes from dimple to cleavage with increase in DPHT temperature. The strain hardening exponent of the as-received steel shows one ‘n’ value, but exhibits two ‘n’ values after DPHT. When the DPHT temperature is 750 °C, the relative content of martensite in the duplex structure is 15-20%, and the impact energy of the steel is similar to that of the as-received S135 drill pipe steel, and the strength is increased by about 15%. Micropores and micro-cracks on the subsurface of tensile fracture surface are mainly formed at the martensite/ferrite phase boundary or in the martensite slit.

36 MATERIALS SCIENCE↗

Microstructure Characteristics and Comparative Analysis of Constitutive Models for Flow Stress Prediction of Inconel 718 Alloy

An accurate constitutive model is essential for analyzing deformation behavior of material and reliable numerical simulations in metal forming processes. In this study, hot tensile tests of Inconel 718 alloy have been conducted over a wide range of temperatures (300-973 K at an interval of 100 K), strains (0.01-0.3 at an interval of 0.01) and quasi-static strain rates (0.0001, 0.001, 0.01 s{sup −1}). Flow stress behavior is significantly affected by test temperatures and strain rates. Microstructure characteristics of deformed test specimens have been examined using scanning electron microscope and electron backscatter diffraction (EBSD). The fractography study revealed that fracture is mix-mode type, i.e., ductile and brittle. Subsequently, EBSD analysis shown that dynamic recrystallization mechanism is more pronounced at a higher temperature. Furthermore, four constitutive models, namely modified Cowper–Symonds, modified Johnson Cook, modified Zerillie-Armstrong and integrated Johnson Cook–Zerillie-Armstrong (JC-ZA) models have been investigated for flow stress prediction. Capability of models has been evaluated based on the correlation coefficient (R), average absolute error (Δ) and its standard deviation (δ). Accurate prediction of flow stress behavior is found by integrated JC-ZA model with R = 0.9873, Δ = 2.44 and δ = 4.08%.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of a SiO{sub 2} Ceramic and TC4 Alloy Joint Brazed with a Nanocomposite Filler

Vacuum brazing of TC4 alloy and SiO{sub 2} ceramic was achieved using a nano-AgCuNi braze alloy. The melting temperature of nano-AgCu powders was analyzed by differential scanning calorimeter. Furthermore, the effects of the Ni content on the microstructure and mechanical properties of the joints were studied. The results showed that the melting temperature of the nano-AgCu filler was 774 °C. A decrease in the melting temperature of 6 °C was observed, compared with the general AgCu filler, and this decrease enabled the interfacial reaction of the joint to begin earlier. The typical interfacial microstructure of the TC4/nano-AgCuNi/SiO{sub 2} ceramic joint brazed at 950 °C for 10 min was TC4/α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectoid structure/Ti{sub 2}(Cu,Ni) compound with α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure/Ti{sub 4}O{sub 7} + TiSi{sub 2}/SiO{sub 2} ceramics. The homogeneous microstructure of α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectoid structure primarily existed in the diffusion layer. Additionally, the refined α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure created via a eutectic reaction and Ti{sub 2}(Cu,Ni) compound was distributed in the brazing seam. The Ni content could influence the formation of Ti-Cu-Ni ternary intermetallic compounds (IMCs). An increase in Ni led to an increase in the α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure in the brazing seam. The shear strength of the brazed joints first increased and then decreased with the increase in the nano-Ni content, and the optimal shear strength of 30.1 MPa was achieved at 10 wt.% Ni. The increase in the α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure and the decrease in brittle compounds enhanced the shear strength of the joint. Fracture analysis of the joints brazed at 950 °C for 10 min indicated that the cracks mainly occurred in SiO{sub 2} ceramic.

36 MATERIALS SCIENCE↗

Effect of Welding Parameters on Junction Structure and Fracture Behavior of Friction-Stir-Welded Joints of 2024 Aluminum Alloys

In this paper, the effect of welding speed and tool rotation speed on the junction structure and fracture behavior of friction-stir-welded joints was investigated with use of 2024 aluminum alloys of 3.2 mm thick. Results show that the formation of junction structure is more affected by tool rotation speed than by welding speed due to the differences of heat input levels. When welding speed is at 100 mm/min and tool rotation speed is in the range of 400-600 r/min, the joint junction structure causes complete bonding with no welding defects. While under improper welding parameters, the junction structure causes the precipitate aggregation on the bonding line and the partial bonding with the appearance of both tunnel defects and kissing bond defects. Meanwhile, the results of tensile tests show that the tensile fracture of all FSW joints occur at the weld center. The failure mode of joints with defects-free junction structure characterized by shear fracture is ductile. While the failure mode of joints with defects-existent junction structure characterized by layered fracture surface is brittle. Furthermore, that heterogeneous microstructure, precipitate aggregation and welding defects converge inside the junction structure is the main factor affecting the tensile properties and fracture behavior of the friction-stir-welded joint.

36 MATERIALS SCIENCE↗

Effect of a Zinc Interlayer on a Cu/Al Lap Joint in Ultrasound-Assisted Friction Stir Welding

This study proposes a welding process, ultrasound-assisted friction stir welding of dissimilar Al/Cu metals. Zinc foil is melted using the heat generated by a pinless stirring tool, and the molten intermediate layer is stirred by ultrasonic cavitation to achieve an effective connection. The metallurgical reaction behavior of the joint under the action of the sound field was studied, and the effects of different microstructures on the joint performance were analyzed. Specifically, the following observations were reported in this study: (1) When ultrasound assistance was used, the cavitation effect changed the brittle intermetallic compounds of Al{sub 2}Cu from a continuous distribution to a block distribution, and the mechanical properties of the joint were greatly improved; (2) the effects of the thickness of the zinc were also determined. The results showed that the highest shear tensile force was obtained when the thickness of the zinc foil was 0.2 mm. When the thickness was 0.3 mm, the ultrasound effect was weakened. The copper-side interface generated a zigzag-shaped Al{sub 4.2}Cu{sub 3.2}Zn{sub 0.7} layer with a thickness of 3.4 μm and had a continuous distribution. Increasing the thickness of the zinc to 0.5 mm, however, drastically decreased the mechanical properties of the joint due to incomplete melting of the zinc layer.

