Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “alloy solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 793 records · Page 44

Measurement and analysis of distribution coefficients in Fe-Ni alloys containing S and/or P. II - K(Ir), K(Ge), and K(Cu)

Crystals of Fe-Ni-S-P alloys containing Ir, Ge, and Cu in small amounts were grown by plane front solidification. The electron microprobe was used to measure the compositions of these alloys. The Ir, Ge, and Cu distribution coefficients were determined by an analytical procedure from the composition data. The distribution coefficients of Ir, Ge, and Cu vary from 1.20 to 11.0, 0.75 to 2.1, and 0.06 to 0.84, respectively. K(Ir) and K(Ge) increase and K(Cu) decreases with the S content of the liquid. K(Cu) increases and K(Ir) and K(Ge) decrease with the P content of the liquid. Mathematical expressions have been formulated to relate the Ir, Ge, and Cu distribution coefficients to the S and P contents of the liquid. These distribution coefficients are important to the study of the solidification behavior of iron meteorites.

Sellamuthu, R.↗

Effect of vanadium on phase composition and hard magnetic properties of as-solidified and heat-treated Sm–Fe–(Ti,V) alloys

Although the intrinsic magnetic properties of Ti-stabilized Sm(Fe,Co,Ti) 12 compounds exhibit potential of excellent rare-earth-lean permanent magnets, it has been much easier to realize large coercivities with the isostructural compounds stabilized by either V or by certain combinations of Ti and V. To elucidate the influence of V on the microstructure and magnetic properties, a series of Sm 8.1 Fe 78.4 (Ti 1-x V x ) 13.5 alloys was studied after arc-melting and annealing at 850–1000 °C. The alloys were found to fall into three groups. For x ≤ 0.2, solidification generates mostly the Sm(Fe,Ti,V) 12 phase, but annealing converts at least part of it into the non-magnetic Sm(Fe,Ti,V) 11 and the magnetically soft Sm 2 (Fe,Ti,V) 17 phases. For 0.2 < x < 0.6, the alloys solidify into a near-equilibrium mixture of the Sm(Fe,Ti,V) 12 , TiFe 2 and Sm-rich phases. For x ≥ 0.6, solidification generates large fractions of α-Fe solid solution and Sm-rich phases; an annealing step is necessary to complete the formation of Sm(Fe,Ti,V) 12 phase. Also, for x ≥ 0.6 the temperature below which the Sm(Fe,Ti,V) 12 phase is stable decreases with x, as does the fraction of this phase formed during solidification. Here, the differences between these three groups of alloys suggest different strategies for developing hard magnetic properties, with the likelihood of a success increasing with increasing x. For x ≥ 0.6, heat treatment alone is demonstrated to generate a microstructure of micron and submicron Sm(Fe,Ti 1-x V x ) 12 crystallites separated by a Sm-rich phase and exhibiting a coercivity with values up to 3.5 and 5.7 kOe for x = 0.8 and 1.0, respectively.

36 MATERIALS SCIENCE↗

Thermal-stress fatigue behavior of twenty-six superalloys

The comparative thermal-stress fatigue resistances of 26 nickeland cobalt-base alloys were determined by fluidized bed tests. Cycles to cracking differed by almost three orders of magnitude for these materials, with directional solidification and surface protection showing definite benefit. The alloy-coating combination with the highest thermal-stress fatigue resistance was directionally solidified NASA TAZ-8A with an RT-SP coating. Its oxidation resistance was also excellent, showing approximately a 1/2 percent weight loss after 14,000 fluidized bed cycles.

