Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Tensile testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 793 records · Page 44

Joint Test Report For Validation of Alternatives to Aliphatic Isocyanate Polyurethanes

National Aeronautics and Space Administration (NASA) and Air Force Space Command (AFSPC) have similar missions and therefore similar facilities and structures in similar environments. The standard practice for protecting metallic substrates in atmospheric environments is the application of an applied coating system. The most common topcoats used in coating systems are polyurethanes that contain isocyanates. Isocyanates are classified as potential human carcinogens and are known to cause cancer in animals. The primary objective of this effort was to demonstrate and validate alternatives to aliphatic isocyanate polyurethanes resulting in one or more isocyanate-free coatings qualified for use at AFSPC and NASA installations participating in this project. This joint Test Report (JTR) documents the results of the laboratory and field testing as well as any test modifications made during the execution of the testing. The technical stakeholders agreed upon test procedure modifications documented in this document. This JTR is made available as a reference for future pollution prevention endeavors by other NASA centers, the Department of Defense and commercial users to minimize duplication of effort. All coating system candidates were tested using approved NASA and AFSPC standard coating systems as experimental controls. This study looked at eight alternative coating systems and two control coating systems and was divided into Phase I Screening Tests, Phase II Tests, and Field Testing. The Phase I Screening Tests were preliminary tests performed on all the selected candidate coating systems. Candidate coating systems that did not meet the acceptance criteria of the screening tests were eliminated from further testing. Phase I Screening Tests included: Ease of Application, Surface Appearance, Dry-To-Touch (Sanding), Accelerated Storage Stability, Pot Life (Viscosity), Cure Time (Solvent Rubs), Cleanability, Knife Test, Tensile (pull-off) Adhesion, and X-Cut Adhesion by Wet Tape After a review of the Phase I test results, four of the alternative coating systems showed substandard performance in relation to the Control Systems and were eliminated from the Phase II testing. Due to the interest of stakeholders and time constraints, however, all eight alternatives were subjected to the following Phase II tests, along with field testing at Stennis Space Center (SSC), Mississippi: Hypergol Compatibility, Liquid Oxygen Compatibility, 18-Month Marine Exposure (Gloss Retention, Color Retention, Blistering, Visual Corrosion, Creepage from Scribe, Heat Adhesion), and Field Exposure (6- and 12-month Evaluation for Coating Condition, Color Retention, Gloss Retention). The remaining four alternative coating systems determined to be the best viable alternatives were carried on to Phase II testing that included: Removability, Repairability, Abrasion Resistance, Gravelometer, Fungus Resistance, Accelerated Weathering, Mandrel Bend Flexibility, and Cyclic Corrosion Resistance. Of the systems that continued to Phase II, three (3) alternative coating systems meet the performance requirements as identified by stakeholders. Two (2) other systems, that were not included in Phase II testing, performed well enough on the 18-Month Marine Exposure, the primary requirement for NASA technical standard NASA-STD-5008, Protective Coating of Carbon Steel, Stainless Steel, and Aluminum on Launch Structures, Facilities, and Ground Support Equipment, that they were also considered to be successful candidates. In total, five (5) alternative coating systems were approved for inclusion in the NASA-STD- 5008 Qualified Products List (QPL). The standard is intended to provide a common framework for consistent practices across NASA and is often used by other entities. The standard's QPL does not connote endorsement of the products by NASA, but lists those products that have been tested and meet the requirements as specified.

Lewis, Pattie↗

Development of a Composite Material Aerodynamic Demise Model for the Object Reentry Survival Analysis Tool (ORSAT)

The reentry demise of fiber-reinforced polymer (FRP) composites is an increasing concern for modern spacecraft at end of life. Unlike traditional materials such as metals, shredding of the material by aerodynamic forces appears to be a major component of the reentry demise mechanism. This paper will describe a new mechanical, strength-based, material demise model for the Object Reentry Survival Analysis Tool (ORSAT) Version 7.1. The model is based on laboratory in-situ and residual strength tests of several FRP materials performed during the NASA Orbital Debris Program Office’s Phase II Composite Material Demise test campaign. To test the residual strength of partially charred FRP materials, the authors tested 107 rectangular shaped samples of different thicknesses that were previously exposed to high-enthalpy flow at the University of Texas at Austin’s Inductively Coupled Plasma Torch facility. Tests were performed under normal atmospheric conditions at NASA Johnson Space Center’s Experimental Impact Laboratory using a Chatillon TCD1000 tensile test machine configured with a three-point bending jig. Mean fracture load, residual strength, delamination, and flexural modulus were measured for each test. An engineering model of aeromechanical demise for each material was developed by correlating the measured residual strength of the samples with the duration and magnitude of the applied heat flux and the mass loss and char progression. This model has been implemented in ORSAT 7.1 for the built-in, charring carbon fiber/epoxy and charring glass fiber/epoxy material models. The new model was verified by calculating the demise of hundreds of FRP composite fragments of various shapes and sizes and checking the calculations for consistency, with specific focus on material characterization in one-dimension. Further tests are planned in hypersonic flow facilities to validate the assumptions used in the model.