36 MATERIALS SCIENCE↗

Crack Detection in High-Velocity Oxygen-Fuel-Sprayed Al{sub 59.2}Cu{sub 25.5}Fe{sub 12.3}B{sub 3} Quasicrystalline Coatings Using Piezoelectric Active Sensors

Quasicrystals have received some attention in recent years regarding their potential usefulness as low friction and wear resistant materials. When quasicrystalline (QC) coatings are exposed to different levels of external loading or are subjected to thermal stresses, crack nucleation, and propagation become life-limiting factors. In this investigation, Al{sub 59.2}Cu{sub 25.5}Fe{sub 12.3}B{sub 3} QC coatings were deposited onto AISI-A36 steel substrates using the high-velocity oxygen-fuel (HVOF) technique. The coatings were deposited at different oxygen-to-fuel ratios. To characterize the integrity of the coatings, the active piezoceramic excitation technique was applied to detect the propagation of cracks during three-point bending tests. The piezoelectric transducer signal was processed using wavelet transformation analysis. The results revealed that the coated samples displayed different densities of cracks depending on the oxygen-to-fuel. The crack density was found higher for coatings formed using a slightly oxidizing flame. The opening of the pre-existing cracks in the coating was the main reason of signal attenuation during piezoelectric excitation. The HVOF-sprayed AlCuFeB quasicrystalline coating, with thickness between 150 and 180 μm, withstands a flexural stress as high as 340 MPa. To the best of our knowledge, this study is the first that provides a quantitative assessment of the viability of QC coatings in mechanical applications in spite of their intrinsic brittleness.

36 MATERIALS SCIENCE↗

Characterization of Laser-Welded Ti Alloy and Stainless Steel Joint Using Cu Interlayer

In this study, Cu was used as an interlayer to restrain the formation of brittle Ti-Fe intermetallics when joining Ti alloy to SS. Microstructures of the joint were analyzed using optical microscopy, scanning electron microscopy and x-ray diffraction. Besides, the tensile strength of the joint was also measured. The melting amount of base materials was controlled by changing thickness of Cu interlayer to control the melting proportion in weld. The melting amount of base materials in weld decreased with the thickness of Cu interlayer. The content of Cu solid solution in weld increased with the thickness of Cu interlayer. Ti-Cu compound layer was formed on the Ti alloy side. The width of the Ti-Cu compound layer increased with the increase in heat input. The tensile strength of joint was largely impacted by Ti-Cu compound layer. The tensile strength of joint first increased and then decreased with the increase in width of the Ti-Cu compound layer.

36 MATERIALS SCIENCE↗

The Effect of Weld Metal Composition on Microstructural and Mechanical Properties of Dissimilar Welds Between Monel 400 and Inconel 600

The current work was carried out to characterize welding of Inconel 600 superalloy and Monel 400. In the present study, gas tungsten arc welding (GTAW) with four types of filler metals (ENiCu, ENiCu-7, ENiCr-3 and ENiCrFe-3) was utilized. The filler metals were categorized into two groups based on the presence of Cr and Nb in their chemical composition. This paper describes the selection and application of welding consumables in manufacturing dissimilar metal combinations. It was found that (Nb/Cr) ratio and Fe content can affect on the size and amount of carbides. During solidification of ENiCr-3 and ENiCrFe-3 filler metals, Nb leaves dendritic cores and is rejected to inter-dendritic regions because of its high tendency for segregation. However, No brittle Laves phase was detected in the welds. The interface between weld metal and base metal and gradual changes in alloying elements were also investigated by scanning electron microscopy. EDX analysis was also applied for different samples. Microhardness measurements and tensile test were performed on the joints. The average hardness value in the weld metal obtained from ENiCrFe-3 is higher than the other welds. ENiCu-7 weld exhibited the highest tensile strength of 540 MPa and percent elongation of 53% in contrast to ENiCrFe-3 weld with the lowest tensile strength (518 MPa) and percent elongation (39%).

36 MATERIALS SCIENCE↗

Fatigue Failure Characteristics of Single-Crystal Fe-3%Al Alloy

To obtain a better understanding of the mechanical properties and failure characteristics of the single-crystal Fe-3%Al alloy (SC), tensile and fatigue properties of the SC and polycrystalline Fe-3%Al alloy (PC) have been investigated. The tensile strength and fracture strain for the SC samples were different depending on the loading direction, i.e., 〈111〉, 〈110〉 and 〈100〉, which could be explained by the Schmid factor. Fatigue strength for the SC samples was basically correlated with their tensile strength. Different fatigue properties were obtained for the PC sample, e.g., the high fatigue strength was obtained in the early fatigue stage, and significant reduction in the fatigue strength was appeared in the later fatigue stage, e.g., low endurance limit at 10{sup 7} cycles. The reason for this was caused by the material brittleness due to the accumulated dislocation at the grain boundaries. Because the high ductile SC samples made severe plastic deformation ahead of the crack tip, the crack growth rate did not enhance even if the high stress intensity factor range was applied in Region II (da/dN versus ΔK). The crack growth rate dropped just before the final fracture. Effective stress intensity factor range was estimated using the crack closure model, but the crack growth rate is found to be affected strongly by the slip system of SC sample.

36 MATERIALS SCIENCE↗