Bizon, P. T.↗

Research on metal solidification in zero-g state

The containerless solidification of several pure metals and metallic alloys was studied in a low gravity environment. The tests were performed in the MSFC 4.2 s drop tower using a rapid wire melting apparatus designed and built for this purpose. Pure iron and nickel, and alloys of iron-nickel, iron-carbon, nickel-aluminum and tungsten-rhenium were all melted and solidified at a gravity level of approximately 100.000/-4 g. Interpretation of the results has led to an appreciation of the factors controlling the successful execution of this drop test experiment and to a delineation of the limits of applicability of the apparatus. Preliminary metallurgical evaluations are presented of the overall shapes, lattice parameters, surface microstructure,, cross-sectional microstructures, solidification and transformation sequences, evaporative segregation, and localized solute redistribution observed in the low-gravity specimens. The effects of low gravity on metallic solidification are discussed with particular emphasis on observations of spontaneous undercooling and evaporative segregation in uncontained melts.

Papazian, J. M.↗

Ultra-soft magnetic properties and correlated phase analysis by {sup 57}Fe Mössbauer spectroscopy of Fe{sub 74}Cu{sub 0.8}Nb{sub 2.7}Si{sub 15.5}B{sub 7} alloy

A detailed study of magnetic softness has been performed on FINEMENT type of ribbons by investigating the BH loop with maximum applied field of 960 A/m. The ribbon with the composition of Fe{sub 74}Cu{sub 0.8}Nb{sub 2.7}Si{sub 15.5}B{sub 7} was synthesized by rapid solidification technique and the compositions volume fraction was controlled by changing the annealing condition. Detail phase analysis was performed through X-ray diffraction (XRD), Differential scanning calorimetry (DSC), Vibrating sample magnetometer (VSM) and Mössbauer spectroscopy in order to correlate the ultrasoft magnetic properties with the volume fraction of amorphous and α-Fe(Si) soft nano composites. Bright (BF) and dark field (DF) image with selective area diffraction (SAD) patterns by the transmission electron microscopy (TEM) of the sample annealed for the optimized annealed condition at 853 K for 3 min reveals nanocrystals with an average size between 10-15 nm possessing the bcc structure which matches with the grain size revealed by the X-ray diffraction. Kinetics of crystallization of α-Fe(Si) phases has been determined by DSC curves. Extremely small coercivity of 30.9 A/m and core loss of 2.5 W/Kg for the sample annealed at 853 K for 3 min was found. Similar values for other crystalline conditions were determined by using BH loop tracer with a maximum applied field of around 960 A/m. Mössbauer spectroscopy was used to determine chemical shift, hyperfine field distribution (HFD), and peak width of different phases. The volume fractions of the relative amount of amorphous and crystalline phases are also determined by Mössbauer spectroscopy. High saturation magnetization along with ultrasoft magnetic properties exhibits very high potentials technological applications.

36 MATERIALS SCIENCE↗

Strontium Effects on the Formation of Iron-Intermetallic Phases in Secondary Al–9Si–0.6Fe Alloys

The presence and morphology of Fe-containing intermetallic phases affect the mechanical properties of aluminum alloys, especially in secondary Al–Si-based cast alloys. Although strontium (Sr) addition of 50 to 500 ppm is known to refine the needle-type eutectic silicon structure, the influence of Sr on the formation of Fe-intermetallic phases remains unclear. The present work investigates the combined additions of Sr and Mn to Al–9Si–0.6Fe–0.35Mg (All compositions are in wt pct except otherwise stated.) alloys on the formation of Fe-intermetallic phases at different solidification rates from ~ 1.5 to ~ 60 °C/s. Long and branched-type AlFeSi phase with size ranging from 50 to 120 µm are more common when solidified at the rate of 1.5 °C/s regardless of Sr and Mn additions. However, at the fast solidification rate of 60 °C/s, a 60 ppm Sr addition significantly reduced the average length of needle-shaped AlFeSi phase to less than 3 to 5 µm. Thermodynamic simulations have been performed using CALculation of PHAse Diagrams (CALPHAD) models to predict the formation of various phases and their possible interactions during solidification. The results indicated that the combination of a high solidification rate and about 60 ppm of Sr is beneficial to refining the δ-Al 3 FeSi 2 phase in Al–Si–Mg alloys containing 0.6 pctFe. As a result, this unexpected finding of Fe-intermetallic refinement by low Sr addition (~60 ppm) provides an important guide in designing secondary alloys for sustainable casting applications.