Priscilla A. Mendoza↗

Development of a Composite Material Aerodynamic Demise Model for the Object Reentry Survival Analysis Tool (ORSAT)

The reentry demise of fiber-reinforced polymer (FRP) composites is an increasing concern for modern spacecraft at end of life. Unlike traditional materials such as metals, shredding of the material by aerodynamic forces appears to be a major component of the reentry demise mechanism. This paper will describe a new mechanical, strength-based, material demise model for the Object Reentry Survival Analysis Tool (ORSAT) Version 7.1. The model is based on laboratory in-situ and residual strength tests of several FRP materials performed during the NASA Orbital Debris Program Office’s Phase II Composite Material Demise test campaign. To test the residual strength of partially charred FRP materials, the authors tested 107 rectangular shaped samples of different thicknesses that were previously exposed to high-enthalpy flow at the University of Texas at Austin’s Inductively Coupled Plasma Torch facility. Tests were performed under normal atmospheric conditions at NASA Johnson Space Center’s Experimental Impact Laboratory using a Chatillon TCD1000 tensile test machine configured with a three-point bending jig. Mean fracture load, residual strength, delamination, and flexural modulus were measured for each test. An engineering model of aeromechanical demise for each material was developed by correlating the measured residual strength of the samples with the duration and magnitude of the applied heat flux and the mass loss and char progression. This model has been implemented in ORSAT 7.1 for the built-in, charring carbon fiber/epoxy and charring glass fiber/epoxy material models. The new model was verified by calculating the demise of hundreds of FRP composite fragments of various shapes and sizes and checking the calculations for consistency, with specific focus on material characterization in one-dimension. Further tests are planned in hypersonic flow facilities to validate the assumptions used in the model.

Priscilla A. Mendoza↗

Friction stir welding joint of dissimilar materials between AZ31B magnesium and 6061 aluminum alloys: Microstructure studies and mechanical characterizations

Friction stir welding is an efficient manufacturing method for joining dissimilar alloys, which can dramatically reduce grain sizes and offer high mechanical joint efficiency. Lap FSW joints between dissimilar AZ31B and Al 6061 alloy sheets were made at various tool rotation and travel speeds. Rotation and travel speeds varied between 560–1400 r/min and 16–40 mm/min respectively, where the ratio between these parameters was such that nearly constant pitch distances were applied during welding. X-ray diffraction pattern (XRD), optical microscopy images (OM), electron probe microanalysis (EPMA) and scanning electron microscopy equipped with an energy-dispersive X-ray spectroscopy (SEM-EDS) were used to investigate the microstructures of the joints welded. Intermetallic phases including Al{sub 12}Mg{sub 17} (γ) and Al{sub 3}Mg{sub 2} (β) were detected in the weld zone (WZ). For different tool rotation speeds, the morphology of the microstructure in the stir zone changed significantly with travel speed. Lap shear tensile test results indicated that by simultaneously increasing the tool rotation and travel speeds to 1400 r/min and 40 mm/min, the joint tensile strength and ductility reached a maximum. Microhardness measurements and tensile stress–strain curves indicated that mechanical properties were affected by FSW parameters and mainly depended on the formation of intermetallic compounds in the weld zone. In addition, a debonding failure mode in the Al/Mg dissimilar weld nugget was investigated by SEM and surface fracture studies indicated that the presence of intermetallic compounds in the weld zone controlled the failure mode. XRD analysis of the fracture surface indicated the presence of brittle intermetallic compounds including Al{sub 12}Mg{sub 17} (γ) and Al{sub 3}Mg{sub 2} (β). - Highlights: • Dissimilar Al/Mg joint was obtained by lap friction stir welding technique. • Effect of rotation and travel speeds on the formation of intermetallic compounds • Microstructure and chemical studies including metallography, XRD, SEM-EDS, and EPMA • Mechanical property tests such as stress–strain curves, failure load and hardness • IMCs as Al{sub 3}Mg{sub 2} and Al{sub 12}Mg{sub 17} were identified in weld nugget and at Al/Mg interface.