36 MATERIALS SCIENCE↗

The effect of varying powder feedstock chemistry and printing atmosphere on the microstructure of additively manufactured nickel-based ODS alloys: Role on stabilization of cellular structures vs. oxide dispersion formation

Nickel-based alloys have a wide variety of structural applications due to their high corrosion resistance and mechanical strength which depend on solid solution strengthening, or the formation of oxides and/or intermetallic precipitation for their properties. In this study, the microstructure of six Ni–Cr–Y–Ti–Al powder batches designed for the production of oxide dispersion strengthened nickel were compared. These batches varied in chemistry and atomization technique used which included Gas Atomization Reactive Synthesis (GARS). The batches of powder were then consolidated via Additive Manufacturing (AM) Powder Bed Fusion using Laser Beam (PBF-LB) and characterized via transmission electron microscopy to elucidate the influence of powder feedstock (i.e. synthesis methodology and chemistry) on the PBF-LB microstructure. The study investigates (i) how the amount of yttrium and titanium additions in the powder feedstock and the addition of oxygen during the processing (through GARS) affect the microstructure of the powder itself and the AM printed microstructure, and (ii) how the control of oxygen addition in the printing atmosphere during the PBF-LB printing process itself is another important parameter for achieving the formation of the wanted oxide dispersion versus the stabilization of the cellular structure (often observed in AM processed alloys). Microstructural characterization of both powder particles and additively manufactured nickel alloys in this study provide important insights into the movement of yttrium within the material upon solidification, particularly along cell boundaries, and how yttrium behaves depending on alloy chemistry. When a threshold of yttrium content is reached within the system, yttrium consistently reacts to form an intermetallic along cell boundaries instead of forming oxide nanoparticles.

36 MATERIALS SCIENCE↗

Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing

Required microstructural attributes of an alloy vary with structural applications. The microstructural fine-tuning capability of laser-powder bed fusion (L-PBF) additive manufacturing (AM) enables application specific manufacture of the components. Such manufacture with L-PBF AM requires alloys that exhibit wide processing window and are amenable to multiple deformation mechanisms. However, high hot cracking susceptibility of Al alloys poses a barrier to such printability-performance synergy. In this work we show that an integration of, a) grain refinement through heterogeneous nucleation, and b) eutectic solidification, leads to crack-free parts at wide range of process parameters, microstructural heterogeneity, and hierarchy in the Al-Ni-Ti-Zr alloy. Such an integration targets hot cracking at multiple stages of solidification in L-PBF as opposed to the contemporary alloy design strategies that target hot-cracking at only specific stages of solidification. The Al-Ni-Ti-Zr alloy exhibits excellent printability and a high as-built tensile performance. Due to the wide processing window and amenability to multiple deformation mechanisms, the alloy microstructure and subsequently the performance, can be fine-tuned. Here, such strategy opens the gateway for application-specific manufacture of Al alloys with L-PBF AM and establishes a fundamental shift in current methodologies for design of these alloys for L-PBF AM.

36 MATERIALS SCIENCE↗

Analysis of segregation trends observed in iron meteorites using measured distribution coefficients

Fe-Ni alloys of meteoritic composition were solidified by a plane front solidification technique. Distribution coefficients of Ni, P, Ir, Ge, and Cu were determined from the composition data of the plane front solidified alloys. Equations that describe the distribution coefficients (P, Ni, Ir, Ge, and Cu) as a function of S and P content as well as S to P ratio were used to calculate solute partitioning between solid and liquid during the solidification of IIAB, IIIAB, and IVA parent bodies. The calculated P versus Ni, Ir versus Ni, Ge versus Ni, and Cu versus Ni trends are in good agreement with the observed meteorite data for each chemical group. It is concluded that each chemical group formed as a single molten pool in a parent body and that solute partitioning that occurred during solidification is responsible for the observed compositional trends within a single meteorite group.

Sellamuthu, R.↗

The Isothermal Dendritic Growth Experiment (IDGE): USMP-4 One-Year-Report

Dendrites describe the tree-like crystal morphology commonly assumed in many material systems--particularly in metals and alloys that freeze from supercooled or supersaturated melts. There remains a high level of engineering interest in dendritic solidification because of the role of dendrites in the determination of cast alloy microstructures. Microstructure plays a key role in determining the physical properties of cast or welded products. In addition, dendritic solidification provides an example of non-equilibrium physics and is one of the simplest non-trivial examples of dynamic pattern formation, where an amorphous melt, under simple starting conditions, evolves into a complex ramified microstructure. Although it is well-known that dendritic growth is controlled by the transport of latent heat from the moving solid-melt interface as the dendrite advances into a supercooled melt, an accurate, and predictive model has not been developed. Current theories consider: 1) the transfer of heat or solute from the solid-liquid interface into the melt, and 2) the interfacial crystal growth and growth selection physics for the interface. However, the effects of gravity-induced convection on the transfer of heat from the interface prevent either element from being adequately tested solely under terrestrial conditions. The Isothermal Dendritic Growth Experiment (IDGE) constituted a series of three NASA-supported microgravity experiments, all of which flew aboard the space shuttle, Columbia. This experimental space flight series was designed and operated to grow and record dendrite solidification in the absence of gravity-induced convective heat transfer, and thereby produce a wealth of benchmark-quality data for testing solidification scaling laws. The data collection from the on-orbit phase of the IDGE flight series is now complete. We are currently completing analyses and moving towards final data archiving.

Glicksman, M. E.↗

Producing Foils From Direct Cast Titanium Alloy Strip

This research was undertaken to demonstrate the feasibility of producing high-quality, thin-gage, titanium foil from direct cast titanium strip. Melt Overflow Rapid Solidification Technology (MORST) was used to cast several different titanium alloys into 500 microns thick strip, 10 cm wide and up to 3 m long. The strip was then either ground, hot pack rolled or cold rolled, as appropriate, into foil. Gamma titanium aluminide (TiAl) was cast and ground to approximately 100 microns thick foil and alpha-2 titanium aluminide (Ti3AI) was cast and hot pack rolled to approximately 70 microns thick foil. CP Ti, Ti6Al2Sn4Zr2Mo, and Ti22AI23Nb (Orthorhombic), were successfully cast and cold-rolled into good quality foil (less than 125 microns thick). The foils were generally fully dense with smooth surfaces, had fine, uniform microstructures, and demonstrated mechanical properties equivalent to conventionally produced titanium. By eliminating many manufacturing steps, this technology has the potential to produce thin gage, titanium foil with good engineering properties at significantly reduced cost relative to conventional ingot metallurgy processing.

Stuart, T. A.↗

Numerical Research on Magnetic Field, Temperature Field and Flow Field During Melting and Directionally Solidifying TiAl Alloys by Electromagnetic Cold Crucible

The electromagnetic cold crucible (EMCC) technique is an effective method to melt and directionally solidify reactive and high-temperature materials without contamination. The temperature field and fluid flow induced by the electromagnetic field are very important for melting and controlling the microstructure. In this article, a 3D EMCC model for calculating the magnetic field in the charges (TiAl alloys) using the T-Ω finite element method was established and verified. Magnetic fields in the charge under different electrical parameters, positions and dimensions of the charge were calculated and analyzed. The calculated results show that the magnetic field concentrates in the skin layer, and the magnetic flux density (B) increases with increasing of the frequency, charge diameter and current. The maximum B in the charge is affected by the position of the charge in EMCC (h{sub 1}) and the charge height (h{sub 2}), which emerges at the middle of coils (h{sub c}) when the relationship of h{sub c} < h{sub 1} + h{sub 2} < h{sub c} + δ is satisfied. Lower frequency and smaller charge diameter can improve the uniformity of the magnetic field in the charge. Consequently, the induced uniform electromagnetic stirring weakens the turbulence and improves temperature uniformity in the vicinity of the solid/liquid (S/L) interface, which is beneficial to forming a planar S/L interface during directional solidification. Based on the above conclusions, the TiAlNb alloy was successfully melted with lower power consumption and directionally solidified by the square EMCC.