36 MATERIALS SCIENCE↗

Effect of Anisotropy on Microstructures and Mechanical Properties of Rolled Ti/Al/Mg/Al/Ti Laminates

TA2/5052Al/AZ31/5052Al/TA2 five-ply laminates were fabricated by hot rolling, and the effect of anisotropy on their microstructures and mechanical properties was studied. After rolling, the Mg/Al and Al/Ti interfaces were both closely connected, but the interfacial shapes were totally different. For the Mg layer microstructures in the middle area, regardless of the direction, dynamic recrystallized (DRXed) grains appeared around the deformation bands. However, twins and a shear zone appeared in the RD sample; the twins decreased in the sample along the 45° angle, and no twins appeared in the TD sample. The Ti layer showed equiaxed grains in different directions, which were attributed to the ability of Ti alloy to anti-deform. The tensile testing results showed that the fracture of the Ti/Al/Mg/Al/Ti laminates can be divided into four stages. The laminate had an ultimate tensile strength of 434 MPa and excellent elongation along the rolling direction (RD), which were attributed to its DRXed grains and twins. In conclusion, the laminates had significant anisotropy due to the presence of Mg alloys.

36 MATERIALS SCIENCE↗

Effects of processing defects on the dynamic tensile mechanical behavior of laser-solid-formed Ti-6Al-4 V

Highlights: • Tensile tests are conducted under coupled effects of strain rate and temperature. • Defects act as crack initiation and propagation sites for dynamic tensile fracture. • Dynamic tension-compression asymmetry is due to different behaviors of defects. • Different deformation of defects results in tensile mechanical anisotropy. • Mechanical anisotropy and asymmetry are sensitive to strain rate and temperature. - Abstract: The initial processing defects, i.e. voids, lack-of-fusion pores and inclusions, are the inevitable and unique microstructural features in the Ti-6Al-4 V (Ti64) alloy manufactured by laser solid forming (LSF). This study was to gain insight into the influences of these processing defects on the tensile thermomechanical response of the material under various strain rates of 0.001/s, 500/s, 1000/s and 3000/s, and under a wide range of temperatures from 298 K to 1273 K. The drastic effects of processing defects on the flow stress were founded to be susceptible to tensile loading and increase with the increasing strain rate. The SEM analysis was carried out to further understand the effect of initial processing defects on the dynamic fracture behavior. These processing defects, such as voids and lack-of-fusion pores, are the most vulnerable position to release impact energy instantaneously and then evolve into the initiation site and propagation path for dynamic tensile crack. The tensile crack under high strain rate and high temperature propagates through the columnar prior-β grain boundary α colony. It was analyzed that the typical tension-compression asymmetry in strength is positively associated with the strain rate in the Ti64 alloy by LSF. Such asymmetry is due to the differences in the deformation mechanism of processing defects and in the activated slip system under tensile and compressive loading. Additionally, the anisotropy of the mechanical property was discussed by examining the positive strain rate effects in two orientations (i.e., perpendicular and parallel to the crystal growth direction). This anisotropy is caused by different mechanical behaviors of lack-of-fusion defects and β grain boundary α colony in different orientations.

36 MATERIALS SCIENCE↗

The comparison of microstructures and mechanical properties between 14Cr-Al and 14Cr-Ti ferritic ODS alloys

In this study, two kinds of 14Cr ODS alloys (14Cr-Al and 14Cr-Ti) were investigated to reveal the different effects between Al and Ti on the microstructures and mechanical properties of 14Cr ferritic ODS alloys. The microstructure information such as grains, minor phases of these two alloys has been investigated by high-energy X-ray diffraction and transmission electron microscopy (TEM). The in situ synchrotron X-ray diffraction tensile test was applied to investigate the mechanical properties of these two alloys. The lattice strains of different phases through the entire tensile deformation process in these two alloys were analyzed to calculate their elastic stresses. From the comparison of elastic stress, the strengthening capability of Y 2 Ti 2 O 7 is better than TiN in 14Cr-Ti, and the strengthening capability of YAH is much better than YAM and AlN in 14Cr-Al ODS. The dislocation densities of 14Cr-Ti and 14Cr-Al ODS alloys during tensile deformation were also examined by modified Williamson-Hall analyses of peak broadening, respectively. In conclusion, the different increasing speed of dislocation density with plastic deformation reveals the better strengthening effect of Y-Ti-O particles in 14Cr-Ti ODS than that of Y-Al-O particles in 14Cr-Al ODS alloy.

36 MATERIALS SCIENCE↗

Cryogenic mechanical behaviors of CrMnFeCoNi high-entropy alloy

The CrMnFeCoNi high-entropy alloy (HEA) exhibits higher yield strength, ultimate strength and ductility at lower temperature. To further clarify the effect of the testing temperature on microstructure evolution, in this study in-situ synchrotron-based high-energy X-ray diffraction tensile tests were carried out from 298 K down to 123 K. The enhanced yield strength of the alloy at cryogenic temperatures can be attributed to the greater lattice distortion prior to plastic deformation. Higher strain hardening rate leads to the simultaneously enhanced strength and ductility of the studied HEA below room temperature. Both dynamic Hall-Petch hardening (twinning) and dislocation hardening provide high work hardening capacity for this alloy during the plastic deformation at cryogenic temperatures. The increased dislocation density and nano-twins at cryogenic temperatures can be attributed to the decrease in the stacking fault energy as the deformation temperature decreases. These studies could provide an in-depth understanding for the strengthening mechanisms of the HEA in different temperature conditions and guide the exploration of HEAs with superb mechanical properties at cryogenic environments.

36 MATERIALS SCIENCE↗

The Lateral Stability of Equal-flanged Aluminum-alloy I-beams Subjected to Pure Bending

Equal-flange beams of a special extruded I-section of 27ST aluminum alloy were tested in pure bending. Complete end fixity was not attained. Loading was continued until a definite maximum value had been reached. Tensile tests were made on specimens cut from the flanges and the web of each beam. Compressive stress-strain characteristics were determined by pack compression tests on specimens cut from the flanges. Values computed from an equation previously suggested by one of the authors for the critical stress at which such beams become unstable were found to be in good agreement with values computed from experimentally determined critically bending moments.

Dumont, C↗

Use of Acoustic Emission to Monitor Progressive Damage Accumulation in Kevlar (R) 49 Composites

Acoustic emission (AE) data acquired during intermittent load hold tensile testing of epoxy impregnated Kevlar(Registeres TradeMark) 49 (K/Ep) composite strands were analyzed to monitor progressive damage during the approach to tensile failure. Insight into the progressive damage of K/Ep strands was gained by monitoring AE event rate and energy. Source location based on energy attenuation and arrival time data was used to discern between significant AE attributable to microstructural damage and spurious AE attributable to noise. One of the significant findings was the observation of increasing violation of the Kaiser effect (Felicity ratio < 1.0) with damage accumulation. The efficacy of three different intermittent load hold stress schedules that allowed the Felicity ratio to be determined analytically is discussed.

Waller, Jess M.↗

Determination of Parachute Joint Factors using Seam and Joint Testing

This paper details the methodology for determining the joint factor for all parachute components. This method has been successfully implemented on the Capsule Parachute Assembly System (CPAS) for the NASA Orion crew module for use in determining the margin of safety for each component under peak loads. Also discussed are concepts behind the joint factor and what drives the loss of material strength at joints. The joint factor is defined as a "loss in joint strength...relative to the basic material strength" that occurs when "textiles are connected to each other or to metals." During the CPAS engineering development phase, a conservative joint factor of 0.80 was assumed for each parachute component. In order to refine this factor and eliminate excess conservatism, a seam and joint testing program was implemented as part of the structural validation. This method split each of the parachute structural joints into discrete tensile tests designed to duplicate the loading of each joint. Breaking strength data collected from destructive pull testing was then used to calculate the joint factor in the form of an efficiency. Joint efficiency is the percentage of the base material strength that remains after degradation due to sewing or interaction with other components; it is used interchangeably with joint factor in this paper. Parachute materials vary in type-mainly cord, tape, webbing, and cloth -which require different test fixtures and joint sample construction methods. This paper defines guidelines for designing and testing samples based on materials and test goals. Using the test methodology and analysis approach detailed in this paper, the minimum joint factor for each parachute component can be formulated. The joint factors can then be used to calculate the design factor and margin of safety for that component, a critical part of the design verification process.