36 MATERIALS SCIENCE↗

Effect of Solute Elements on Boron Segregation in Boron-Containing Steels

The addition of boron to steel alloys results in an increase in both hardenability and casting defects. The casting difficulties are predicted to stem from a metatectic reaction, δ + γ → L + γ, where a fully solidified material begins to locally remelt as the temperature decreases. Another possible source of casting defects is a boride-rich phase that is predicted to remain liquid at low temperatures. To experimentally determine which reaction is the likely source of the casting defects, the predicted reactions and the effect of solute elements on those reactions are investigated. Levitation zone melting is used to control segregation in a ternary Fe–C–B alloy and a commercial 22MnB5 alloy. Carbon segregation and a peritectic reaction result in a peritectic jump during directional solidification where the first directionally solidified (DS) zone undergoes δ-bcc solidification followed by a peritectic jump to steady state planar solidification of γ-fcc in the second DS zone. The presence of other solute elements in the zone melted 22MnB5 alloy lead to a breakdown in the planar solidification front before steady state solidification could be achieved in the second DS zone. With a cellular solid/liquid interface, boron-rich intercellular liquid formed low melting iron boro-carbide particles. The controlled solidification conditions in a levitation zone melter were unable to prevent ~0.003 wt% boron from segregating to high enough levels to form boride particles. Therefore, it is likely that during commercial casting, the formation of the low melting boride phase from interdendritic segregation is a key source of the casting issues.

36 MATERIALS SCIENCE↗

Nonlinear Convection in Mushy Layers

When alloys solidify in a gravitational field there are complex interactions between solidification and natural, buoyancy-driven convection that can alter the composition and impair the structure of the solid product. The particular focus of this project has been the compositional convection within mushy layers that occurs in situations where the lighter component of the alloy is rejected into the melt during solidification by cooling from below. The linear stability of such a situation was previously described and has been further elucidated in a number of published articles. Here we describe some recent developments in the study of nonlinear evolution of convection in mushy layers.

Worster, M. Grae↗

Effects of Undercooling and Cooling Rate on Peritectic Phase Crystallization Within Ni-Zr Alloy Melt

The liquid Ni-16.75 at. pct Zr peritectic alloy was substantially undercooled and containerlessly solidified by an electromagnetic levitator and a drop tube. The dependence of the peritectic solidification mode on undercooling was established based on the results of the solidified microstructures, crystal growth velocity, as well as X-ray diffraction patterns. Below a critical undercooling of 124 K, the primary Ni{sub 7}Zr{sub 2} phase preferentially nucleates and grows from the undercooled liquid, which is followed by a peritectic reaction of Ni{sub 7}Zr{sub 2}+L → Ni{sub 5}Zr. The corresponding microstructure is composed of the Ni{sub 7}Zr{sub 2} dendrites, peritectic Ni{sub 5}Zr phase, and inter-dendritic eutectic. Nevertheless, once the liquid undercooling exceeds the critical undercooling, the peritectic Ni{sub 5}Zr phase directly precipitates from this undercooled liquid. However, a negligible amount of residual Ni{sub 7}Zr{sub 2} phase still appears in the microstructure, indicating that nucleation and growth of the Ni{sub 7}Zr{sub 2} phase are not completely suppressed. The micromechanical property of the peritectic Ni{sub 5}Zr phase in terms of the Vickers microhardness is enhanced, which is ascribed to the transition of the peritectic solidification mode. To suppress the formation of the primary phase completely, this alloy was also containerlessly solidified in free fall experiments. Typical peritectic solidified microstructure forms in large droplets, while only the peritectic Ni{sub 5}Zr phase appears in smaller droplets, which gives an indication that the peritectic Ni{sub 5}Zr phase directly precipitates from the undercooled liquid by completely suppressing the growth of the primary Ni{sub 7}Zr{sub 2} phase and the peritectic reaction due to the combined effects of the large undercooling and high cooling rate.

36 MATERIALS SCIENCE↗

Report on FY 2020 Welding Parameters Optimization and the Fabrication of Qualified Alloy 709 Welds

Alloy 709 is an attractive candidate construction material for the Sodium Fast Reactor (SFR). As part of the Alloy 709 Intermediate Term Test Program, this work covers the development of the technical basis for weld fabrication and weld qualification of Alloy 709. The phase of research reported herein focused on the issue of weld solidification cracking recently experienced in both experimental heats and a commercial heat of Alloy 709 with relatively high phosphorous levels.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Substrate temperature effects on laser crystallized NiTi thin films

Amorphous sputter-deposited NiTi thin films were subjected to pulsed, melt-mediated laser crystallization techniques to engineer their microstructure. The effects of laser processing of preheated films are examined. Laser processing of films at an elevated substrate temperature has a significant effect on the rate with which solidification occurs. It is observed that the preheating temperature at which processing is carried out has significant implications for the resulting phase and microstructure, and therefore mechanical properties. Furthermore, the microstructural effects of varying incident laser energy density are examined via atomic force microscopy, scanning electron microscopy, and x-ray diffraction, and mechanical/shape memory properties are characterized via nanoindentation.

36 MATERIALS SCIENCE↗

Solid Phase Gradient Alloying Method via ShAPE

Alloying has been used to confer desirable properties to various metallic systems since the bronze age. For example, Ni, Mn, and Cr are alloyed into an Fe matrix to make steel, which has improved strength and corrosion resistance (as displayed in Fig. 1). In addition to the type of alloying elements, the amount of alloying elements added into a matrix is also very critical for a material’s mechanical property, physical property, machinability, and cost. Conventionally, new alloys are discovered by combining alloy precursors and elemental constituents into a mixture and melting them together. The solidified product or ingot represents a usually non-homogeneous combination of the chemistry with a microstructure dictated by the physics of solidification. It is time and energy intensive to optimize the alloying amounts via the casting process and hence, economically not conducive to rapid alloy discovery. In addition, the cast microstructure seen in the as-cast ingot is often not the ideal, nor even desired structure for optimized performance. Cast materials often need further processing such as homogenization, annealing, and deformation work put in through rolling, forging, extruding, etc. to have favorable microstructures and properties. A faster method to discover new alloy combinations and evaluate them in their worked or processed form is needed. Recently, Laser Engineered Net Shaping was applied to fabricate gradient compositional material for alloy designing. However, the mechanical properties of this gradient alloy were poor due to the existence of impurities, oxidation and cracks that are inherent in the melt-solidification process. Because of these limitations, we propose to use a solid-phase process (ShAPE) to create bulk materials (extrudates) that vary in composition from one end of the extruded solid to the other. Various manufacturing methods for alloy design including conventional casting method, laser based combinatorial method and current solid phase gradient alloying method are displayed and compared in Fig. 2. ShAPE machine and a schematic of ShAPE process are displayed in Fig. 3. Starting material is processed by a rotating and plunging die to form an extrudate. We are proposing through this methodology to invent a new, bulk-scale combinatorial technique. With this novel technique, alloying element can be dissolved into the matrix with a continued gradient without bulk melting. Formation of inter-metallics and defects originating from melt processing can be avoided. In addition, the ShAPE process creates the mixed alloy chemistry, and meanwhile subjects the material to severe plastic strain, which induces the favorable “worked” microstructure. Products from the ShAPE process can be tested in hardness directly providing a path to rapid evaluation of mechanical properties. The ability to create graded structures using friction stir processing (FSP) has been demonstrated, however using the ShAPE process we believe will lead to much faster and higher fidelity results. When combined with high throughput screening methods of physical, mechanical and microstructural property characterization, efficiency and accuracy of alloy design can be significantly improved.

36 MATERIALS SCIENCE↗