Mollmann, Catherine↗

Characterizing Transformation Phenomena and Elastic Moduli of Austenite and Oriented Martensite of Superelastic Thin NiTi Wire through Isothermal Dynamic Mechanical Analysis

In this paper, superelastic behavior of nickel-titanium thin wires is characterized using the method of dynamic mechanical analysis. Nominal dynamic storage modulus E{sup ′} is measured as function of nominal strain and stress during isothermal superelastic tensile tests at three testing temperatures above the reverse martensitic transformation finish temperature. The method brings new information on deformation mechanisms compared to the consideration of only tensile stress–strain curves. It is shown that determination of the elastic moduli E, especially at high strain, requires to calculate the true storage modulus E{sub t}{sup ′}. Using E{sub t}{sup ′} and not E{sup ′}, elastic modulus of oriented martensite E{sub M} is determined equal to 73 GPa of the same order than the elastic modulus of austenite E{sub A} equal to 70 GPa. Two models are then proposed to simulate experimental storage moduli evolution during the tests. A first model explains the E{sup ′} evolution during stress plateau by the localization phenomenon; it leads to express E{sup ′} as function of the nominal strain. A second model describes the evolution of E{sub t}{sup ′} after the stress plateau as function of true stress and test temperature. This model permits to determine the Clausius–Clapeyron coefficient of the forward transformation.

36 MATERIALS SCIENCE↗

Low-Temperature Thermally-Activated Deformation and Irradiation Softening in Neutron-irradiated Molybdenum

The effect of neutron irradiation on low-temperature deformation of Mo in two heat treatments, i.e. annealed and stress-relieved, was investigated. Specimens were irradiated at reactor coolant temperature ({approx}80 C) to doses ranging from 7.2 x 10{sup -5} to 0.28 dpa in the High Flux Isotope Reactor. Tensile tests were carried out between -50 and 100 C at strain rates of 1 x 10{sup -5}-1 x 10{sup -2} s{sup -1}. Thermal activation analysis based on tensile data was performed to understand the low-temperature deformation mechanism. Irradiation softening and reduced dependence on test temperature and strain rate of the yield stress was observed in the annealed Mo after low-dose neutron irradiation (<{approx}0.003 dpa). Higher dose neutron irradiation caused a thermal hardening only. The stress-relieved Mo showed a weaker dependence on test temperature and strain rate of the yield stress than the annealed Mo, and the dependence of the yield stress of the stress-relieved Mo was nearly unchanged after irradiation. Comparison of the experimental values of activation parameters with the theoretical predictions of dislocation models indicates that the Fleischer model of interactions of dislocations with tetragonal strains gave a better description of the activation process than the double-kink model, which implies a scavenging effect. The reduced test temperature and strain rate dependence following irradiation may be explained by the decreased effective stress due to trapping of interstitial solute species by neutron-produced defects.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Modeling and characterization of through-the-thickness properties of 3D woven composites

The through-the-thickness properties of three-dimensionally (3D) woven carbon/epoxy composites have been studied. The investigation aimed at the evaluation and development of test methodologies for the property characterization in the thickness direction, and the establishment of fiber architectures were studied: layer-to-layer Angle Interlock, through-the-thickness Orthogonal woven preform with surface pile was also designed and manufactured for the fabrication of tensile test coupons with integrated grips. All the preforms were infiltrated by the resin transfer molding technique. The microstructures of the composites were characterized along the warp and fill (weft) directions to determine the degree of yarn undulations, yarn cross-sectional shapes, and microstructural dimensions. These parameters were correlated to the fiber architecture. Specimens were designed and tested for the direct measurement of the through-the-thickness tensile, compressive and shear properties of the composites. Design optimization was conducted through the analysis of the stress fields within the specimen coupled with experimental verification. The experimentally-derived elastic properties in the thickness direction compared well with analytical predictions obtained from a volume averaging model.

Hartranft, Dru↗

Electric field enhanced diffusion welding of alloy 617: Microstructural characteristics and mechanical properties

This study investigated the microstructural characteristics and mechanical behavior of diffusion welded nickel-based Alloy 617 obtained by electric field-assisted sintering (EFAS) using various parameters. The interfacial microstructure exhibited different characteristics including good grain boundary (GB) migration across the interface in the samples diffusion-welded at 1100 °C and a flat interface in the samples joined at 1000 °C and 1050 °C. The interface consisted of fine Al 2 O 3 oxides, while precipitation of interfacial M 23 C 6 carbides was not observed. Grain boundaries migrated across the Al 2 O 3 oxides, leaving these oxides within the grains. Graded grain size was observed, with grain coarsening being more significant near the sample surface due to the temperature gradient induced by EFAS. Tensile testing revealed that the specimens fractured in the matrix away from the interface, indicting strong diffusion-welded joints. Further, the peak tensile strength of 807 MPa was obtained in the samples welded at 1000 °C due to minimal grain growth. The materials obtained at 1100 °C exhibited reduced tensile strength but improved ductility. Strain maps revealed by digital image correlation showed alternating high and low strain segments in the samples produced at 1000 °C and 1050 °C, indicating that the flat interfaces with no GB migration were less ductile compared to the matrix. A greater strain uniformity was observed along the bond interfaces with improved GB migration. The hardness reduced near the sample surfaces due to enlarged grains induced by temperature gradient. This study demonstrates that GB migration and enhanced mechanical strength can be achieved in diffusion-welded Alloy 617.

36 MATERIALS SCIENCE↗

Microstructure and thermomechanical properties relationship of segmented thermoplastic polyurethane (TPU)

Thermoplastic polyurethanes (TPU) are important polymeric materials for seals. In competition with Acrylonitrile butadiene rubbers (NBR), TPU exhibits higher strength and a considerable better abrasion resistance. The advantage of NBR over TPU is a smaller compression set but however TPU excels in its much shorter processing cycle times. Generally a TPU is a block copolymer composed of hard and soft segments, which plays an important role in determining the material properties. TPU can be processed either to ready moulded parts or can be incorporated by multi component moulding, in both cases it shows decent mechanical properties. In the present work, the relationship between melt-process induced TPU morphology and resultant thermo mechanical properties were examined and determined by means of quasi-static tensile test, creep experiment, tension test and dynamical mechanical analysis (DMA). Scanning electron beam microscope (SEM) and differential scanning calorimeter (DSC) were used to study the morphology of the samples. A significant mathematical description of the stress-strain behaviour of TPU was found using a 3 term approach. Moreover it became evident that processing conditions such as processing temperature have crucial influence on morphology as well as short and long-term performance. To be more precise, samples processed at higher temperatures showed a lack of large hard segment agglomerates, a smaller strength for strains up to 250% and higher creep compliance.

36 MATERIALS SCIENCE↗

Investigation of the adhesive bonding technology for the insulator structure of EAST neutral beam injector

A key issue on the development of EAST ion source was the junction design of insulator structure, which consists of three insulators and four supporting flanges of electrode grid. Because the ion source is installed on the vertical plane, the insulator structure has to withstand large bending and shear stress due to the gravity of whole ion source. Through a mechanical analysis, it was calculated that the maximum bending normal stress was 0.34 MPa and shear stress was 0.23 MPa on the insulator structure. Due to the advantages of simplicity and high strength, the adhesive bonding technology was applied to the junction of insulator structure. A tensile testing campaign of different junction designs between insulator and supporting flange was performed, and a junction design of stainless steel and fiber enhanced epoxy resin with epoxy adhesive was determined. The insulator structure based on the determined design can satisfy both the requirements of high-voltage holding and mechanical strength.

42 ENGINEERING↗

An experimental investigation on the mechanical properties of the interface between large-sized graphene and a flexible substrate

In this paper, the interfacial mechanical properties of large-sized monolayer graphene attached to a flexible polyethylene terephthalate (PET) substrate are investigated. Using a micro-tensile test and Raman spectroscopy, in situ measurements are taken to obtain the full-field deformation of graphene subjected to a uniaxial tensile loading and unloading cycle. The results of the full-field deformation are subsequently used to identify the status of the interface between the graphene and the substrate as one of perfect adhesion, one showing slide or partial debonding, and one that is fully debonded. The interfacial stress/strain transfer and the evolution of the interface from one status to another during the loading and unloading processes are discussed and the mechanical parameters, such as interfacial strength and interfacial shear strength, are obtained quantitatively demonstrating a relatively weak interface between large-sized graphene and PET.

36 MATERIALS SCIENCE↗